In situ formation of oxidation resistant refractory coatings on SiC-reinforced ZrB 2 ultra high temperature ceramics

Author keywords

[No Author keywords available]

Indexed keywords

AMORPHOUS SILICATES; CRYSTALLINE OXIDES; DENSE LAYER; IN-SITU FORMATIONS; IN-SITU OXIDATION; INTERMEDIATE LAYERS; LEADING EDGE; OXIDATION RESISTANT; REFRACTORY COATINGS; SOLID OXIDATION; STATIC AIR; ULTRA-HIGH-TEMPERATURE CERAMICS;

EID: 84862777675     PISSN: 00027820     EISSN: 15512916     Source Type: Journal    
DOI: 10.1111/j.1551-2916.2011.05032.x     Document Type: Article
Times cited : (73)

References (42)
  • 2
    • 60649090599 scopus 로고    scopus 로고
    • 2-Based Composites and Their Mechanical and Physical Properties: A Review
    • 2-Based Composites and Their Mechanical and Physical Properties: A Review," J. Eur. Ceram. Soc., 29 [ 6 ] 995-1011 (2009).
    • (2009) J. Eur. Ceram. Soc. , vol.29 , Issue.6 , pp. 995-1011
    • Guo, S.Q.1
  • 4
    • 14644400504 scopus 로고    scopus 로고
    • Aerothermodynamic Study of UHTC-Based Thermal Protection Systems
    • R. Savino, M. D. Fumo, D. Paterna, and, M. Serpico, " Aerothermodynamic Study of UHTC-Based Thermal Protection Systems," Aerosp. Sci. Technol., 9 [ 2 ] 151-60 (2005).
    • (2005) Aerosp. Sci. Technol. , vol.9 , Issue.2 , pp. 151-160
    • Savino, R.1    Fumo, M.D.2    Paterna, D.3    Serpico, M.4
  • 5
    • 0033323434 scopus 로고    scopus 로고
    • Mechanical, Thermal, and Oxidation Properties of Refractory Hafnium and Zirconium Compounds
    • M. M. Opeka, I. G. Talmy, E. J. Wuchina, J. A. Zaykoski, and, S. J. Causey, " Mechanical, Thermal, and Oxidation Properties of Refractory Hafnium and Zirconium Compounds," J. Eur. Ceram. Soc., 19 [ 13-14 ] 2405-14 (1999).
    • (1999) J. Eur. Ceram. Soc. , vol.19 , Issue.13-14 , pp. 2405-2414
    • Opeka, M.M.1    Talmy, I.G.2    Wuchina, E.J.3    Zaykoski, J.A.4    Causey, S.J.5
  • 9
    • 84963784490 scopus 로고
    • 2 in Temperature Range of 800°C to 1500°C
    • 2 in Temperature Range of 800°C to 1500°C," J. Electrochem. Soc., 118 [ 7 ] 1195-9 (1971).
    • (1971) J. Electrochem. Soc. , vol.118 , Issue.7 , pp. 1195-1199
    • Tripp, W.C.1    Graham, H.C.2
  • 11
    • 60849108043 scopus 로고    scopus 로고
    • 2-SiC: Influence of SiC Content on Solid and Liquid Oxide Phase Formation
    • 2-SiC: Influence of SiC Content on Solid and Liquid Oxide Phase Formation," J. Am. Ceram. Soc., 92 [ 2 ] 481-6 (2009).
    • (2009) J. Am. Ceram. Soc. , vol.92 , Issue.2 , pp. 481-486
    • Karlsdottir, S.N.1    Halloran, J.W.2
  • 12
    • 33748936677 scopus 로고    scopus 로고
    • Oxidation of Zirconium Diboride-Silicon Carbide at 1500°C at a Low Partial Pressure of Oxygen
    • A. Rezaie, W. G. Fahrenholtz, and, G. E. Hilmas, " Oxidation of Zirconium Diboride-Silicon Carbide at 1500°C at a Low Partial Pressure of Oxygen," J. Am. Ceram. Soc., 89 [ 10 ] 3240-5 (2006).
