Lead-free (Ba 0.7Ca 0.3)TiO 3-Ba(Zr 0.2Ti 0.8)O 3-xwt %CuO ceramics with high piezoelectric coefficient by low-temperature sintering

Author keywords

[No Author keywords available]

Indexed keywords

DISSIPATION FACTORS; ELECTROMECHANICAL COEFFICIENTS; HIGH DIELECTRIC CONSTANTS; LEAD-FREE; LOW-TEMPERATURE SINTERING; PIEZOELECTRIC COEFFICIENT; PIEZOELECTRIC PROPERTY; PURE PEROVSKITE PHASE; SEM IMAGE; SINTERABILITY; SINTERING TEMPERATURES; SOLID-STATE REACTION PROCESS; TIO;

EID: 84863987894     PISSN: 09574522     EISSN: 1573482X     Source Type: Journal    
DOI: 10.1007/s10854-011-0596-2     Document Type: Article