Volumn 53, Issue 6, 2011, Pages 2106-2114

Erosion-corrosion resistance of microcrystalline and near-nanocrystalline WC-17Co high velocity oxy-fuel thermal spray coatings

Author keywords

A. Coatings; B. EIS; B. Erosion; B. Polarization; B. Weight loss; C. Crevice corrosion

Indexed keywords

A. COATINGS; B. EIS; B. EROSION; B. POLARIZATION; B. WEIGHT LOSS; C. CREVICE CORROSION;

EID: 79955044440     PISSN: 0010938X     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.corsci.2011.02.028     Document Type: Article
Times cited : (79)

References (24)
  • 1
    • 1442330083 scopus 로고    scopus 로고
    • Effects of powder composition on the erosion, corrosion and erosion-corrosion properties of HVOF sprayed WC based coatings, in: Proceedings of 15th International Thermal Spray Conference, Nice, France
    • J. Berget, E. Bardal, T. Rogne, Effects of powder composition on the erosion, corrosion and erosion-corrosion properties of HVOF sprayed WC based coatings, in: Proceedings of 15th International Thermal Spray Conference, Nice, France, 1998, pp. 305-312.
    • (1998) , pp. 305-312
    • Berget, J.1    Bardal, E.2    Rogne, T.3
  • 3
    • 0031104201 scopus 로고    scopus 로고
    • Solid particle erosion of Ni-Cr/WC metal matrix composites at elevated temperatures: construction of erosion mechanism and process control maps
    • Stack M.M., Pena D. Solid particle erosion of Ni-Cr/WC metal matrix composites at elevated temperatures: construction of erosion mechanism and process control maps. Wear 1997, 203-204:489-497.
    • (1997) Wear , pp. 489-497
    • Stack, M.M.1    Pena, D.2
  • 4
    • 33748528962 scopus 로고    scopus 로고
    • Mapping erosion-corrosion of WC/Co-Cr based composite coatings: particle velocity and applied potential effects
    • Stack M.M., Abd El Badia T.M. Mapping erosion-corrosion of WC/Co-Cr based composite coatings: particle velocity and applied potential effects. Surf. Coat. Technol. 2006, 201:1335-1347.
    • (2006) Surf. Coat. Technol. , vol.201 , pp. 1335-1347
    • Stack, M.M.1    Abd El Badia, T.M.2
  • 5
    • 0003178586 scopus 로고    scopus 로고
    • Elevated temperature erosion of range of composite layers of Ni-Cr based functionally graded material
    • Stack M.M., Chacon-Nava J., Jordan M.P. Elevated temperature erosion of range of composite layers of Ni-Cr based functionally graded material. Mater. Sci. Technol. 1996, 12:171-177.
    • (1996) Mater. Sci. Technol. , vol.12 , pp. 171-177
    • Stack, M.M.1    Chacon-Nava, J.2    Jordan, M.P.3
  • 6
    • 0029352895 scopus 로고
    • The influence of corrosion on the erosion of aluminium by aqueous silica slurries
    • Li Y., Burstein G.T., Hutchings I.M. The influence of corrosion on the erosion of aluminium by aqueous silica slurries. Wear 1995, 186-187:515-522.
    • (1995) Wear , pp. 515-522
    • Li, Y.1    Burstein, G.T.2    Hutchings, I.M.3
  • 7
    • 0034059409 scopus 로고    scopus 로고
    • Mechanisms of wear on a Co-based alloy in liquid-solid slurries
    • Neville A., Reyes M., Hodgkiess T., Gledhill A. Mechanisms of wear on a Co-based alloy in liquid-solid slurries. Wear 2000, 238:138-150.
    • (2000) Wear , vol.238 , pp. 138-150
    • Neville, A.1    Reyes, M.2    Hodgkiess, T.3    Gledhill, A.4
  • 8
    • 0036771634 scopus 로고    scopus 로고
    • Particulate erosion-corrosion of Al in aqueous conditions: some perspectives on pH effects on the erosion-corrosion map
