Volumn 301, Issue 1-2, 2013, Pages 626-635

Sliding wear mechanisms of magnesium composites AM60 reinforced with Al2O3 fibres under ultra-mild wear conditions

Author keywords

Fibre fracture; Mg alloy (AM60); Sliding wear; Squeeze casting

Indexed keywords

AUTOMOTIVE ENGINE BLOCK; BOUNDARY LUBRICATED SLIDING CONTACT; DISLOCATION DENSITIES; FRACTURE AND FRAGMENTATIONS; MAGNESIUM COMPOSITE; MG ALLOY; MICROMECHANICAL MODEL; SLIDING WEAR;

EID: 84879146598     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.wear.2013.01.091     Document Type: Article
Times cited : (43)

References (30)
  • 1
    • 0001610497 scopus 로고    scopus 로고
    • Squeeze casting of magnesium alloys and their composites
    • Hu H. Squeeze casting of magnesium alloys and their composites. Journal of Materials Science 1998, 33:1579-1589.
    • (1998) Journal of Materials Science , vol.33 , pp. 1579-1589
    • Hu, H.1
  • 2
    • 0041627777 scopus 로고    scopus 로고
    • Wear behaviour of SiCp-reinforced magnesium matrix composites
    • Lim C.Y.H., Lim S.C., Gupta M. Wear behaviour of SiCp-reinforced magnesium matrix composites. Wear 2003, 255:629-637.
    • (2003) Wear , vol.255 , pp. 629-637
    • Lim, C.Y.H.1    Lim, S.C.2    Gupta, M.3
  • 3
    • 0027610883 scopus 로고
    • On the wear of aluminium and magnesium metal matrix composites
    • Alahelisten A., Bergman F., Olsson M., Hogmark S. On the wear of aluminium and magnesium metal matrix composites. Wear 1993, 165:221-226.
    • (1993) Wear , vol.165 , pp. 221-226
    • Alahelisten, A.1    Bergman, F.2    Olsson, M.3    Hogmark, S.4
  • 4
    • 0034324958 scopus 로고    scopus 로고
    • Sliding wear map for the magnesium alloy Mg-9Al-0.9 Zn (AZ91)
    • Chen H., Alpas A.T. Sliding wear map for the magnesium alloy Mg-9Al-0.9 Zn (AZ91). Wear 2000, 246:106-116.
    • (2000) Wear , vol.246 , pp. 106-116
    • Chen, H.1    Alpas, A.T.2
  • 5
    • 0033948702 scopus 로고    scopus 로고
    • Evaluation of sliding wear behaviour of feldspar particle-reinforced magnesium alloy composites
    • Sharma S.C., Anand B., Krishna M. Evaluation of sliding wear behaviour of feldspar particle-reinforced magnesium alloy composites. Wear 2000, 241:33-40.
    • (2000) Wear , vol.241 , pp. 33-40
    • Sharma, S.C.1    Anand, B.2    Krishna, M.3
  • 6
    • 79953652601 scopus 로고    scopus 로고
    • Dry sliding wear behavior of Saffil fiber-reinforced Mg-10Gd-3Y-0.5Zr magnesium alloy-based composites
    • Hu B., Peng L., Ding W. Dry sliding wear behavior of Saffil fiber-reinforced Mg-10Gd-3Y-0.5Zr magnesium alloy-based composites. Journal of Composite Materials 2011, 45:683-693.
    • (2011) Journal of Composite Materials , vol.45 , pp. 683-693
    • Hu, B.1    Peng, L.2    Ding, W.3
  • 7
    • 0021645421 scopus 로고
    • A review of scuffing and running-in of lubricated surfaces, with asperities and oxides in perspective
    • Ludema K.C. A review of scuffing and running-in of lubricated surfaces, with asperities and oxides in perspective. Wear 1984, 100:315-331.
    • (1984) Wear , vol.100 , pp. 315-331
    • Ludema, K.C.1
  • 8
    • 65249084133 scopus 로고    scopus 로고
