Volumn 60, Issue , 2012, Pages 238-245

The role of second phases in the corrosion behavior of Mg-5Zn alloy

Author keywords

A. Magnesium; B. Polarization; B. Weight loss; C. Pitting corrosion

Indexed keywords

CONTINUOUS DISTRIBUTION; CORROSION BEHAVIOR; DISCRETE DISTRIBUTION; T6 TREATMENT; WEIGHT LOSS;

EID: 84861194015     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2012.03.030     Document Type: Article
Times cited : (174)

References (29)
  • 1
    • 33751324577 scopus 로고    scopus 로고
    • Formation and breakdown of surface films on magnesium and its alloys in aqueous solutions
    • Hara N., Kobayashi Y., Kagaya D., Akao N. Formation and breakdown of surface films on magnesium and its alloys in aqueous solutions. Corros. Sci. 2007, 49:166-175.
    • (2007) Corros. Sci. , vol.49 , pp. 166-175
    • Hara, N.1    Kobayashi, Y.2    Kagaya, D.3    Akao, N.4
  • 2
    • 33751536689 scopus 로고    scopus 로고
    • Corrosion product formation during NaCl induced atmospheric corrosion of magnesium alloy AZ91D
    • Jonsson M., Persson D., Thierry D. Corrosion product formation during NaCl induced atmospheric corrosion of magnesium alloy AZ91D. Corros. Sci. 2007, 49:1540-1558.
    • (2007) Corros. Sci. , vol.49 , pp. 1540-1558
    • Jonsson, M.1    Persson, D.2    Thierry, D.3
  • 3
    • 79954572520 scopus 로고    scopus 로고
    • Effect of naturally formed oxide films and other variables in the early stages of Mg-alloy corrosion in NaCl solution
    • Feliú S., Maffiotte C., Samaniego A., Galván J.C., Barranco V. Effect of naturally formed oxide films and other variables in the early stages of Mg-alloy corrosion in NaCl solution. Electrochim. Acta 2011, 56:4554-4565.
    • (2011) Electrochim. Acta , vol.56 , pp. 4554-4565
    • Feliú, S.1    Maffiotte, C.2    Samaniego, A.3    Galván, J.C.4    Barranco, V.5
  • 4
    • 50149110038 scopus 로고    scopus 로고
    • Influence of microstructure and composition on the corrosion behaviour of Mg/Al alloys in chloride media
    • Pardo A., Merino M.C., Coy A.E., Viejo F., Arrabal R., Feliú S. Influence of microstructure and composition on the corrosion behaviour of Mg/Al alloys in chloride media. Electrochim. Acta 2008, 53:7890-7902.
    • (2008) Electrochim. Acta , vol.53 , pp. 7890-7902
    • Pardo, A.1    Merino, M.C.2    Coy, A.E.3    Viejo, F.4    Arrabal, R.5    Feliú, S.6
  • 5
    • 33847256447 scopus 로고    scopus 로고
    • The relation between microstructure and corrosion behavior of Mg-Y-RE-Zr alloys
    • Ben-Hamu G., Eliezer D., Shin K.S., Cohen S. The relation between microstructure and corrosion behavior of Mg-Y-RE-Zr alloys. J. Alloys Compd. 2007, 431:269-276.
    • (2007) J. Alloys Compd. , vol.431 , pp. 269-276
    • Ben-Hamu, G.1    Eliezer, D.2    Shin, K.S.3    Cohen, S.4
  • 6
    • 79952899195 scopus 로고    scopus 로고
    • Corrosion of hot extrusion AZ91 magnesium alloy: I - relation between the microstructure and corrosion behavior
    • Zhang T., Shao Y.W., Meng G.Z., Cui Z.Y., Wang F.H. Corrosion of hot extrusion AZ91 magnesium alloy: I - relation between the microstructure and corrosion behavior. Corros. Sci. 2011, 53:1960-1968.
    • (2011) Corros. Sci. , vol.53 , pp. 1960-1968
    • Zhang, T.1    Shao, Y.W.2    Meng, G.Z.3    Cui, Z.Y.4    Wang, F.H.5
  • 7
    • 77950248237 scopus 로고    scopus 로고
    • The surface, microstructure and corrosion of magnesium alloy AZ31 sheet
