Volumn 27, Issue 6, 2011, Pages 527-534

A novel polymer infiltrated ceramic dental material

Author keywords

CAD CAM; Mechanical properties; Nanoindentation; Polymer infiltrated ceramic

Indexed keywords

CAD/CAMS; DENTAL CAD/CAM; FRACTURE MECHANISMS; FRACTURE TOUGHNESS VALUES; FRACTURED SURFACES; HUMAN ENAMEL; INDENTATION CREEP; INDENTATION SIZE EFFECTS; INTERPENETRATING POLYMERS; MANUFACTURING PROCEDURE; MECHANICAL BEHAVIOR; NEW MEMBERS; NOVEL POLYMERS; POROUS CERAMICS; PROCESSING PRESSURE; SAMPLE PREPARATION; SEM; SINGLE-EDGE-NOTCHED; STRESS-STRAIN RELATIONSHIPS;

EID: 79955639497     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.dental.2011.02.002     Document Type: Article
Times cited : (157)

References (20)
  • 2
    • 52449118551 scopus 로고    scopus 로고
    • Factors essential for successful all-ceramic restorations
    • T.E. Donovan Factors essential for successful all-ceramic restorations J Am Dent Assoc 139 2008 14S 18S
    • (2008) J Am Dent Assoc , vol.139
    • Donovan, T.E.1
  • 3
    • 38949178423 scopus 로고    scopus 로고
    • Wear of ceramic and antagonist-A systematic evaluation of influencing factors in vitro
    • DOI 10.1016/j.dental.2007.06.016, PII S0109564107001376
    • S.D. Heintze, A. Cavalleri, M. Forjanic, G. Zellweger, and V. Rousson Wear of ceramic and antagonist - a systematic evaluation of influencing factors in vitro Dent Mater 24 2008 433 449 (Pubitemid 351222672)
    • (2008) Dental Materials , vol.24 , Issue.4 , pp. 433-449
    • Heintze, S.D.1    Cavalleri, A.2    Forjanic, M.3    Zellweger, G.4    Rousson, V.5
  • 4
    • 0026875935 scopus 로고
    • An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments
    • W.C. Oliver, and G.M. Pharr An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments J Mater Res 7 1992 1564 1583
    • (1992) J Mater Res , vol.7 , pp. 1564-1583
    • Oliver, W.C.1    Pharr, G.M.2
  • 6
    • 34248394385 scopus 로고    scopus 로고
    • Nanoindentation derived stress-strain properties of dental materials
    • DOI 10.1016/j.dental.2006.06.017, PII S0109564106001722
    • L.H. He, and M.V. Swain Nanoindentation derived stress-strain properties of dental materials Dent Mater 23 2007 814 821 (Pubitemid 46734309)
    • (2007) Dental Materials , vol.23 , Issue.7 , pp. 814-821
    • He, L.H.1    Swain, M.V.2
  • 7
    • 33646371962 scopus 로고    scopus 로고
    • Elastic modulus and stress-strain response of human enamel by nano-indentation
    • DOI 10.1016/j.biomaterials.2006.03.045, PII S0142961206002973
    • L.H. He, N. Fujisawa, and M.V. Swain Elastic modulus and stress-strain response of human enamel by nano-indentation Biomaterials 27 2006 4388 4398 (Pubitemid 43674178)
    • (2006) Biomaterials , vol.27 , Issue.24 , pp. 4388-4398
    • He, L.H.1    Fujisawa, N.2    Swain, M.V.3
  • 8
    • 34047276805 scopus 로고    scopus 로고
    • Enamel - A "metallic-like" deformable biocomposite
    • L.H. He, and M.V. Swain Enamel - a "metallic-like" deformable biocomposite J Dent 35 2007 431 437
    • (2007) J Dent , vol.35 , pp. 431-437
    • He, L.H.1    Swain, M.V.2
  • 10
    • 84979434138 scopus 로고
    • Hardness, toughness, and brittleness - Indentation analysis
    • B.R. Lawn, and D.B. Marshall Hardness, toughness, and brittleness - indentation analysis J Am Ceram Soc 62 1979 347 350
    • (1979) J Am Ceram Soc , vol.62 , pp. 347-350
    • Lawn, B.R.1    Marshall, D.B.2
  • 11
    • 77951206661 scopus 로고    scopus 로고
    • Material properties and fractography of an indirect dental resin composite
    • J.B. Quinn, and G.D. Quinn Material properties and fractography of an indirect dental resin composite Dent Mater 26 2010 589 599
