Volumn 96, Issue 4, 2011, Pages 703-707

Degradability of linear polyolefins under natural weathering

Author keywords

Antioxidant and pro oxidant additives; HDPE; LLDPE; Polyolefin weathering and degradation; PP

Indexed keywords

ABIOTIC DEGRADATION; ANTIOXIDANT ADDITIVES; ANTIOXIDANT AND PRO-OXIDANT ADDITIVES; BIODEGRADABLE BLENDS; CARBONYL GROUPS; DEGRADABILITY; HDPE; HINDERED PHENOL; ISOTACTIC POLYPROPYLENE; LLDPE; NATURAL WEATHERING; OLEFIN POLYMER; OXIDATIVE DEGRADATION; PHOTO-OXIDATIVE DEGRADATION; PP; PROOXIDANT; SUBSTANTIAL REDUCTION; TERTIARY CARBON ATOM; THERMAL AND MECHANICAL PROPERTIES;

EID: 79952195987     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymdegradstab.2010.12.004     Document Type: Article
Times cited : (228)

References (30)
  • 4
    • 0037177437 scopus 로고    scopus 로고
    • Photooxidative and thermal degradation of polyethylenes: Interrelationship by chemiluminescence, thermal gravimetric analysis and FTIR data
    • T. Corrales, F. Catalina, C. Peinado, N.S. Allen, and E. Fontan Photooxidative and thermal degradation of polyethylenes: interrelationship by chemiluminescence, thermal gravimetric analysis and FTIR data J Photochem Photobiol A 147 2002 213 224
    • (2002) J Photochem Photobiol A , vol.147 , pp. 213-224
    • Corrales, T.1    Catalina, F.2    Peinado, C.3    Allen, N.S.4    Fontan, E.5
  • 5
    • 0035068472 scopus 로고    scopus 로고
    • Chemical and morphologial modifications of irradiated linear low density polyethylene (LLDPE)
    • DOI 10.1016/S0141-3910(01)00024-6, PII S0141391001000246
    • L. Guadagno, C. Naddeo, V. Vittoria, G. Camino, and C. Cagnani Chemical and morphological modifications of irradiated linear low density polyethylene (LLDPE) Polym Degrad Stab 72 2001 175 186 (Pubitemid 32284747)
    • (2001) Polymer Degradation and Stability , vol.72 , Issue.1 , pp. 175-186
    • Guadagno, L.1    Naddeo, C.2    Vittoria, V.3    Camino, G.4    Cagnani, C.5
  • 7
    • 79952191054 scopus 로고    scopus 로고
    • Biodegradable and degradable polymers and plastics in landfill sites
    • G. Swift, and D.M. Wiles Biodegradable and degradable polymers and plastics in landfill sites J.I. Kroschwitz, Encyclopedia of polymer science and technology 2004 John Wiley & Sons Hoboken, NJ 40 50
    • (2004) Encyclopedia of Polymer Science and Technology , pp. 40-50
    • Swift, G.1    Wiles, D.M.2
  • 8
  • 9
    • 0013834162 scopus 로고
    • Biodegradation: Problems of molecular recalcitrance and microbial fallibility
    • M. Alexander Biodegradation: problems of molecular recalcitrance and microbial fallibility Adv Appl Microbiol 7 1965 35 80
    • (1965) Adv Appl Microbiol , vol.7 , pp. 35-80
    • Alexander, M.1
  • 12
    • 77953326987 scopus 로고    scopus 로고
    • Oxidation and biodegradation of polyethylene films containing pro-oxidant additives: Synergistic effects of sunlight exposure, thermal aging and fungal biodegradation
    • A. Corti, S. Muniyasamy, M. Vitali, S.H. Imam, and E. Chiellini Oxidation and biodegradation of polyethylene films containing pro-oxidant additives: synergistic effects of sunlight exposure, thermal aging and fungal biodegradation Polym Degrad Stab 95 2010 1106 1114
    • (2010) Polym Degrad Stab , vol.95 , pp. 1106-1114
    • Corti, A.1    Muniyasamy, S.2    Vitali, M.3    Imam, S.H.4    Chiellini, E.5
  • 13
    • 2942633967 scopus 로고    scopus 로고
    • Environmental degradation of polyethylene
