Volumn 53, Issue 9, 2011, Pages 2778-2784

The corrosion behaviour of Zr-based bulk metallic glasses in 0.5M NaCl solution

Author keywords

A. Alloy; B. SEM; B. XPS; C. Passive films; C. Pitting corrosion

Indexed keywords

A. ALLOY; BULK METALLIC GLASS; CORROSION BEHAVIOUR; ELECTROCHEMICAL MEASUREMENTS; ENERGY DISPERSIVE X RAY SPECTROSCOPY; NACL SOLUTION; OXYHYDROXIDES; PASSIVE FILMS; SCANNING ELECTRON MICROSCOPES; TAKE-OFF ANGLE; XPS ANALYSIS; ZR BASED BULK METALLIC GLASS;

EID: 79959372656     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2011.05.014     Document Type: Article
Times cited : (79)

References (31)
  • 3
    • 0034993695 scopus 로고    scopus 로고
    • New Fe-Cr-Mo-(Nb, Ta)-C-B glassy alloys with high glass-forming ability and good corrosion resistance
    • Pang S.J., Zhang T., Asami K., Inoue A. New Fe-Cr-Mo-(Nb, Ta)-C-B glassy alloys with high glass-forming ability and good corrosion resistance. Mater. Trans. 2001, 42:376-379.
    • (2001) Mater. Trans. , vol.42 , pp. 376-379
    • Pang, S.J.1    Zhang, T.2    Asami, K.3    Inoue, A.4
  • 4
    • 78650045325 scopus 로고    scopus 로고
    • Localized corrosion resistance of Fe-Cr-Mo-W-B-C bulk metallic glasses containing Mn+Si or Y in neutral and acidified chloride solutions
    • 035003-1-035003-15
    • Huang R., Horton D.J., Bocher F., Scully J.R. Localized corrosion resistance of Fe-Cr-Mo-W-B-C bulk metallic glasses containing Mn+Si or Y in neutral and acidified chloride solutions. Corrosion 2010, 66:035003-1-035003-15.
    • (2010) Corrosion , vol.66
    • Huang, R.1    Horton, D.J.2    Bocher, F.3    Scully, J.R.4
  • 5
    • 0035978605 scopus 로고    scopus 로고
    • Highly corrosion-resistant Ni-based bulk amorphous alloys
    • Kawashima A., Habazaki H., Hashimoto K. Highly corrosion-resistant Ni-based bulk amorphous alloys. Mater. Sci. Eng. A 2001, 304-307:753-757.
    • (2001) Mater. Sci. Eng. A , pp. 753-757
    • Kawashima, A.1    Habazaki, H.2    Hashimoto, K.3
  • 8
    • 0038543497 scopus 로고    scopus 로고
    • Corrosion behaviour of Cu-Zr-Ti-Nb bulk glassy alloys
    • Qin C.L., Asami K., Zhang T., Zhang W., Inoue A. Corrosion behaviour of Cu-Zr-Ti-Nb bulk glassy alloys. Mater. Trans. 2003, 44:749-753.
    • (2003) Mater. Trans. , vol.44 , pp. 749-753
    • Qin, C.L.1    Asami, K.2    Zhang, T.3    Zhang, W.4    Inoue, A.5
  • 11
    • 0035888221 scopus 로고    scopus 로고
    • Hot water corrosion behaviour of Zr-Cu-Al-Ni bulk metallic glass
    • Gebert A., Buchholz K., El-Aziz A.M., Eckert J. Hot water corrosion behaviour of Zr-Cu-Al-Ni bulk metallic glass. Mater. Sci. Eng. A 2001, 316:60-65.
    • (2001) Mater. Sci. Eng. A , vol.316 , pp. 60-65
    • Gebert, A.1    Buchholz, K.2    El-Aziz, A.M.3    Eckert, J.4
  • 14
    • 33644898806 scopus 로고    scopus 로고
    • Stress-corrosion fatigue-crack growth in a Zr-based bulk amorphous metal
    • Schroeder V., Ritchie R.O. Stress-corrosion fatigue-crack growth in a Zr-based bulk amorphous metal. Acta Mater. 2006, 54:1785-1794.
    • (2006) Acta Mater. , vol.54 , pp. 1785-1794
    • Schroeder, V.1    Ritchie, R.O.2
  • 16
    • 77953957962 scopus 로고    scopus 로고
    • Zr-based bulk glassy alloy with improved resistance to stress corrosion cracking in sodium chloride solutions
    • Kawashima A., Yokoyama Y., Inoue A. Zr-based bulk glassy alloy with improved resistance to stress corrosion cracking in sodium chloride solutions. Corros. Sci. 2010, 52:2950-2957.
    • (2010) Corros. Sci. , vol.52 , pp. 2950-2957
    • Kawashima, A.1    Yokoyama, Y.2    Inoue, A.3
  • 17
    • 67651243895 scopus 로고    scopus 로고
    • Malleable hypoeutectic Zr-Ni-Cu-Al bulk glassy alloys with tensile plastic elongation at room temperature
