1
-
-
0027610802
-
Wear resistance of Ni-hard 4 and high chromium cast iron re-evaluated
-
Jinzhu L., Shizhuo L., Yongfa M. Wear resistance of Ni-hard 4 and high chromium cast iron re-evaluated. Wear 1993, 166:37-40.
-
(1993)
Wear
, vol.166
, pp. 37-40
-
-
Jinzhu, L.1
Shizhuo, L.2
Yongfa, M.3
-
2
-
-
59449106663
-
Microstructural modifications of as-cast high-chromium white iron by heat treatment
-
Karantzalis A.E., Lekatou A., Mavros H. Microstructural modifications of as-cast high-chromium white iron by heat treatment. J Mater Eng Perform 2009, 18:174-181.
-
(2009)
J Mater Eng Perform
, vol.18
, pp. 174-181
-
-
Karantzalis, A.E.1
Lekatou, A.2
Mavros, H.3
-
3
-
-
18944392938
-
Effect of titanium on the as-cast microstructure of a 16%chromium white iron
-
Bedolla-Jacuinde A., Correa R., Quezada J.G., Maldonado C. Effect of titanium on the as-cast microstructure of a 16%chromium white iron. Mater Sci Eng A 2005, 398:297-308.
-
(2005)
Mater Sci Eng A
, vol.398
, pp. 297-308
-
-
Bedolla-Jacuinde, A.1
Correa, R.2
Quezada, J.G.3
Maldonado, C.4
-
4
-
-
0028516838
-
The influence of vanadium on fracture toughness and abrasion resistance in high chromium white cast irons
-
Radulovic M., Fiset M., Peev K., Tomovic M. The influence of vanadium on fracture toughness and abrasion resistance in high chromium white cast irons. J Mater Sci 1994, 29:5085-5094.
-
(1994)
J Mater Sci
, vol.29
, pp. 5085-5094
-
-
Radulovic, M.1
Fiset, M.2
Peev, K.3
Tomovic, M.4
-
5
-
-
65949086388
-
Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe-25wt%Cr-4wt%C
-
Chung R.J., Tang X., Li D.Y., Hinckley B., Dolman K. Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe-25wt%Cr-4wt%C. Wear 2009, 267:356-361.
-
(2009)
Wear
, vol.267
, pp. 356-361
-
-
Chung, R.J.1
Tang, X.2
Li, D.Y.3
Hinckley, B.4
Dolman, K.5
-
7
-
-
33947207617
-
Effects of tungsten on erosion-corrosion behavior of high chromium white cast iron
-
Mousavi Anijdan S.H., Bahrami A., Varahram N., Davami P. Effects of tungsten on erosion-corrosion behavior of high chromium white cast iron. Mater Sci Eng A 2007, 454:623-628.
-
(2007)
Mater Sci Eng A
, vol.454
, pp. 623-628
-
-
Mousavi Anijdan, S.H.1
Bahrami, A.2
Varahram, N.3
Davami, P.4
-
8
-
-
37349093005
-
Effect of niobium on the as-cast microstructure of hypereutectic high chromium cast iron
-
Xiaohui Z., Jiandong X., Hanguang F., Bing X. Effect of niobium on the as-cast microstructure of hypereutectic high chromium cast iron. Mater Lett 2008, 62:857-860.
-
(2008)
Mater Lett
, vol.62
, pp. 857-860
-
-
Xiaohui, Z.1
Jiandong, X.2
Hanguang, F.3
Bing, X.4
-
9
-
-
0027579522
-
Development of abrasion-resistant Ni-hard 4 cast irons
-
Jinzhu Liu L., Yongfa M. Development of abrasion-resistant Ni-hard 4 cast irons. Wear 1993, 162:833-836.
-
(1993)
Wear
, vol.162
, pp. 833-836
-
-
Jinzhu Liu, L.1
Yongfa, M.2
-
10
-
-
33947143524
-
Effect of nanocrystalline TiC powder addition on the hardness and wear resistance of cast iron
-
Razavi M., Rahimipour M.R., Rajabi-Zamani A.H. Effect of nanocrystalline TiC powder addition on the hardness and wear resistance of cast iron. Mater Sci Eng A 2007, 454:144-147.
-
(2007)
Mater Sci Eng A
, vol.454
, pp. 144-147
-
-
Razavi, M.1
Rahimipour, M.R.2
Rajabi-Zamani, A.H.3
-
11
-
-
65749092745
-
Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: the relationship between microstructure and wear
-
Scandian C., Boher C., de Mello J.D.B., Rézaï-Aria F. Effect of molybdenum and chromium contents in sliding wear of high-chromium white cast iron: the relationship between microstructure and wear. Wear 2009, 267:401-408.
-
(2009)
Wear
, vol.267
, pp. 401-408
-
-
Scandian, C.1
Boher, C.2
de Mello, J.D.B.3
Rézaï-Aria, F.4
-
13
-
-
78049529227
-
Effect of heat treatment on microstructure and mechanical properties of high boron white cast iron
-
Xiang C., Yanxiang L. Effect of heat treatment on microstructure and mechanical properties of high boron white cast iron. Mater Sci Eng A 2010, 528:770-775.
-
(2010)
Mater Sci Eng A
, vol.528
, pp. 770-775
-
-
Xiang, C.1
Yanxiang, L.2
-
14
-
-
43549112944
-
Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron
-
Xiaohui Z., Jiandong X., Yimin G. Effect of heat treatment on microstructure and mechanical properties of a Ti-bearing hypereutectic high chromium white cast iron. Mater Sci Eng A 2008, 487:171-179.
