Volumn 53, Issue 12, 2011, Pages 4102-4108

The oxidation behavior and mechanical properties of MoSi2-CrSi2-SiC-Si coated carbon/carbon composites in high-temperature oxidizing atmosphere

Author keywords

A. Ceramic matrix composites; A. Intermetallic; C. Oxidation

Indexed keywords

C/C COMPOSITES; CARBON/CARBON; HIGH-TEMPERATURE OXIDIZING; INTERMEDIATE TEMPERATURES; MASS LOSS; MULTI-COMPONENT COATINGS; OXIDATION BEHAVIORS; PACK-CEMENTATION METHOD; ROOM TEMPERATURE; THERMAL CYCLE; THERMAL MISMATCH;

EID: 80053445030     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2011.08.018     Document Type: Article
Times cited : (32)

References (27)
  • 1
    • 5744233935 scopus 로고    scopus 로고
    • Oxidation resistant carbon materials derived from boronated carbon-silicon alloys
    • Westwood A.V.K., Rand B., Lu S. Oxidation resistant carbon materials derived from boronated carbon-silicon alloys. Carbon 2004, 42:3071-3080.
    • (2004) Carbon , vol.42 , pp. 3071-3080
    • Westwood, A.V.K.1    Rand, B.2    Lu, S.3
  • 2
    • 43349085320 scopus 로고    scopus 로고
    • Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites
    • Corral E., Loehman R. Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites. J. Am. Ceram. Soc. 2008, 91:1495-1502.
    • (2008) J. Am. Ceram. Soc. , vol.91 , pp. 1495-1502
    • Corral, E.1    Loehman, R.2
  • 3
    • 33644982737 scopus 로고    scopus 로고
    • Oxidation microstructure studies of reinforced carbon/carbon
    • Jacobson N.S., Curry D.M. Oxidation microstructure studies of reinforced carbon/carbon. Carbon 2006, 44:1142-1150.
    • (2006) Carbon , vol.44 , pp. 1142-1150
    • Jacobson, N.S.1    Curry, D.M.2
  • 4
    • 0027798044 scopus 로고
    • Oxidation protection of carbon-carbon composites using chemical vapour deposition and glaze technology
    • Buchanan F.J., Little J.A. Oxidation protection of carbon-carbon composites using chemical vapour deposition and glaze technology. Corros. Sci. 1993, 35:1243-1250.
    • (1993) Corros. Sci. , vol.35 , pp. 1243-1250
    • Buchanan, F.J.1    Little, J.A.2
  • 5
    • 74849133693 scopus 로고    scopus 로고
    • A simple model for the oxidation of carbon-containing composites
    • Hou X.M., Chou K.C. A simple model for the oxidation of carbon-containing composites. Corros. Sci. 2010, 52:1093-1097.
    • (2010) Corros. Sci. , vol.52 , pp. 1093-1097
    • Hou, X.M.1    Chou, K.C.2
  • 6
    • 2542471748 scopus 로고    scopus 로고
    • Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites
    • Huang J.F., Zeng X.R., Li H.J., Xiong X.B., Fu Y.W. Influence of the preparation temperature on the phase, microstructure and anti-oxidation property of a SiC coating for C/C composites. Carbon 2004, 42:1517-1521.
    • (2004) Carbon , vol.42 , pp. 1517-1521
    • Huang, J.F.1    Zeng, X.R.2    Li, H.J.3    Xiong, X.B.4    Fu, Y.W.5
  • 8
    • 27744510122 scopus 로고    scopus 로고
    • SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites
    • Li H.J., Fu Q.G., Shi X.H., Li K.Z., Hu Z.B. SiC whisker-toughened SiC oxidation protective coating for carbon/carbon composites. Carbon 2006, 44:602-605.
    • (2006) Carbon , vol.44 , pp. 602-605
    • Li, H.J.1    Fu, Q.G.2    Shi, X.H.3    Li, K.Z.4    Hu, Z.B.5
  • 9
    • 69649086417 scopus 로고    scopus 로고
    • A Si-Mo-W coating to protect SiC-coated carbon/carbon composites against oxidation
    • Fu Q.G., Li H.J., Li K.Z., Tong Ke A Si-Mo-W coating to protect SiC-coated carbon/carbon composites against oxidation. J. Am. Ceram. Soc. 2009, 92:2132-2135.
    • (2009) J. Am. Ceram. Soc. , vol.92 , pp. 2132-2135
    • Fu, Q.G.1    Li, H.J.2    Li, K.Z.3    Tong, K.4
  • 10
    • 62849105031 scopus 로고    scopus 로고
    • Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites
    • Liu Y.S., Zhang L.T., Cheng L.F., Yang W.B., Zhang W.H., Xu Y.D. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites. Corros. Sci. 2009, 51:820-826.
    • (2009) Corros. Sci. , vol.51 , pp. 820-826
    • Liu, Y.S.1    Zhang, L.T.2    Cheng, L.F.3    Yang, W.B.4    Zhang, W.H.5    Xu, Y.D.6
  • 12
    • 74849138851 scopus 로고    scopus 로고
    • Multilayer oxidation protective coating for C/C composites from room temperature to 1500 C
    • Fu Q.G., Li H.J., Wang Y.J., Li K.Z., Tao J. Multilayer oxidation protective coating for C/C composites from room temperature to 1500 C. Surf. Coat. Technol. 2010, 204:1831-1835.
    • (2010) Surf. Coat. Technol. , vol.204 , pp. 1831-1835
