Volumn 183, Issue 9, 2010, Pages 2004-2011
|
Controlled synthesis and luminescent properties of Eu2+(Eu 3+), Dy3+-doped Sr3Al2O6 phosphors by hydrothermal treatment and postannealing approach
|
Author keywords
Hydrothermal; Phosphor; Postannealing; Sr3Al2O6
|
Indexed keywords
CALCINATION TEMPERATURE;
CONTROLLED SYNTHESIS;
DECAY CURVES;
EMISSION SPECTRUMS;
EXCITATION SPECTRUM;
HYDROTHERMAL;
HYDROTHERMAL REACTION;
HYDROTHERMAL TREATMENTS;
LUMINESCENT PROPERTY;
MOLE RATIO;
POST ANNEALING;
REACTION PARAMETERS;
REDUCING ATMOSPHERE;
SCIENTIFIC MERITS;
SHAPE AND SIZE;
SODIUM CITRATE;
SR3AL2O6;
STARTING MATERIALS;
ALUMINUM;
CALCINATION;
EMISSION SPECTROSCOPY;
LUMINESCENCE;
PHOSPHORS;
SODIUM;
SYNTHESIS (CHEMICAL);
EUROPIUM;
|
EID: 80052749059
PISSN: 00224596
EISSN: 1095726X
Source Type: Journal
DOI: 10.1016/j.jssc.2010.04.008 Document Type: Article |
Times cited : (22)
|
References (20)
|