Volumn 197, Issue , 2012, Pages 306-313

Natural graphite tailings as heterogeneous Fenton catalyst for the decolorization of rhodamine B

Author keywords

Graphite tailing; Heterogeneous Fenton process; Rhodamine B

Indexed keywords

BRUNAUER-EMMETT-TELLER METHOD; ENERGY DISPERSIVE SPECTROMETRY; FENTON REACTIONS; HETEROGENEOUS FENTON; INITIAL CONCENTRATION; IRON IONS; MESOPOROUS STRUCTURES; NATURAL GRAPHITE; OPTIMAL CONDITIONS; OPTIMUM PH; PH VALUE; REACTION TEMPERATURE; RHODAMINE B; STIRRING SPEED; TOC REMOVAL; WAVELENGTH SHIFT;

EID: 84863219961     PISSN: 13858947     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.cej.2012.04.108     Document Type: Article
Times cited : (72)

References (41)
  • 1
    • 74449092402 scopus 로고    scopus 로고
    • Decolorization of acid red 1 by Fenton-like process using rice husk ash-based catalyst
    • Daud N.K., Hameed B.H. Decolorization of acid red 1 by Fenton-like process using rice husk ash-based catalyst. J. Hazard Mater. 2010, 176:938-944.
    • (2010) J. Hazard Mater. , vol.176 , pp. 938-944
    • Daud, N.K.1    Hameed, B.H.2
  • 2
    • 77955508825 scopus 로고    scopus 로고
    • Degradation and decolorization of reactive red X-3B aqueous solution by ozone integrated with internal micro-electrolysis
    • Ruan X.C., Liu M.Y., Zeng Q.F., Ding Y.H. Degradation and decolorization of reactive red X-3B aqueous solution by ozone integrated with internal micro-electrolysis. Sep. Purif. Technol. 2010, 74:195-201.
    • (2010) Sep. Purif. Technol. , vol.74 , pp. 195-201
    • Ruan, X.C.1    Liu, M.Y.2    Zeng, Q.F.3    Ding, Y.H.4
  • 3
    • 0030871901 scopus 로고    scopus 로고
    • Ligninase-catalysed decolorization of synthetic dyes
    • Young L., Yu J. Ligninase-catalysed decolorization of synthetic dyes. Water Res. 1997, 31:1187-1193.
    • (1997) Water Res. , vol.31 , pp. 1187-1193
    • Young, L.1    Yu, J.2
  • 4
    • 0033622713 scopus 로고    scopus 로고
    • Photocatalytic degradation of commercial azo dyes
    • Tanaka K., Padermpole K., Hisanaga T. Photocatalytic degradation of commercial azo dyes. Water Res. 2000, 34:327-333.
    • (2000) Water Res. , vol.34 , pp. 327-333
    • Tanaka, K.1    Padermpole, K.2    Hisanaga, T.3
  • 6
    • 80052384461 scopus 로고    scopus 로고
    • A comparison between the efficiency of CdS nanoparticles/zeolite A and CdO/zeolite A as catalysts in photodecolorization of crystal violet
    • Nezamzadeh-Ejhieh A., Banan Z. A comparison between the efficiency of CdS nanoparticles/zeolite A and CdO/zeolite A as catalysts in photodecolorization of crystal violet. Desalination 2011, 279:146-151.
    • (2011) Desalination , vol.279 , pp. 146-151
    • Nezamzadeh-Ejhieh, A.1    Banan, Z.2
  • 8
    • 76749114708 scopus 로고    scopus 로고
    • Iron pillared vermiculite as a heterogeneous photo-Fenton catalyst for photocatalytic degradation of azo dye reactive brilliant orange X-GN
    • Chen Q.Q., Wu P.X., Dang Z., Zhu N.W., Li P., Wu J.H., Wang X.D. Iron pillared vermiculite as a heterogeneous photo-Fenton catalyst for photocatalytic degradation of azo dye reactive brilliant orange X-GN. Sep. Purif. Technol. 2010, 71:315-323.
    • (2010) Sep. Purif. Technol. , vol.71 , pp. 315-323
    • Chen, Q.Q.1    Wu, P.X.2    Dang, Z.3    Zhu, N.W.4    Li, P.5    Wu, J.H.6    Wang, X.D.7
  • 9
    • 36349009364 scopus 로고    scopus 로고
    • Solar degradation of formic acid: temperature effects on the photo-fenton reaction
    • Farias J., Rossetti G.H., Albizzati E.D., Alfano O.M. Solar degradation of formic acid: temperature effects on the photo-fenton reaction. Ind. Eng. Chem. Res. 2007, 46:7580-7586.