    • Fu, Q.G.1    Li, H.J.2    Wang, Y.J.3    Li, K.Z.4    Tao, J.5
  • 14
    • 38849140327 scopus 로고    scopus 로고
    • An oxidation protective Si-Mo-Cr coating for C/SiC coated carbon/carbon composites
    • Zhang Y.L., Li H.J., Fu Q.G., Yao X.Y., Li K.Z., Jiao G.S. An oxidation protective Si-Mo-Cr coating for C/SiC coated carbon/carbon composites. Carbon 2008, 46:179-182.
    • (2008) Carbon , vol.46 , pp. 179-182
    • Zhang, Y.L.1    Li, H.J.2    Fu, Q.G.3    Yao, X.Y.4    Li, K.Z.5    Jiao, G.S.6
  • 15
    • 34548203896 scopus 로고    scopus 로고
    • Si-W-Mo coating for SiC coated carbon/carbon composites against oxidation
    • Li K.Z., Hou D.S., Li H.J., Fu Q.G., Jiao G.S. Si-W-Mo coating for SiC coated carbon/carbon composites against oxidation. Surf. Coat. Technol. 2007, 201:9598-9602.
    • (2007) Surf. Coat. Technol. , vol.201 , pp. 9598-9602
    • Li, K.Z.1    Hou, D.S.2    Li, H.J.3    Fu, Q.G.4    Jiao, G.S.5
  • 17
    • 75749107857 scopus 로고    scopus 로고
    • 2-Si/SiC coated C/C composites in static and aerodynamic oxidation environment
    • 2-Si/SiC coated C/C composites in static and aerodynamic oxidation environment. Carbon 2010, 48:1636-1642.
    • (2010) Carbon , vol.48 , pp. 1636-1642
    • Li, H.J.1    Feng, T.2    Fu, Q.G.3    Wu, H.4    Shen, X.T.5
  • 19
    • 39749154748 scopus 로고    scopus 로고
    • Influence of the matrix texture on the fracture behavior of 2D carbon/carbon composites
    • Xu G.Z., Li H.J., Bai R.C., Wei J., Zhai Y.Q. Influence of the matrix texture on the fracture behavior of 2D carbon/carbon composites. Mater. Sci. Eng. A 2008, 478:319-323.
    • (2008) Mater. Sci. Eng. A , vol.478 , pp. 319-323
    • Xu, G.Z.1    Li, H.J.2    Bai, R.C.3    Wei, J.4    Zhai, Y.Q.5
  • 20
    • 0031421149 scopus 로고    scopus 로고
    • Microstructure and oxidation behaviour of chromium-molybdenum silicides
    • Tomasi A., Ceccato R., Nazmy M., Gialanella S. Microstructure and oxidation behaviour of chromium-molybdenum silicides. Mater. Sci. Eng. A 1997, 239-240:877-881.
    • (1997) Mater. Sci. Eng. A , pp. 877-881
    • Tomasi, A.1    Ceccato, R.2    Nazmy, M.3    Gialanella, S.4
  • 21
    • 69449089060 scopus 로고    scopus 로고
    • 2 oxidation resistant coating for carbon/carbon composites by a two-step pack cementation
    • 2 oxidation resistant coating for carbon/carbon composites by a two-step pack cementation. Corros. Sci. 2009, 51:2450-2454.
    • (2009) Corros. Sci. , vol.51 , pp. 2450-2454
    • Fu, Q.G.1    Li, H.J.2    Wang, Y.J.3    Li, K.Z.4    Shi, X.H.5
  • 23
    • 19944406834 scopus 로고    scopus 로고
    • Design of a C/SiC functionally graded coating for the oxidation protection of C/C composites
    • Kim J.I., Kim J.W., Choi D.J., Park J.Y., Ryu W.S. Design of a C/SiC functionally graded coating for the oxidation protection of C/C composites. Carbon 2005, 43:1749-1757.
    • (2005) Carbon , vol.43 , pp. 1749-1757
    • Kim, J.I.1    Kim, J.W.2    Choi, D.J.3    Park, J.Y.4    Ryu, W.S.5
  • 24
    • 33846534109 scopus 로고    scopus 로고
    • Effect of thermal expansion coefficient on the stress distribution in solar panel
    • Wang X.Y., Geng H.B., He S.Y., Pokhyl Y.O., Koval K.V. Effect of thermal expansion coefficient on the stress distribution in solar panel. Int. J. Adhes. Adhes. 2007, 27:288-297.
    • (2007) Int. J. Adhes. Adhes. , vol.27 , pp. 288-297
    • Wang, X.Y.1    Geng, H.B.2    He, S.Y.3    Pokhyl, Y.O.4    Koval, K.V.5
  • 25
    • 0035275936 scopus 로고    scopus 로고
    • Functionally gradient ceramic coating for carbon-carbon antioxidation protection
    • Cairo C.A.A., Graca M.L.A., Silva C.R.M., Bressiani J.C. Functionally gradient ceramic coating for carbon-carbon antioxidation protection. J. Eur. Ceram. Soc. 2001, 21:325-329.
    • (2001) J. Eur. Ceram. Soc. , vol.21 , pp. 325-329
    • Cairo, C.A.A.1    Graca, M.L.A.2    Silva, C.R.M.3    Bressiani, J.C.4
  • 26
    • 0023963893 scopus 로고
    • Ceramic coating for carbon-carbon composites
    • Strife J.R. Ceramic coating for carbon-carbon composites. Ceram. Bull. 1988, 67:369-374.
    • (1988) Ceram. Bull. , vol.67 , pp. 369-374
    • Strife, J.R.1
  • 27
    • 0027282886 scopus 로고
    • Corrosion of silicon-based ceramics in combustion environment
    • Jacobson N.S. Corrosion of silicon-based ceramics in combustion environment. J. Am. Ceram. Soc. 1993, 76:3-28.
    • (1993) J. Am. Ceram. Soc. , vol.76 , pp. 3-28
    • Jacobson, N.S.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.