Corrosion of magnesium electrolytes: Chlorides-the culprit

Author keywords

[No Author keywords available]

Indexed keywords

CHLORINE COMPOUNDS; CORROSION; ELECTROLYTES; POSITIVE IONS; PRECIOUS METALS;

EID: 84873153460     PISSN: 17545692     EISSN: 17545706     Source Type: Journal    
DOI: 10.1039/c2ee23686a     Document Type: Article
Times cited : (187)

References (25)
  • 6
    • 7644227934 scopus 로고    scopus 로고
    • K. Xu Chem. Rev. 2004 104 4303 4418
    • (2004) Chem. Rev. , vol.104 , pp. 4303-4418
    • Xu, K.1
  • 22
    • 2342437604 scopus 로고    scopus 로고
    • Crystal data for C72H104 B2MgO 7; Mr = 1127.48; monoclinic; space group P21/c; a = 12.339(2) Å; b = 12.934(2) Å; c = 40.333(7) Å; α = 90°; β = 91.938(3)°; γ = 90°; V = 6433.3(18) Å3; Z = 4; T = 120(2) K; λ(Mo-Kα) = 0.71073 Å; μ(Mo-Kα) = 0.081 mm-1; dcalc = 1.164g cm-3; 62567 reflections collected; 9356 unique (Rint = 0.0715); giving R1 = 0.0990, wR2 = 0.2769 for 5725 data with [I > 2σ(I)] and R1 = 0.1423, wR2 = 0.3105 for all 9356 data. Residual electron density (e- Å -3) max/min: 0.665/-0.626
    • D. Aurbach I. Weissman Y. Gofer E. Levi Chem. Rec. 2003 3 61 73
    • (2003) Chem. Rec. , vol.3 , pp. 61-73
    • Aurbach, D.1    Weissman, I.2    Gofer, Y.3    Levi, E.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.