The shape of a strain-based failure assessment diagram

Author keywords

Defects; Failure assessment diagram; Fracture; Strain based

Indexed keywords

FAILURE ASSESSMENT DIAGRAM; FE ANALYSIS; FINITE ELEMENTS; FITNESS FOR SERVICE; FRACTURE ASSESSMENT; IN-LINE; STRAIN-BASED; STRAIN-HARDENING CAPACITY; WORKED EXAMPLES;

EID: 83955161700     PISSN: 03080161     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijpvp.2011.09.004     Document Type: Article
Times cited : (42)

References (17)
  • 2
    • 83955164134 scopus 로고    scopus 로고
    • R6 Revision 4, Assessment of the integrity of structures containing defects, British Energy, 2001, with Amendments to March 2010, British Energy, Gloucester.
    • R6 Revision 4, Assessment of the integrity of structures containing defects, British Energy, 2001, with Amendments to March 2010, British Energy, Gloucester.
  • 4
    • 61749099698 scopus 로고    scopus 로고
    • GKSS, Geesthacht, Germany, M. Koçak, S. Webster, J.J. Janosch, R.A. Ainsworth, R. Koers (Eds.)
    • FITNET fitness for service procedure 2008, GKSS, Geesthacht, Germany. M. Koçak, S. Webster, J.J. Janosch, R.A. Ainsworth, R. Koers (Eds.).
    • (2008) FITNET fitness for service procedure
  • 5
    • 0004224318 scopus 로고    scopus 로고
    • American Petroleum Institute/ASME, Washington, DC, API 579-1/ASME FFS-1
    • API 579-1/ASME FFS-1 Fitness-for-service 2007, American Petroleum Institute/ASME, Washington, DC.
    • (2007) Fitness-for-service
  • 7
    • 11344257669 scopus 로고    scopus 로고
    • Fracture response of pipelines subject to large plastic deformation under bending
    • Østby E., Jayadevan K.R., Thaulow C. Fracture response of pipelines subject to large plastic deformation under bending. Int J Pres Ves Piping 2005, 82:201-215.
    • (2005) Int J Pres Ves Piping , vol.82 , pp. 201-215
    • Østby, E.1    Jayadevan, K.R.2    Thaulow, C.3
  • 10
    • 30444461213 scopus 로고    scopus 로고
    • Failure assessment diagram methods for strain-based fracture
    • Budden P.J. Failure assessment diagram methods for strain-based fracture. Engng Fract Mech 2006, 73:537-552.
    • (2006) Engng Fract Mech , vol.73 , pp. 537-552
    • Budden, P.J.1
  • 12
    • 83955165785 scopus 로고    scopus 로고
    • Numerical validation of a strain-based failure assessment diagram approach to fracture. In: Proc ASME PVP2009, PVP2009-77377, Prague, July 26-30, 2009.
    • Budden PJ, Smith MC. Numerical validation of a strain-based failure assessment diagram approach to fracture. In: Proc ASME PVP2009, PVP2009-77377, Prague, July 26-30, 2009.
    • Budden, P.J.1    Smith, M.C.2
  • 13
    • 83955165783 scopus 로고    scopus 로고
    • The treatment of secondary strains within a strain-based failure assessment diagram, submitted for publication.
    • Ainsworth RA, Budden PJ, Oh C-Y, Kim Y-J. The treatment of secondary strains within a strain-based failure assessment diagram, submitted for publication.
    • Ainsworth, R.A.1    Budden, P.J.2    Oh, C.-Y.3    Kim, Y.-J.4
  • 14
    • 0021214889 scopus 로고
    • The assessment of defects in structures of strain hardening material
    • Ainsworth R.A. The assessment of defects in structures of strain hardening material. Engng Fract Mech 1984, 19:633-642.
    • (1984) Engng Fract Mech , vol.19 , pp. 633-642
    • Ainsworth, R.A.1
  • 17
    • 1542715929 scopus 로고    scopus 로고
    • J-integral and limit load analysis of semi-elliptical surface cracks in plates under tension
    • Lei Y. J-integral and limit load analysis of semi-elliptical surface cracks in plates under tension. Int J Pres Vessels Piping 2004, 81:21-30.
    • (2004) Int J Pres Vessels Piping , vol.81 , pp. 21-30
    • Lei, Y.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.