1
-
-
0021877895
-
An investigation of abrasive wear resistance of unidirectionally solidified high chromium iron
-
ASME
-
Su J.-Y., Zhou Q.-D., Jia Y.-D. An investigation of abrasive wear resistance of unidirectionally solidified high chromium iron. Proceeding Conference on Wear of Materials 1985, 621-624. ASME.
-
(1985)
Proceeding Conference on Wear of Materials
, pp. 621-624
-
-
Su, J.-Y.1
Zhou, Q.-D.2
Jia, Y.-D.3
-
2
-
-
0023163439
-
Effect of orientation and thickness of carbides on abrasive wear resistance of high chromium iron
-
Junyi S., Yuding J. Effect of orientation and thickness of carbides on abrasive wear resistance of high chromium iron. Proceeding Conference on Wear of Materials, ASME, New York 1987, Vol. 2:661-671.
-
(1987)
Proceeding Conference on Wear of Materials, ASME, New York
, vol.2
, pp. 661-671
-
-
Junyi, S.1
Yuding, J.2
-
4
-
-
0029387320
-
Effect of carbide orientation on abrasion of high Cr white cast iron
-
Dogan O.N., Hawk J.A. Effect of carbide orientation on abrasion of high Cr white cast iron. Wear 1995, 189:136-142.
-
(1995)
Wear
, vol.189
, pp. 136-142
-
-
Dogan, O.N.1
Hawk, J.A.2
-
5
-
-
4243245941
-
Abrasion resistance of the columnar zone in high Cr white cast irons
-
Dogan O.N., Laird G., Hawk J.A. Abrasion resistance of the columnar zone in high Cr white cast irons. Wear 1995, 181-183:342-349.
-
(1995)
Wear
, vol.181-183
, pp. 342-349
-
-
Dogan, O.N.1
Laird, G.2
Hawk, J.A.3
-
6
-
-
78650677181
-
3 carbide orientation on abrasion wear resistance and fracture toughness
-
3 carbide orientation on abrasion wear resistance and fracture toughness. Wear 2011, 270:287-293.
-
(2011)
Wear
, vol.270
, pp. 287-293
-
-
Coronado, J.J.1
-
7
-
-
65749095407
-
Load effect in abrasive wear mechanism of cast iron with graphite and cementite
-
Coronado J.J., Sinatora A. Load effect in abrasive wear mechanism of cast iron with graphite and cementite. Wear 2009, 267:6-11.
-
(2009)
Wear
, vol.267
, pp. 6-11
-
-
Coronado, J.J.1
Sinatora, A.2
-
10
-
-
0026875935
-
An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments
-
Oliver W.C., Pharr G.M. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. Journal of the Materials Research 1992, 7(6):1564-1583.
-
(1992)
Journal of the Materials Research
, vol.7
, Issue.6
, pp. 1564-1583
-
-
Oliver, W.C.1
Pharr, G.M.2
-
11
-
-
3042606295
-
Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology
-
Oliver W.C., Pharr G.M. Measurement of hardness and elastic modulus by instrumented indentation: advances in understanding and refinements to methodology. Journal of the Materials Research 2004, 19:3-20.
-
(2004)
Journal of the Materials Research
, vol.19
, pp. 3-20
-
-
Oliver, W.C.1
Pharr, G.M.2
-
12
-
-
0020751889
-
Fracture mechanics analysis of indentation-induced Palmqvist crack in ceramics
-
Niihara K.A. Fracture mechanics analysis of indentation-induced Palmqvist crack in ceramics. Journal of Materials Science Letters 1983, 2(5):221-223.
-
(1983)
Journal of Materials Science Letters
, vol.2
, Issue.5
, pp. 221-223
-
-
Niihara, K.A.1
-
13
-
-
0003171562
-
Alloy phase diagrams
-
ASM International (The Materials Information Society), Materials Park, Ohio, USA, H. Baker (Ed.)
-
Alloy phase diagrams. ASM Handbook 1992, vol. 3. ASM International (The Materials Information Society), Materials Park, Ohio, USA. 3rd ed. H. Baker (Ed.).
-
(1992)
ASM Handbook
, vol.3
-
-
-
16
-
-
0037293126
-
Fractal characteristics of the surface of tungsten carbide-manganese steel composite after plastic deformation
-
Sevostjanova I.N., Kulkov S.N. Fractal characteristics of the surface of tungsten carbide-manganese steel composite after plastic deformation. Technical Physics 2003, 48(2):215-218.
-
(2003)
Technical Physics
, vol.48
, Issue.2
, pp. 215-218
-
-
Sevostjanova, I.N.1
Kulkov, S.N.2
|