Volumn 69, Issue 8, 2012, Pages 937-953

Effect of processing methods and functional groups on the properties of multi-walled carbon nanotube filled poly(dimethyl siloxane) composites

Author keywords

Electrical conductivity; Mini extruder; Solution mixing; Tensile strength; Thermal analysis

Indexed keywords

ELECTRICAL CONDUCTIVITY; FRACTURE SURFACES; FUNCTIONALIZATION OF NANOTUBES; FUNCTIONALIZED MULTI-WALLED CARBON NANOTUBES; HIGH ASPECT RATIO; INTERFACIAL ADHESIONS; MINI-EXTRUDER; NANOTUBE LENGTHS; POLYDIMETHYLSILOXANE PDMS; PROCESSING METHOD; SCANNING ELECTRON MICROGRAPHS; SOLUTION MIXING;

EID: 84868632652     PISSN: 01700839     EISSN: None     Source Type: Journal    
DOI: 10.1007/s00289-012-0777-z     Document Type: Article
Times cited : (40)

References (29)
  • 1
    • 0342819025 scopus 로고
    • Helical microtubules of graphitic carbon
    • Iijima S (1991) Helical microtubules of graphitic carbon. Nature 354:56-58 (Pubitemid 21896780)
    • (1991) Nature , vol.354 , Issue.6348 , pp. 56-58
    • Iijima, S.1
  • 2
    • 33748700413 scopus 로고    scopus 로고
    • Advances in the science and technology of carbon nanotubes and their
    • DOI 10.1016/S0266-3538(01)00094-X, PII S026635380100094X
    • Thostenson ET, Ren Z, Chou T-W (2001) Advances in the science and technology of carbon nanotubes and their composites: a review. Compos Sci Technol 61(13):1899-1912. doi:10.1016/s0266-3538(01)00094-x (Pubitemid 32956545)
    • (2001) Composites Science and Technology , vol.61 , Issue.13 , pp. 1899-1912
    • Thostenson, E.T.1    Ren, Z.2    Chou, T.-W.3
  • 3
    • 42249109990 scopus 로고    scopus 로고
    • Functionalization of multi-wall carbon nanotubes with silane and its reinforcement on polypropylene composites
    • doi:10.1016/j.compscitech.2008.02.003
    • Zhou Z, Wang S, Lu L, Zhang Y, Zhang Y (2008) Functionalization of multi-wall carbon nanotubes with silane and its reinforcement on polypropylene composites. Compos Sci Technol 68(7-8): 1727-1733. doi:10.1016/j.compscitech. 2008.02.003
    • (2008) Compos Sci Technol , vol.68 , Issue.7-8 , pp. 1727-1733
    • Zhou, Z.1    Wang, S.2    Lu, L.3    Zhang, Y.4    Zhang, Y.5
  • 4
    • 0032800017 scopus 로고    scopus 로고
    • Development of a dispersion process for carbon nanotubes in an epoxy matrix and the resulting electrical properties
    • PII S0032386199001664
    • Sandler J, Shaffer MSP, Prasse T, Bauhofer W, Schulte K, Windle AH (1999) Development of a dispersion process for carbon nanotubes in an epoxy matrix and the resulting electrical properties. Polymer 40(21):5967-5971. doi:10.1016/s0032-3861(99)00166-4 (Pubitemid 29339374)
    • (1999) Polymer , vol.40 , Issue.21 , pp. 5967-5971
    • Sandler, J.1    Shaffer, M.S.P.2    Prasse, T.3    Bauhofer, W.4    Schulte, K.5    Windle, A.H.6
  • 5
    • 76549125925 scopus 로고    scopus 로고
    • Effects of surface-functionalized multi-walled carbon nanotubes on the properties of poly(dimethyl siloxane) nanocomposites
    • doi:10.1016/j.compscitech.2009.12.023
    • Chua TP, Mariatti M, Azizan A, Rashid AA (2010) Effects of surface-functionalized multi-walled carbon nanotubes on the properties of poly(dimethyl siloxane) nanocomposites. Compos Sci Technol 70(4):671-677. doi:10.1016/j.compscitech.2009.12.023
