메뉴 건너뛰기




Volumn 57, Issue , 2012, Pages 114-121

On the oxidation mechanism of pure tungsten in the temperature range 600-800°C

Author keywords

C. High temperature corrosion; C. Kinetic parameters; C. Oxidation

Indexed keywords

DRY AIR; GROWTH STRESS; HIGH TEMPERATURE CORROSIONS; INTERNATIONAL THERMONUCLEAR EXPERIMENTAL REACTOR; MASS GAIN; OXIDATION BEHAVIORS; OXIDATION MECHANISMS; OXYGEN PARTIAL PRESSURE; OXYGEN TRANSPORT; PURE TUNGSTEN; SCALE THICKNESS; TEMPERATURE RANGE;

EID: 84857057310     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2011.12.027     Document Type: Article
Times cited : (92)

References (30)
  • 3
    • 80053597942 scopus 로고    scopus 로고
    • Review on the EFDA programme on tungsten materials technology and science
    • in press. doi:10.1016/j.jnucmat.2011.01.075
    • M. Rieth, J.L. Boutard, S.L. Dudarev, T. Ahlgren, S. Antusch, et al., Review on the EFDA programme on tungsten materials technology and science, J. Nucl. Mater., in press. doi:10.1016/j.jnucmat.2011.01.075.
    • J. Nucl. Mater.
    • Rieth, M.1    Boutard, J.L.2    Dudarev, S.L.3    Ahlgren, T.4    Antusch, S.5
  • 5
    • 0030260166 scopus 로고    scopus 로고
    • An overview of safety and environmental considerations in the selection of materials for fusion facilities
    • D.A. Petti, K.A. McCarthy, W. Gulden, S.J. Piet, Y. Seki, B. Kolbasov, An overview of safety and environmental considerations in the selection of materials for fusion facilities, J. Nucl. Mater. 233-237 (part I) (1996) 37-43.
    • (1996) J. Nucl. Mater. , vol.233-237 , Issue.PART I , pp. 37-43
    • Petti, D.A.1    McCarthy, K.A.2    Gulden, W.3    Piet, S.J.4    Seki, Y.5    Kolbasov, B.6
  • 6
    • 79951550272 scopus 로고    scopus 로고
    • An investigation for ground state features of some structural fusion materials
    • Aytekin H., Tel E., Baldik R., Aydin A. An investigation for ground state features of some structural fusion materials. J. Fusion Energ. 2011, 30:21-25.
    • (2011) J. Fusion Energ. , vol.30 , pp. 21-25
    • Aytekin, H.1    Tel, E.2    Baldik, R.3    Aydin, A.4
  • 7
    • 0036863185 scopus 로고    scopus 로고
    • Tritium inventory and recovery in next-step fusion devices
    • Causey R.A., Brooks J.N., Federici G. Tritium inventory and recovery in next-step fusion devices. Fusion Eng. Des. 2002, 61-62:525-536.
    • (2002) Fusion Eng. Des. , pp. 525-536
    • Causey, R.A.1    Brooks, J.N.2    Federici, G.3
  • 8
    • 84857060319 scopus 로고    scopus 로고
    • Materials Assessment Report (MAR), ITER Doc. G 74 MA 10 01-07-11 W 0.2
    • Materials Assessment Report (MAR), ITER Doc. G 74 MA 10 01-07-11 W 0.2, 2001.
    • (2001)
  • 11
    • 34147115097 scopus 로고    scopus 로고
    • Plasma-wall interaction: important ion induced surface processes and strategy of the EU task force
    • Roth J., Tsitrone E., Loarte A. Plasma-wall interaction: important ion induced surface processes and strategy of the EU task force. Nucl. Instrum. Meth. B 2007, 258:253-263.
    • (2007) Nucl. Instrum. Meth. B , vol.258 , pp. 253-263
    • Roth, J.1    Tsitrone, E.2    Loarte, A.3
  • 12
    • 0037267795 scopus 로고    scopus 로고
    • Temperature transients of a fusion-fission ITER pebble bed reactor in loss of coolant accident