    • (2007) Ind. Eng. Chem. Res. , vol.46 , pp. 7580-7586
    • Farias, J.1    Rossetti, G.H.2    Albizzati, E.D.3    Alfano, O.M.4
  • 10
    • 33645749510 scopus 로고    scopus 로고
    • A comparison of Al-Fe and Zr-Fe pillared clays for catalytic wet peroxide oxidation
    • Molina C.B., Casas J.A., Zazo J.A., Rodriguez J.J. A comparison of Al-Fe and Zr-Fe pillared clays for catalytic wet peroxide oxidation. Chem. Eng. J. 2006, 118:29-35.
    • (2006) Chem. Eng. J. , vol.118 , pp. 29-35
    • Molina, C.B.1    Casas, J.A.2    Zazo, J.A.3    Rodriguez, J.J.4
  • 11
    • 0036170131 scopus 로고    scopus 로고
    • Pre-oxidation and coagulation of textile wastewater by the Fenton process
    • Kang S.F., Liao C.H., Chen M.C. Pre-oxidation and coagulation of textile wastewater by the Fenton process. Chemosphere 2002, 46:923-928.
    • (2002) Chemosphere , vol.46 , pp. 923-928
    • Kang, S.F.1    Liao, C.H.2    Chen, M.C.3
  • 14
    • 79551686098 scopus 로고    scopus 로고
    • Acid Red 1 dye decolorization by heterogeneous Fenton-like reaction using Fe/kaolin catalyst
    • Daud N.K., Hameed B.H. Acid Red 1 dye decolorization by heterogeneous Fenton-like reaction using Fe/kaolin catalyst. Desalination 2011, 269:291-293.
    • (2011) Desalination , vol.269 , pp. 291-293
    • Daud, N.K.1    Hameed, B.H.2
  • 15
    • 79551567337 scopus 로고    scopus 로고
    • Rapid decolourization and mineralization of the azo dye CI Acid Red 14 by heterogeneous Fenton reaction
    • Idel-aouad R., Valiente M., Yaacoubi A., Tanouti B., Lopez-Mesas M. Rapid decolourization and mineralization of the azo dye CI Acid Red 14 by heterogeneous Fenton reaction. J. Hazard. Mater. 2011, 186:745-750.
    • (2011) J. Hazard. Mater. , vol.186 , pp. 745-750
    • Idel-aouad, R.1    Valiente, M.2    Yaacoubi, A.3    Tanouti, B.4    Lopez-Mesas, M.5
  • 16
    • 72249112169 scopus 로고    scopus 로고
    • A silica-supported iron oxide catalyst capable of activating hydrogen peroxide at neutral pH values
    • Pham A.L.T., Lee C., Doyle F.M., Sedlak D.L. A silica-supported iron oxide catalyst capable of activating hydrogen peroxide at neutral pH values. Environ. Sci. Technol. 2009, 43:8930-8935.
    • (2009) Environ. Sci. Technol. , vol.43 , pp. 8930-8935
    • Pham, A.L.T.1    Lee, C.2    Doyle, F.M.3    Sedlak, D.L.4
  • 17
    • 67349110450 scopus 로고    scopus 로고
    • Suhas, application of low-cost adsorbents for dye removal - a review
    • Gupta V.K. Suhas, application of low-cost adsorbents for dye removal - a review. J. Environ. Manage. 2009, 90:2313-2342.
    • (2009) J. Environ. Manage. , vol.90 , pp. 2313-2342
    • Gupta, V.K.1
  • 18
    • 34548455872 scopus 로고    scopus 로고
    • Degradation of DMSO by ozone-based advanced oxidation processes
    • Wu J.J., Muruganandham M., Chen S.H. Degradation of DMSO by ozone-based advanced oxidation processes. J. Hazard. Mater. 2007, 149:218-225.
    • (2007) J. Hazard. Mater. , vol.149 , pp. 218-225
    • Wu, J.J.1    Muruganandham, M.2    Chen, S.H.3
  • 19
    • 77954212600 scopus 로고    scopus 로고
    • Novel NaY zeolite-supported nanoscale zero-valent iron as an efficient heterogeneous Fenton catalyst
    • Zhou M.H., Wang W., Mao Q.O., Yue J.J., Wang X. Novel NaY zeolite-supported nanoscale zero-valent iron as an efficient heterogeneous Fenton catalyst. Catal. Commun. 2010, 11:937-941.
    • (2010) Catal. Commun. , vol.11 , pp. 937-941
    • Zhou, M.H.1    Wang, W.2    Mao, Q.O.3    Yue, J.J.4    Wang, X.5
  • 20
    • 38349111660 scopus 로고    scopus 로고
    • Photoinduced degradation of orange II on different iron (Hydr) oxides in aqueous suspension: rate enhancement on addition of hydrogen peroxide, silver nitrate, and sodium fluoride
