Volumn 95, Issue 3, 2012, Pages 859-861

Novel sialon-based ceramics toughened by ferro-molybdenum alloy

Author keywords

[No Author keywords available]

Indexed keywords

ALLOY PARTICLES; CERAMIC COMPOSITES; CRACK BRIDGING; CRACK DEFLECTIONS; CRACK PROPAGATION BEHAVIOR; LOW TEMPERATURES; SECOND PHASE PARTICLES; SIALON CERAMICS; TOUGHENING MECHANISMS;

EID: 84862783017     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2011.05051.x     Document Type: Article
Times cited : (28)

References (25)
  • 1
    • 0002890750 scopus 로고
    • Ceramics Based on the Si-Al-O-N and Relates Systems
    • K. H. Jack, and, W. I. Wilson, " Ceramics Based on the Si-Al-O-N and Relates Systems," Nat. Phys. Sci., 238, 28-9 (1972).
    • (1972) Nat. Phys. Sci. , vol.238 , pp. 28-29
    • Jack, K.H.1    Wilson, W.I.2
  • 3
    • 33751500834 scopus 로고
    • Alpha'-Sialon Ceramics: A Review
    • G. Z. Cao, and, R. Metselaar, " Alpha'-Sialon Ceramics: A Review," Chem. Mater., 3, 242-52 (1991).
    • (1991) Chem. Mater. , vol.3 , pp. 242-252
    • Cao, G.Z.1    Metselaar, R.2
  • 4
    • 37049181852 scopus 로고
    • New Materials and Composites
    • W. B. Hilling, " New Materials and Composites," Science, 191, 733-9 (1976).
    • (1976) Science , vol.191 , pp. 733-739
    • Hilling, W.B.1
  • 5
    • 0004524545 scopus 로고
    • High-Temperature Structural Ceramics
    • R. N. Katz, " High-Temperature Structural Ceramics," Science, 208, 841-7 (1980).
    • (1980) Science , vol.208 , pp. 841-847
    • Katz, R.N.1
  • 6
    • 0030671549 scopus 로고    scopus 로고
    • 4 with a whisker-like microstructure
    • DOI 10.1038/39542
    • 4 with a Whisker-Like Microstructure," Nature, 389, 701-4 (1997). (Pubitemid 27458950)
    • (1997) Nature , vol.389 , Issue.6652 , pp. 701-704
    • Chen, I.-W.1    Rosenflanz, A.2
  • 7
    • 0037118057 scopus 로고    scopus 로고
    • Formation of tough interlocking microstuctures in silicon nitride ceramics by dynamic ripening
    • DOI 10.1038/417266a
    • Z.-J. Shen, Z. Zhao, H. Peng, and, M. Nygren, " Formation of Tough Interlocking Microstructures in Silicon Nitride Ceramics by Dynamic Ripening," Nature, 417, 266-9 (2002). (Pubitemid 34534704)
    • (2002) Nature , vol.417 , Issue.6886 , pp. 266-269
    • Shen, Z.1    Zhao, Z.2    Peng, H.3    Nygren, M.4
  • 8
    • 0036132937 scopus 로고    scopus 로고
    • The effect of processing conditions, amount of additives and composition on the microstructures and mechanical properties of α-SiAlON ceramics
    • DOI 10.1016/S0955-2219(01)00237-0, PII S0955221901002370
    • S. Kurama, M. Herrmann, and, H. Mandal, " The Effect of Processing Conditions, Amount of Additives and Composition on the Microstructures and Mechanical Properties of α-SiAlON Ceramics," J. Eur. Ceram. Soc., 22, 109-19 (2002). (Pubitemid 33122366)
    • (2002) Journal of the European Ceramic Society , vol.22 , Issue.1 , pp. 109-119
    • Kurama, S.1    Herrmann, M.2    Mandal, H.3
  • 9
    • 33750498923 scopus 로고    scopus 로고
    • Pressureless sintered self-reinforced Y-α-SiAlON ceramics
    • DOI 10.1016/j.jeurceramsoc.2006.04.185, PII S0955221906004067