    • (2010) Compos Sci Technol , vol.70 , Issue.4 , pp. 671-677
    • Chua, T.P.1    Mariatti, M.2    Azizan, A.3    Rashid, A.A.4
  • 6
    • 69349099926 scopus 로고    scopus 로고
    • Effect of dispersion state of carbon nanotube on the thermal conductivity of poly(dimethyl siloxane) composites
    • doi: 10.1016/j.cap.2009.06.028
    • Hong J, Lee J, Hong CK, Shim SE (2010) Effect of dispersion state of carbon nanotube on the thermal conductivity of poly(dimethyl siloxane) composites. Curr Appl Phys 10(1):359-363. doi: 10.1016/j.cap.2009.06.028
    • (2010) Curr Appl Phys , vol.10 , Issue.1 , pp. 359-363
    • Hong, J.1    Lee, J.2    Hong, C.K.3    Shim, S.E.4
  • 7
    • 65649112517 scopus 로고    scopus 로고
    • Static and dynamic mechanical properties of polydimethylsiloxane/carbon nanotube nanocomposites
    • doi: 10.1016/j.tsf.2009.03.146
    • Wu C-L, Lin H-C, Hsu J-S, Yip M-C, Fang W (2009) Static and dynamic mechanical properties of polydimethylsiloxane/carbon nanotube nanocomposites. Thin Solid Films 517(17):4895-4901. doi: 10.1016/j.tsf.2009.03.146
    • (2009) Thin Solid Films , vol.517 , Issue.17 , pp. 4895-4901
    • Wu, C.-L.1    Lin, H.-C.2    Hsu, J.-S.3    Yip, M.-C.4    Fang, W.5
  • 8
    • 47249145101 scopus 로고    scopus 로고
    • Mechanical and thermal properties of epoxy nanocomposites reinforced with amino-functionalized multi-walled carbon nanotubes
    • doi:10.1016/j.msea.2008.04.044
    • Chen X, Wang J, Lin M, Zhong W, Feng T, Chen J, Xue F (2008) Mechanical and thermal properties of epoxy nanocomposites reinforced with amino-functionalized multi-walled carbon nanotubes. Mater Sci Eng A 492(1-2):236-242. doi:10.1016/j.msea.2008.04.044
    • (2008) Mater Sci Eng A , vol.492 , Issue.1-2 , pp. 236-242
    • Chen, X.1    Wang, J.2    Lin, M.3    Zhong, W.4    Feng, T.5    Chen, J.6    Xue, F.7
  • 9
    • 64749083253 scopus 로고    scopus 로고
    • Effects of carbon nanotube functionalization on the mechanical and thermal properties of epoxy composites
    • doi:10.1016/j.carbon.2009.02.029
    • Yang K, Gu M, Guo Y, Pan X, Mu G (2009) Effects of carbon nanotube functionalization on the mechanical and thermal properties of epoxy composites. Carbon 47(7):1723-1737. doi:10.1016/j.carbon.2009.02.029
    • (2009) Carbon , vol.47 , Issue.7 , pp. 1723-1737
    • Yang, K.1    Gu, M.2    Guo, Y.3    Pan, X.4    Mu, G.5
  • 10
    • 36048967615 scopus 로고    scopus 로고
    • The extraordinary reinforcing efficiency of single-walled carbon nanotubes in oriented poly(vinyl alcohol) tapes
    • DOI 10.1088/0957-4484/18/45/455709, PII S0957448407545861
    • Wang Z, Ciselli P, Peijs T (2007) The extraordinary reinforcing efficiency of single-walled carbon nanotubes in oriented poly(vinyl alcohol) tapes. Nanotechnology 18(45):455709. doi:10.1088/0957-4484/18/45/455709 (Pubitemid 350093280)
    • (2007) Nanotechnology , vol.18 , Issue.45 , pp. 455709
    • Wang, Z.1    Ciselli, P.2    Peijs, T.3
  • 11
    • 77955275614 scopus 로고    scopus 로고
    • Effective reinforcement of carbon nanotubes in polypropylene matrices
    • doi:10.1002/app.30783
