메뉴 건너뛰기




Volumn 59, Issue 2, 2012, Pages 57-62

Effect of the macro-pore structure on the anodic polarization behavior of porous titanium

Author keywords

Anodic polarization; Corrosion resistance; Macro pores; Porosity; Porous titanium; Powder metallurgy; Titanium

Indexed keywords

CORROSION POTENTIALS; DESIGN/METHODOLOGY/APPROACH; ELECTROCHEMICAL CORROSION TESTS; INTERCONNECTED PORES; MACRO-PORES; MICRO-PORE STRUCTURES; NACL SOLUTION; POLARIZATION BEHAVIOR; POROUS TITANIUM; SELF-PASSIVATION; TRANSITION BEHAVIOR;

EID: 84863356244     PISSN: 00035599     EISSN: None     Source Type: Journal    
DOI: 10.1108/00035591211210811     Document Type: Article
Times cited : (4)

References (22)
  • 1
    • 69649106531 scopus 로고    scopus 로고
    • In situ impedance spectroscopy study of the electrochemical corrosion of Ti and Ti-6Al-4V in simulated body fluid at 25°C and 37°C
    • Alves, V.A., Reis, R.Q., Santos, I.C.B., Souza, D.G., Groncalves, T., de, F., Pereira-da-Silva, M.A., Rossi, A. and da Silva, L.A. (2009), "In situ impedance spectroscopy study of the electrochemical corrosion of Ti and Ti-6Al-4V in simulated body fluid at 25°C and 37°C" in Corrosion Science, Vol. 51, No. 10, pp. 2473-82.
    • (2009) Corrosion Science , vol.51 , Issue.10 , pp. 2473-2482
    • Alves, V.A.1    Reis, R.Q.2    Santos, I.C.B.3    Souza, D.G.4    Groncalves, T.5    de, F.6    Pereira-da-Silva, M.A.7    Rossi, A.8    da Silva, L.A.9
  • 2
    • 0037209960 scopus 로고    scopus 로고
    • Corrosion behavior of commercially pure titanium shot blasted with different materials and size of shot particles for dental implant applications
    • Aparicio, C., Javier Gil, F., Foseca, C., Barbosa, M. and Planell, J.A. (2003), "Corrosion behavior of commercially pure titanium shot blasted with different materials and size of shot particles for dental implant applications" in Biomaterials, Vol. 24, No. 2, pp. 263-73.
    • (2003) Biomaterials , vol.24 , Issue.2 , pp. 263-273
    • Aparicio, C.1    Javier Gil, F.2    Foseca, C.3    Barbosa, M.4    Planell, J.A.5
  • 4
    • 0036497708 scopus 로고    scopus 로고
    • Stability of protective oxide films formed on a porous titanium
    • Blackwood, D.J. and Chooi, S.K.M. (2002), "Stability of protective oxide films formed on a porous titanium" in Corrosion Science, Vol. 44, No. 3, pp. 395-405.
    • (2002) Corrosion Science , vol.44 , Issue.3 , pp. 395-405
    • Blackwood, D.J.1    Chooi, S.K.M.2
  • 5
    • 0035772150 scopus 로고    scopus 로고
    • Behavior of porous titanium and catalytically active electrodes based on it in acidic chloride solutions
    • Chviruk, V.P., Zaverach, E.M. and Linyucheva, O.V. (2001), "Behavior of porous titanium and catalytically active electrodes based on it in acidic chloride solutions" in Russian Journal of Electrochemistry, Vol. 37, No. 5, pp. 512-17.
    • (2001) Russian Journal of Electrochemistry , vol.37 , Issue.5 , pp. 512-517
    • Chviruk, V.P.1    Zaverach, E.M.2    Linyucheva, O.V.3
  • 6
    • 61549093771 scopus 로고    scopus 로고
    • The influence of chloride and sulphate ions on the corrosion behavior of Ti and Ti-6Al-4V alloy in oxalic acid
    • Fekry, A.M. (2009), "The influence of chloride and sulphate ions on the corrosion behavior of Ti and Ti-6Al-4V alloy in oxalic acid" in Electrochimica Acta, Vol. 54, No. 12, pp. 3480-9.
    • (2009) Electrochimica Acta , vol.54 , Issue.12 , pp. 3480-3489
    • Fekry, A.M.1
  • 7
    • 79952453576 scopus 로고    scopus 로고
    • The effect of pore structure on the electrical conductivity of Ti
    • Li, B.Q. and Lu, X. (2011), "The effect of pore structure on the electrical conductivity of Ti" in Transport in Porous Media, Vol. 87, No. 1, pp. 179-89.
    • (2011) Transport in Porous Media , vol.87 , Issue.1 , pp. 179-189
    • Li, B.Q.1    Lu, X.2
  • 8
    • 48049124536 scopus 로고    scopus 로고
    • Electronic theoretical study on the corrosion and passivation mechanism of Ti metal
    • Liu, G.L. (2008), "Electronic theoretical study on the corrosion and passivation mechanism of Ti metal" in Acta Physica Sinica, Vol. 57, No. 7, pp. 4441-5.
    • (2008) Acta Physica Sinica , vol.57 , Issue.7 , pp. 4441-4445
    • Liu, G.L.1
  • 9
    • 3943108850 scopus 로고    scopus 로고