    • C.-R. Zhou, Z.-B. Yu, and, V. D. Krstic, " Pressureless Sintered Self-Reinforced Y-α-SiAlON Ceramics," J. Eur. Ceram. Soc., 27, 437-43 (2007). (Pubitemid 44660800)
    • (2007) Journal of the European Ceramic Society , vol.27 , Issue.1 , pp. 437-443
    • Zhou, C.R.1    Yu, Z.B.2    Krstic, V.D.3
  • 10
    • 0346306162 scopus 로고    scopus 로고
    • Effect of the Amount of Additives and Post-Heat Treatment on the Microstructure and Mechanical Properties of Yttrium-α-Sialon Ceramics
    • F. Ye, M. J. Hoffmann, S. Holzer, Y. Zhou, and, M. Iwasa, " Effect of the Amount of Additives and Post-Heat Treatment on the Microstructure and Mechanical Properties of Yttrium-α-Sialon Ceramics," J. Am. Ceram. Soc., 86, 2136-42 (2003).
    • (2003) J. Am. Ceram. Soc. , vol.86 , pp. 2136-2142
    • Ye, F.1    Hoffmann, M.J.2    Holzer, S.3    Zhou, Y.4    Iwasa, M.5
  • 11
    • 34248398419 scopus 로고    scopus 로고
    • Lower-temperature hot-pressed Dy-α-sialon ceramics with an LiF additive
    • DOI 10.1111/j.1551-2916.2007.01558.x
    • J.-M. Xue, Q. Liu, and, L.-H. Gui, " Lower-Temperature Hot-Pressed Dy-a-Sialon Ceramics with a LiF Additive," J. Am. Ceram. Soc., 90, 1623-5 (2007). (Pubitemid 46743833)
    • (2007) Journal of the American Ceramic Society , vol.90 , Issue.5 , pp. 1623-1625
    • Xue, J.1    Liu, Q.2    Gui, L.3
  • 14
    • 27744547568 scopus 로고    scopus 로고
    • Preparation of sialon-transition metal silicide composites
    • DOI 10.1016/j.jeurceramsoc.2004.10.014, PII S0955221904004546
    • W.-W. Chen, Y.-B. Cheng, and, W.-H. Tuan, " Preparation of Sialon-Transition Metal Silicide Composites," J. Am. Ceram. Soc., 26, 193-9 (2006). (Pubitemid 41613323)
    • (2006) Journal of the European Ceramic Society , vol.26 , Issue.1-2 , pp. 193-199
    • Chen, W.-W.1    Cheng, Y.-B.2    Tuan, W.-H.3
  • 15
    • 84862798861 scopus 로고    scopus 로고
    • High-Performance SiC-Fibre Reinforced β-Sialon CMCs Prepared from Heat-Treated Nicalon Fibres
    • A. Demir, and, D. P. Thompson, " High-Performance SiC-Fibre Reinforced β-Sialon CMCs Prepared from Heat-Treated Nicalon Fibres," J. Eur. Ceram. Soc., 26, 193-9 (2006).
    • (2006) J. Eur. Ceram. Soc. , vol.26 , pp. 193-199
    • Demir, A.1    Thompson, D.P.2
  • 16
    • 0036466698 scopus 로고    scopus 로고
    • 2 particles in strengthening and toughening Li-α-sialon composites
    • DOI 10.1016/S0955-2219(01)00262-X, PII S095522190100262X
    • 2 Particles in Strengthening and Toughening Li-α-Sialon Composites," J. Eur. Ceram. Soc., 22, 225-35 (2002). (Pubitemid 33119418)
    • (2002) Journal of the European Ceramic Society , vol.22 , Issue.2 , pp. 225-235
    • Yu, Z.B.1    Thompson, D.P.2    Bhatti, A.R.3
  • 17
    • 0343090953 scopus 로고    scopus 로고
    • 3/Mo composite
    • DOI 10.1016/S1359-6454(99)00349-3
    • 3/Mo Composite," Acta Mater., 48, 985-92 (2000). (Pubitemid 30563200)
    • (2000) Acta Materialia , vol.48 , Issue.4 , pp. 985-992
    • Sbaizero, O.1    Pezzotti, G.2
  • 18
    • 0037465010 scopus 로고    scopus 로고
    • Influence of molybdenum particles on thermal shock resistance of alumina matrix ceramics
    • DOI 10.1016/S0921-5093(02)00370-2, PII S0921509302003702