    • Deng H, Bilotti E, Zhang R, Peijs T (2010) Effective reinforcement of carbon nanotubes in polypropylene matrices. J Appl Polym Sci 118(1):30-41. doi:10.1002/app.30783
    • (2010) J Appl Polym Sci , vol.118 , Issue.1 , pp. 30-41
    • Deng, H.1    Bilotti, E.2    Zhang, R.3    Peijs, T.4
  • 12
    • 67349195964 scopus 로고    scopus 로고
    • Effect of chemical functionalization of multi-walled carbon nanotubes with 3-aminopropyltriethoxysilane on mechanical and morphological properties of epoxy nanocomposites
    • Kathi J, Rhee K-Y, Lee JH (2009) Effect of chemical functionalization of multi-walled carbon nanotubes with 3-aminopropyltriethoxysilane on mechanical and morphological properties of epoxy nanocomposites. Compos A 40(6-7):800-809
    • (2009) Compos A , vol.40 , Issue.6-7 , pp. 800-809
    • Kathi, J.1    Rhee, K.-Y.2    Lee, J.H.3
  • 13
    • 0037375618 scopus 로고    scopus 로고
    • Surface properties of fluorinated single-walled carbon nanotubes
    • DOI 10.1016/S0022-1139(02)00316-0, PII S0022113902003160
    • Lee Y (2003) Surface properties of fluorinated single-walled carbon nanotubes. J Fluorine Chem 120(2):99-104. doi:10.1016/s0022-1139(02)00316-0 (Pubitemid 36313036)
    • (2003) Journal of Fluorine Chemistry , vol.120 , Issue.2 , pp. 99-104
    • Lee, Y.S.1    Cho, T.H.2    Lee, B.K.3    Rho, J.S.4    An, K.H.5    Lee, Y.H.6
  • 14
    • 9444288138 scopus 로고    scopus 로고
    • Electrical conductivity of chemically modified multiwalled carbon nanotube/epoxy composites
    • doi: 10.1016/j.carbon.2004.08.015
    • Kim YJ, Shin TS, Choi HD, Kwon JH, Chung Y-C, Yoon HG (2005) Electrical conductivity of chemically modified multiwalled carbon nanotube/epoxy composites. Carbon 43(1):23-30. doi: 10.1016/j.carbon.2004.08.015
    • (2005) Carbon , vol.43 , Issue.1 , pp. 23-30
    • Kim, Y.J.1    Shin, T.S.2    Choi, H.D.3    Kwon, J.H.4    Chung, Y.-C.5    Yoon, H.G.6
  • 15
    • 36048936057 scopus 로고    scopus 로고
    • Correlations between percolation threshold, dispersion state, and aspect ratio of carbon nanotubes
    • DOI 10.1002/adfm.200700065
    • Li J, Ma PC, Chow WS, To CK, Tang BZ, Kim J-K (2007) Correlations between percolation threshold, dispersion state, and aspect ratio of carbon nanotubes. Adv Funct Mater 17(16):3207-3215. doi:10.1002/adfm.200700065 (Pubitemid 350099953)
    • (2007) Advanced Functional Materials , vol.17 , Issue.16 , pp. 3207-3215
    • Li, J.1    Ma, P.C.2    Chow, W.S.3    To, C.K.4    Tang, B.Z.5    Kim, J.-K.6
  • 16
    • 17844366289 scopus 로고    scopus 로고
    • Influence of dispersion states of carbon nanotubes on physical properties of epoxy nanocomposites
    • DOI 10.1016/j.carbon.2005.01.007, PII S0008622305000527
    • Song YS, Youn JR (2005) Influence of dispersion states of carbon nanotubes on physical properties of epoxy nanocomposites. Carbon 43(7):1378-1385. doi:10.1016/j.carbon.2005.01.007 (Pubitemid 40584255)
    • (2005) Carbon , vol.43 , Issue.7 , pp. 1378-1385
    • Song, Y.S.1    Youn, J.R.2
  • 17
    • 75749125302 scopus 로고    scopus 로고
    • Carbon nanotube-polymer composites: Chemistry, processing, mechanical and electrical properties