    • M. Hakkarainen, and A.-C. Albertsson Environmental degradation of polyethylene Adv Polym Sci 169 2004 177 199
    • (2004) Adv Polym Sci , vol.169 , pp. 177-199
    • Hakkarainen, M.1    Albertsson, A.-C.2
  • 14
    • 3342901096 scopus 로고    scopus 로고
    • Photooxidation of spherilene linear low-density polyethylene films subjected to environmental weathering. 1. Changes in mechanical properties
    • C. Naddeo, L. Guadagno, and V. Vittoria Photooxidation of spherilene linear low-density polyethylene films subjected to environmental weathering. 1. Changes in mechanical properties Polym Degrad Stab 85 2004 1009 1013
    • (2004) Polym Degrad Stab , vol.85 , pp. 1009-1013
    • Naddeo, C.1    Guadagno, L.2    Vittoria, V.3
  • 17
    • 33645139447 scopus 로고    scopus 로고
    • Polyolefins with controlled environmental degradability
    • D.M. Wiles, and G. Scott Polyolefins with controlled environmental degradability Polym Degrad Stab 91 2006 1581 1592
    • (2006) Polym Degrad Stab , vol.91 , pp. 1581-1592
    • Wiles, D.M.1    Scott, G.2
  • 18
    • 0038009397 scopus 로고    scopus 로고
    • Biodegradation of thermally-oxidized, fragmented low-density polyethylenes
    • E. Chiellini, A. Corti, and G. Swif Biodegradation of thermally-oxidized, fragmented low-density polyethylenes Polym Degrad Stab 81 2003 341 351
    • (2003) Polym Degrad Stab , vol.81 , pp. 341-351
    • Chiellini, E.1    Corti, A.2    Swif, G.3
  • 21
    • 33748288386 scopus 로고    scopus 로고
    • Oxo-biodegradable carbon backbone polymers - Oxidative degradation of polyethylene under accelerated test conditions
    • DOI 10.1016/j.polymdegradstab.2006.03.022, PII S0141391006001509
    • E. Chiellini, A. Corti, S. D'Antone, and R. Baciu Oxo-biodegradable carbon backbone polymers - oxidative degradation of polyethylene under accelerated test conditions Polym Degrad Stab 91 2006 2739 2747 (Pubitemid 44331398)
    • (2006) Polymer Degradation and Stability , vol.91 , Issue.11 , pp. 2739-2747
    • Chiellini, E.1    Corti, A.2    D'Antone, S.3    Baciu, R.4
  • 22
    • 0000440586 scopus 로고
    • Near-infrared spectrophotometric analysis of ethylene-propylene copolymers
    • T. Takeuchi, S. Tsuge, and Y. Sugimura Near-infrared spectrophotometric analysis of ethylene-propylene copolymers Anal Chem 41 1969 184 186
    • (1969) Anal Chem , vol.41 , pp. 184-186
    • Takeuchi, T.1    Tsuge, S.2    Sugimura, Y.3
  • 26
    • 0037233216 scopus 로고    scopus 로고
    • Degradation profile of polyethylene after artificial accelerated weathering
    • J.V. Gulmine, P.R. Janissek, H.M. Heise, and L. Akcelrud Degradation profile of polyethylene after artificial accelerated weathering Polym Degrad Stab 79 2003 385 397
    • (2003) Polym Degrad Stab , vol.79 , pp. 385-397
    • Gulmine, J.V.1    Janissek, P.R.2    Heise, H.M.3    Akcelrud, L.4
  • 27
    • 84943707563 scopus 로고
    • Photooxidation of high polymers
    • F.H. Winslow Photooxidation of high polymers Pure Appl Chem 49 1977 495 502
    • (1977) Pure Appl Chem , vol.49 , pp. 495-502
    • Winslow, F.H.1
  • 30
    • 0031446734 scopus 로고    scopus 로고
    • Crystallization and melting behavior of photodegraded polypropylene. 2. Recrystallization of degraded molecules
    • M.S. Rabello, and J.R. White Crystallization and melting behavior of photodegraded polypropylene. 2. Recrystallization of degraded molecules Polymer 38 1997 6389 6399
    • (1997) Polymer , vol.38 , pp. 6389-6399
    • Rabello, M.S.1    White, J.R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.