Volumn 53, Issue 10, 2011, Pages 3114-3121

Use of inkjet printing to deposit magnesium chloride salt patterns for investigation of atmospheric corrosion of 304 stainless steel

Author keywords

A. Stainless steel; C. Atmospheric corrosion

Indexed keywords

304 STAINLESS STEEL; A. STAINLESS STEEL; C. ATMOSPHERIC CORROSION; MAGNESIUM CHLORIDES; OHMIC DROP; SALT DEPOSITION;

EID: 79960717206     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2011.05.055     Document Type: Article
Times cited : (34)

References (32)
  • 1
    • 84934953224 scopus 로고
    • Environmental factors affecting critical potential for pitting in 18-8 stainless steel
    • Leckie H.P., Uhlig H.H. Environmental factors affecting critical potential for pitting in 18-8 stainless steel. J. Electrochem. Soc. 1966, 113:1262.
    • (1966) J. Electrochem. Soc. , vol.113 , pp. 1262
    • Leckie, H.P.1    Uhlig, H.H.2
  • 2
    • 38849189337 scopus 로고    scopus 로고
    • An analytical modeling method for calculating the maximum cathode current deliverable by a circular cathode under atmospheric exposure
    • Wit Press/Computational Mechanics Publications, Southampton, V.G. DeGiorgi, C.A. Brebbia, R.A. Adey (Eds.)
    • Chen Z.Y., Kelly R.G. An analytical modeling method for calculating the maximum cathode current deliverable by a circular cathode under atmospheric exposure. Simulation of Electrochemical Processes II 2007, 33-41. Wit Press/Computational Mechanics Publications, Southampton. V.G. DeGiorgi, C.A. Brebbia, R.A. Adey (Eds.).
    • (2007) Simulation of Electrochemical Processes II , pp. 33-41
    • Chen, Z.Y.1    Kelly, R.G.2
  • 3
    • 0031117719 scopus 로고    scopus 로고
    • Influence of electrolyte layer thickness and pH on the initial stage of the atmospheric corrosion of iron
    • Nishikata A., Ichihara Y., Hayashi Y., Tsuru T. Influence of electrolyte layer thickness and pH on the initial stage of the atmospheric corrosion of iron. J. Electrochem. Soc. 1997, 144:1244-1252.
    • (1997) J. Electrochem. Soc. , vol.144 , pp. 1244-1252
    • Nishikata, A.1    Ichihara, Y.2    Hayashi, Y.3    Tsuru, T.4
  • 4
    • 27644568955 scopus 로고    scopus 로고
    • Computational modeling of cathodic limitations on localized corrosion of wetted SS 316L at room temperature
    • Cui F.S., Presuel-Moreno F.J., Kelly R.G. Computational modeling of cathodic limitations on localized corrosion of wetted SS 316L at room temperature. Corros. Sci. 2005, 47:2987-3005.
    • (2005) Corros. Sci. , vol.47 , pp. 2987-3005
    • Cui, F.S.1    Presuel-Moreno, F.J.2    Kelly, R.G.3
  • 5
    • 0025445155 scopus 로고
    • The atmospheric corrosion of iron - A discussion of the physicochemical fundamentals of this omnipresent corrosion process - Invited review
    • Stratmann M. The atmospheric corrosion of iron - A discussion of the physicochemical fundamentals of this omnipresent corrosion process - Invited review. Ber. Bunsen-Ges. Phys. Chem. Chem. Phys. 1990, 94:626-639.
    • (1990) Ber. Bunsen-Ges. Phys. Chem. Chem. Phys. , vol.94 , pp. 626-639
    • Stratmann, M.1
  • 6
    • 0025192732 scopus 로고
    • On the atmospheric corrosion of metals which are covered with thin electrolyte layers. 1. Verification of the experimental-technique
    • Stratmann M., Streckel H. On the atmospheric corrosion of metals which are covered with thin electrolyte layers. 1. Verification of the experimental-technique. Corros. Sci. 1990, 30:681-696.
    • (1990) Corros. Sci. , vol.30 , pp. 681-696
    • Stratmann, M.1    Streckel, H.2
  • 7
    • 0000503980 scopus 로고
    • Effect of supplementary alloying elements on pitting corrosion susceptibility of 18Cr-14Ni stainless steel
    • Tomashov N.D., Chernova G.P., Marcova O.N. Effect of supplementary alloying elements on pitting corrosion susceptibility of 18Cr-14Ni stainless steel. Corrosion 1964, 20:T166.
    • (1964) Corrosion , vol.20
    • Tomashov, N.D.1    Chernova, G.P.2    Marcova, O.N.3
  • 8