    • doi: 10.1016/j.progpolymsci.2009.09.003
    • Spitalsky Z, Tasis D, Papagelis K, Galiotis C (2010) Carbon nanotube-polymer composites: chemistry, processing, mechanical and electrical properties. Prog Polym Sci 35(3):357-401. doi: 10.1016/j.progpolymsci.2009.09. 003
    • (2010) Prog Polym Sci , vol.35 , Issue.3 , pp. 357-401
    • Spitalsky, Z.1    Tasis, D.2    Papagelis, K.3    Galiotis, C.4
  • 18
    • 18544384089 scopus 로고    scopus 로고
    • Sonochemical oxidation of multiwalled carbon nanotubes
    • DOI 10.1021/la047268e
    • Xing Y, Li L, Chusuei CC, Hull RV (2005) Sonochemical oxidation of multiwalled carbon nanotubes. Langmuir 21(9):4185-4190. doi:10.1021/la047268e (Pubitemid 40654631)
    • (2005) Langmuir , vol.21 , Issue.9 , pp. 4185-4190
    • Xing, Y.1    Li, L.2    Chusuei, C.C.3    Hull, R.V.4
  • 19
    • 80054730489 scopus 로고    scopus 로고
    • Carbon nanotube-reinforced thermotropic liquid crystal polymer nanocomposites
    • doi:10.3390/ma2041955
    • Kim JY (2009) Carbon nanotube-reinforced thermotropic liquid crystal polymer nanocomposites. Materials 2(4):1955-1974. doi:10.3390/ma2041955
    • (2009) Materials , vol.2 , Issue.4 , pp. 1955-1974
    • Kim, J.Y.1
  • 20
    • 79751476887 scopus 로고    scopus 로고
    • Thermal, mechanical and acoustic damping properties of flexible open-cell polyurethane/multi-walled carbon nanotube foams: Effect of surface functionality of nanotubes
    • Bandarian M, Shojaei A, Rashidi AM (2011) Thermal, mechanical and acoustic damping properties of flexible open-cell polyurethane/multi-walled carbon nanotube foams: effect of surface functionality of nanotubes. Polym Int 60(3):475-482
    • (2011) Polym Int , vol.60 , Issue.3 , pp. 475-482
    • Bandarian, M.1    Shojaei, A.2    Rashidi, A.M.3
  • 21
    • 54249153203 scopus 로고    scopus 로고
    • Flame-retardant-wrapped carbon nanotubes for simultaneously improving the flame retardancy and mechanical properties of polypropylene
    • Song P, Xu L, Guo Z, Zhang Y, Fan Z (2008) Flame-retardant-wrapped carbon nanotubes for simultaneously improving the flame retardancy and mechanical properties of polypropylene. J Mater Chem 18(42):5083-5091
    • (2008) J Mater Chem , vol.18 , Issue.42 , pp. 5083-5091
    • Song, P.1    Xu, L.2    Guo, Z.3    Zhang, Y.4    Fan, Z.5
  • 22
    • 56949102404 scopus 로고    scopus 로고
    • Dispersion and thermal conductivity of carbon nanotube composites
    • doi:10.1016/j.carbon.2008.08.024
    • Wang S, Liang R, Wang B, Zhang C (2009) Dispersion and thermal conductivity of carbon nanotube composites. Carbon 47(1):53-57. doi:10.1016/j.carbon.2008.08.024
    • (2009) Carbon , vol.47 , Issue.1 , pp. 53-57
    • Wang, S.1    Liang, R.2    Wang, B.3    Zhang, C.4
  • 23
    • 0001703564 scopus 로고
    • Percolation theory and electrical conductivity
    • Last BJ, Thouless DJ (1971) Percolation theory and electrical conductivity. Phys Rev Lett 27(25): 1719
    • (1971) Phys Rev Lett , vol.27 , Issue.25 , pp. 1719
    • Last, B.J.1    Thouless, D.J.2
  • 24
    • 77949398377 scopus 로고    scopus 로고
    • Piezoresistive polymer composites based on EPDM and MWNTs for strain sensing applications