    • Microstructural evolution of a eutectic Al-Si engine subjected to severe running conditions
    • Slattery B.E., Perry T., Edrisy A. Microstructural evolution of a eutectic Al-Si engine subjected to severe running conditions. Materials Science and Engineering A 2009, 512:76-81.
    • (2009) Materials Science and Engineering A , vol.512 , pp. 76-81
    • Slattery, B.E.1    Perry, T.2    Edrisy, A.3
  • 9
    • 54249132014 scopus 로고    scopus 로고
    • Micromechanisms and mechanics of ultra-mild wear in Al-Si alloys
    • Chen M., Meng-Burany X., Perry T.A., Alpas A.T. Micromechanisms and mechanics of ultra-mild wear in Al-Si alloys. Acta Materialia 2008, 56:5605-5616.
    • (2008) Acta Materialia , vol.56 , pp. 5605-5616
    • Chen, M.1    Meng-Burany, X.2    Perry, T.A.3    Alpas, A.T.4
  • 10
    • 0038756367 scopus 로고    scopus 로고
    • Wear measurement using radionuclide-technique (RNT)
    • Scherge M., Pöhlmann K., Gervé A. Wear measurement using radionuclide-technique (RNT). Wear 2003, 254:801-817.
    • (2003) Wear , vol.254 , pp. 801-817
    • Scherge, M.1    Pöhlmann, K.2    Gervé, A.3
  • 11
    • 34548186112 scopus 로고    scopus 로고
    • Origins of the wear resistance of AlSi cylinder bore surfaces studies by surface analytical tools
    • Dienwiebel M., Pöhlmann K., Scherge M. Origins of the wear resistance of AlSi cylinder bore surfaces studies by surface analytical tools. Tribology International 2007, 40:1597-1602.
    • (2007) Tribology International , vol.40 , pp. 1597-1602
    • Dienwiebel, M.1    Pöhlmann, K.2    Scherge, M.3
  • 12
    • 78650676563 scopus 로고    scopus 로고
    • Subsurface sliding wear damage characterization in Al-Si alloys using focused ion beam and cross-sectional TEM techniques
    • Meng-Burany X., Perry T.A., Sachdev A.K., Alpas A.T. Subsurface sliding wear damage characterization in Al-Si alloys using focused ion beam and cross-sectional TEM techniques. Wear 2011, 270:152-162.
    • (2011) Wear , vol.270 , pp. 152-162
    • Meng-Burany, X.1    Perry, T.A.2    Sachdev, A.K.3    Alpas, A.T.4
  • 13
    • 79960662686 scopus 로고    scopus 로고
    • Ultra-mild wear mechanisms of Al-12.6wt% Si alloys at elevated temperature
    • Dey S.K., Lukitsch M.J., Balogh M.P., Meng-Burany X., Alpas A.T. Ultra-mild wear mechanisms of Al-12.6wt% Si alloys at elevated temperature. Wear 2011, 271:1842-1853.
    • (2011) Wear , vol.271 , pp. 1842-1853
    • Dey, S.K.1    Lukitsch, M.J.2    Balogh, M.P.3    Meng-Burany, X.4    Alpas, A.T.5
  • 16
    • 41149119012 scopus 로고    scopus 로고
    • Ultra-mild wear of a hypereutectic Al-18.5wt% Si alloy
    • Chen M., Alpas A.T. Ultra-mild wear of a hypereutectic Al-18.5wt% Si alloy. Wear 2008, 265:186-195.
    • (2008) Wear , vol.265 , pp. 186-195
    • Chen, M.1    Alpas, A.T.2
  • 17
    • 65749107020 scopus 로고    scopus 로고
    • Micromechanisms of low load wear in an 1Al-18.5% Si alloy
    • Dey S.K., Perry T.A., Alpas A.T. Micromechanisms of low load wear in an 1Al-18.5% Si alloy. Wear 2009, 267:515-524.
    • (2009) Wear , vol.267 , pp. 515-524
    • Dey, S.K.1    Perry, T.A.2    Alpas, A.T.3
  • 18