    • 0031247948 scopus 로고    scopus 로고
    • Localised dissolution kinetics, salt films and pitting potentials
    • Laycock N.J., Newman R.C. Localised dissolution kinetics, salt films and pitting potentials. Corros. Sci. 1997, 39:1771-1790.
    • (1997) Corros. Sci. , vol.39 , pp. 1771-1790
    • Laycock, N.J.1    Newman, R.C.2
  • 10
    • 8644277100 scopus 로고    scopus 로고
    • Holistic model for atmospheric corrosion - Part 6 - From wet aerosol to salt deposit
    • Cole I.S., Lau D., Paterson D.A. Holistic model for atmospheric corrosion - Part 6 - From wet aerosol to salt deposit. Corros. Eng., Sci. Technol. 2004, 39:209-218.
    • (2004) Corros. Eng., Sci. Technol. , vol.39 , pp. 209-218
    • Cole, I.S.1    Lau, D.2    Paterson, D.A.3
  • 11
    • 2542485674 scopus 로고    scopus 로고
    • Effect of sodium chloride particles on the atmospheric corrosion of pure copper
    • Chen Z.Y., Zakipour S., Persson D., Leygraf C. Effect of sodium chloride particles on the atmospheric corrosion of pure copper. Corrosion 2004, 60:479-491.
    • (2004) Corrosion , vol.60 , pp. 479-491
    • Chen, Z.Y.1    Zakipour, S.2    Persson, D.3    Leygraf, C.4
  • 12
  • 13
    • 33645167230 scopus 로고    scopus 로고
    • Micro-droplets formation during the deliquescence of salt particles in atmosphere
    • Zhang J., Wang J., Wang Y. Micro-droplets formation during the deliquescence of salt particles in atmosphere. Corrosion 2005, 61:1167-1172.
    • (2005) Corrosion , vol.61 , pp. 1167-1172
    • Zhang, J.1    Wang, J.2    Wang, Y.3
  • 14
    • 77749330220 scopus 로고    scopus 로고
    • Atmospheric corrosion initiation on steel from predeposited NaCl salt particles in high humidity atmospheres
    • Li S.X., Hihara L.H. Atmospheric corrosion initiation on steel from predeposited NaCl salt particles in high humidity atmospheres. Corros. Eng., Sci. Technol. 2010, 45:49-56.
    • (2010) Corros. Eng., Sci. Technol. , vol.45 , pp. 49-56
    • Li, S.X.1    Hihara, L.H.2
  • 15
    • 0038547018 scopus 로고    scopus 로고
    • Mechanism of atmospheric corrosion of copper in the presence of ammonium sulfate particles - Effect of surface particle concentration
    • Lobnig R., Sinclair J.D., Unger M., Stratmann M. Mechanism of atmospheric corrosion of copper in the presence of ammonium sulfate particles - Effect of surface particle concentration. J. Electrochem. Soc. 2003, 150:A835-A849.
    • (2003) J. Electrochem. Soc. , vol.150
    • Lobnig, R.1    Sinclair, J.D.2    Unger, M.3    Stratmann, M.4
  • 16
    • 2442613774 scopus 로고    scopus 로고
    • Formation and growth of micro-droplets during the initial stage of atmospheric corrosion
    • Tsuru T., Tamiya K.I., Nishikata A. Formation and growth of micro-droplets during the initial stage of atmospheric corrosion. Electrochim. Acta 2004, 49:2709-2715.
    • (2004) Electrochim. Acta , vol.49 , pp. 2709-2715
    • Tsuru, T.1    Tamiya, K.I.2    Nishikata, A.3
  • 17
    • 33751538868 scopus 로고    scopus 로고
    • Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions
    • Tsutsumi Y., Nishikata A., Tsuru T. Pitting corrosion mechanism of Type 304 stainless steel under a droplet of chloride solutions. Corros. Sci. 2007, 49:1394-1407.
    • (2007) Corros. Sci. , vol.49 , pp. 1394-1407
    • Tsutsumi, Y.1    Nishikata, A.2    Tsuru, T.3
  • 18
    • 33745034226 scopus 로고    scopus 로고
    • Study of the atmospheric corrosion of galvanised steel in a micrometric electrolytic droplet
    • Dubuisson E., Lavie P., Dalard F., Caire J.P., Szunerits S. Study of the atmospheric corrosion of galvanised steel in a micrometric electrolytic droplet. Electrochem. Commun. 2006, 8:911-915.
    • (2006) Electrochem. Commun. , vol.8 , pp. 911-915
    • Dubuisson, E.1    Lavie, P.2    Dalard, F.3    Caire, J.P.4    Szunerits, S.5
  • 20
    • 77950299665 scopus 로고    scopus 로고
    • Pitting corrosion of Type 430 stainless steel under chloride solution droplet