    • (2006) J. Am. Ceram. Soc. , vol.89 , Issue.10 , pp. 3240-3245
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 13
    • 34547755179 scopus 로고    scopus 로고
    • Oxidation Behavior of Zirconium Diboride-Silicon Carbide at 1800°C
    • P. Hu, X. H. Zhang, and, S. H. Meng, " Oxidation Behavior of Zirconium Diboride-Silicon Carbide at 1800°C," Scr. Mater., 57 [ 9 ] 825-8 (2007).
    • (2007) Scr. Mater. , vol.57 , Issue.9 , pp. 825-828
    • Hu, P.1    Zhang, X.H.2    Meng, S.H.3
  • 14
    • 69649095305 scopus 로고    scopus 로고
    • Oxidation Behavior of Zirconium Diboride Silicon Carbide Produced by the Spark Plasma Sintering Method
    • C. M. Carney, P. Mogilvesky, and, T. A. Parthasarathy, " Oxidation Behavior of Zirconium Diboride Silicon Carbide Produced by the Spark Plasma Sintering Method," J. Am. Ceram. Soc., 92 [ 9 ] 2046-52 (2009).
    • (2009) J. Am. Ceram. Soc. , vol.92 , Issue.9 , pp. 2046-2052
    • Carney, C.M.1    Mogilvesky, P.2    Parthasarathy, T.A.3
  • 15
    • 0029656765 scopus 로고    scopus 로고
    • Determination of the Active-to-Passive Transition in the Oxidation of Silicon Carbide in Standard and Microwave Excited Air
    • M. J. H. Balat, " Determination of the Active-to-Passive Transition in the Oxidation of Silicon Carbide in Standard and Microwave Excited Air," J. Eur. Ceram. Soc., 16, 55-62 (1996).
    • (1996) J. Eur. Ceram. Soc. , vol.16 , pp. 55-62
    • Balat, M.J.H.1
  • 17
    • 33846372666 scopus 로고    scopus 로고
    • Evolution of Structure during the Oxidation of Zirconium Diboride-Silicon Carbide in Air up to 1500°C
    • A. Rezaie, W. G. Fahrenholtz, and, G. E. Hilmas, " Evolution of Structure During the Oxidation of Zirconium Diboride-Silicon Carbide in Air up to 1500°C," J. Eur. Ceram. Soc., 27 [ 6 ] 2495-501 (2007).
    • (2007) J. Eur. Ceram. Soc. , vol.27 , Issue.6 , pp. 2495-2501
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 18
    • 66949162633 scopus 로고    scopus 로고
    • 2-15 vol% SiC Composites during Oxidation: Evolution with Time and Temperature
    • 2-15 vol% SiC Composites During Oxidation: Evolution with Time and Temperature," J. Am. Ceram. Soc., 92 [ 6 ] 1328-32 (2009).
    • (2009) J. Am. Ceram. Soc. , vol.92 , Issue.6 , pp. 1328-1332
    • Karlsdottir, S.N.1    Halloran, J.W.2
  • 19
    • 56749150324 scopus 로고    scopus 로고
    • Formation of Oxide Scales on Zirconium Diboride-Silicon Carbide Composites during Oxidation: Relation of Subscale Recession to Liquid Oxide Flow
    • S. N. Karlsdottir, and, J. W. Halloran, " Formation of Oxide Scales on Zirconium Diboride-Silicon Carbide Composites During Oxidation: Relation of Subscale Recession to Liquid Oxide Flow," J. Am. Ceram. Soc., 91 [ 11 ] 3652-8 (2008).