    • 34748903607 scopus 로고    scopus 로고
    • Ultra-mild wear in eutectic Al-Si alloys
    • Chen M., Perry T., Alpas A.T. Ultra-mild wear in eutectic Al-Si alloys. Wear 2007, 263:552-561.
    • (2007) Wear , vol.263 , pp. 552-561
    • Chen, M.1    Perry, T.2    Alpas, A.T.3
  • 20
    • 0037465008 scopus 로고    scopus 로고
    • Scuffing resistances of Al-Si alloys: effects of etching condition surface roughness and particle morphology
    • Riahi A.R., Perry T., Alpas A.T. Scuffing resistances of Al-Si alloys: effects of etching condition surface roughness and particle morphology. Materials Science and Engineering A 2003, 343:76-81.
    • (2003) Materials Science and Engineering A , vol.343 , pp. 76-81
    • Riahi, A.R.1    Perry, T.2    Alpas, A.T.3
  • 21
    • 84879147331 scopus 로고
    • Tribology: Friction and Wear of Engineering Materials, CRC Press, Florida,
    • I.M. Hutchings, Tribology: Friction and Wear of Engineering Materials, CRC Press, Florida, 1992, pp. 68-70.
    • (1992) , pp. 68-70
    • Hutchings, I.M.1
  • 22
    • 0041680087 scopus 로고    scopus 로고
    • ASTM Standard G99-04a, Standard test method for wear testing with a pin-on-disk apparatus, ASTM International, West Conshohocken, PA,
    • ASTM Standard G99-04a, Standard test method for wear testing with a pin-on-disk apparatus, ASTM International, West Conshohocken, PA, 2004, http://dx.doi.org/10.1520/G0099-04A.
    • (2004)
  • 23
    • 0000975159 scopus 로고
    • The elastic contact of rough spheres, Transactions of the ASME Series E
    • Greenwood J.A., Tripp J.H. The elastic contact of rough spheres, Transactions of the ASME Series E. Journal of Applied Mechanics 1967, 34:153-159.
    • (1967) Journal of Applied Mechanics , vol.34 , pp. 153-159
    • Greenwood, J.A.1    Tripp, J.H.2
  • 24
    • 0017482707 scopus 로고
    • Compressive strength and microplasticity in polycrystalline alumina
    • Lankford J. Compressive strength and microplasticity in polycrystalline alumina. Journal of Materials Processing Technology 1977, 12:791-796.
    • (1977) Journal of Materials Processing Technology , vol.12 , pp. 791-796
    • Lankford, J.1
  • 27
    • 0029755634 scopus 로고    scopus 로고
    • An analytical study on strengthening of particulate reinforced metal matrix composites
    • Ramakrishnan N. An analytical study on strengthening of particulate reinforced metal matrix composites. Acta Materialia 1996, 44:69-77.
    • (1996) Acta Materialia , vol.44 , pp. 69-77
    • Ramakrishnan, N.1
  • 28
    • 84879133567 scopus 로고
    • Mechanical Metallurgy, McGraw-Hill Book Company, INC., New York,
    • G.E. Dieter Jr., Mechanical Metallurgy, McGraw-Hill Book Company, INC., New York, 1961, p. 224.
    • (1961) , pp. 224
    • Dieter Jr., G.E.1
  • 30
    • 0031235729 scopus 로고    scopus 로고
    • High angle boundaries formed by grain subdivision mechanisms
    • Hughes D.A., Hansen N. High angle boundaries formed by grain subdivision mechanisms. Acta Materialia 1997, 45:3871-3886.
    • (1997) Acta Materialia , vol.45 , pp. 3871-3886
    • Hughes, D.A.1    Hansen, N.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.