Volumn 191, Issue 1, 2011, Pages 61-67

Oxygen exchange kinetics of La0.58Sr0.4Co 0.2Fe0.8O3 at 600 °c in dry and humid atmospheres

Author keywords

Cathode; Degradation; LSCF; Oxygen exchange kinetics; Solid oxide fuel cell

Indexed keywords

CHEMICAL SURFACES; CORE-LEVEL SPECTRA; DC CONDUCTIVITY; DEPTH PROFILE; DRY AIR; DRY ATMOSPHERES; ELEMENTAL SURFACES; GLASS-CERAMIC SEALS; HUMID ATMOSPHERES; INTERMEDIATE TEMPERATURES; LONG-TERM OPERATION; LSCF; OXYGEN CONCENTRATIONS; OXYGEN CONTENT; OXYGEN EXCHANGE; OXYGEN EXCHANGE KINETICS; RELAXATION MEASUREMENTS; SAMPLE SURFACE; SECONDARY PHASIS; SEM ANALYSIS; SILICATE LAYERS; SOFC STACK; SOLID OXIDE; SURFACE OXYGEN; THERMAL INSULATION MATERIALS; TIME-DEPENDENT; TIME-DEPENDENT DECAY; XPS;