메뉴 건너뛰기




Volumn 21, Issue 9, 2012, Pages 1873-1878

Effect of the spinning deformation processing on mechanical properties of Al-7Si-0.3Mg alloys

Author keywords

Aluminum; Elongation; Spinning

Indexed keywords

A356 ALLOYS; CAST STRUCTURES; CASTING DEFECT; DEFORMATION PROCESSING; EUTECTIC SILICON; QUALITY INDICES; RE-ARRANGEMENT;

EID: 84869494986     PISSN: 10599495     EISSN: None     Source Type: Journal    
DOI: 10.1007/s11665-011-0089-8     Document Type: Article
Times cited : (7)

References (16)
  • 1
    • 0345897836 scopus 로고    scopus 로고
    • Wheel design and engineering
    • D. Carney, Wheel Design and Engineering, Autom. Eng. Int., 2001, 109, p 54-59
    • (2001) Autom. Eng. Int. , vol.109 , pp. 54-59
    • Carney, D.1
  • 2
    • 58149174379 scopus 로고    scopus 로고
    • Impact behaviour of A356 alloy for low-pressure die casting automotive wheels
    • M. Merlin, G. Timelli, F. Bonollo, and G.L. Garagnani, Impact Behaviour of A356 Alloy for Low-pressure Die Casting Automotive Wheels, J. Mater. Process. Technol., 2009, 209, p 1060-1073
    • (2009) J. Mater. Process. Technol. , vol.209 , pp. 1060-1073
    • Merlin, M.1    Timelli, G.2    Bonollo, F.3    Garagnani, G.L.4
  • 3
    • 0141496063 scopus 로고    scopus 로고
    • A review of spinning, shear forming and flow forming processes
    • C.C. Wong, T.A. Dean, and J. Lin, A Review of Spinning, Shear Forming and Flow Forming Processes, Int. J. Mach. Tools Manuf., 2003, 43, p 1419-1435
    • (2003) Int. J. Mach. Tools Manuf. , vol.43 , pp. 1419-1435
    • Wong, C.C.1    Dean, T.A.2    Lin, J.3
  • 4
    • 0029280639 scopus 로고
    • Metal spinning in the automotive industry
    • D. Polit, Metal Spinning in the Automotive Industry, Sheet Met. Ind., 1995, 72, p 31-32
    • (1995) Sheet Met. Ind. , vol.72 , pp. 31-32
    • Polit, D.1
  • 5
    • 77955452980 scopus 로고    scopus 로고
    • Effect of spinning deformation processing on the wear and corrosion properties of Al-7Si-0.3Mg alloys
    • Y.C. Cheng, C.K. Lin, A.H. Tan, J.C. Lin, and S.L. Lee, Effect of Spinning Deformation Processing on the Wear and Corrosion Properties of Al-7Si-0.3Mg Alloys, Mater. Manuf. Process., 2010, 25, p 689-695
    • (2010) Mater. Manuf. Process. , vol.25 , pp. 689-695
    • Cheng, Y.C.1    Lin, C.K.2    Tan, A.H.3    Lin, J.C.4    Lee, S.L.5
  • 7
    • 67649449243 scopus 로고    scopus 로고
    • Influence of additives on the microstructure and tensile properties of near-eutectic Al-10.8%Si cast alloy
    • A.M.A. Mohamed, A.M. Samuel, F.H. Samuel, and H.W. Doty, Influence of Additives on the Microstructure and Tensile Properties of Near-Eutectic Al-10.8%Si Cast Alloy, Mater. Des., 2009, 30, p 3943-3957
    • (2009) Mater. Des. , vol.30 , pp. 3943-3957
    • Mohamed, A.M.A.1    Samuel, A.M.2    Samuel, F.H.3    Doty, H.W.4
  • 8
    • 70350620728 scopus 로고    scopus 로고
    • Effect of trace la addition on the microstructures and mechanical properties of A356 (Al-7Si-0.35Mg) aluminum alloys
    • Y.C. Tsai, C.Y. Chou, S.L. Lee, C.K. Lin, J.C. Lin, and S.W. Lim, Effect of Trace La Addition on the Microstructures and Mechanical Properties of A356 (Al-7Si-0.35Mg) Aluminum Alloys, J. Alloys Compd., 2009, 487, p 157-162
    • (2009) J. Alloys Compd. , vol.487 , pp. 157-162
    • Tsai, Y.C.1    Chou, C.Y.2    Lee, S.L.3    Lin, C.K.4    Lin, J.C.5    Lim, S.W.6
  • 9
    • 77953285145 scopus 로고    scopus 로고
