1
-
-
28244436214
-
Swelling and hydrolytic degradation of poly(d, l-lactic acid) in aqueous solutions
-
C.S. Proikakis, N.J. Mamouzelos, P.A. Tarantili, and A.G. Andreopoulos Swelling and hydrolytic degradation of poly(d, l-lactic acid) in aqueous solutions Polymer Degradation and Stability 91 2006 614 619
-
(2006)
Polymer Degradation and Stability
, vol.91
, pp. 614-619
-
-
Proikakis, C.S.1
Mamouzelos, N.J.2
Tarantili, P.A.3
Andreopoulos, A.G.4
-
2
-
-
77950805148
-
Polylactide stereocomplexation leads to higher hydrolytic stability but more acidic hydrolysis product pattern
-
S.R. Andersson, M. Hakkarainen, S. Inkinen, A. Södergård, and A.-C. Albertsson Polylactide stereocomplexation leads to higher hydrolytic stability but more acidic hydrolysis product pattern Biomacromolecules 11 2010 1067 1073
-
(2010)
Biomacromolecules
, vol.11
, pp. 1067-1073
-
-
Andersson, S.R.1
Hakkarainen, M.2
Inkinen, S.3
Södergård, A.4
Albertsson, A.-C.5
-
3
-
-
73949137505
-
Migration and hydrolysis of hydrophobic polylactide plasticizer
-
A. Höglund, M. Hakkarainen, and A.-C. Albertsson Migration and hydrolysis of hydrophobic polylactide plasticizer Biomacromolecules 11 2009 277 283
-
(2009)
Biomacromolecules
, vol.11
, pp. 277-283
-
-
Höglund, A.1
Hakkarainen, M.2
Albertsson, A.-C.3
-
4
-
-
34249041978
-
Tuning the release rate of acidic degradation products through macromolecular design of caprolactone-based copolymers
-
M. Hakkarainen, A. Höglund, K. Odelius, and A.-C. Albertsson Tuning the release rate of acidic degradation products through macromolecular design of caprolactone-based copolymers Journal of the American Chemical Society 129 2007 6308 6312
-
(2007)
Journal of the American Chemical Society
, vol.129
, pp. 6308-6312
-
-
Hakkarainen, M.1
Höglund, A.2
Odelius, K.3
Albertsson, A.-C.4
-
5
-
-
78650288294
-
Tuning the polylactide hydrolysis rate by plasticizer architecture and hydrophilicity without introducing new migrants
-
S.R. Andersson, M. Hakkarainen, and A.-C. Albertsson Tuning the polylactide hydrolysis rate by plasticizer architecture and hydrophilicity without introducing new migrants Biomacromolecules 11 2010 3617 3623
-
(2010)
Biomacromolecules
, vol.11
, pp. 3617-3623
-
-
Andersson, S.R.1
Hakkarainen, M.2
Albertsson, A.-C.3
-
6
-
-
4944240923
-
Thermal degradation behaviour of poly(lactic acid) stereocomplex
-
Y. Fan, H. Nishida, Y. Shirai, Y. Tokiwa, and T. Endo Thermal degradation behaviour of poly(lactic acid) stereocomplex Polymer Degradation and Stability 86 2004 197 208
-
(2004)
Polymer Degradation and Stability
, vol.86
, pp. 197-208
-
-
Fan, Y.1
Nishida, H.2
Shirai, Y.3
Tokiwa, Y.4
Endo, T.5
-
7
-
-
0030247823
-
Thermal decomposition of biodegradable polyesters-II. Poly(lactic acid)
-
F.D. Kopinke, M. Remmler, K. Mackenzie, M. Möder, and O. Wachsen Thermal decomposition of biodegradable polyesters-II. Poly(lactic acid) Polymer Degradation and Stability 53 1996 329 342
-
(1996)
Polymer Degradation and Stability
, vol.53
, pp. 329-342
-
-
Kopinke, F.D.1
Remmler, M.2
MacKenzie, K.3
Möder, M.4
Wachsen, O.5
-
8
-
-
0031119482
-
Influence of residual monomers and metals on poly (-lactide) thermal stability
-
D. Cam, and M. Marucci Influence of residual monomers and metals on poly (-lactide) thermal stability Polymer 38 1997 1879 1884
-
(1997)
Polymer
, vol.38
, pp. 1879-1884
-
-
Cam, D.1
Marucci, M.2
-
9
-
-
33645370775
-
The stability of poly(lactic acid) packaging films as influenced by humidity and temperature
-
V.K. Holm, S. Ndoni, and J. Risbo The stability of poly(lactic acid) packaging films as influenced by humidity and temperature Journal of Food Science 71 2006 E40 E44
-
(2006)
Journal of Food Science
, vol.71
-
-
Holm, V.K.1
Ndoni, S.2
