메뉴 건너뛰기




Volumn 97, Issue 2, 2012, Pages 192-199

Depletion mechanism of antioxidants in MDPE-clay nanocomposites under thermal aging

Author keywords

Antioxidant; Heat aging; Nanoclay; Nanocomposite; Polyethylene

Indexed keywords

AGING TIME; ANTIOXIDANT; DEPLETION MECHANISM; FIRST ORDER REACTIONS; HEAT AGING; LINEAR STRUCTURES; NANO CLAYS; PHENOLIC ANTIOXIDANT; SURFACE REGION;

EID: 84855526555     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymdegradstab.2011.10.010     Document Type: Article
Times cited : (18)

References (23)
  • 2
    • 0000301688 scopus 로고    scopus 로고
    • Polymer-silicate nanocomposites: Model systems for confined polymers and polymer brushes
    • E. Giannelis, R. Krishnamoorti, and E. Manias Polymer-silicate nanocomposites: model systems for confined polymers and polymer brushes Polymers in Confined Environments 138 1999 107 147
    • (1999) Polymers in Confined Environments , vol.138 , pp. 107-147
    • Giannelis, E.1    Krishnamoorti, R.2    Manias, E.3
  • 3
    • 0032755689 scopus 로고    scopus 로고
    • Flammability and thermal stability studies of polymer layered-silicate (clay) nanocomposites
    • W.G. Jeffrey Flammability and thermal stability studies of polymer layered-silicate (clay) nanocomposites Applied Clay Science 15 1999 31 49
    • (1999) Applied Clay Science , vol.15 , pp. 31-49
    • Jeffrey, W.G.1
  • 4
    • 0029777844 scopus 로고    scopus 로고
    • Polymer layered silicate nanocomposites
    • E.P. Giannelis Polymer layered silicate nanocomposites Advanced Materials 8 1996 29 35 (Pubitemid 126557654)
    • (1996) Advanced Materials , vol.8 , Issue.1 , pp. 29-35
    • Giannelis, E.P.1
  • 5
  • 6
    • 0242407166 scopus 로고    scopus 로고
    • Polymer/layered silicate nanocomposites: A review from preparation to processing
    • S. Sinha Ray, and M. Okamoto Polymer/layered silicate nanocomposites: a review from preparation to processing Progress in Polymer Science 28 2003 1539 1641
    • (2003) Progress in Polymer Science , vol.28 , pp. 1539-1641
    • Sinha Ray, S.1    Okamoto, M.2
  • 8
    • 77349105294 scopus 로고    scopus 로고
    • Accelerating effect of montmorillonite on oxidative degradation of polyethylene nanocomposites
    • T.O. Kumanayaka, R. Parthasarathy, and M. Jollands Accelerating effect of montmorillonite on oxidative degradation of polyethylene nanocomposites Polymer Degradation and Stability 95 2010 672 676
    • (2010) Polymer Degradation and Stability , vol.95 , pp. 672-676
    • Kumanayaka, T.O.1    Parthasarathy, R.2    Jollands, M.3
  • 9
    • 14844297062 scopus 로고    scopus 로고
    • Photooxidation of polypropylene/montmorillonite nanocomposites. 2. Interactions with antioxidants
    • DOI 10.1021/cm040172l
    • S. Morlat-Therias, B. Mailhot, D. Gonzalez, and J.-L. Gardette Photooxidation of polypropylene/montmorillonite nanocomposites. 2. interactions with antioxidants Chemistry of Materials 17 2005 1072 1078 (Pubitemid 40344030)
    • (2005) Chemistry of Materials , vol.17 , Issue.5 , pp. 1072-1078
    • Morlat-Therias, S.1    Mailhot, B.2    Gonzalez, D.3    Gardette, J.-L.4
  • 10
    • 0020982330 scopus 로고
    • Thermogravimetric studies of the thermooxidation stability of irradiated and unirradiated polyethylene - Part i. Effect of antioxidant
    • DOI 10.1016/0146-5724(83)90072-9
