High temperature degradation behavior of sputtered nanostructured Co-Al coatings on superalloy

Author keywords

Cyclic high temperature; Nanostructured Co Al coatings; Oxidation; Protective oxide scale; Scale spallation; Sputter deposition

Indexed keywords

ALUMINA; ALUMINUM ALLOYS; ALUMINUM OXIDE; BINARY ALLOYS; CHROMIUM COMPOUNDS; COBALT ALLOYS; OXIDATION; OXIDATION RESISTANCE; SCALE (DEPOSITS); SPALLING; SPUTTER DEPOSITION; SUPERALLOYS; THERMOOXIDATION;

EID: 84871932105     PISSN: 01694332     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.apsusc.2012.10.002     Document Type: Article
Times cited : (12)

References (35)
  • 1
    • 33746775065 scopus 로고    scopus 로고
    • I.O. Physics Series in Materials Science and Engineering CRC Press Philadelphia
    • B. Cantor, and H. Assender I.O. Physics Aerospace Materials Series in Materials Science and Engineering 2001 CRC Press Philadelphia 312
    • (2001) Aerospace Materials , pp. 312
    • Cantor, B.1    Assender, H.2
  • 2
    • 33747151321 scopus 로고    scopus 로고
    • Oxidation and hot corrosion behavior of gradient NiCoCrAlYSiB coatings deposited by a combination of arc ion plating and magnetron sputtering techniques
    • M.H. Guo, Q.M. Wang, J. Gong, C. Sun, R.F. Huang, and L.S. Wen Oxidation and hot corrosion behavior of gradient NiCoCrAlYSiB coatings deposited by a combination of arc ion plating and magnetron sputtering techniques Corrosion Science 48 2006 2750 2764
    • (2006) Corrosion Science , vol.48 , pp. 2750-2764
    • Guo, M.H.1    Wang, Q.M.2    Gong, J.3    Sun, C.4    Huang, R.F.5    Wen, L.S.6
  • 4
  • 5
    • 0032629762 scopus 로고    scopus 로고
    • Cyclic oxidation of sputter-deposited nanocrystalline Fe-Cr-Ni-Al alloy coatings
    • Z. Liu, W. Gao, and M. Li Cyclic oxidation of sputter-deposited nanocrystalline Fe-Cr-Ni-Al alloy coatings Oxidation of Metals 51 1999 403 419
    • (1999) Oxidation of Metals , vol.51 , pp. 403-419
    • Liu, Z.1    Gao, W.2    Li, M.3
  • 6
    • 0042897007 scopus 로고    scopus 로고
    • Oxidation behaviour of nanocrystalline Fe-Ni-Cr-Al alloy coatings
    • Z. Liu, W. Gao, and Y. He Oxidation behaviour of nanocrystalline Fe-Ni-Cr-Al alloy coatings Materials Science and Technology 15 1999 1447 1450
    • (1999) Materials Science and Technology , vol.15 , pp. 1447-1450
    • Liu, Z.1    Gao, W.2    He, Y.3
  • 7
    • 0035806586 scopus 로고    scopus 로고
    • Nano- and microcrystal coatings and their high-temperature applications
    • W. Gao, Z. Liu, and Z. Li Nano- and microcrystal coatings and their high-temperature applications Advanced Materials 13 2001 1001 1004
    • (2001) Advanced Materials , vol.13 , pp. 1001-1004
    • Gao, W.1    Liu, Z.2    Li, Z.3
  • 9
    • 79960282791 scopus 로고    scopus 로고
    • Cyclic high temperature oxidation behavior of sputtered Cr/Al multilayer coatings on superalloy
    • A. Rahman, R. Jayaganthan, S. Prakash, V. Chawla, and R. Chandra Cyclic high temperature oxidation behavior of sputtered Cr/Al multilayer coatings on superalloy Surface Engineering 27 2011 393 401
    • (2011) Surface Engineering , vol.27 , pp. 393-401
    • Rahman, A.1    Jayaganthan, R.2    Prakash, S.3    Chawla, V.4    Chandra, R.5
  • 10
    • 0001669809 scopus 로고    scopus 로고
    • Hot-corrosion resistance of a sputtered K38G nanocrystalline coating in molten sulfate at 900°C
    • S. Geng, F. Wang, S. Zhu, and W. Wu Hot-corrosion resistance of a sputtered K38G nanocrystalline coating in molten sulfate at 900°C Oxidation of Metals 57 2002 549 557
    • (2002) Oxidation of Metals , vol.57 , pp. 549-557
    • Geng, S.1    Wang, F.2    Zhu, S.3    Wu, W.4
  • 12
    • 77952422114 scopus 로고    scopus 로고
    • Cyclic oxidation behavior and microstructure of nanocrystalline Ni-20Cr-4Al coating
    • N.S. Cheruvu, R. Wei, M.R. Govindaraju, and D.W. Gandy Cyclic oxidation behavior and microstructure of nanocrystalline Ni-20Cr-4Al coating Oxidation of Metals 73 2010 493 511