    • Tang V., Parker R.R. Temperature transients of a fusion-fission ITER pebble bed reactor in loss of coolant accident. Fusion Eng. Des. 2003, 65:11-26.
    • (2003) Fusion Eng. Des. , vol.65 , pp. 11-26
    • Tang, V.1    Parker, R.R.2
  • 13
    • 0033683507 scopus 로고    scopus 로고
    • Simulation of the sublimation process in the preparation of photochromic WO3 film by laser microprobe mass spectrometry
    • Yang Y.A., Ma Y., Yao J.N., Loo B.H. Simulation of the sublimation process in the preparation of photochromic WO3 film by laser microprobe mass spectrometry. J. Non-Cryst. Solids 2000, 272:71-74.
    • (2000) J. Non-Cryst. Solids , vol.272 , pp. 71-74
    • Yang, Y.A.1    Ma, Y.2    Yao, J.N.3    Loo, B.H.4
  • 14
    • 0011513080 scopus 로고
    • Kinetics of the oxidation of pure tungsten from 500 to 1300°C
    • Gulbransen E.A., Andrew K.F. Kinetics of the oxidation of pure tungsten from 500 to 1300°C. J. Electrochem. Soc. 1960, 107:619-628.
    • (1960) J. Electrochem. Soc. , vol.107 , pp. 619-628
    • Gulbransen, E.A.1    Andrew, K.F.2
  • 15
    • 0042033403 scopus 로고
    • The structure of oxide layers on tungsten
    • Kellet E.A., Rogers S.E. The structure of oxide layers on tungsten. J. Electrochem. Soc. 1963, 110:502-504.
    • (1963) J. Electrochem. Soc. , vol.110 , pp. 502-504
    • Kellet, E.A.1    Rogers, S.E.2
  • 16
    • 0019047175 scopus 로고
    • Oxidation mechanism of niobium (673-823K) and tungsten (773-973K)
    • Rosa C.J., Chen G.C., Sikka V.K. Oxidation mechanism of niobium (673-823K) and tungsten (773-973K). Z. Metallk. 1980, 71:529-534.
    • (1980) Z. Metallk. , vol.71 , pp. 529-534
    • Rosa, C.J.1    Chen, G.C.2    Sikka, V.K.3
  • 18
    • 0040775398 scopus 로고
    • Thin oxide films on tungsten
    • Gulbransen E.A., Wysong W.S. Thin oxide films on tungsten. Trans. AIME 1948, 175:611-627.
    • (1948) Trans. AIME , vol.175 , pp. 611-627
    • Gulbransen, E.A.1    Wysong, W.S.2
  • 19
    • 0042028722 scopus 로고
    • Eigenschaften von molybdän und wolfram bei niedrigen und mittleren temperaturen
    • Nachtigall E. Eigenschaften von molybdän und wolfram bei niedrigen und mittleren temperaturen. Z. Metallk. 1952, 43:23-26.
    • (1952) Z. Metallk. , vol.43 , pp. 23-26
    • Nachtigall, E.1
  • 21
    • 84886179285 scopus 로고
    • High pressure oxidation of metals-Tungsten in oxygen
    • Baur J.P., Bridges D.W., Fassell W.M. High pressure oxidation of metals-Tungsten in oxygen. J. Electrochem. Soc. 1956, 103:266-272.
    • (1956) J. Electrochem. Soc. , vol.103 , pp. 266-272
    • Baur, J.P.1    Bridges, D.W.2    Fassell, W.M.3
  • 22
    • 0345182105 scopus 로고
    • The formation of porous oxides on metals. II. Tungsten and the paralinear rate law
    • Jepson W.B., Aylmore D.W. The formation of porous oxides on metals. II. Tungsten and the paralinear rate law. J. Electrochem. Soc. 1961, 108:942-947.
    • (1961) J. Electrochem. Soc. , vol.108 , pp. 942-947
    • Jepson, W.B.1    Aylmore, D.W.2
  • 23
    • 84857052355 scopus 로고
    • High temperature oxidation protection of tungsten, NASA Tecnichal Traslations, NASA TT F-583, Translation from " Atom" Press, 1968.
