Volumn 108, Issue 17, 2012, Pages

Structural origins of the excellent glass forming ability of Pd 40Ni 40P 20

Author keywords

[No Author keywords available]

Indexed keywords

ATOMIC PACKING; BULK METALLIC GLASS; BULK METALLIC GLASS FORMATION; GLASS FORMING ABILITY; METALLIC ELEMENTS; STRUCTURAL ORIGIN;

EID: 84860309355     PISSN: 00319007     EISSN: 10797114     Source Type: Journal    
DOI: 10.1103/PhysRevLett.108.175501     Document Type: Article
Times cited : (137)

References (25)
  • 1
    • 5544258257 scopus 로고    scopus 로고
    • NMAACR 1476-1122 10.1038/nmat1219
    • D.B. Miracle, Nature Mater. 3, 697 (2004). NMAACR 1476-1122 10.1038/nmat1219
    • (2004) Nature Mater. , vol.3 , pp. 697
    • Miracle, D.B.1
  • 2
    • 31444444206 scopus 로고    scopus 로고
    • Materials science: A new order for metallic glasses
    • DOI 10.1038/439405a, PII 439405A
    • A.R. Yavari, Nature (London) NATUAS 0028-0836 439, 405 (2006). 10.1038/439405a (Pubitemid 43152822)
    • (2006) Nature , vol.439 , Issue.7075 , pp. 405-406
    • Yavari, A.R.1
  • 3
    • 4544242366 scopus 로고    scopus 로고
    • PRLTAO 0031-9007 10.1103/PhysRevLett.91.115505
    • Z.P. Lu and C.T. Liu, Phys. Rev. Lett. 91, 115505 (2003). PRLTAO 0031-9007 10.1103/PhysRevLett.91.115505
    • (2003) Phys. Rev. Lett. , vol.91 , pp. 115505
    • Lu, Z.P.1    Liu, C.T.2
  • 4
    • 84863116100 scopus 로고    scopus 로고
    • 1884-4057 10.1038/asiamat.2011.30
    • M.W. Chen, NPG Asia Materials 1884-4057 3, 82 (2011). 10.1038/asiamat.2011.30
    • (2011) NPG Asia Materials , vol.3 , pp. 82
    • Chen, M.W.1
  • 5
    • 34548391332 scopus 로고    scopus 로고
    • Correlation of atomic cluster symmetry and glass-forming ability of metallic glass
    • DOI 10.1103/PhysRevLett.99.095501
    • X.k. Xi, L.l. Li, B. Zhang, W.h. Wang, and Y. Wu, Phys. Rev. Lett. 99, 095501 (2007). PRLTAO 0031-9007 10.1103/PhysRevLett.99.095501 (Pubitemid 47357785)
    • (2007) Physical Review Letters , vol.99 , Issue.9 , pp. 095501
    • Xi, X.K.1    Li, L.L.2    Zhang, B.3    Wang, W.H.4    Wu, Y.5
  • 7
    • 67449141697 scopus 로고    scopus 로고
    • PRLTAO 0031-9007 10.1103/PhysRevLett.102.245501
    • Y.Q. Cheng, E. Ma, and H.W. Sheng, Phys. Rev. Lett. 102, 245501 (2009). PRLTAO 0031-9007 10.1103/PhysRevLett.102.245501
    • (2009) Phys. Rev. Lett. , vol.102 , pp. 245501
    • Cheng, Y.Q.1    Ma, E.2    Sheng, H.W.3
  • 8
    • 31444451528 scopus 로고    scopus 로고
    • Atomic packing and short-to-medium-range order in metallic glasses
    • DOI 10.1038/nature04421, PII NATURE04421
    • H.W. Sheng, W.K. Luo, F.M. Alamgir, J.M. Bai, and E. Ma, Nature (London) NATUAS 0028-0836 439, 419 (2006). 10.1038/nature04421 (Pubitemid 43152826)
    • (2006) Nature , vol.439 , Issue.7075 , pp. 419-425
    • Sheng, H.W.1    Luo, W.K.2    Alamgir, F.M.3    Bai, J.M.4    Ma, E.5
  • 12
    • 0032630264 scopus 로고    scopus 로고
    • ACMAFD 1359-6454 10.1016/S1359-6454(99)00030-0
    • N. Nishiyama and A. Inoue, Acta Mater. 47, 1487 (1999). ACMAFD 1359-6454 10.1016/S1359-6454(99)00030-0