    • (2010) Oxidation of Metals , vol.73 , pp. 493-511
    • Cheruvu, N.S.1    Wei, R.2    Govindaraju, M.R.3    Gandy, D.W.4
  • 13
    • 0343446739 scopus 로고
    • H. Felix, L. Fischmeister, Y. Habraken, Linblon M.O. Speidel, Applied Science Publishers Ltd. London
    • D.P. Whittle, and D.P. Coutsouradis H. Felix, L. Fischmeister, Y. Habraken, Linblon M.O. Speidel, High Temperature Alloys for Gas Turbines 1978 Applied Science Publishers Ltd. London 209 224
    • (1978) High Temperature Alloys for Gas Turbines , pp. 209-224
    • Whittle, D.P.1    Coutsouradis, D.P.2
  • 14
    • 43949126837 scopus 로고    scopus 로고
    • Oxidation and hot corrosion behavior of sputtered nanocrystalline coating of superalloy K52
    • F. Wang, X. Tian, Q. Li, L. Li, and X. Peng Oxidation and hot corrosion behavior of sputtered nanocrystalline coating of superalloy K52 Thin Solid Films 516 2008 5740 5747
    • (2008) Thin Solid Films , vol.516 , pp. 5740-5747
    • Wang, F.1    Tian, X.2    Li, Q.3    Li, L.4    Peng, X.5
  • 15
    • 0037461211 scopus 로고    scopus 로고
    • High temperature oxidation behavior of a sputtered pure Ni nanocrystalline coating at 700-900°C
    • S. Geng, F. Wang, and S. Zhang High temperature oxidation behavior of a sputtered pure Ni nanocrystalline coating at 700-900°C Surface and Coatings Technology 167 2003 212 216
    • (2003) Surface and Coatings Technology , vol.167 , pp. 212-216
    • Geng, S.1    Wang, F.2    Zhang, S.3
  • 16
    • 0000020609 scopus 로고    scopus 로고
    • Oxidation behavior of sputtered microcrystalline coating of superalloy K17F at high temperature
    • H. Lou, Y. Tangb, X. Sunb, and H. Guanb Oxidation behavior of sputtered microcrystalline coating of superalloy K17F at high temperature Materials Science and Engineering A 207 1996 121 128
    • (1996) Materials Science and Engineering A , vol.207 , pp. 121-128
    • Lou, H.1    Tangb, Y.2    Sunb, X.3    Guanb, H.4
  • 17
    • 40449130472 scopus 로고    scopus 로고
    • Study of oxidation behavior of nanostructured NiCrAlY bond coatings deposited by cold spraying
    • Q. Zhang, C.-J. Li, C.-X. Li, G.-J. Yang, and S.-C. Lui Study of oxidation behavior of nanostructured NiCrAlY bond coatings deposited by cold spraying Surface and Coatings Technology 202 14 2008 3378 3384
    • (2008) Surface and Coatings Technology , vol.202 , Issue.14 , pp. 3378-3384
    • Zhang, Q.1    Li, C.-J.2    Li, C.-X.3    Yang, G.-J.4    Lui, S.-C.5
  • 19
    • 0032472963 scopus 로고    scopus 로고
    • Oxidation behaviour of sputtered-deposited Ni-Cr-Al micro crystalline coating
    • Z. Liu, W. Gao, K.L. Dahm, and F. Wang Oxidation behaviour of sputtered-deposited Ni-Cr-Al micro crystalline coating Acta Materialia 26 5 1998 1691 1700
    • (1998) Acta Materialia , vol.26 , Issue.5 , pp. 1691-1700
    • Liu, Z.1    Gao, W.2    Dahm, K.L.3    Wang, F.4
  • 20
    • 3543148317 scopus 로고    scopus 로고
    • Influence of cryomilling on the morphology and composition of the oxide scales formed on HVOF CoNiCrAlY coating
    • F. Tang, L. Ajdelsztajn, and J.M. Schoenung Influence of cryomilling on the morphology and composition of the oxide scales formed on HVOF CoNiCrAlY coating Oxidation of Metals 61 3 2004 219 238
    • (2004) Oxidation of Metals , vol.61 , Issue.3 , pp. 219-238
    • Tang, F.1    Ajdelsztajn, L.2    Schoenung, J.M.3
  • 22
    • 0031244964 scopus 로고    scopus 로고
    • The effect of nanocrystallization on the selective oxidation and adhesion of A1203 scales
    • F. Wang The effect of nanocrystallization on the selective oxidation and adhesion of A1203 scales Oxidation of Metals 48 1997 215 224
    • (1997) Oxidation of Metals , vol.48 , pp. 215-224
    • Wang, F.1
  • 24
    • 0041703393 scopus 로고    scopus 로고
    • The main degradation modes of an aluminide coating on a Co-base superalloy during high-temperature oxidation in air
    • P.S. Liu The main degradation modes of an aluminide coating on a Co-base superalloy during high-temperature oxidation in air Oxidation of Metals 58 3-4 2002 331 336