    • Xu Y.M., Du W.P., Wang Y.S. Photoinduced degradation of orange II on different iron (Hydr) oxides in aqueous suspension: rate enhancement on addition of hydrogen peroxide, silver nitrate, and sodium fluoride. Langmuir 2008, 24:175-181.
    • (2008) Langmuir , vol.24 , pp. 175-181
    • Xu, Y.M.1    Du, W.P.2    Wang, Y.S.3
  • 21
    • 77954535790 scopus 로고    scopus 로고
    • The decolorization of Acid Orange II in non-homogeneous Fenton reaction catalyzed by natural vanadium-titanium magnetite
    • He H.P., Liang X.L., Zhong Y.H., Zhu S.Y., Zhu J.X., Yuan P., Zhang J. The decolorization of Acid Orange II in non-homogeneous Fenton reaction catalyzed by natural vanadium-titanium magnetite. J. Hazard. Mater. 2010, 181:112-120.
    • (2010) J. Hazard. Mater. , vol.181 , pp. 112-120
    • He, H.P.1    Liang, X.L.2    Zhong, Y.H.3    Zhu, S.Y.4    Zhu, J.X.5    Yuan, P.6    Zhang, J.7
  • 22
    • 41349117368 scopus 로고    scopus 로고
    • Electro-Fenton treatment of dye solution containing Orange. II: Influence of operational parameters
    • Daneshvar N., Aber S., Vatanpour V., Rasoulifard M.H. Electro-Fenton treatment of dye solution containing Orange. II: Influence of operational parameters. J. Electroanal. Chem. 2008, 615:165-174.
    • (2008) J. Electroanal. Chem. , vol.615 , pp. 165-174
    • Daneshvar, N.1    Aber, S.2    Vatanpour, V.3    Rasoulifard, M.H.4
  • 23
    • 79952446610 scopus 로고    scopus 로고
    • Heterogeneous photodecolorization of Eriochrome Black T using Ni/P zeolite catalyst
    • Nezamzadeh-Ejhieh A., Khorsandi M. Heterogeneous photodecolorization of Eriochrome Black T using Ni/P zeolite catalyst. Desalination 2010, 262:79-85.
    • (2010) Desalination , vol.262 , pp. 79-85
    • Nezamzadeh-Ejhieh, A.1    Khorsandi, M.2
  • 24
    • 2442549395 scopus 로고    scopus 로고
    • Effect of Fenton-like oxidation on enhanced oxidative degradation of para-chlorobenzoic acid by ultrasonic irradiation
    • Neppolian B., Park J.S., Choi H. Effect of Fenton-like oxidation on enhanced oxidative degradation of para-chlorobenzoic acid by ultrasonic irradiation. Ultrason. Sonochem. 2004, 11:273-279.
    • (2004) Ultrason. Sonochem. , vol.11 , pp. 273-279
    • Neppolian, B.1    Park, J.S.2    Choi, H.3
  • 25
    • 48649096053 scopus 로고    scopus 로고
    • Homogeneus ferrioxalate-assisted solar photo-Fenton degradation of Orange II aqueous solutions
    • Monteagudo J.M., Duran A., Lopez-Almodovar C. Homogeneus ferrioxalate-assisted solar photo-Fenton degradation of Orange II aqueous solutions. Appl. Catal. B-Environ. 2008, 83:46-55.
    • (2008) Appl. Catal. B-Environ. , vol.83 , pp. 46-55
    • Monteagudo, J.M.1    Duran, A.2    Lopez-Almodovar, C.3
  • 26
    • 42649124034 scopus 로고    scopus 로고
    • Mineralization of bisphenol A (BPA) by anodic oxidation with boron-doped diamond (BDD) electrode
    • Murugananthan M., Yoshihara S., Rakuma T., Shirakashi T. Mineralization of bisphenol A (BPA) by anodic oxidation with boron-doped diamond (BDD) electrode. J. Hazard. Mater. 2008, 154:213-220.
    • (2008) J. Hazard. Mater. , vol.154 , pp. 213-220
    • Murugananthan, M.1    Yoshihara, S.2    Rakuma, T.3    Shirakashi, T.4
  • 28
    • 74449087015 scopus 로고    scopus 로고
    • Photodecolorization of Eriochrome Black T using NiS-P zeolite as a heterogeneous catalyst
    • Ejhieha A.N., Khorsandi M. Photodecolorization of Eriochrome Black T using NiS-P zeolite as a heterogeneous catalyst. J. Hazard. Mater. 2010, 176:629-637.
    • (2010) J. Hazard. Mater. , vol.176 , pp. 629-637
    • Ejhieha, A.N.1    Khorsandi, M.2
