Volumn 32, Issue 2, 2013, Pages 221-230

Compression and tensile properties of self-reinforced poly(ethylene terephthalate)-composites

Author keywords

Compression testing; Mechanical properties; Polymer matrix composite; Self reinforced

Indexed keywords

BULK POLYMER; CATASTROPHIC FAILURES; COMPRESSION PROPERTIES; ELASTIC-PERFECTLY PLASTIC MATERIAL; ENERGY-ABSORBING MATERIALS; FAILURE STRAIN; FIBRE REINFORCED COMPOSITES; HIGH STRAINS; RECYCLABILITY; SELF REINFORCED; STRESS-STRAIN RESPONSE;

EID: 84872065467     PISSN: 01429418     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymertesting.2012.11.002     Document Type: Article
Times cited : (47)

References (17)
  • 2
    • 33748534446 scopus 로고    scopus 로고
    • Single-polymer composites based on slowly crystallizing polymers
    • D. Yao, R. Li, and P. Nagarajan Single-polymer composites based on slowly crystallizing polymers Polym. Eng. Sci. 46 2006 1123 1230
    • (2006) Polym. Eng. Sci. , vol.46 , pp. 1123-1230
    • Yao, D.1    Li, R.2    Nagarajan, P.3
  • 5
  • 6
    • 0037449596 scopus 로고    scopus 로고
    • The hot compaction behaviour of woven oriented polypropylene fibres and tapes. I. Mechanical properties
    • DOI 10.1016/S0032-3861(02)00809-1, PII S0032386102008091
    • P.J. Hine, I.M. Ward, N.D. Jordan, R. Olley, and D.C. Bassett The hot compaction behaviour of woven orientated polypropylene fibres and tapes. 1. Mechanical properties Polymer 44 2003 1117 1131 (Pubitemid 36133701)
    • (2003) Polymer , vol.44 , Issue.4 , pp. 1117-1131
    • Hinea, P.J.1    Warda, I.M.2    Jordan, N.D.3    Olley, R.4    Bassett, D.C.5
  • 7
    • 0942279266 scopus 로고    scopus 로고
    • Hot compaction of woven poly(ethylene terephthalate) multifilaments
    • DOI 10.1002/app.13343
    • P.J. Hine, and I.M. Ward Hot compaction of woven poly(ethylene terephthalate) multifilaments J. Appl. Polym. Sci. 91 4 2003 2223 2233 (Pubitemid 38136682)
    • (2004) Journal of Applied Polymer Science , vol.91 , Issue.4 , pp. 2223-2233
    • Hine, P.J.1    Ward, I.M.2
  • 8
    • 84872093449 scopus 로고    scopus 로고
    • ® ApS DK 8883 Gjer, Denmark, 10
    • ® ApS. Thermoplastic Composites, DK 8883 Gjer, Denmark, 10.2011, www.comfil.biz.
    • (2011) Thermoplastic Composites
  • 12
    • 84872066078 scopus 로고    scopus 로고
    • GOM mbh Braunschweig, Germany
    • GOM mbh. User Manual: Aramis v5.3.0, Braunschweig, Germany http://www.gom.com.
    • User Manual: Aramis v5.3.0
  • 13
    • 0002617678 scopus 로고    scopus 로고
    • Compression failure of fiber composites
    • N.A. Fleck Compression failure of fiber composites Adv. Appl. Mech. 3 1997 43 117
    • (1997) Adv. Appl. Mech. , vol.3 , pp. 43-117
    • Fleck, N.A.1
  • 14
    • 0024017216 scopus 로고
    • Experimental verification of microbuckling model for the axial compressive failure of high performance polymer fibres
    • S.J. DeTeresa, R.S. Porter, and R.J. Farris Experimental verification of microbuckling model for the axial compressive failure of high performance polymer fibres J. Mater. Sci. 23 1988 1886 1894
    • (1988) J. Mater. Sci. , vol.23 , pp. 1886-1894
    • Deteresa, S.J.1    Porter, R.S.2    Farris, R.J.3
  • 17
    • 0001600571 scopus 로고    scopus 로고
    • A model for the tensile curve with yield of a polymer fibre
    • J.J.M. Baltussen, and M.G. Northolt A model for the tensile curve with yield of a polymer fibre Polym. Bull. 36 1996 125 131 (Pubitemid 126455391)
    • (1996) Polymer Bulletin , vol.36 , Issue.1 , pp. 125-131
    • Baltussen, J.J.M.1    Northolt, M.G.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.