Mechanism of dehydroxylation temperature decrease and high temperature phase transition of coal-bearing strata kaolinite intercalated by potassium acetate

Author keywords

Coal bearing strata kaolinite; Dehydroxylation; Intercalation complex; Potassium acetate; Structural model

Indexed keywords

BEARING STRATA; DEHYDROXYLATIONS; HIGH TEMPERATURE PHASE TRANSITIONS; INFRARED EMISSION SPECTROSCOPY; INTERCALATION COMPLEXES; INTERLAYER SPACES; MASS LOSS; MASS SPECTROMETRIC ANALYSIS; POSITIVE CORRELATIONS; POTASSIUM ACETATE; STRUCTURAL MODELS; TEMPERATURE DECREASE; THERMAL DECOMPOSITION PRODUCTS; XRD;

EID: 84859757869     PISSN: 00219797     EISSN: 10957103     Source Type: Journal    
DOI: 10.1016/j.jcis.2012.02.065     Document Type: Article
Times cited : (54)

References (54)
  • 34
    • 0002694636 scopus 로고
    • in: L. Heller (Ed.), Proceedings of the International Clay Conference Israel University Press, Jerusalem, Tokyo
    • A. Wiewióra, G.W. Brindley, in: L. Heller (Ed.), Proceedings of the International Clay Conference Israel University Press, Jerusalem, Tokyo, 1969, p. 723.
    • (1969) , pp. 723
    • Wiewióra, A.1    Brindley, G.W.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.