  • 29
    • 52049101582 scopus 로고    scopus 로고
    • Degradation of Acid Blue 74 using Fe-ZSM5 zeolite as a heterogeneous photo-Fenton catalyst
    • Aleboyeh A., Kasiri M.B., Aleboyeh H. Degradation of Acid Blue 74 using Fe-ZSM5 zeolite as a heterogeneous photo-Fenton catalyst. Appl. Catal. B-Environ. 2008, 84:9-15.
    • (2008) Appl. Catal. B-Environ. , vol.84 , pp. 9-15
    • Aleboyeh, A.1    Kasiri, M.B.2    Aleboyeh, H.3
  • 31
    • 18144415440 scopus 로고    scopus 로고
    • Iron(II)-catalyzed enhancement of ultrasonic-induced degradation of diethylstilbestrol (DES)
    • Ben Abderrazik N., Azmani A., R'kiek C., Song W.H., O'Shea K.E. Iron(II)-catalyzed enhancement of ultrasonic-induced degradation of diethylstilbestrol (DES). Catal. Today 2005, 101:369-373.
    • (2005) Catal. Today , vol.101 , pp. 369-373
    • Ben Abderrazik, N.1    Azmani, A.2    R'kiek, C.3    Song, W.H.4    O'Shea, K.E.5
  • 32
    • 10644250849 scopus 로고    scopus 로고
    • Oxidation kinetics and effect of pH on the degradation of MTBE with Fenton reagent
    • Burbano A.A., Dionysiou D.D., Suidan M.T., Richardson T.L. Oxidation kinetics and effect of pH on the degradation of MTBE with Fenton reagent. Water Res. 2005, 39:107-118.
    • (2005) Water Res. , vol.39 , pp. 107-118
    • Burbano, A.A.1    Dionysiou, D.D.2    Suidan, M.T.3    Richardson, T.L.4
  • 33
    • 77958016983 scopus 로고    scopus 로고
    • Solar photodecolorization of methylene blue by CuO/X zeolite as a heterogeneous catalyst
    • Nezamzadeh-Ejhieh A., Hushmandrad S. Solar photodecolorization of methylene blue by CuO/X zeolite as a heterogeneous catalyst. Appl. Catal. a-Gen. 2010, 388:149-159.
    • (2010) Appl. Catal. a-Gen. , vol.388 , pp. 149-159
    • Nezamzadeh-Ejhieh, A.1    Hushmandrad, S.2
  • 34
    • 71749118976 scopus 로고    scopus 로고
    • Degradation of CI Acid Orange 7 by ultrasound enhanced heterogeneous Fenton-like process
    • Zhang H., Fu H., Zhang D.B. Degradation of CI Acid Orange 7 by ultrasound enhanced heterogeneous Fenton-like process. J. Hazard. Mater. 2009, 172:654-660.
    • (2009) J. Hazard. Mater. , vol.172 , pp. 654-660
    • Zhang, H.1    Fu, H.2    Zhang, D.B.3
  • 35
    • 26844535467 scopus 로고    scopus 로고
    • Experimental design to optimize the degradation of the synthetic dye Orange II using Fenton's reagent
    • Ramirez J.H., Costa C.A., Madeira L.M. Experimental design to optimize the degradation of the synthetic dye Orange II using Fenton's reagent. Catal. Today 2005, 107-08:68-76.
    • (2005) Catal. Today , pp. 68-76
    • Ramirez, J.H.1    Costa, C.A.2    Madeira, L.M.3
  • 36
    • 83255185124 scopus 로고    scopus 로고
    • Sunlight assisted photodecolorization of crystal violet catalyzed by CdS nanoparticles embedded on zeolite A
    • Nezamzadeh-Ejhieh A., Banan Z. Sunlight assisted photodecolorization of crystal violet catalyzed by CdS nanoparticles embedded on zeolite A. Desalination 2012, 284:157-166.
    • (2012) Desalination , vol.284 , pp. 157-166
    • Nezamzadeh-Ejhieh, A.1    Banan, Z.2
  • 37
    • 46449110643 scopus 로고    scopus 로고
    • The decoloration and mineralization of azo dye CI Acid Red 14 by sonochemical process: Rate improvement via Fenton's reactions
    • Xu H., Lin J.J., Zhao X.S., Liu D., Yu Z.G., Zhang Y. The decoloration and mineralization of azo dye CI Acid Red 14 by sonochemical process: Rate improvement via Fenton's reactions. J. Hazard. Mater. 2008, 157:541-546.
    • (2008) J. Hazard. Mater. , vol.157 , pp. 541-546
    • Xu, H.1    Lin, J.J.2    Zhao, X.S.3    Liu, D.4    Yu, Z.G.5    Zhang, Y.6


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.