Volumn 70, Issue 6, 1997, Pages 173-185

Interaction between lead crystal glass (24 % PbO) and acetic acid

Author keywords

[No Author keywords available]

Indexed keywords


EID: 8444223974     PISSN: 09467475     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (3)

References (47)
  • 1
    • 0022009338 scopus 로고
    • The durability of glass - A review
    • Newton, R. G.: The durability of glass - a review. Glass Technol. 26 (1985) no. 1, p. 21-38.
    • (1985) Glass Technol. , vol.26 , Issue.1 , pp. 21-38
    • Newton, R.G.1
  • 2
    • 8444224938 scopus 로고
    • Chemical durability of glass containing high proportions of lead oxide in relation to their structure
    • Abou-El-Azm, A.; Hussein, A. L.: Chemical durability of glass containing high proportions of lead oxide in relation to their structure. J. Chem. U. A. R. 5 (1962) no. 1, p. 1-20.
    • (1962) J. Chem. U. A. R. , vol.5 , Issue.1 , pp. 1-20
    • Abou-El-Azm, A.1    Hussein, A.L.2
  • 4
    • 0016926571 scopus 로고
    • Interaction of dilute acetic acid with lead-containing vitreous surfaces
    • Eppler, R. A.; Schweikert, W. F.: Interaction of dilute acetic acid with lead-containing vitreous surfaces. Am. Ceram. Soc. Bull. 55 (1976) no. 3. p. 277-280, 285.
    • (1976) Am. Ceram. Soc. Bull. , vol.55 , Issue.3 , pp. 277-280
    • Eppler, R.A.1    Schweikert, W.F.2
  • 5
    • 0020129341 scopus 로고
    • Lead-ion stability in vitreous systems
    • Krajewski, A.; Ravaglioli, A.: Lead-ion stability in vitreous systems. J. Am. Ceram. Soc. 65 (1982) no. 5, p. 265-269.
    • (1982) J. Am. Ceram. Soc. , vol.65 , Issue.5 , pp. 265-269
    • Krajewski, A.1    Ravaglioli, A.2
  • 6
    • 0018057839 scopus 로고
    • Influence of complexing agents and nature of buffer solution on the chemical durability of glass. Pt. 1. Theoretical discussion
    • Paul, A.: Influence of complexing agents and nature of buffer solution on the chemical durability of glass. Pt. 1. Theoretical discussion. Glass Technol. 19 (1978) no. 6, p. 162-165.
    • (1978) Glass Technol. , vol.19 , Issue.6 , pp. 162-165
    • Paul, A.1
  • 7
    • 0018057839 scopus 로고
    • Influence of complexing agents and nature of buffer solution on the chemical durability of glass. Pt. 2. Effect of EDTA, ethyl alcohol and sugar in the leach solution
    • Paul, A.; Youssefi, A.: Influence of complexing agents and nature of buffer solution on the chemical durability of glass. Pt. 2. Effect of EDTA, ethyl alcohol and sugar in the leach solution. Glass Technol. 19 (1978) no. 6, p. 166-170.
    • (1978) Glass Technol. , vol.19 , Issue.6 , pp. 166-170
    • Paul, A.1    Youssefi, A.2
  • 10
    • 0018011766 scopus 로고
    • Mechanism of modifier release from lead containing glasses in acid solution
    • Lehman, R. L.; Yoon, S. C.; McLaren, M. G. et al.: Mechanism of modifier release from lead containing glasses in acid solution. Am. Ceram. Soc. Bull. 57 (1978) no. 9, p. 802-805.
    • (1978) Am. Ceram. Soc. Bull. , vol.57 , Issue.9 , pp. 802-805
    • Lehman, R.L.1    Yoon, S.C.2    McLaren, M.G.3
  • 11
    • 0005964793 scopus 로고
    • Lead-ion stability in soda-lime lead silicate glasses
    • Lehman, R. L.: Lead-ion stability in soda-lime lead silicate glasses. J. Am. Ceram. Soc. 75 (1992) no. 8, p. 2194-2199.
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.8 , pp. 2194-2199
    • Lehman, R.L.1
  • 12
    • 4243050190 scopus 로고
    • Leaching of lead from lead crystal
    • Rybařiková, L.; Lejbl, L.; Hradecká, H.: Leaching of lead from lead crystal. (Orig. Czech.) Sklař Keram. 42 (1992) no. 10, p. 317-320.
    • (1992) Sklař Keram. , vol.42 , Issue.10 , pp. 317-320
    • Rybařiková, L.1    Lejbl, L.2    Hradecká, H.3
  • 13
    • 0027577349 scopus 로고
    • How much lead leaches from crystal glassware?
