1
-
-
78549240630
-
Flash sintering of nanograin zirconia in <5s at 850
-
Cologna M., Rashkova B., Raj R. Flash sintering of nanograin zirconia in <5s at 850. CJ Am Ceram Soc 2010, 93(11):3557-3559. 10.1111/j. 1551-2916.2010.04089.x.
-
(2010)
CJ Am Ceram Soc
, vol.93
, Issue.11
, pp. 3557-3559
-
-
Cologna, M.1
Rashkova, B.2
Raj, R.3
-
2
-
-
79751508920
-
Flash-sintering of cubic yttria-stabilized zirconia at 750°C for possible use in SOFC manufacturing
-
2Cologna M., Prette A.L.G., Raj R. Flash-sintering of cubic yttria-stabilized zirconia at 750°C for possible use in SOFC manufacturing. J Am Ceram Soc 2011, 94(2):316-319.
-
(2011)
J Am Ceram Soc
, vol.94
, Issue.2
, pp. 316-319
-
-
2Cologna, M.1
Prette, A.L.G.2
Raj, R.3
-
3
-
-
68849093037
-
A huge effect of weak dc electrical fields on grain growth in zirconia
-
Ghosh S., Chokshi A.H., Lee P., Raj R. A huge effect of weak dc electrical fields on grain growth in zirconia. J Am Ceram Soc 2009, 92(8):1856-1859. 10.1111/j. 1551-2916.2009.03102.x.
-
(2009)
J Am Ceram Soc
, vol.92
, Issue.8
, pp. 1856-1859
-
-
Ghosh, S.1
Chokshi, A.H.2
Lee, P.3
Raj, R.4
-
4
-
-
78649517270
-
Enhanced sintering rate of zirconia (3Y-TZP) through the effect of a weak dc electric field on grain growth
-
Yang D., Raj R., Conrad H. Enhanced sintering rate of zirconia (3Y-TZP) through the effect of a weak dc electric field on grain growth. J Am Ceram Soc 2010, 93(10):2935-2937. 10.1111/j. 1551-2916.2010.03905.x.
-
(2010)
J Am Ceram Soc
, vol.93
, Issue.10
, pp. 2935-2937
-
-
Yang, D.1
Raj, R.2
Conrad, H.3
-
5
-
-
80052354036
-
Field assisted and flash sintering of alumina and its relationship to conductivity and MgO-doping
-
Cologna M., Francis J.S.C., Raj R. Field assisted and flash sintering of alumina and its relationship to conductivity and MgO-doping. J Eur Ceram Soc 2011, 31(11):2827-2837. 10.1016/j.jeurceramsoc.2011.07.004.
-
(2011)
J Eur Ceram Soc
, vol.31
, Issue.11
, pp. 2827-2837
-
-
Cologna, M.1
Francis, J.S.C.2
Raj, R.3
-
7
-
-
84862496628
-
Defect structure of flash sintered strontium titanate
-
in press
-
Karakuscu A, Cologna M, Yarotski D, Won J, Raj R, Uberuaga BP, Defect structure of flash sintered strontium titanate. JACerS, in press.
-
JACerS
-
-
Karakuscu, A.1
Cologna, M.2
Yarotski, D.3
Won, J.4
Raj, R.5
Uberuaga, B.P.6
-
8
-
-
79551658414
-
Modeling of the temperature distribution of flash sintered zirconia
-
Grasso S., Sakka Y., Rendtroff N., Hu C., Maizza V., Borodianska H., Vasylkiv O. Modeling of the temperature distribution of flash sintered zirconia. J Ceram Soc Jpn 2011, 119(2):144-146. 10.2109/jcersj2.119.144.
-
(2011)
J Ceram Soc Jpn
, vol.119
, Issue.2
, pp. 144-146
-
-
Grasso, S.1
Sakka, Y.2
Rendtroff, N.3
Hu, C.4
Maizza, V.5
Borodianska, H.6
Vasylkiv, O.7
-
9
-
-
79953324310
-
Flash grain welding in yttria stabilized zirconia
-
Muccillo R., Kleitz M., Muccillo E.N.S. Flash grain welding in yttria stabilized zirconia. J Eur Ceram Soc 2011, 31:1517-1521. 10.1016/j.jeurceramsoc.2011.02.030.