    • Stack M.M., Pungwiwat N. Particulate erosion-corrosion of Al in aqueous conditions: some perspectives on pH effects on the erosion-corrosion map. Tribol. Int. 2002, 35:651-660.
    • (2002) Tribol. Int. , vol.35 , pp. 651-660
    • Stack, M.M.1    Pungwiwat, N.2
  • 9
    • 33847612930 scopus 로고    scopus 로고
    • Erosion-corrosion of 2205 duplex stainless steel in flowing seawater containing sand particles
    • Hussain E.A.M., Robinson M.J. Erosion-corrosion of 2205 duplex stainless steel in flowing seawater containing sand particles. Corr. Sci. 2007, 49:1737-1754.
    • (2007) Corr. Sci. , vol.49 , pp. 1737-1754
    • Hussain, E.A.M.1    Robinson, M.J.2
  • 10
    • 26044455631 scopus 로고    scopus 로고
    • Interaction of mechanical and electrochemical factors in erosion-corrosion of carbon steel
    • Guo H.X., Lu B.T., Luo J.L. Interaction of mechanical and electrochemical factors in erosion-corrosion of carbon steel. Electrochim. Acta 2005, 51:315-323.
    • (2005) Electrochim. Acta , vol.51 , pp. 315-323
    • Guo, H.X.1    Lu, B.T.2    Luo, J.L.3
  • 11
    • 34548419782 scopus 로고    scopus 로고
    • Protective iron carbonate films-part 3: simultaneous chemo-mechanical removal in single phase aqueous flow
    • Ruzic V., Veidt M., Nesic S. Protective iron carbonate films-part 3: simultaneous chemo-mechanical removal in single phase aqueous flow. Corrosion 2007, 63:758-769.
    • (2007) Corrosion , vol.63 , pp. 758-769
    • Ruzic, V.1    Veidt, M.2    Nesic, S.3
  • 12
    • 42749097912 scopus 로고    scopus 로고
    • Synergistic effects of fluid flow and sand particles on erosion-corrosion of aluminium in ethylene glycol-water solutions
    • Niu L., Cheng Y.F. Synergistic effects of fluid flow and sand particles on erosion-corrosion of aluminium in ethylene glycol-water solutions. Wear 2008, 265:367-374.
    • (2008) Wear , vol.265 , pp. 367-374
    • Niu, L.1    Cheng, Y.F.2
  • 13
    • 0033492297 scopus 로고    scopus 로고
    • Comparison of slurry and dry erosion behaviour of some HVOF thermal sprayed coatings
    • Hawthorne H.M., Arsenault B., Immarigeon J.P., Legoux J.G., Parameswaran V.R. Comparison of slurry and dry erosion behaviour of some HVOF thermal sprayed coatings. Wear 1999, 225-229:825-834.
    • (1999) Wear , pp. 825-834
    • Hawthorne, H.M.1    Arsenault, B.2    Immarigeon, J.P.3    Legoux, J.G.4    Parameswaran, V.R.5
  • 14
    • 0035062671 scopus 로고    scopus 로고
    • Assessment of the corrosion rates and mechanisms of a WC-Co-Cr HVOF coating in static and liquid-solid impingement saline environments
    • Perry J.M., Neville A., Wilson V.A., Hodgkiess T. Assessment of the corrosion rates and mechanisms of a WC-Co-Cr HVOF coating in static and liquid-solid impingement saline environments. Surf. Coat. Technol. 2001, 137:43-51.
    • (2001) Surf. Coat. Technol. , vol.137 , pp. 43-51
    • Perry, J.M.1    Neville, A.2    Wilson, V.A.3    Hodgkiess, T.4
  • 15
    • 79955042224 scopus 로고    scopus 로고
    • Corrosion, erosion-corrosion and wear resistance of HVOF sprayed WC type coatings with a corrosion resistant binder
    • Rogne T., Berget J. Corrosion, erosion-corrosion and wear resistance of HVOF sprayed WC type coatings with a corrosion resistant binder. Corrosion 1999, 48:1-11.
    • (1999) Corrosion , vol.48 , pp. 1-11
    • Rogne, T.1    Berget, J.2
  • 16