    • O. Gal, L. Novakovic, V. Markovic, and V.T. Stannett Thermogravimetric studies of the thermooxidative stability of irradiated and unirradiated polyethylene part I. effect of antioxidant Radiation Physics and Chemistry 22 1977 627 634 (Pubitemid 14619439)
    • (1982) Radiation Physics and Chemistry , vol.22 , Issue.3-5 , pp. 627-634
    • Gal, O.1    Novakovic, Lj.2    Markovic, V.3    Stannett, V.T.4
  • 11
    • 33646820081 scopus 로고    scopus 로고
    • Organoclay degradation in melt processed polyethylene nanocomposites
    • DOI 10.1016/j.polymer.2006.02.031, PII S0032386106002060
    • R.K. Shah, and D.R. Paul Organoclay degradation in melt processed polyethylene nanocomposites Polymer 47 2006 4075 4084 (Pubitemid 43767364)
    • (2006) Polymer , vol.47 , Issue.11 , pp. 4075-4084
    • Shah, R.K.1    Paul, D.R.2
  • 13
    • 0035202944 scopus 로고    scopus 로고
    • Thermal degradation chemistry of alkyl quaternary ammonium Montmorillonite
    • DOI 10.1021/cm010305s
    • W. Xie, Z. Gao, W.-P. Pan, D. Hunter, A. Singh, and R. Vaia Thermal degradation chemistry of alkyl quaternary ammonium montmorillonite Chemistry of Materials 13 2001 2979 2990 (Pubitemid 33121305)
    • (2001) Chemistry of Materials , vol.13 , Issue.9 , pp. 2979-2990
    • Xie, W.1    Gao, Z.2    Pan, W.-P.3    Hunter, D.4    Singh, A.5    Vaia, R.6
  • 14
    • 84989029849 scopus 로고
    • Modeling of antioxidant loss from polyolefins in hot-water applications. I: Model and application to medium density polyethylene pipes
    • G.D. Smith, K. Karlsson, and U.W. Gedde Modeling of antioxidant loss from polyolefins in hot-water applications. I: model and application to medium density polyethylene pipes Polymer Engineering & Science 32 1992 658 667
    • (1992) Polymer Engineering & Science , vol.32 , pp. 658-667
    • Smith, G.D.1    Karlsson, K.2    Gedde, U.W.3
  • 16
    • 0031248429 scopus 로고    scopus 로고
    • Evaluation of the oxidation behavior of polyethylene geomembranes using oxidative induction time tests
    • Y.G. Hsuan Evaluation of the oxidation behavior of polyethylene geomembranes using oxidative induction time tests Alan T. Riga, G.H. Patterson, Oxidative behavior of materials by thermal analytical techniques 1997 ASTM Special Technical Publication West Conshohocken, PA 19428 76 90 (Pubitemid 127637329)
    • (1997) ASTM Special Technical Publication , vol.1326 , pp. 76-90
    • Hsuan, Y.G.1    Guan, Z.2
  • 17
    • 0032304697 scopus 로고    scopus 로고
    • Influence of various stabilizer systems on the ageing behavior of PE-MD - I. Hot-water ageing of compression molded plaques
    • PII S0141391098000482
    • G. Dörner, and R.W. Lang Influence of various stabilizer systems on the ageing behavior of PE-MD-I. hot-water ageing of compression molded plaques Polymer Degradation and Stability 62 1998 421 430 (Pubitemid 128425950)
    • (1998) Polymer Degradation and Stability , vol.62 , Issue.3 , pp. 421-430
    • Dorner, G.1    Lang, R.W.2
  • 22
    • 0032099818 scopus 로고    scopus 로고
    • Antioxidant depletion lifetime in high density polyethylene geomembranes
    • DOI 10.1061/(ASCE)1090-0241(1998)124:6(532)
    • Y.G. Hsuan, and R.M. Koerner Antioxidant depletion lifetime in high density polyethylene geomembranes Journal of Geotechnical and Geoenvironmental Engineering 124 1998 532 541 (Pubitemid 28429879)
    • (1998) Journal of Geotechnical and Geoenvironmental Engineering , vol.124 , Issue.6 , pp. 532-541
    • Hsuan, Y.G.1    Koerner, R.M.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.