-
(2008)
Mater Sci Eng A
, vol.487
, pp. 171-179
-
-
Xiaohui, Z.1
Jiandong, X.2
Yimin, G.3
-
15
-
-
0020310772
-
Eutectic solidification of high chromium cast iron-eutectic mechanism of eutectic growth
-
Ogi K., Matsubara Y., Matsuda K. Eutectic solidification of high chromium cast iron-eutectic mechanism of eutectic growth. AFS Trans 1982, 89:197-204.
-
(1982)
AFS Trans
, vol.89
, pp. 197-204
-
-
Ogi, K.1
Matsubara, Y.2
Matsuda, K.3
-
16
-
-
23844523219
-
Microstructural and crystallographical study of carbides in 30wt%Cr cast irons
-
Wiengmoon A., Chairuangsri T., Brown A., Brydson R., Edmonds D.V., Pearce J.T.H. Microstructural and crystallographical study of carbides in 30wt%Cr cast irons. Acta Mater 2005, 53:4143-4145.
-
(2005)
Acta Mater
, vol.53
, pp. 4143-4145
-
-
Wiengmoon, A.1
Chairuangsri, T.2
Brown, A.3
Brydson, R.4
Edmonds, D.V.5
Pearce, J.T.H.6
-
17
-
-
67649395488
-
Effect of misch metal inoculation on microstructure, mechanical and wear properties of hypoeutectic gray cast irons
-
Vadiraj A., Balachandran G., Kamaraj M. Effect of misch metal inoculation on microstructure, mechanical and wear properties of hypoeutectic gray cast irons. Mater Des 2009, 30:4488-4492.
-
(2009)
Mater Des
, vol.30
, pp. 4488-4492
-
-
Vadiraj, A.1
Balachandran, G.2
Kamaraj, M.3
-
18
-
-
0348136157
-
Relationship between microstructure, hardness, impact toughness and wear performance of selected grinding media for mineral ore milling operations
-
Chenje T.W., Simbi D.J., Navara E. Relationship between microstructure, hardness, impact toughness and wear performance of selected grinding media for mineral ore milling operations. Mater Des 2004, 25:11-18.
-
(2004)
Mater Des
, vol.25
, pp. 11-18
-
-
Chenje, T.W.1
Simbi, D.J.2
Navara, E.3
-
19
-
-
65749083929
-
Variations in microstructure of high chromium cast irons and resultant changes in resistance to wear, corrosion and corrosive wear
-
Tang X.H., Chung R., Li D.Y., Hinckley B., Dolman K. Variations in microstructure of high chromium cast irons and resultant changes in resistance to wear, corrosion and corrosive wear. Wear 2009, 267:116-121.
-
(2009)
Wear
, vol.267
, pp. 116-121
-
-
Tang, X.H.1
Chung, R.2
Li, D.Y.3
Hinckley, B.4
Dolman, K.5
-
20
-
-
28844483506
-
Influence of secondary carbides precipitation and transformation on hardening behavior of a 15 Cr-1 Mo-1.5 V white iron
-
Wang J., Zuo R.L., Sun Z.P., Li C., Liu H.H., Yang H.S., et al. Influence of secondary carbides precipitation and transformation on hardening behavior of a 15 Cr-1 Mo-1.5 V white iron. Mater Charact 2005, 55:234-240.
-
(2005)
Mater Charact
, vol.55
, pp. 234-240
-
-
Wang, J.1
Zuo, R.L.2
Sun, Z.P.3
Li, C.4
Liu, H.H.5
Yang, H.S.6
-
21
-
-
47849118700
-
Effect of titanium on the as-cast microstructure of hypereutectic high chromium cast iron
-
Xiaohui Z., Jiandong X., Hanguang F., Yiming G. Effect of titanium on the as-cast microstructure of hypereutectic high chromium cast iron. Mater Charact 2008, 59:1221-1226.
-
(2008)
Mater Charact
, vol.59
, pp. 1221-1226
-
-
Xiaohui, Z.1
Jiandong, X.2
Hanguang, F.3
Yiming, G.4
-
22
-
-
79961128432
-
Wear mechanism of abrasion resistant wear parts in raw material vertical roller mills
-
Jensen R.D., Fundal E., Moller P., Jespersen M. Wear mechanism of abrasion resistant wear parts in raw material vertical roller mills. Wear 2011, 271:2707-2719.
-
(2011)
Wear
, vol.271
, pp. 2707-2719
-
-
Jensen, R.D.1
Fundal, E.2
Moller, P.3
Jespersen, M.4
-
23
-
-
0028726411
-
Wear mechanism of Ni-Hard4 rollers in chromite ore crushing
-
Nieminen R., Autio J., Suomalainen E., Husu N., Kauppi M. Wear mechanism of Ni-Hard4 rollers in chromite ore crushing. Wear 1994, 179:95-100.
-
(1994)
Wear
, vol.179
, pp. 95-100
-
-
Nieminen, R.1
Autio, J.2
Suomalainen, E.3
Husu, N.4
Kauppi, M.5
-
24
-
-
0035308957
-
Friction measurement on Ni-Hard 4 during high pressure crushing of silica
-
Yao M., Page N.W. Friction measurement on Ni-Hard 4 during high pressure crushing of silica. Wear 2001, 249:117-126.
-
(2001)
Wear
, vol.249
, pp. 117-126
-
-
Yao, M.1
Page, N.W.2
|