    • Varshneya, A. K.; Frederes, K. P.: How much lead leaches from crystal glassware? Glass Ind. 74 (1993) no. 5, p. 22-23.
    • (1993) Glass Ind. , vol.74 , Issue.5 , pp. 22-23
    • Varshneya, A.K.1    Frederes, K.P.2
  • 14
    • 0027585808 scopus 로고
    • The extraction of lead from lead crystalware
    • Seddon, A. B.; Whall, M. E.: The extraction of lead from lead crystalware. Glass Technol. 34 (1993) no. 2, p. 71-73.
    • (1993) Glass Technol. , vol.34 , Issue.2 , pp. 71-73
    • Seddon, A.B.1    Whall, M.E.2
  • 21
    • 0028515546 scopus 로고
    • Testing procedures for food contact hollowware
    • Testing procedures for food contact hollowware. Am. Ceram. Soc. Bull. 73 (1994) no. 9, p. 93-95.
    • (1994) Am. Ceram. Soc. Bull. , vol.73 , Issue.9 , pp. 93-95
  • 23
    • 8444237718 scopus 로고
    • The preparation of glass grain samples for durability tests
    • Sykes, R. F. R.: The preparation of glass grain samples for durability tests. Glass Technol. 6 (1965) no. 6, p. 178-183.
    • (1965) Glass Technol. , vol.6 , Issue.6 , pp. 178-183
    • Sykes, R.F.R.1
  • 25
    • 0005926263 scopus 로고
    • Attack of lead crystal glass (24% PbO) by solutions of some organic acids
    • Ahemd, A. A.; Abbas, A. F.; Youssof, I. M.: Attack of lead crystal glass (24% PbO) by solutions of some organic acids. Glastech. Ber. Glass Sci. Technol. 68C1 (1995) p. 223-229.
    • (1995) Glastech. Ber. Glass Sci. Technol. , vol.68 C1 , pp. 223-229
    • Ahemd, A.A.1    Abbas, A.F.2    Youssof, I.M.3
  • 26
    • 0030086160 scopus 로고    scopus 로고
    • Dissolution of lead crystal glass (24 % PbO) in aqueous solutions of ethyl and methyl alcohols
    • Ahmed, A. A.; Youssof, I. M.: Dissolution of lead crystal glass (24 % PbO) in aqueous solutions of ethyl and methyl alcohols. Glass Technol. 37 (1996) no. 1, p. 21-28.
    • (1996) Glass Technol. , vol.37 , Issue.1 , pp. 21-28
    • Ahmed, A.A.1    Youssof, I.M.2
  • 27
    • 8444226656 scopus 로고
    • Some surface area estimations of grains used in glass durability testing
    • Sewell, P. A.: Some surface area estimations of grains used in glass durability testing. Glass Technol. 10 (1969) no. 1, p. 9-14.
    • (1969) Glass Technol. , vol.10 , Issue.1 , pp. 9-14
    • Sewell, P.A.1
  • 30
    • 0042188297 scopus 로고
    • Effect of glass surface area to solution volume ratio on glass corrosion
    • Ethridge, E. C.; Clark, D. E.; Hench, L. L.: Effect of glass surface area to solution volume ratio on glass corrosion. Phys. Chem. Glasses 20 (1979) no. 2, p. 35-40.
    • (1979) Phys. Chem. Glasses , vol.20 , Issue.2 , pp. 35-40
    • Ethridge, E.C.1    Clark, D.E.2    Hench, L.L.3
  • 32
    • 0023998694 scopus 로고
    • Surface area measurements on glass fibres and glass powders and the influence of corrosion
    • Wittkopf, H.; Bösel, M.: Surface area measurements on glass fibres and glass powders and the influence of corrosion. Glass Technol. 29 (1988) no. 2, p. 60-63.
    • (1988) Glass Technol. , vol.29 , Issue.2 , pp. 60-63
    • Wittkopf, H.1    Bösel, M.2
  • 33
    • 84977686322 scopus 로고
    • Reactions of glasses with aqueous solutions
    • Douglas, R. W.; El-Shamy, T. M. M,: Reactions of glasses with aqueous solutions. J. Am. Ceram. Soc. 50 (1967) no. 1, p. 1-8.
    • (1967) J. Am. Ceram. Soc. , vol.50 , Issue.1 , pp. 1-8
    • Douglas, R.W.1    El-Shamy, T.M.M.2
  • 34
    • 84980128694 scopus 로고
    • Interference films on glass. Pt. 2. Some observations during acid leaching of X-ray plate glass
    • Anderson, S.; Kimpton, D. D.: Interference films on glass. Pt. 2. Some observations during acid leaching of X-ray plate glass. J. Am. Ceram. Soc. 36 (1953) no. 6, p. 175-179.
    • (1953) J. Am. Ceram. Soc. , vol.36 , Issue.6 , pp. 175-179
    • Anderson, S.1    Kimpton, D.D.2
  • 35
    • 84975545928 scopus 로고
