Volumn 96, Issue 6, 2011, Pages 1141-1148

Photo-degradation of poly(neopentyl isophthalate). Part II: Mechanism of cross-linking

Author keywords

Coating; Gel formation; Methanolysis; Polyester; UV exposure

Indexed keywords

CHAIN COUPLING; COATING SURFACE; DECOMPOSITION PRODUCTS; GEL FORMATION; GEL MATERIALS; INSOLUBLE MATERIALS; ISOPHTHALATE; METHANOLYSIS; MOLECULAR LEVELS; NEOPENTYL GLYCOL; NITROGEN ATMOSPHERES; SEM; UV EXPOSURE; UV LIGHT;

EID: 79955626591     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymdegradstab.2011.02.016     Document Type: Article
Times cited : (19)

References (14)
  • 2
    • 84981932165 scopus 로고
    • Photochemical degradation of poly(ethylene terephthalate). I. Irradiation experiments with the xenon and carbon arc
    • M. Day, and D.M. Wiles Photochemical degradation of poly(ethylene terephthalate). I. Irradiation experiments with the xenon and carbon arc J Appl Polym Sci 16 1972 175 189
    • (1972) J Appl Polym Sci , vol.16 , pp. 175-189
    • Day, M.1    Wiles, D.M.2
  • 3
    • 84981946630 scopus 로고
    • Photochemical degradation of poly(ethylene terephthalate). II. Effect of wavelength and environment on the decomposition process
    • M. Day, and D.M. Wiles Photochemical degradation of poly(ethylene terephthalate). II. Effect of wavelength and environment on the decomposition process J Appl Polym Sci 16 1972 191 202
    • (1972) J Appl Polym Sci , vol.16 , pp. 191-202
    • Day, M.1    Wiles, D.M.2
  • 4
    • 84981945499 scopus 로고
    • Photochemical degradation of poly(ethylene terephthalate). III. Determination of decomposition products and reaction mechanism
    • M. Day, and D.M. Wiles Photochemical degradation of poly(ethylene terephthalate). III. Determination of decomposition products and reaction mechanism J Appl Polym Sci 16 1972 203 215
    • (1972) J Appl Polym Sci , vol.16 , pp. 203-215
    • Day, M.1    Wiles, D.M.2
  • 5
    • 0027262930 scopus 로고
    • Photochemistry of poly(butyleneterephthalate): 1 - identification of the IR-absorbing photolysis products
    • DOI 10.1016/0141-3910(93)90075-T
    • A. Rivaton Photochemistry of poly(butyleneterephthalate): 1 identification of the IR-absorbing photolysis products Polym Degrad Stab 41 1993 283 296 (Pubitemid 23694946)
    • (1993) Polymer Degradation and Stability , vol.41 , Issue.3 , pp. 283-296
    • Rivaton Agnes1
  • 6
    • 0027262929 scopus 로고
    • Photochemistry of poly(butyleneterephthalate): 2 - identification of the IR-absorbing photooxidation products
    • DOI 10.1016/0141-3910(93)90076-U
    • A. Rivaton Photochemistry of poly(butyleneterephthalate): 2 identification of the IR-absorbing photooxidation products Polym Degrad Stab 41 1993 297 310 (Pubitemid 23694945)
    • (1993) Polymer Degradation and Stability , vol.41 , Issue.3 , pp. 297-310
    • Rivaton Agnes1
  • 7
    • 47149112353 scopus 로고    scopus 로고
    • Comparative investigation of photo- and thermal-oxidation processes in poly(butylene terephthalate)
    • S. Carroccio, P. Rizzarelli, G. Scaltro, and C. Puglisi Comparative investigation of photo- and thermal-oxidation processes in poly(butylene terephthalate) Polymer 49 2008 3371 3381
    • (2008) Polymer , vol.49 , pp. 3371-3381
    • Carroccio, S.1    Rizzarelli, P.2    Scaltro, G.3    Puglisi, C.4
  • 14
    • 0037074283 scopus 로고    scopus 로고
    • The thermal degradation of PET and analogous polyesters measured by thermal analysis-Fourier transform infrared spectroscopy
    • DOI 10.1016/S0032-3861(01)00775-3, PII S0032386101007753
    • B.J. Holland, and J.N. Hay The thermal degradation of PET and analogous polyesters measured by thermal analysis Polymer 43 2002 1835 1847 (Pubitemid 34073751)
    • (2002) Polymer , vol.43 , Issue.6 , pp. 1835-1847
    • Holland, B.J.1    Hay, J.N.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.