    • (2002) Oxidation of Metals , vol.58 , Issue.34 , pp. 331-336
    • Liu, P.S.1
  • 26
    • 0035400448 scopus 로고    scopus 로고
    • High-temperature oxidation behavior of aluminide coatings on a new cobalt-base superalloy in air
    • P.S. Liu, K.M. Lang, and S.R. Gu High-temperature oxidation behavior of aluminide coatings on a new cobalt-base superalloy in air Corrosion Science 43 7 2001 1217 1226
    • (2001) Corrosion Science , vol.43 , Issue.7 , pp. 1217-1226
    • Liu, P.S.1    Lang, K.M.2    Gu, S.R.3
  • 27
    • 0042203885 scopus 로고    scopus 로고
    • Oxidation behavior and breakdown of an aluminide coating on DZ40M alloy at high temperatures
    • P.S. Liu, K.M. Liang, H.Y. Zhou, H.R. Guan, X.F. Sun, T. Jin, and K.N. Yang Oxidation behavior and breakdown of an aluminide coating on DZ40M alloy at high temperatures Oxidation of Metals 55 5-6 2001 543 550
    • (2001) Oxidation of Metals , vol.55 , Issue.56 , pp. 543-550
    • Liu, P.S.1    Liang, K.M.2    Zhou, H.Y.3    Guan, H.R.4    Sun, X.F.5    Jin, T.6    Yang, K.N.7
  • 28
    • 0035054776 scopus 로고    scopus 로고
    • Using theoretical formula to calculate degradation life for an aluminide coating during high-temperature oxidation in air
    • P.S. Liu, K.M. Liang, and S.R. Gu Using theoretical formula to calculate degradation life for an aluminide coating during high-temperature oxidation in air Surface and Coatings Technology 132 1-2 2000 60 64
    • (2000) Surface and Coatings Technology , vol.132 , Issue.12 , pp. 60-64
    • Liu, P.S.1    Liang, K.M.2    Gu, S.R.3
  • 29
    • 0034300860 scopus 로고    scopus 로고
    • Failure behavior of an aluminide coating on a Co-base superalloy during high-temperature oxidation in air
    • P.S. Liu, K.M. Liang, and S.R. Gu Failure behavior of an aluminide coating on a Co-base superalloy during high-temperature oxidation in air Oxidation of Metals 54 3/4 2000 277 283
    • (2000) Oxidation of Metals , vol.54 , Issue.3-4 , pp. 277-283
    • Liu, P.S.1    Liang, K.M.2    Gu, S.R.3
  • 30
    • 0034599724 scopus 로고    scopus 로고
    • A new way to evaluate the high-temperature oxidation life of aluminide coatings on Co-base superalloys in air
    • P.S. Liu, and K.M. Liang A new way to evaluate the high-temperature oxidation life of aluminide coatings on Co-base superalloys in air Surface and Coatings Technology 126 1 2000 64 68
    • (2000) Surface and Coatings Technology , vol.126 , Issue.1 , pp. 64-68
    • Liu, P.S.1    Liang, K.M.2
  • 31
    • 38049123265 scopus 로고    scopus 로고
    • Characterization of nanostructured TiN coatings fabricated by pulse laser
    • D. Zou, D. Yan, L. Xiao, and Y. Dong Characterization of nanostructured TiN coatings fabricated by pulse laser Surface and Coatings Technology 202 2008 1928 1934
    • (2008) Surface and Coatings Technology , vol.202 , pp. 1928-1934
    • Zou, D.1    Yan, D.2    Xiao, L.3    Dong, Y.4
  • 34
    • 33745933815 scopus 로고    scopus 로고
    • High-temperature oxidation and hot-corrosion behavior of a sputtered NiCrAlY coating with and without aluminizing
    • X. Ren, and F. Wang High-temperature oxidation and hot-corrosion behavior of a sputtered NiCrAlY coating with and without aluminizing Surface and Coatings Technology 201 2006 30 37
    • (2006) Surface and Coatings Technology , vol.201 , pp. 30-37
    • Ren, X.1    Wang, F.2
  • 35
    • 58849134811 scopus 로고    scopus 로고
    • High temperature cyclic oxidation behavior of magnetron sputtered Ni-Al thin films on Ni- and Fe-based superalloys
    • R.A. Mahesh, R. Jayaganthan, and S. Prakash High temperature cyclic oxidation behavior of magnetron sputtered Ni-Al thin films on Ni- and Fe-based superalloys Materials Chemistry and Physics 114 2009 629 635
    • (2009) Materials Chemistry and Physics , vol.114 , pp. 629-635
    • Mahesh, R.A.1    Jayaganthan, R.2    Prakash, S.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.