    • Some problems on mechanical properties of foamed metals
    • Liu, P.S. (2004), "Some problems on mechanical properties of foamed metals" in Rare Metal Materials and Engineering, Vol. 33, No. 5, pp. 473-7.
    • (2004) Rare Metal Materials and Engineering , vol.33 , Issue.5 , pp. 473-477
    • Liu, P.S.1
  • 11
    • 0031852795 scopus 로고    scopus 로고
    • Review on corrosion performance titanium biomedical materials
    • Mu, Z.Q. and Liang, C.H. (1998), "Review on corrosion performance titanium biomedical materials" in Corrosion Science and Protection Technology, Vol. 10, No. 2, pp. 103-8.
    • (1998) Corrosion Science and Protection Technology , vol.10 , Issue.2 , pp. 103-108
    • Mu, Z.Q.1    Liang, C.H.2
  • 12
    • 0347081829 scopus 로고    scopus 로고
    • An assessment of the instability of Ti and its alloys in acidic environments at elevated temperature
    • Neville, A. and Xu, J. (2001), "An assessment of the instability of Ti and its alloys in acidic environments at elevated temperature" in Journal of Light Metals, Vol. 1, No. 2, pp. 119-26.
    • (2001) Journal of Light Metals , vol.1 , Issue.2 , pp. 119-126
    • Neville, A.1    Xu, J.2
  • 13
    • 33748301939 scopus 로고    scopus 로고
    • Pore throat size and connectivity determine bone and tissue ingrowth into porous implants: Three-dimensional micro-CT based structural analyses of porous bioactive titanium implants
    • Otsuki, B., Takemoto, M., Fujibayashi, S., Neo, M., Kokubo, T. and Nakamura, T. (2006), "Pore throat size and connectivity determine bone and tissue ingrowth into porous implants: three-dimensional micro-CT based structural analyses of porous bioactive titanium implants" in Biomaterials, Vol. 27, No. 35, pp. 5892-900.
    • (2006) Biomaterials , vol.27 , Issue.35 , pp. 5892-5900
    • Otsuki, B.1    Takemoto, M.2    Fujibayashi, S.3    Neo, M.4    Kokubo, T.5    Nakamura, T.6
  • 14
  • 15
    • 33745271072 scopus 로고    scopus 로고
    • Photo-electrochemical properties of oxide semiconductors on porous titanium metal electrodes
    • Sayama, K., Oi, T., Abe, R., Yanagida, M., Sugihara, H. and Iwasaki, Y. (2006), "Photo-electrochemical properties of oxide semiconductors on porous titanium metal electrodes" in Solar Energy Materials and Solar Cells, Vol. 90, No. 15, pp. 2429-37.
    • (2006) Solar Energy Materials and Solar Cells , vol.90 , Issue.15 , pp. 2429-2437
    • Sayama, K.1    Oi, T.2    Abe, R.3    Yanagida, M.4    Sugihara, H.5    Iwasaki, Y.6
  • 16
    • 0027693004 scopus 로고
    • A comparison between the corrosion characteristics of 316 stainless steel, solid titanium and porous titanium
    • Seah, K.H.W. and Chen, X. (1993), "A comparison between the corrosion characteristics of 316 stainless steel, solid titanium and porous titanium" in Corrosion Science, Vol. 34, No. 11, pp. 1841-51.
    • (1993) Corrosion Science , vol.34 , Issue.11 , pp. 1841-1851
    • Seah, K.H.W.1    Chen, X.2
  • 17
    • 0032051708 scopus 로고    scopus 로고
    • The influence of pore morphology on corrosion
    • Seah, K.H.W., Thampuran, R. and Teoh, S.H. (1998), "The influence of pore morphology on corrosion" in Corrosion Science, Vol. 40, Nos 4/5, pp. 547-56.
    • (1998) Corrosion Science , vol.40 , Issue.4-5 , pp. 547-556
    • Seah, K.H.W.1    Thampuran, R.2    Teoh, S.H.3
  • 18
    • 0029360968 scopus 로고
    • A comparison between the corrosion behavior of sintered and unsintered porous titanium
    • Seah, K.H.W., Thampuran, R., Chen, X. and Teoh, S.H. (1995), "A comparison between the corrosion behavior of sintered and unsintered porous titanium" in Corrosion Science, Vol. 37, No. 8, pp. 1330-40.
    • (1995) Corrosion Science , vol.37 , Issue.8 , pp. 1330-1340
    • Seah, K.H.W.1    Thampuran, R.2    Chen, X.3    Teoh, S.H.4
  • 21
    • 34249275999 scopus 로고    scopus 로고
    • Electrochemical generation of hydrogen peroxide using surface area-enhanced Ti-mesh electrodes
    • Yang, K.S., Mul, G. and Moulijn, J.A. (2007), "Electrochemical generation of hydrogen peroxide using surface area-enhanced Ti-mesh electrodes" in Electrochimica Acta, Vol. 52, No. 22, pp. 6304-9.
    • (2007) Electrochimica Acta , vol.52 , Issue.22 , pp. 6304-6309
    • Yang, K.S.1    Mul, G.2    Moulijn, J.A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.