    • Ciselli P, Lu L, Busfield JJC, Peijs T (2010) Piezoresistive polymer composites based on EPDM and MWNTs for strain sensing applications. e-Polymers 14
    • (2010) E-Polymers , vol.14
    • Ciselli, P.1    Lu, L.2    Jjc, B.3    Peijs, T.4
  • 25
    • 0043133887 scopus 로고    scopus 로고
    • Effect of the length and the aggregate size of MWNTs on the improvement efficiency of the mechanical and electrical properties of nanocomposites - Experimental investigation
    • doi:10.1016/s1359-835x(03)00140-4
    • Bai J, Allaoui A (2003) Effect of the length and the aggregate size of MWNTs on the improvement efficiency of the mechanical and electrical properties of nanocomposites - experimental investigation. Compos A 34(8):689-694. doi:10.1016/s1359-835x(03)00140-4
    • (2003) Compos A , vol.34 , Issue.8 , pp. 689-694
    • Bai, J.1    Allaoui, A.2
  • 26
    • 33644772468 scopus 로고    scopus 로고
    • Evaluation and identification of electrical and thermal conduction mechanisms in carbon nanotube/epoxy composites
    • DOI 10.1016/j.polymer.2006.01.029, PII S0032386106000474
    • Gojny FH, Wichmann MHG, Fiedler B, Kinloch IA, Bauhofer W, Windle AH, Schulte K (2006) Evaluation and identification of electrical and thermal conduction mechanisms in carbon nanotube/epoxy composites. Polymer 47(6):2036-2045. doi:10.1016/j.polymer.2006.01.029 (Pubitemid 43344380)
    • (2006) Polymer , vol.47 , Issue.6 , pp. 2036-2045
    • Gojny, F.H.1    Wichmann, M.H.G.2    Fiedler, B.3    Kinloch, I.A.4    Bauhofer, W.5    Windle, A.H.6    Schulte, K.7
  • 27
    • 70449587261 scopus 로고    scopus 로고
    • Electrical and dielectric properties of hydroxylated carbon nanotube-elastomer composites
    • doi:10.1021/jp901082c
    • Kohlmeyer RR, Javadi A, Pradhan B, Pilla S, Setyowati K, Chen J, Gong S (2009) Electrical and dielectric properties of hydroxylated carbon nanotube-elastomer composites. J Phys Chem C 113(41):17626-17629. doi:10.1021/jp901082c
    • (2009) J Phys Chem C , vol.113 , Issue.41 , pp. 17626-17629
    • Kohlmeyer, R.R.1    Javadi, A.2    Pradhan, B.3    Pilla, S.4    Setyowati, K.5    Chen, J.6    Gong, S.7
  • 28
    • 65249124061 scopus 로고    scopus 로고
    • Electrical conductivity behavior of chemical functionalized MWCNTs epoxy nanocomposites
    • Sulong AB, Muhamad N, Sahari J, Ramli R, Deros BM, Park J (2009) Electrical conductivity behavior of chemical functionalized MWCNTs epoxy nanocomposites. Eur J Scientific Res 29(1): 13-21
    • (2009) Eur J Scientific Res , vol.29 , Issue.1 , pp. 13-21
    • Sulong, A.B.1    Muhamad, N.2    Sahari, J.3    Ramli, R.4    Deros, B.M.5    Park, J.6
  • 29
    • 33644909888 scopus 로고    scopus 로고
    • Effect of amino-functionalization of multi-walled carbon nanotubes on the dispersion with epoxy resin matrix
    • doi: 10.1002/app.22647
    • Wang J, Fang Z, Gu A, Xu L, Liu F (2006) Effect of amino- functionalization of multi-walled carbon nanotubes on the dispersion with epoxy resin matrix. J Appl Polym Sci 100(1):97-104. doi: 10.1002/app.22647
    • (2006) J Appl Polym Sci , vol.100 , Issue.1 , pp. 97-104
    • Wang, J.1    Fang, Z.2    Gu, A.3    Xu, L.4    Liu, F.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.