    • Influence of aging treatments and alloying additives on the hardness of Al-11Si-2.5Cu-Mg alloys
    • Z. Ma, E. Samuel, A.M.A. Mohamed, A.M. Samuel, F.H. Samuel, and H.W. Doty, Influence of Aging Treatments and Alloying Additives on the Hardness of Al-11Si-2.5Cu-Mg Alloys, Mater. Des., 2010, 31, p 3791-3803
    • (2010) Mater. Des. , vol.31 , pp. 3791-3803
    • Ma, Z.1    Samuel, E.2    Mohamed, A.M.A.3    Samuel, A.M.4    Samuel, F.H.5    Doty, H.W.6
  • 10
    • 41949136407 scopus 로고    scopus 로고
    • Modifying Al-7Si-0.35Mg alloys using equal channel angular extrusion
    • C.Y. Chou, K.W. Wang, S.L. Lee, and T.S. Yang, Modifying Al-7Si-0.35Mg Alloys Using Equal Channel Angular Extrusion, Mater. Lett., 2008, 62, p 2469-2472
    • (2008) Mater. Lett. , vol.62 , pp. 2469-2472
    • Chou, C.Y.1    Wang, K.W.2    Lee, S.L.3    Yang, T.S.4
  • 11
    • 58149172198 scopus 로고    scopus 로고
    • Evolution of plastic strain during a flow forming process
    • M.J. Roy, R.J. Klassen, and J.T. Wood, Evolution of Plastic Strain During a Flow Forming Process, J. Mater. Process. Technol., 2009, 209, p 1018-1025
    • (2009) J. Mater. Process. Technol. , vol.209 , pp. 1018-1025
    • Roy, M.J.1    Klassen, R.J.2    Wood, J.T.3
  • 12
    • 0030387317 scopus 로고    scopus 로고
    • The quench sensitivity of cast Al-7 Wt Pct Si-0.4 Wt Pct Mg alloy
    • D.L. Zhang and L. Zheng, The Quench Sensitivity of Cast Al-7 Wt Pct Si-0.4 Wt Pct Mg Alloy, Metall. Mater. Trans. A, 1996, 27A, p 3983-3991
    • (1996) Metall. Mater. Trans. A , vol.27 A , pp. 3983-3991
    • Zhang, D.L.1    Zheng, L.2
  • 13
    • 33750948999 scopus 로고    scopus 로고
    • Effect of Sr and Sb modifiers on the sliding wear of A357 alloy under varying pressure and speed conditions
    • C.Y. Yang, S.L. Lee, C.K. Lee, and J.C. Lin, Effect of Sr and Sb Modifiers on the Sliding Wear of A357 Alloy Under Varying Pressure and Speed Conditions, Wear, 2006, 261, p 1348-1358
    • (2006) Wear , vol.261 , pp. 1348-1358
    • Yang, C.Y.1    Lee, S.L.2    Lee, C.K.3    Lin, J.C.4
  • 14
    • 0029321911 scopus 로고
    • Effect of silicon particles on the fatigue crack growth characteristics of Al-12 wt pct Si-0.35 wt pct Mg-(0 to 0.02) wt pct Sr casting alloys
    • F.T. Lee, J.F. Major, and F.H. Samuel, Effect of Silicon Particles on the Fatigue Crack Growth Characteristics of Al-12 wt pct Si-0.35 wt pct Mg-(0 to 0.02) wt pct Sr Casting Alloys, Metall. Mater. Trans. A, 1995, 26, p 1553-1570
    • (1995) Metall. Mater. Trans. A , vol.26 , pp. 1553-1570
    • Lee, F.T.1    Major, J.F.2    Samuel, F.H.3
  • 15
    • 18244377986 scopus 로고    scopus 로고
    • Effect of friction stir processing on mechanical properties of the cast aluminum alloys A319 and A356
    • M.L. Santella, T. Engstron, D. Storjohann, and T.Y. Pan, Effect of Friction Stir Processing on Mechanical Properties of the Cast Aluminum Alloys A319 and A356, Scripta Mater., 2005, 53, p 201-206
    • (2005) Scripta Mater. , vol.53 , pp. 201-206
    • Santella, M.L.1    Engstron, T.2    Storjohann, D.3    Pan, T.Y.4
  • 16
    • 0016939376 scopus 로고
    • Le diagramme charge de rupture des alliages d'aluminium
    • M. Drouzy, S. Jacob, and M. Richard, Le Diagramme Charge de Rupture des Alliages d'aluminium, Foundries, 1976, 355, p 139-147
    • (1976) Foundries , vol.355 , pp. 139-147
    • Drouzy, M.1    Jacob, S.2    Richard, M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.