Effect of surface oxidation on thermal shock resistance of the ZrB2-SiC-ZrC ceramic

Author keywords

A. Ceramics; B. Strength; D. SEM

Indexed keywords

A. CERAMICS; B. STRENGTH; CONSTANT TEMPERATURE; ISOTHERMAL OXIDATIONS; OXIDE LAYER; STATIC AIR; SURFACE OXIDATIONS; THERMAL SHOCK RESISTANCE; WATER QUENCHING;

EID: 79961210778     PISSN: 02663538     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.compscitech.2011.06.008     Document Type: Article
Times cited : (44)

References (23)
  • 2
    • 42249098072 scopus 로고    scopus 로고
    • 2-SiC ultra high temperature ceramics under simulated atmospheric re-entry conditions
    • 2-SiC ultra high temperature ceramics under simulated atmospheric re-entry conditions. Compos Sci Technol 2008, 68:1718-1726.
    • (2008) Compos Sci Technol , vol.68 , pp. 1718-1726
    • Zhang, X.H.1    Hu, P.2    Han, J.C.3    Meng, S.H.4
  • 6
    • 0035331482 scopus 로고    scopus 로고
    • Microstructure, mechanical performance and oxidation mechanism of boride in situ composites
    • Chen C.M., Zhang L.T., Zhou W.C., Hao Z.Z., Jiang Y.J., Yang S.L. Microstructure, mechanical performance and oxidation mechanism of boride in situ composites. Compos Sci Technol 2001, 61:971-975.
    • (2001) Compos Sci Technol , vol.61 , pp. 971-975
    • Chen, C.M.1    Zhang, L.T.2    Zhou, W.C.3    Hao, Z.Z.4    Jiang, Y.J.5    Yang, S.L.6
  • 7
    • 34248595626 scopus 로고    scopus 로고
    • 2 in situ composite by SHS dynamic compaction: a novel approach
    • 2 in situ composite by SHS dynamic compaction: a novel approach. Compos Sci Technol 2007, 67:2447-2453.
    • (2007) Compos Sci Technol , vol.67 , pp. 2447-2453
    • Mishra, S.K.1    Das, S.K.2    Sherbacov, V.3
  • 8
    • 84980119785 scopus 로고
    • Factors affecting thermal stress resistance of ceramic materials
    • Kingery W.D. Factors affecting thermal stress resistance of ceramic materials. J Am Ceram Soc 1955, 38(1):3-15.
    • (1955) J Am Ceram Soc , vol.38 , Issue.1 , pp. 3-15
    • Kingery, W.D.1
  • 11
    • 0015681016 scopus 로고
    • Crack propagation studies in brittle materials
    • Griffith A.A. Crack propagation studies in brittle materials. J Mater Sci 1920, 8:1527-1533.
    • (1920) J Mater Sci , vol.8 , pp. 1527-1533
    • Griffith, A.A.1
  • 12
    • 0942266769 scopus 로고    scopus 로고
    • Crack-healing in reaction-bonded silicon carbide
    • Chu M.C., Cho S.J., Park H.M., Yoon K.J., Ryu H. Crack-healing in reaction-bonded silicon carbide. Mater Lett 2004, 58:1313-1316.
    • (2004) Mater Lett , vol.58 , pp. 1313-1316
    • Chu, M.C.1    Cho, S.J.2    Park, H.M.3    Yoon, K.J.4    Ryu, H.5
  • 15
    • 47749138531 scopus 로고    scopus 로고
    • 2-ZrC-SiC composites fabricated by hot pressing and reactive hot pressing
    • 2-ZrC-SiC composites fabricated by hot pressing and reactive hot pressing. Scr Mater 2008, 59:753-756.
    • (2008) Scr Mater , vol.59 , pp. 753-756
    • Zhang, X.H.1    Qu, Q.2    Han, J.C.3    Han, W.B.4    Hong, C.Q.5
  • 16
    • 0037008364 scopus 로고    scopus 로고
    • A thermoanalytical study on the oxidation of ZrC and HfC powders with formation of carbon
    • Shimada S. A thermoanalytical study on the oxidation of ZrC and HfC powders with formation of carbon. Solid State Ionics 2002, 149:319-326.
    • (2002) Solid State Ionics , vol.149 , pp. 319-326
    • Shimada, S.1
  • 18
    • 33846372666 scopus 로고    scopus 로고
    • Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C
    • Rezaie A., Fahrenholtz W.G., Hilmas G.E. Evolution of structure during the oxidation of zirconium diboride-silicon carbide in air up to 1500°C. J Eur Ceram Soc 2007, 27:2495-2501.
    • (2007) J Eur Ceram Soc , vol.27 , pp. 2495-2501
    • Rezaie, A.1    Fahrenholtz, W.G.2    Hilmas, G.E.3
  • 19
    • 60849108043 scopus 로고    scopus 로고
    • 2-SiC: influence of SiC content on solid and liquid oxide phase formation
    • 2-SiC: influence of SiC content on solid and liquid oxide phase formation. J Am Ceram Soc 2009, 92(2):481-486.
    • (2009) J Am Ceram Soc , vol.92 , Issue.2 , pp. 481-486
    • Karlsdottir, S.N.1    Halloran, J.W.2
  • 21
    • 57849135454 scopus 로고    scopus 로고
    • Microstructure and properties of silicon carbide whisker reinforced zirconium diboride ultra-high temperature ceramics
    • Zhang X.H., Xu L., Han W.B., Weng L., Han J.C. Microstructure and properties of silicon carbide whisker reinforced zirconium diboride ultra-high temperature ceramics. Solid State Sci 2009, 11:156-161.
    • (2009) Solid State Sci , vol.11 , pp. 156-161
    • Zhang, X.H.1    Xu, L.2    Han, W.B.3    Weng, L.4    Han, J.C.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.