Risbo, J.3
-
10
-
-
1542358206
-
Effects of ultraviolet light (315 nm), temperature and relative humidity on the degradation of polylactic acid plastic films
-
A. Copinet, C. Bertrand, S. Govindin, V. Coma, and Y. Couturier Effects of ultraviolet light (315 nm), temperature and relative humidity on the degradation of polylactic acid plastic films Chemosphere 55 2004 763 773
-
(2004)
Chemosphere
, vol.55
, pp. 763-773
-
-
Copinet, A.1
Bertrand, C.2
Govindin, S.3
Coma, V.4
Couturier, Y.5
-
11
-
-
0031077635
-
Thermal decomposition of biodegradable polyesters-III. Studies on the mechanisms of thermal degradation of oligo-lactide using SEC, LACCC and MALDI-TOF-MS
-
O. Wachsen, K.H. Reichert, R.P. Krüger, H. Much, and G. Schulz Thermal decomposition of biodegradable polyesters-III. Studies on the mechanisms of thermal degradation of oligo-lactide using SEC, LACCC and MALDI-TOF-MS Polymer Degradation and Stability 55 1997 225 231
-
(1997)
Polymer Degradation and Stability
, vol.55
, pp. 225-231
-
-
Wachsen, O.1
Reichert, K.H.2
Krüger, R.P.3
Much, H.4
Schulz, G.5
-
12
-
-
39149084357
-
In-line monitoring of the thermal degradation of poly(l-lactic acid) during melt extrusion by UV-vis spectroscopy
-
Y. Wang, B. Steinhoff, C. Brinkmann, and I. Alig In-line monitoring of the thermal degradation of poly(l-lactic acid) during melt extrusion by UV-vis spectroscopy Polymer 49 2008 1257 1265
-
(2008)
Polymer
, vol.49
, pp. 1257-1265
-
-
Wang, Y.1
Steinhoff, B.2
Brinkmann, C.3
Alig, I.4
-
13
-
-
33845490667
-
Kinetics of thermo-oxidative and thermal degradation of poly(d, l-lactide) (PDLLA) at processing temperature
-
X. Liu, Y. Zou, W. Li, G. Cao, and W. Chen Kinetics of thermo-oxidative and thermal degradation of poly(d, l-lactide) (PDLLA) at processing temperature Polymer Degradation and Stability 91 2006 3259 3265
-
(2006)
Polymer Degradation and Stability
, vol.91
, pp. 3259-3265
-
-
Liu, X.1
Zou, Y.2
Li, W.3
Cao, G.4
Chen, W.5
-
14
-
-
0037432869
-
Enhanced thermal stability of poly(lactide)s in the melt by enantiomeric polymer blending
-
H. Tsuji, and I. Fukui Enhanced thermal stability of poly(lactide)s in the melt by enantiomeric polymer blending Polymer 44 2003 2891 2896
-
(2003)
Polymer
, vol.44
, pp. 2891-2896
-
-
Tsuji, H.1
Fukui, I.2
-
15
-
-
59149103202
-
Nanosize and microsize clay effects on the kinetics of the thermal degradation of polylactides
-
Q. Zhou, and M. Xanthos Nanosize and microsize clay effects on the kinetics of the thermal degradation of polylactides Polymer Degradation and Stability 94 2009 327 338
-
(2009)
Polymer Degradation and Stability
, vol.94
, pp. 327-338
-
-
Zhou, Q.1
Xanthos, M.2
-
17
-
-
22544451597
-
Poly(lactide) stereocomplexes: Formation, structure, properties, degradation, and applications
-
H. Tsuji Poly(lactide) stereocomplexes: formation, structure, properties, degradation, and applications Macromolecular Bioscience 5 2005 569 597
-
(2005)
Macromolecular Bioscience
, vol.5
, pp. 569-597
-
-
Tsuji, H.1
-
18
-
-
0011786536
-
Investigation of the structure of solution grown crystals of lactide copolymers by means of chemical reactions
-
E.W. Fischer, H.J. Sterzel, and G. Wegner Investigation of the structure of solution grown crystals of lactide copolymers by means of chemical reactions Colloid & Polymer Science 251 1973 980 990
-
(1973)
Colloid & Polymer Science
, vol.251
, pp. 980-990
-
-
Fischer, E.W.1
Sterzel, H.J.2
Wegner, G.3
-
21
-
-
0020132870
-
Thermal oxidative degradation of poly-lactic acid
-
M.C. Gupta, and V.G. Deshmukh Thermal oxidative degradation of poly-lactic acid Colloid & Polymer Science 260 1982 514 517
-
(1982)
Colloid & Polymer Science
, vol.260
, pp. 514-517
-
-
Gupta, M.C.1
Deshmukh, V.G.2
|