    • Song G.L., Xu Z.Q. The surface, microstructure and corrosion of magnesium alloy AZ31 sheet. Electrochim. Acta 2010, 55:4148-4161.
    • (2010) Electrochim. Acta , vol.55 , pp. 4148-4161
    • Song, G.L.1    Xu, Z.Q.2
  • 9
    • 33646063555 scopus 로고    scopus 로고
    • The influence of microstructure on the corrosion behaviour of AZ91D studied by scanning Kelvin probe force microscopy and scanning Kelvin probe
    • Jonsson M., Thierry D., LeBozec N. The influence of microstructure on the corrosion behaviour of AZ91D studied by scanning Kelvin probe force microscopy and scanning Kelvin probe. Corros. Sci. 2006, 48:1193-1208.
    • (2006) Corros. Sci. , vol.48 , pp. 1193-1208
    • Jonsson, M.1    Thierry, D.2    LeBozec, N.3
  • 10
    • 0345711477 scopus 로고    scopus 로고
    • Influence of microstructure on the corrosion of diecast AZ91D
    • Song G.L., Atrens A., Dargusch M. Influence of microstructure on the corrosion of diecast AZ91D. Corros. Sci. 1999, 41:249-273.
    • (1999) Corros. Sci. , vol.41 , pp. 249-273
    • Song, G.L.1    Atrens, A.2    Dargusch, M.3
  • 11
    • 0034131359 scopus 로고    scopus 로고
    • Evaluation of microstructural effects on corrosion behaviour of AZ91D magnesium alloy
    • Ambat R., Aung N.N., Zhou W. Evaluation of microstructural effects on corrosion behaviour of AZ91D magnesium alloy. Corros. Sci. 2000, 42:1433-1455.
    • (2000) Corros. Sci. , vol.42 , pp. 1433-1455
    • Ambat, R.1    Aung, N.N.2    Zhou, W.3
  • 12
    • 0348107298 scopus 로고    scopus 로고
    • Corrosion resistance of aged die cast magnesium alloy AZ91D
    • Song G.L., Bowles A.L., St John D.H. Corrosion resistance of aged die cast magnesium alloy AZ91D. Mater. Sci. Eng. A 2004, 366:74-86.
    • (2004) Mater. Sci. Eng. A , vol.366 , pp. 74-86
    • Song, G.L.1    Bowles, A.L.2    St John, D.H.3
  • 13
    • 47049114453 scopus 로고    scopus 로고
    • Influence of the β-phase morphology on the corrosion of the Mg alloy AZ91
    • Zhao M.C., Liu M., Song G.L., Atrens A. Influence of the β-phase morphology on the corrosion of the Mg alloy AZ91. Corros. Sci. 2008, 50:1939-1953.
    • (2008) Corros. Sci. , vol.50 , pp. 1939-1953
    • Zhao, M.C.1    Liu, M.2    Song, G.L.3    Atrens, A.4
  • 14
    • 77949288875 scopus 로고    scopus 로고
    • Effect of second phases on the corrosion behaviour of wrought Mg-Zn-Y-Zr alloy
    • Song Y.W., Shan D.Y., Chen R.S., Han E.H. Effect of second phases on the corrosion behaviour of wrought Mg-Zn-Y-Zr alloy. Corros. Sci. 2010, 52:1830-1837.
    • (2010) Corros. Sci. , vol.52 , pp. 1830-1837
    • Song, Y.W.1    Shan, D.Y.2    Chen, R.S.3    Han, E.H.4
  • 17
    • 74849121638 scopus 로고    scopus 로고
    • Effect of heat treatment on corrosion behaviour of magnesium alloy AZ91D in simulated body fluid
    • Zhou W., Shen T., Aung N.N. Effect of heat treatment on corrosion behaviour of magnesium alloy AZ91D in simulated body fluid. Corros. Sci. 2010, 52:1035-1041.
    • (2010) Corros. Sci. , vol.52 , pp. 1035-1041
    • Zhou, W.1    Shen, T.2    Aung, N.N.3
  • 20
    • 33646434503 scopus 로고    scopus 로고
    • Roles of β phase in the corrosion process of AZ91D magnesium alloy
    • Zhang T., Li Y., Wang F.H. Roles of β phase in the corrosion process of AZ91D magnesium alloy. Corros. Sci. 2006, 48:1249-1264.
    • (2006) Corros. Sci. , vol.48 , pp. 1249-1264
    • Zhang, T.1    Li, Y.2    Wang, F.H.3