    • (2010) Dent Mater , vol.26 , pp. 589-599
    • Quinn, J.B.1    Quinn, G.D.2
  • 12
    • 0032204219 scopus 로고    scopus 로고
    • Estimation of hardness by nanoindentation of rough surfaces
    • M.S. Bobji, and S.K. Biswas Estimation of hardness by nanoindentation of rough surfaces J Mater Res 13 1998 3227 3233 (Pubitemid 128563200)
    • (1998) Journal of Materials Research , vol.13 , Issue.11 , pp. 3227-3233
    • Bobji, M.S.1    Biswas, S.K.2
  • 13
    • 0029449260 scopus 로고
    • Enamel wear caused by three different restorative materials
    • J.D. Hudson, G.R. Goldstein, and M. Georgescu Enamel wear caused by three different restorative materials J Prosthet Dent 74 1995 647 654
    • (1995) J Prosthet Dent , vol.74 , pp. 647-654
    • Hudson, J.D.1    Goldstein, G.R.2    Georgescu, M.3
  • 14
    • 0029282732 scopus 로고
    • An in-vitro investigation into the wear effects of selected restorative materials on enamel
    • D.C. Jagger, and A. Harrison An in-vitro investigation into the wear effects of selected restorative materials on enamel J Oral Rehabil 22 1995 275 281
    • (1995) J Oral Rehabil , vol.22 , pp. 275-281
    • Jagger, D.C.1    Harrison, A.2
  • 15
    • 43449093485 scopus 로고    scopus 로고
    • Esthetic restorative materials and opposing enamel wear
    • A.B. Olivera, and M.M. Marques Esthetic restorative materials and opposing enamel wear Oper Dent 33 2008 332 337
    • (2008) Oper Dent , vol.33 , pp. 332-337
    • Olivera, A.B.1    Marques, M.M.2
  • 16
    • 0031104342 scopus 로고    scopus 로고
    • Effect of hardness on three very different forms of wear
    • G.J. Gore, and J.D. Gates Effect of hardness on three very different forms of wear Wear 203 1997 544 563
    • (1997) Wear , vol.203 , pp. 544-563
    • Gore, G.J.1    Gates, J.D.2
  • 17
    • 35048830491 scopus 로고    scopus 로고
    • Understanding the mechanical behaviour of human enamel from its structural and compositional characteristics
    • DOI 10.1016/j.jmbbm.2007.05.001, PII S1751616107000082
    • L.H. He, and M.V. Swain Understanding the mechanical behaviour of human enamel from its structural and compositional characteristics J Mech Behav Biomed Mater 1 2008 18 29 (Pubitemid 47557530)
    • (2008) Journal of the Mechanical Behavior of Biomedical Materials , vol.1 , Issue.1 , pp. 18-29
    • He, L.H.1    Swain, M.V.2
  • 18
    • 0035383233 scopus 로고    scopus 로고
    • Properties and applications of a new composite block for CAD/CAM
    • R.P. Rusin Properties and applications of a new composite block for CAD/CAM Compend Cont Educ Dent 22 6 Suppl 2001 35 41
    • (2001) Compend Cont Educ Dent , vol.22 , Issue.6 SUPPL. , pp. 35-41
    • Rusin, R.P.1
  • 19
    • 0030196150 scopus 로고    scopus 로고
    • Assessment of brittleness in glass-ceramics and participate glass matrix composites by indentation data
    • A.R. Boccaccini Assessment of brittleness in glass-ceramics and particulate glass matrix composites by indentation data J Mater Sci Lett 15 1996 1119 1121 (Pubitemid 126739244)
    • (1996) Journal of Materials Science Letters , vol.15 , Issue.13 , pp. 1119-1121
    • Boccaccini, A.R.1
  • 20
    • 36048992830 scopus 로고    scopus 로고
    • Brittleness index of machinable dental materials and its relation to the marginal chipping factor
    • E.A. Tsitrou, S.E. Northeast, and R. Van Noort Brittleness index of machinable dental materials and its relation to the marginal chipping factor J Dent 35 2007 897 902
    • (2007) J Dent , vol.35 , pp. 897-902
    • Tsitrou, E.A.1    Northeast, S.E.2    Van Noort, R.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.