    • V.Y. Ivanov, Y.P. Nechiporenko, L.N. Yefimenko, M.I. Yurchenko, High temperature oxidation protection of tungsten, NASA Tecnichal Traslations, NASA TT F-583, 1969, Translation from " Atom" Press, 1968.
    • (1969)
    • Ivanov, V.Y.1    Nechiporenko, Y.P.2    Yefimenko, L.N.3    Yurchenko, M.I.4
  • 24
    • 67349153827 scopus 로고    scopus 로고
    • Cracking failure study of ITER-reference tungsten grade under single pulse thermal shock loads at elevated temperatures
    • Hirai T., Pintsuk G., Linke J., Batilliot M. Cracking failure study of ITER-reference tungsten grade under single pulse thermal shock loads at elevated temperatures. J. Nucl. Mater. 2009, 390-391:751-754.
    • (2009) J. Nucl. Mater. , pp. 751-754
    • Hirai, T.1    Pintsuk, G.2    Linke, J.3    Batilliot, M.4
  • 25
    • 0019286973 scopus 로고
    • The oxidation kinetics of tungsten and the determination of oxygen diffusion coefficient in tungsten trioxide
    • Sikka V.K., Rosa C.J. The oxidation kinetics of tungsten and the determination of oxygen diffusion coefficient in tungsten trioxide. Corros. Sci. 1980, 20:1201-1219.
    • (1980) Corros. Sci. , vol.20 , pp. 1201-1219
    • Sikka, V.K.1    Rosa, C.J.2
  • 26
    • 84857058146 scopus 로고
    • An electron diffraction study of oxide films formed on molybdenum tungsten, and alloys of molybdenum, tungsten and nickel
    • Hickman J.W., Gulbransen E.A. An electron diffraction study of oxide films formed on molybdenum tungsten, and alloys of molybdenum, tungsten and nickel. Trans. AIME 1947, 171:371-388.
    • (1947) Trans. AIME , vol.171 , pp. 371-388
    • Hickman, J.W.1    Gulbransen, E.A.2
  • 27
    • 0029621564 scopus 로고
    • Formation and incorporation of dopant phases during technical reduction of NS-doped tungsten blue oxide
    • Schubert W.D., Lux B., Zeiler B. Formation and incorporation of dopant phases during technical reduction of NS-doped tungsten blue oxide. Int. J. Refract. Met. Hard Mater. 1995, 13:119-135.
    • (1995) Int. J. Refract. Met. Hard Mater. , vol.13 , pp. 119-135
    • Schubert, W.D.1    Lux, B.2    Zeiler, B.3
  • 28
    • 0342699736 scopus 로고    scopus 로고
    • The effect of niobium on the oxidation behavior of titanium in N2/20% O2 atmospheres
    • Pérez P., Haanappel V.A.C., Stroosnijder M.F. The effect of niobium on the oxidation behavior of titanium in N2/20% O2 atmospheres. Mater. Sci. Eng. 2000, A284:126-137.
    • (2000) Mater. Sci. Eng. , vol.A284 , pp. 126-137
    • Pérez, P.1    Haanappel, V.A.C.2    Stroosnijder, M.F.3
  • 29
    • 33751509941 scopus 로고    scopus 로고
    • On the influence of water vapour on the oxidation behavior of pure Ti
    • Pérez P. On the influence of water vapour on the oxidation behavior of pure Ti. Corros. Sci. 2007, 49:1172-1185.
    • (2007) Corros. Sci. , vol.49 , pp. 1172-1185
    • Pérez, P.1
  • 30
    • 0018480328 scopus 로고
    • Surface electrical properties of tungsten oxides in equilibrium with the gas phase
    • Bonnet J.P., Nowotny J., Onillon M., Sikora I. Surface electrical properties of tungsten oxides in equilibrium with the gas phase. Oxid. Met. 1979, 13:273-282.
    • (1979) Oxid. Met. , vol.13 , pp. 273-282
    • Bonnet, J.P.1    Nowotny, J.2    Onillon, M.3    Sikora, I.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.