    • (2008) J. Am. Ceram. Soc. , vol.91 , Issue.11 , pp. 3652-3658
    • Karlsdottir, S.N.1    Halloran, J.W.2
  • 21
    • 38049178364 scopus 로고    scopus 로고
    • 2/SiC as a Protective Coating for 2D C-f/SiC Composites: Effect of High Temperature Oxidation on Mechanical Properties
    • 2/SiC as a Protective Coating for 2D C-f/SiC Composites: Effect of High Temperature Oxidation on Mechanical Properties," Surf. Coat. Technol., 202 [ 10 ] 2059-67 (2008).
    • (2008) Surf. Coat. Technol. , vol.202 , Issue.10 , pp. 2059-2067
    • Pavese, A.1    Fino, P.2    Badini, C.3    Ortona, A.4    Marino, G.5
  • 24
    • 34248595595 scopus 로고    scopus 로고
    • 2 Ultra-High Temperature Ceramics Containing SiC Nanodispersoids
    • 2 Ultra-High Temperature Ceramics Containing SiC Nanodispersoids," Mater. Sci. Eng. A, 464 [ 1-2 ] 216-24 (2007).
    • (2007) Mater. Sci. Eng. A , vol.464 , Issue.12 , pp. 216-224
    • Hwang, S.S.1    Vasiliev, A.L.2    Padture, N.P.3
  • 25
    • 69549135101 scopus 로고    scopus 로고
    • Oxidation Resistance of Hafnium Diboride-Silicon Carbide from 1400 to 2000°C
    • C. M. Carney, " Oxidation Resistance of Hafnium Diboride-Silicon Carbide from 1400 to 2000°C," J. Mater. Sci., 44 [ 20 ] 5673-81 (2009).
    • (2009) J. Mater. Sci. , vol.44 , Issue.20 , pp. 5673-5681
    • Carney, C.M.1
  • 27
    • 0021660604 scopus 로고
    • The Effect of Boron Additives on the Oxidation Behaviour of Carbons
    • D. W. McKee, C. L. Spiro, and, E. J. Lamby, " The Effect of Boron Additives on the Oxidation Behaviour of Carbons," Carbon, 22 [ 6 ] 507-11 (1984).
    • (1984) Carbon , vol.22 , Issue.6 , pp. 507-511
    • McKee, D.W.1    Spiro, C.L.2    Lamby, E.J.3
  • 28
    • 37849006084 scopus 로고    scopus 로고
    • Zirconia Transport by Liquid Convection during Oxidation of Zirconium Diboride-Silicon Carbide
    • S. N. Karlsdottir, J. W. Halloran, and, A. N. Grundy, " Zirconia Transport by Liquid Convection During Oxidation of Zirconium Diboride-Silicon Carbide," J. Am. Ceram. Soc., 91 [ 1 ] 272-7 (2008).
    • (2008) J. Am. Ceram. Soc. , vol.91 , Issue.1 , pp. 272-277
    • Karlsdottir, S.N.1    Halloran, J.W.2    Grundy, A.N.3
  • 29
    • 33846188476 scopus 로고    scopus 로고
    • 2-SiC Oxidation: Formation of a SiC-Depleted Region
    • 2-SiC Oxidation: Formation of a SiC-Depleted Region," J. Am. Ceram. Soc., 90 [ 1 ] 143-8 (2007).
    • (2007) J. Am. Ceram. Soc. , vol.90 , Issue.1 , pp. 143-148
    • Fahrenholtz, W.G.1
  • 30
    • 48749087268 scopus 로고    scopus 로고
    • 2-SiC during the Oxidation in Air
    • 2-SiC During the Oxidation in Air," J. Mater. Res., 23 [ 7 ] 1961-72 (2008).
    • (2008) J. Mater. Res. , vol.23 , Issue.7 , pp. 1961-1972
    • Zhang, X.H.1    Hu, P.2    Han, J.C.3
  • 31
    • 34247200063 scopus 로고    scopus 로고
    • Resistance to Thermal Shock and to Oxidation of Metal Diborides-SiC Ceramics for Aerospace Application
    • F. Monteverde, and, L. Scatteia, " Resistance to Thermal Shock and to Oxidation of Metal Diborides-SiC Ceramics for Aerospace Application," J. Am. Ceram. Soc., 90 [ 4 ] 1130-8 (2007).