    • O. Sbaizero, and, G. Pezzotti, " Influence of Molybdenum Particles on Thermal Shock Resistance of Alumina Matrix Ceramics," Mater. Sci. Eng. A, 343, 273-81 (2003). (Pubitemid 36029448)
    • (2003) Materials Science and Engineering A , vol.343 , Issue.1-2 , pp. 273-281
    • Sbaizero, O.1    Pezzotti, G.2
  • 19
    • 0037292148 scopus 로고    scopus 로고
    • Electrical conductivity of an insulator matrix (alumina) and conductor particle (molybdenum) composites
    • DOI 10.1016/S0955-2219(02)00185-1, PII S0955221902001851
    • S. Hussain, I. Barbariol, S. Roitti, and, O. Sbaizero, " Electrical Conductivity of an Insulator Matrix (Alumina) and Conductor Particle (Molybdenum) Composites," J. Eur. Ceram. Soc., 23, 315-21 (2003). (Pubitemid 36021913)
    • (2003) Journal of the European Ceramic Society , vol.23 , Issue.2 , pp. 315-321
    • Hussain, S.1    Barbariol, I.2    Roitti, S.3    Sbaizero, O.4
  • 20
    • 0036883866 scopus 로고    scopus 로고
    • Toughening of alumina/zirconia ceramic composites with silver particles
    • DOI 10.1016/S0955-2219(02)00031-6, PII S0955221902000316
    • J. Lalande, S. Scheppokat, R. Janssen, and, N. Claussen, " Toughening of Alumina/Zirconia Ceramic Composites with Silver Particles," J. Eur. Ceram. Soc., 22, 2165-71 (2002). (Pubitemid 35016043)
    • (2002) Journal of the European Ceramic Society , vol.22 , Issue.13 , pp. 2165-2171
    • Lalande, J.1    Scheppokat, S.2    Janssen, R.3    Claussen, N.4
  • 22
    • 0038713932 scopus 로고    scopus 로고
    • Crack bridging and trapping mechanisms used to toughen brittle matrix composite
    • DOI 10.1016/S0167-8442(03)00032-6
    • M. Kotoul, and, J. Vrbka, " Crack Bridging and Trapping Mechanisms Used to Toughen Brittle Matrix Composite," Theor. Appl. Fract. Mec., 40, 23-44 (2003). (Pubitemid 36873010)
    • (2003) Theoretical and Applied Fracture Mechanics , vol.40 , Issue.1 , pp. 23-44
    • Kotoul, M.1    Vrbka, J.2
  • 23
    • 0018479776 scopus 로고
    • Fracture of a Brittle Particulate Composite
    • D. J. Green, P. S. Nicholson, and, J. D. Embury, " Fracture of a Brittle Particulate Composite," J. Mater. Sci., 14, 1413-20 (1979).
    • (1979) J. Mater. Sci. , vol.14 , pp. 1413-1420
    • Green, D.J.1    Nicholson, P.S.2    Embury, J.D.3
  • 24
    • 0000357002 scopus 로고
    • The Phenomena of Rupture and Flow in Solids
    • A. A. Griffith, " The Phenomena of Rupture and Flow in Solids," Phil. Trans. R. Soc. A, 221, 163-98 (1920).
    • (1920) Phil. Trans. R. Soc. A , vol.221 , pp. 163-198
    • Griffith, A.A.1
  • 25
    • 0035311137 scopus 로고    scopus 로고
    • Ambient to high temperature fracture toughness and fatigue-crack propagation behavior in a Mo - 12Si - 8.5B (at.%) intermetallic
    • DOI 10.1016/S0966-9795(01)00008-5, PII S0966979501000085
    • H. Choe, D. Chen, J. H. Schneibel, and, R. O. Ritchie, " Ambient to High Temperature Fracture Toughness and Fatigue-Crack Propagation Behavior in a Mo-12Si-8.5B (at.%) Intermetallic," Intermetallics, 9, 319-29 (2001). (Pubitemid 32335330)
    • (2001) Intermetallics , vol.9 , Issue.4 , pp. 319-329
    • Choe, H.1    Chen, D.2    Schneibel, J.H.3    Ritchie, R.O.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.