  • 21
    • 65049091088 scopus 로고    scopus 로고
    • Corrosion characterization of Mg-8Li alloy in NaCl solution
    • Song Y.W., Shan D.Y., Chen R.S., Han E.H. Corrosion characterization of Mg-8Li alloy in NaCl solution. Corros. Sci. 2009, 51:1087-1094.
    • (2009) Corros. Sci. , vol.51 , pp. 1087-1094
    • Song, Y.W.1    Shan, D.Y.2    Chen, R.S.3    Han, E.H.4
  • 22
    • 42049122612 scopus 로고    scopus 로고
    • Effects of dust and salt particles on the formation and spreading of micro-droplets on AZ91 magnesium alloy
    • Chen J., Wang J.Q., Han E.H., Ke W. Effects of dust and salt particles on the formation and spreading of micro-droplets on AZ91 magnesium alloy. Corros. Sci. 2008, 50:1449-1459.
    • (2008) Corros. Sci. , vol.50 , pp. 1449-1459
    • Chen, J.1    Wang, J.Q.2    Han, E.H.3    Ke, W.4
  • 23
    • 42049118534 scopus 로고    scopus 로고
    • States and transport of hydrogen in the corrosion process of an AZ91 magnesium alloy in aqueous solution
    • Chen J., Wang J.Q., Han E.H., Dong J.H., Ke W. States and transport of hydrogen in the corrosion process of an AZ91 magnesium alloy in aqueous solution. Corros. Sci. 2008, 50:1292-1305.
    • (2008) Corros. Sci. , vol.50 , pp. 1292-1305
    • Chen, J.1    Wang, J.Q.2    Han, E.H.3    Dong, J.H.4    Ke, W.5
  • 25
    • 0031148490 scopus 로고    scopus 로고
    • The electrochemical corrosion of pure magnesium in 1N NaCl
    • Song G., Atrens A., St. John D., Nairn J., Li Y. The electrochemical corrosion of pure magnesium in 1N NaCl. Corros. Sci. 1997, 39:855-875.
    • (1997) Corros. Sci. , vol.39 , pp. 855-875
    • Song, G.1    Atrens, A.2    St John, D.3    Nairn, J.4    Li, Y.5
  • 26
    • 38849110122 scopus 로고    scopus 로고
    • Structure and formation mechanism of phosphate conversion coating on die-cast AZ91D magnesium alloy
    • Zhou W.Q., Shan D.Y., Han E.H., Ke W. Structure and formation mechanism of phosphate conversion coating on die-cast AZ91D magnesium alloy. Corros. Sci. 2008, 50:329-337.
    • (2008) Corros. Sci. , vol.50 , pp. 329-337
    • Zhou, W.Q.1    Shan, D.Y.2    Han, E.H.3    Ke, W.4
  • 27
    • 49949098939 scopus 로고    scopus 로고
    • Influence of the microstructure on the corrosion behavior of AXJ530 magnesium alloy in 3.5% NaCl solution
    • Amira S., Dubé D., Tremblay R., Ghali E. Influence of the microstructure on the corrosion behavior of AXJ530 magnesium alloy in 3.5% NaCl solution. Mater. Charact. 2008, 59:1508-1517.
    • (2008) Mater. Charact. , vol.59 , pp. 1508-1517
    • Amira, S.1    Dubé, D.2    Tremblay, R.3    Ghali, E.4
  • 28
    • 0032193643 scopus 로고    scopus 로고
    • Corrosion behavior of AZ10, AZ490 and AZ80 in sodium chloride
    • Song G.L., Atrens A., Wu X.L., Zhang B. Corrosion behavior of AZ10, AZ490 and AZ80 in sodium chloride. Corros. Sci. 1998, 40:1769-1791.
    • (1998) Corros. Sci. , vol.40 , pp. 1769-1791
    • Song, G.L.1    Atrens, A.2    Wu, X.L.3    Zhang, B.4
  • 29
    • 0347983907 scopus 로고    scopus 로고
    • A corrosion study of the main constituent phases of AZ91 magnesium alloys
    • Mathieu S., Rapin C., Steinmetz J., Steinmetz P. A corrosion study of the main constituent phases of AZ91 magnesium alloys. Corros. Sci. 2003, 45:2741-2755.
    • (2003) Corros. Sci. , vol.45 , pp. 2741-2755
    • Mathieu, S.1    Rapin, C.2    Steinmetz, J.3    Steinmetz, P.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.