    • 70350330605 scopus 로고    scopus 로고
    • Development of wear resistant nanostructured duplex coatings by high velocity oxy-fuel process for use in oil sands industry
    • Saha G.C., Khan T.I., Glenesk L.B. Development of wear resistant nanostructured duplex coatings by high velocity oxy-fuel process for use in oil sands industry. J. Nanosci. Nanotechnol. 2009, 9:4316-4323.
    • (2009) J. Nanosci. Nanotechnol. , vol.9 , pp. 4316-4323
    • Saha, G.C.1    Khan, T.I.2    Glenesk, L.B.3
  • 17
    • 0026223457 scopus 로고
    • A comparative study of the slurry erosion and free-fall particle erosion of aluminium
    • Zu J.B., Burstein G.T., Hutchings I.M. A comparative study of the slurry erosion and free-fall particle erosion of aluminium. Wear 1991, 149:73-84.
    • (1991) Wear , vol.149 , pp. 73-84
    • Zu, J.B.1    Burstein, G.T.2    Hutchings, I.M.3
  • 18
    • 0033626868 scopus 로고    scopus 로고
    • Effect of impact angle on the slurry erosion-corrosion of 304L stainless steel
    • Burstein G.T., Sasaki K. Effect of impact angle on the slurry erosion-corrosion of 304L stainless steel. Wear 2000, 240:80-94.
    • (2000) Wear , vol.240 , pp. 80-94
    • Burstein, G.T.1    Sasaki, K.2
  • 20
    • 58549089678 scopus 로고    scopus 로고
    • Investigation of erosion-corrosion of 3003 aluminum alloy in ethylene glycol-water solution by impingement jet system
    • Zhang G.A., Xu L.Y., Cheng Y.F. Investigation of erosion-corrosion of 3003 aluminum alloy in ethylene glycol-water solution by impingement jet system. Corros. Sci. 2009, 51:283-290.
    • (2009) Corros. Sci. , vol.51 , pp. 283-290
    • Zhang, G.A.1    Xu, L.Y.2    Cheng, Y.F.3
  • 21
    • 79955000205 scopus 로고    scopus 로고
    • Corrosion and Erosion-Corrosion of WC-based Cermet Coatings - A Kinetic and Mechanistic Study, Ph.D. Thesis, Heriot-Watt University, Edinburgh, UK
    • V.A. de Souza, Corrosion and Erosion-Corrosion of WC-based Cermet Coatings - A Kinetic and Mechanistic Study, Ph.D. Thesis, Heriot-Watt University, Edinburgh, UK, 2004.
    • (2004)
    • de Souza, V.A.1
  • 22
    • 23044440906 scopus 로고    scopus 로고
    • Corrosion and synergy in a WC-Co-Cr HVOF thermal spray coating understanding their role in erosion-corrosion degradation
    • de Souza V.A., Neville A. Corrosion and synergy in a WC-Co-Cr HVOF thermal spray coating understanding their role in erosion-corrosion degradation. Wear 2005, 259:171-180.
    • (2005) Wear , vol.259 , pp. 171-180
    • de Souza, V.A.1    Neville, A.2
  • 23
    • 78049447425 scopus 로고    scopus 로고
    • The corrosion and wear performance of microcrystalline WC-10Co-4Cr and near-nanocrystalline WC-17Co high velocity oxy-fuel sprayed coatings on steel substrate
    • Saha G.C., Khan T.I. The corrosion and wear performance of microcrystalline WC-10Co-4Cr and near-nanocrystalline WC-17Co high velocity oxy-fuel sprayed coatings on steel substrate. Metall. Mater. Trans. A 2010, 41:3000-3009.
    • (2010) Metall. Mater. Trans. A , vol.41 , pp. 3000-3009
    • Saha, G.C.1    Khan, T.I.2
  • 24
    • 0005239611 scopus 로고
    • Electrochemical and chemical corrosion of tungsten carbide (WC)
    • Voorhies J.D. Electrochemical and chemical corrosion of tungsten carbide (WC). J. Electrochem. Soc. 1972, 119:219-222.
    • (1972) J. Electrochem. Soc. , vol.119 , pp. 219-222
    • Voorhies, J.D.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.