Volumn 65, Issue 6, 2011, Pages 520-523
|
Ultrafine-grained surface layer on Mg-Al-Zn alloy produced by cryogenic burnishing for enhanced corrosion resistance
|
Author keywords
Corrosion; Magnesium alloys; Severe plastic deformation (SPD); Texture; Ultrafine grained microstructure
|