    • Fundamental condition of glass formation
    • Sun, K.-H.: Fundamental condition of glass formation. J. Am. Ceram. Soc. 30 (1947) no. 9, p. 277-281.
    • (1947) J. Am. Ceram. Soc. , vol.30 , Issue.9 , pp. 277-281
    • Sun, K.-H.1
  • 36
    • 0016950113 scopus 로고
    • Lead release from glazes and glasses in contact with acid solutions
    • Yoon, S.-C.; Krefft, G. B.; McLaren, M. G.: Lead release from glazes and glasses in contact with acid solutions. Am. Ceram. Soc. Bull. 55 (1976) no. 5, p. 508-510, 512.
    • (1976) Am. Ceram. Soc. Bull. , vol.55 , Issue.5 , pp. 508-510
    • Yoon, S.-C.1    Krefft, G.B.2    McLaren, M.G.3
  • 37
    • 8444222267 scopus 로고
    • Dissolution phenomenon of some optical glass in an acid
    • Tsuchihashi, S.: Dissolution phenomenon of some optical glass in an acid. Bull. Chem. Soc. Jap. 24 (1951) no. 4, p. 161-164.
    • (1951) Bull. Chem. Soc. Jap. , vol.24 , Issue.4 , pp. 161-164
    • Tsuchihashi, S.1
  • 40
    • 4243169264 scopus 로고
    • The use of radioactive tracers to investigate corrosion mechanisms of glasses in aqueous solutions
    • Cockram, D. R.; Fyles, K. M.; Wilson, C. J.: The use of radioactive tracers to investigate corrosion mechanisms of glasses in aqueous solutions. Riv. Stn. Sper. Vetro 14 (1984) no. 5, p. 83-89.
    • (1984) Riv. Stn. Sper. Vetro , vol.14 , Issue.5 , pp. 83-89
    • Cockram, D.R.1    Fyles, K.M.2    Wilson, C.J.3
  • 41
    • 4243057328 scopus 로고
    • Reactions of glass with aqueous solutions and nonaqueous environments
    • Doremus, R. H.: Reactions of glass with aqueous solutions and nonaqueous environments. Mater. Res. Soc. Symp. Proc. 125 (1988) p. 177-188.
    • (1988) Mater. Res. Soc. Symp. Proc. , vol.125 , pp. 177-188
    • Doremus, R.H.1
  • 42
    • 0028438194 scopus 로고
    • Dissolution kinetics of silica glass as a function of pH between 40 and 85 °C
    • Mazer, J. J.; Walther, J. V.: Dissolution kinetics of silica glass as a function of pH between 40 and 85 °C. J. Non-Cryst. Solids 170 (1994) p. 32-45.
    • (1994) J. Non-Cryst. Solids , vol.170 , pp. 32-45
    • Mazer, J.J.1    Walther, J.V.2
  • 43
    • 4243180455 scopus 로고
    • Über die physikalisch-chemischen Vorgänge bei der Wasserauslaugung von Glasoberflächen
    • Žagar, L.; Schillmöller, A.: Über die physikalisch-chemischen Vorgänge bei der Wasserauslaugung von Glasoberflächen. Glastech. Ber. 33 (1960) no. 4, p. 109-116.
    • (1960) Glastech. Ber. , vol.33 , Issue.4 , pp. 109-116
    • Žagar, L.1    Schillmöller, A.2
  • 44
    • 8444222636 scopus 로고
    • Time and temperature dependence of the mechanism of corrosion of soda-lime-silica glass
    • Beijing 1995. Beijing: Chinese Ceram. Soc.
    • Ahmed, A. A.; Youssof, I. M.: Time and temperature dependence of the mechanism of corrosion of soda-lime-silica glass. In: Proc. XVII International Congress on Glass, Beijing 1995. Vol. 3 Beijing: Chinese Ceram. Soc., 1995. p. 704-709.
    • (1995) Proc. XVII International Congress on Glass , vol.3 , pp. 704-709
    • Ahmed, A.A.1    Youssof, I.M.2
  • 46
    • 0017559946 scopus 로고
    • Chemical durability of glasses: A thermodynamic approach
    • Paul, A.: Chemical durability of glasses: a thermodynamic approach. J. Mater. Sci. 12 (1977) no. 11, p. 2246-2268.
    • (1977) J. Mater. Sci. , vol.12 , Issue.11 , pp. 2246-2268
    • Paul, A.1
  • 47
    • 0015354252 scopus 로고
    • The dependence on the pH of the decomposition of glasses by aqueous solutions
    • El-Shamy, T. M. M.; Lewins, J.; Douglas, R. W: The dependence on the pH of the decomposition of glasses by aqueous solutions. Glass Technol. 13 (1972) no. 3, p. 81-87.
    • (1972) Glass Technol. , vol.13 , Issue.3 , pp. 81-87
    • El-Shamy, T.M.M.1    Lewins, J.2    Douglas, R.W.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.