    • Yokoyama Y., Fujita K., Yavari A.R., Inoue A. Malleable hypoeutectic Zr-Ni-Cu-Al bulk glassy alloys with tensile plastic elongation at room temperature. Philos. Mag. Lett. 2009, 89:322-334.
    • (2009) Philos. Mag. Lett. , vol.89 , pp. 322-334
    • Yokoyama, Y.1    Fujita, K.2    Yavari, A.R.3    Inoue, A.4
  • 19
    • 0036761604 scopus 로고    scopus 로고
    • Pseudo float melting state in ladle arc-melt-type furnace for preparing crystalline inclusion-free bulk amorphous alloy
    • Yokoyama Y., Inoue K., Fukaura K. Pseudo float melting state in ladle arc-melt-type furnace for preparing crystalline inclusion-free bulk amorphous alloy. Mater. Trans. 2002, 43:2316-2319.
    • (2002) Mater. Trans. , vol.43 , pp. 2316-2319
    • Yokoyama, Y.1    Inoue, K.2    Fukaura, K.3
  • 20
    • 0036859869 scopus 로고    scopus 로고
    • Cast structure and mechanical properties of Zr-Cu-Ni-Al bulk glassy alloys
    • Yokoyama Y., Fukaura K., Inoue A. Cast structure and mechanical properties of Zr-Cu-Ni-Al bulk glassy alloys. Intermetallics 2002, 10:1113-1124.
    • (2002) Intermetallics , vol.10 , pp. 1113-1124
    • Yokoyama, Y.1    Fukaura, K.2    Inoue, A.3
  • 22
    • 0014866053 scopus 로고
    • Significance of protection potential in pitting and intergranular corrosion
    • Pourbaix M. Significance of protection potential in pitting and intergranular corrosion. Corrosion 1970, 26:431-440.
    • (1970) Corrosion , vol.26 , pp. 431-440
    • Pourbaix, M.1
  • 25
    • 77949281098 scopus 로고    scopus 로고
    • Effect of surface finishing of a Zr-based bulk metallic glass on its corrosion behaviour
    • Gebert A., Gostin P.F., Schultz L. Effect of surface finishing of a Zr-based bulk metallic glass on its corrosion behaviour. Corros. Sci. 2010, 52:1711-1720.
    • (2010) Corros. Sci. , vol.52 , pp. 1711-1720
    • Gebert, A.1    Gostin, P.F.2    Schultz, L.3
  • 26
    • 0017632531 scopus 로고
    • XPS determination and the compositions of alloy surface and surface oxides on mechanically polished iron-chromium alloys
    • Asami K., Hashimoto K., Shimodaira S. XPS determination and the compositions of alloy surface and surface oxides on mechanically polished iron-chromium alloys. Corros. Sci. 1977, 17:713-723.
    • (1977) Corros. Sci. , vol.17 , pp. 713-723
    • Asami, K.1    Hashimoto, K.2    Shimodaira, S.3
  • 28
    • 0034042250 scopus 로고    scopus 로고
    • Interpretation of Ni 2p XPS spectra of Ni conductors and Ni insulators
    • Nesbitt H.W., Legrand D., Bancroft G.M. Interpretation of Ni 2p XPS spectra of Ni conductors and Ni insulators. Phys. Chem. Miner. 2000, 27:357-366.
    • (2000) Phys. Chem. Miner. , vol.27 , pp. 357-366
    • Nesbitt, H.W.1    Legrand, D.2    Bancroft, G.M.3
  • 29
    • 0021294961 scopus 로고
    • An XPS study of anodic behaviour of amorphous nickel-phosphorus alloys containing chromium, molybdenum or tungsten in 1M HCl
    • Kawashima A., Asami K., Hashimoto K. An XPS study of anodic behaviour of amorphous nickel-phosphorus alloys containing chromium, molybdenum or tungsten in 1M HCl. Corros. Sci. 1984, 24:807-823.
    • (1984) Corros. Sci. , vol.24 , pp. 807-823
    • Kawashima, A.1    Asami, K.2    Hashimoto, K.3
  • 30
    • 0036475814 scopus 로고    scopus 로고
    • Surface characterization of amorphous Zr-Al-(Ni, Cu) alloys immersed in cell-culture medium
    • Hiromoto S., Asami K., Hanawa T. Surface characterization of amorphous Zr-Al-(Ni, Cu) alloys immersed in cell-culture medium. Mater. Trans. 2002, 43:261-266.
    • (2002) Mater. Trans. , vol.43 , pp. 261-266
    • Hiromoto, S.1    Asami, K.2    Hanawa, T.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.