    • (1999) Acta Mater. , vol.47 , pp. 1487
    • Nishiyama, N.1    Inoue, A.2
  • 13
    • 32344452090 scopus 로고    scopus 로고
    • 20 alloys studied by electron diffraction
    • DOI 10.2320/matertrans.46.2781
    • A. Hirata, Y. Hirotsu, and E. Matsubara, Mater. Trans., JIM 46, 2781 (2005). MTJIEY 0916-1821 10.2320/matertrans.46.2781 (Pubitemid 43219847)
    • (2005) Materials Transactions , vol.46 , Issue.12 , pp. 2781-2784
    • Hirata, A.1    Hirotsu, Y.2    Matsubara, E.3
  • 14
    • 33745208078 scopus 로고
    • NATUAS 0028-0836 10.1038/276484a0
    • P.H. Gaskell, Nature (London) NATUAS 0028-0836 276, 484 (1978). 10.1038/276484a0
    • (1978) Nature (London) , vol.276 , pp. 484
    • Gaskell, P.H.1
  • 15
    • 0021410957 scopus 로고
    • JNCSBJ 0022-3093 10.1016/0022-3093(84)90210-2
    • T. Egami and Y. Waseda, J. Non-Cryst. Solids JNCSBJ 0022-3093 64, 113 (1984). 10.1016/0022-3093(84)90210-2
    • (1984) J. Non-Cryst. Solids , vol.64 , pp. 113
    • Egami, T.1    Waseda, Y.2
  • 17
    • 2442537377 scopus 로고    scopus 로고
    • PRBMDO 0163-1829 10.1103/PhysRevB.54.11169
    • G. Kresse and J. Furthmuller, Phys. Rev. B PRBMDO 0163-1829 54, 11169 (1996). 10.1103/PhysRevB.54.11169
    • (1996) Phys. Rev. B , vol.54 , pp. 11169
    • Kresse, G.1    Furthmuller, J.2
  • 19
    • 25744460922 scopus 로고
    • PRBMDO 0163-1829 10.1103/PhysRevB.50.17953
    • P.E. Blöchl, Phys. Rev. B PRBMDO 0163-1829 50, 17953 (1994). 10.1103/PhysRevB.50.17953
    • (1994) Phys. Rev. B , vol.50 , pp. 17953
    • Blöchl, P.E.1
  • 20
    • 0000620927 scopus 로고
    • PRBMDO 0163-1829 10.1103/PhysRevB.44.13298
    • Y. Wang and J.P. Perdew, Phys. Rev. B PRBMDO 0163-1829 44, 13298 (1991). 10.1103/PhysRevB.44.13298
    • (1991) Phys. Rev. B , vol.44 , pp. 13298
    • Wang, Y.1    Perdew, J.P.2
  • 21
    • 84860285981 scopus 로고    scopus 로고
    • See Supplemental Material at
    • See Supplemental Material at http://link.aps.org/supplemental/10.1103/ PhysRevLett.108.175501 for the details of simulation, experiment, and structure analysis of Pd x Ni 80 - x P 20 (x = 0, 20, 40, 60) glasses, as well as the hybrid packing method.
  • 23
    • 33745193984 scopus 로고
    • NATUAS 0028-0836 10.1038/266309a0
    • J.L. Finney, Nature (London) NATUAS 0028-0836 266, 309 (1977). 10.1038/266309a0
    • (1977) Nature (London) , vol.266 , pp. 309
    • Finney, J.L.1
  • 24
    • 0040725971 scopus 로고
    • ARKEAD 0365-6128
    • S. Rundqvist, Arkiv. Kemi ARKEAD 0365-6128 20, 67 (1962).
    • (1962) Arkiv. Kemi , vol.20 , pp. 67
    • Rundqvist, S.1
  • 25
    • 33645755595 scopus 로고    scopus 로고
    • Frustration on the way to crystallization in glass
    • DOI 10.1038/nphys235, PII N235
    • H. Shintani and H. Tanaka, Nature Phys. 2, 200 (2006). NPAHAX 1745-2473 10.1038/nphys235 (Pubitemid 43553503)
    • (2006) Nature Physics , vol.2 , Issue.3 , pp. 200-206
    • Shintani, H.1    Tanaka, H.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.