    • (2007) J. Am. Ceram. Soc. , vol.90 , Issue.4 , pp. 1130-1138
    • Monteverde, F.1    Scatteia, L.2
  • 32
    • 34548833048 scopus 로고    scopus 로고
    • Rapid Oxidation Characterization of Ultra-High Temperature Ceramics
    • S. N. Karlsdottir, and, J. W. Halloran, " Rapid Oxidation Characterization of Ultra-High Temperature Ceramics," J. Am. Ceram. Soc., 90, 3233-8 (2007).
    • (2007) J. Am. Ceram. Soc. , vol.90 , pp. 3233-3238
    • Karlsdottir, S.N.1    Halloran, J.W.2
  • 33
    • 4544280225 scopus 로고    scopus 로고
    • 2 Ceramics Modified with SiC and Group IV-VI Transition Metal Borides
    • p in, Edited by M. McNallan and E. Opila, The Electrochemical Society, Inc. Pennington, NJ.
    • 2 Ceramics Modified with SiC and Group IV-VI Transition Metal Borides "; p 144 in High Temperature Corrosion and Material Chemistry III, Edited by, M. McNallan, and, E. Opila, The Electrochemical Society, Inc., Pennington, NJ, 2001.
    • (2001) High Temperature Corrosion and Material Chemistry III , pp. 144
    • Talmy, I.G.1    Zaykovski, J.A.2    Opeka, M.M.3    Dallek, S.4
  • 34
    • 0027568527 scopus 로고
    • A Structure Model for Immiscibility in Silicate Glass-Forming Melts
    • B. G. Varshal, " A Structure Model for Immiscibility in Silicate Glass-Forming Melts," Glass Phys. Chem., 19 [ 2 ] 218-25 (1993).
    • (1993) Glass Phys. Chem. , vol.19 , Issue.2 , pp. 218-225
    • Varshal, B.G.1
  • 38
    • 4544366215 scopus 로고    scopus 로고
    • 2-Based Ultra-High Temperature Ceramics: Effect of Ta Additions
    • 2-Based Ultra-High Temperature Ceramics: Effect of Ta Additions," J. Mater. Sci., 39 [ 19 ] 5969-77 (2004).
    • (2004) J. Mater. Sci. , vol.39 , Issue.19 , pp. 5969-5977
    • Opila, E.1    Levine, S.2    Lorincz, J.3
  • 39
    • 56749115762 scopus 로고    scopus 로고
    • Improved Oxidation Resistance of Zirconium Diboride by Tungsten Carbide Additions
    • S. C. Zhang, G. E. Hilmas, and, W. G. Fahrenholtz, " Improved Oxidation Resistance of Zirconium Diboride by Tungsten Carbide Additions," J. Am. Ceram. Soc., 91 [ 11 ] 3530-5 (2008).
    • (2008) J. Am. Ceram. Soc. , vol.91 , Issue.11 , pp. 3530-3535
    • Zhang, S.C.1    Hilmas, G.E.2    Fahrenholtz, W.G.3
  • 42
    • 33644682617 scopus 로고    scopus 로고
    • Liquid Phase Sintering and Mechanical Properties of SiC with Rare-Earth Oxide
    • S. Tabata, Y. Hirata, S. Sameshima, N. Matsunga, and, K. Ijichi, " Liquid Phase Sintering and Mechanical Properties of SiC with Rare-Earth Oxide," J. Ceram. Soc. Jpn., 114, 247-52 (2006).
    • (2006) J. Ceram. Soc. Jpn. , vol.114 , pp. 247-252
    • Tabata, S.1    Hirata, Y.2    Sameshima, S.3    Matsunga, N.4    Ijichi, K.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.