Elimination of Start/Stop defects in laser cladding

Author keywords

Defects; Dilution; Laser cladding; Microstructure

Indexed keywords

CIRCULAR GEOMETRY; COATING POWDER; CONTROLLED THICKNESS; HARDNESS VARIATION; LASER TRACKS; METALLIC SUBSTRATE; METALLOGRAPHIC METHOD; MICROHARDNESS MEASUREMENT; MICROSTRUCTURAL FEATURES; MICROSTRUCTURE AND PROPERTIES; NON-HOMOGENEOUS; OVERLAPPING AREA; STEEL SUBSTRATE; WEAR RESISTANT;

EID: 84855273684     PISSN: 02578972     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.surfcoat.2011.10.040     Document Type: Article
Times cited : (52)

References (24)
  • 1
    • 84893141176 scopus 로고    scopus 로고
    • Woodhead Publishing Limited and CRC Press, Oxford, L.J. Pou, D.K.Y. Low, E. Toyserkani (Eds.)
    • Ocelík V., De Hosson J.Th.M. Advances in Laser Materials Processing 2010, 426. Woodhead Publishing Limited and CRC Press, Oxford. L.J. Pou, D.K.Y. Low, E. Toyserkani (Eds.).
    • (2010) Advances in Laser Materials Processing , pp. 426
    • Ocelík, V.1    De Hosson, J.2
  • 24
    • 84855294992 scopus 로고    scopus 로고
    • visited in June 2011
    • visited in June 2011. http://www.uddeholm.ee/english/files/vanadis_23-english.pdf.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.