    • Hastuty S., Nishikata A., Tsuru T. Pitting corrosion of Type 430 stainless steel under chloride solution droplet. Corros. Sci. 2010, 52:2035-2043.
    • (2010) Corros. Sci. , vol.52 , pp. 2035-2043
    • Hastuty, S.1    Nishikata, A.2    Tsuru, T.3
  • 21
    • 0034773430 scopus 로고    scopus 로고
    • Inkjet printing for materials and devices
    • Calvert P. Inkjet printing for materials and devices. Chem. Mater. 2001, 13:3299-3305.
    • (2001) Chem. Mater. , vol.13 , pp. 3299-3305
    • Calvert, P.1
  • 22
    • 0344034235 scopus 로고    scopus 로고
    • Inkjet printing of functional materials
    • Sirringhaus H., Shimoda T. Inkjet printing of functional materials. MRS Bull. 2003, 28:802-803.
    • (2003) MRS Bull. , vol.28 , pp. 802-803
    • Sirringhaus, H.1    Shimoda, T.2
  • 23
    • 1542285058 scopus 로고    scopus 로고
    • Inkjet printing of polymers: state of the art and future developments
    • de Gans B.J., Duineveld P.C., Schubert U.S. Inkjet printing of polymers: state of the art and future developments. Adv. Mater. 2004, 16:203-213.
    • (2004) Adv. Mater. , vol.16 , pp. 203-213
    • de Gans, B.J.1    Duineveld, P.C.2    Schubert, U.S.3
  • 24
    • 0024768463 scopus 로고
    • Design criteria and future-directions in inkjet ink technology
    • Croucher M.D., Hair M.L. Design criteria and future-directions in inkjet ink technology. Ind. Eng. Chem. Res. 1989, 28:1712-1718.
    • (1989) Ind. Eng. Chem. Res. , vol.28 , pp. 1712-1718
    • Croucher, M.D.1    Hair, M.L.2
  • 26
    • 25444459649 scopus 로고    scopus 로고
    • Inkjet printing of nanosized silver colloids
    • Lee H.H., Chou K.S., Huang K.C. Inkjet printing of nanosized silver colloids. Nanotechnology 2005, 16:2436-2441.
    • (2005) Nanotechnology , vol.16 , pp. 2436-2441
    • Lee, H.H.1    Chou, K.S.2    Huang, K.C.3
  • 27
    • 77955737171 scopus 로고    scopus 로고
    • Application of inkjet printing for depositing salt prior to atmospheric corrosion testing
    • Schindelholz E., Kelly R.G. Application of inkjet printing for depositing salt prior to atmospheric corrosion testing. Electrochem. Solid State Lett. 2010, 13:C29-C31.
    • (2010) Electrochem. Solid State Lett. , vol.13
    • Schindelholz, E.1    Kelly, R.G.2
  • 29
    • 60849083250 scopus 로고    scopus 로고
    • Low-temperature stress corrosion cracking of stainless steels in the atmosphere in the presence of chloride deposits
    • Prosek T., Iversen A., Taxen C., Thierry D. Low-temperature stress corrosion cracking of stainless steels in the atmosphere in the presence of chloride deposits. Corrosion 2009, 65:105-117.
    • (2009) Corrosion , vol.65 , pp. 105-117
    • Prosek, T.1    Iversen, A.2    Taxen, C.3    Thierry, D.4
  • 30
    • 0036497710 scopus 로고    scopus 로고
    • The initiation mechanism of corrosion of zinc by sodium chloride particle deposition
    • Neufeld A.K., Cole I.S., Bond A.M., Furman S.A. The initiation mechanism of corrosion of zinc by sodium chloride particle deposition. Corros. Sci. 2002, 44:555-572.
    • (2002) Corros. Sci. , vol.44 , pp. 555-572
    • Neufeld, A.K.1    Cole, I.S.2    Bond, A.M.3    Furman, S.A.4
  • 31
    • 77956220092 scopus 로고    scopus 로고
    • Pitting corrosion of bare stainless steel 304 under chloride solution droplets
    • Maier B., Frankel G.S. Pitting corrosion of bare stainless steel 304 under chloride solution droplets. J. Electrochem. Soc. 2010, 157:C302-C312.
    • (2010) J. Electrochem. Soc. , vol.157
    • Maier, B.1    Frankel, G.S.2
  • 32
    • 73849138528 scopus 로고    scopus 로고
    • Computational modeling of bounding conditions for pit size on stainless steel in atmospheric environments
    • Chen Z.Y., Kelly R.G. Computational modeling of bounding conditions for pit size on stainless steel in atmospheric environments. J. Electrochem. Soc. 2010, 157:C69-C78.
    • (2010) J. Electrochem. Soc. , vol.157
    • Chen, Z.Y.1    Kelly, R.G.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.