-
(2011)
J Eur Ceram Soc
, vol.31
, pp. 1517-1521
-
-
Muccillo, R.1
Kleitz, M.2
Muccillo, E.N.S.3
-
10
-
-
84858703144
-
Welding of yttrium-doped zirconia granules by electric current activated sintering
-
Cordier A., Kleitz M., Steil C. Welding of yttrium-doped zirconia granules by electric current activated sintering. J Eur Ceram Soc 2012, 32:1473-1479. 10.1016/j.jeurceramsoc.2011.12.022.
-
(2012)
J Eur Ceram Soc
, vol.32
, pp. 1473-1479
-
-
Cordier, A.1
Kleitz, M.2
Steil, C.3
-
11
-
-
84860595834
-
Joule Heating During Flash-Sintering
-
To be published online, doi:10.1016/j.jeurceramsoc.2012.02.030
-
Raj, R, Joule Heating During Flash-Sintering, J. Eur. Ceram. Soc., 2011, to be published online, doi:10.1016/j.jeurceramsoc.2012.02.030.
-
(2011)
J. Eur. Ceram. Soc
-
-
Raj, R.1
-
12
-
-
79960234780
-
Influence of externally imposed and internally generated electrical fields on grain growth, diffusional creep, sintering and related phenomena in ceramics
-
Raj R., Cologna M., Francis J.S.C. Influence of externally imposed and internally generated electrical fields on grain growth, diffusional creep, sintering and related phenomena in ceramics. J Am Ceram Soc 2011, 94(7):1941-1965. 10.1111/j. 1551-2916.2011.04652.x.
-
(2011)
J Am Ceram Soc
, vol.94
, Issue.7
, pp. 1941-1965
-
-
Raj, R.1
Cologna, M.2
Francis, J.S.C.3
-
13
-
-
0001829740
-
Separation of cavitation-strain and creep-strain during deformation
-
Raj R. Separation of cavitation-strain and creep-strain during deformation. J Am Ceram Soc 1982, 65(3):C46.
-
(1982)
J Am Ceram Soc
, vol.65
, Issue.3
-
-
Raj, R.1
-
14
-
-
84855351743
-
Effect of electrical field/current on sintering of fully stabilized zirconia
-
Baraki R., Schwarz S., Guillon O. Effect of electrical field/current on sintering of fully stabilized zirconia. J Am Ceram Soc 2012, 95(1):75-78. 10.1111/j. 1551-2916.2011.04980.x.
-
(2012)
J Am Ceram Soc
, vol.95
, Issue.1
, pp. 75-78
-
-
Baraki, R.1
Schwarz, S.2
Guillon, O.3
-
16
-
-
80052260607
-
Microtructure evolution during field-assisted sintering of zirconia spheres
-
Deminskyi D., Borodianska H., Grasso S., et al. Microtructure evolution during field-assisted sintering of zirconia spheres. Scr Mater 2011, 65(8):683-686. 10.1016/j.scriptamat.2011.07.006.
-
(2011)
Scr Mater
, vol.65
, Issue.8
, pp. 683-686
-
-
Deminskyi, D.1
Borodianska, H.2
Grasso, S.3
-
17
-
-
79751507105
-
Surface diffusion-controlled neck growth kinetics in early stage sintering of zirconia, with and without applied DC electrical field
-
Cologna M., Raj R. Surface diffusion-controlled neck growth kinetics in early stage sintering of zirconia, with and without applied DC electrical field. J Am Ceram Soc 2010, 94(2):391-395. 10.1111/j. 1551-2916.2010.04088.x.
-
(2010)
J Am Ceram Soc
, vol.94
, Issue.2
, pp. 391-395
-
-
Cologna, M.1
Raj, R.2
|