Anodic mesoporous TiO2 layer on Ti for enhanced formation of biomimetic hydroxyapatite

Author keywords

Anodization; Hydroxyapatite; Mesopores; Simulated body fluid

Indexed keywords

BODY FLUIDS; ELECTROLYTES; HYDROXYAPATITE; LINEARIZATION; SCANNING ELECTRON MICROSCOPY; TITANIUM DIOXIDE; X RAY DIFFRACTION; X RAY PHOTOELECTRON SPECTROSCOPY;

EID: 79952191951     PISSN: 17427061     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.actbio.2010.11.011     Document Type: Article
Times cited : (62)

References (25)
  • 4
    • 32144437418 scopus 로고    scopus 로고
    • How useful is SBF in predicting in vivo bone bioactivity?
    • DOI 10.1016/j.biomaterials.2006.01.017, PII S0142961206000457
    • T. Kokubo, and H. Takadama How useful is SBF in predicting in vivo bone bioactivity? Biomaterials 27 2006 2907 2915 (Pubitemid 43208916)
    • (2006) Biomaterials , vol.27 , Issue.15 , pp. 2907-2915
    • Kokubo, T.1    Takadama, H.2
  • 5
    • 0025807957 scopus 로고
    • Effect of surface treatment on the dissolution of titanium based implant materials
    • A. Wisbey, P.J. Gregson, L.M. Peter, and M. Tuke Effect of surface treatment on the dissolution of titanium based implant materials Biometrials 12 1991 470 473
    • (1991) Biometrials , vol.12 , pp. 470-473
    • Wisbey, A.1    Gregson, P.J.2    Peter, L.M.3    Tuke, M.4
  • 7
    • 1042298416 scopus 로고    scopus 로고
    • Biochemical modification of titanium surfaces
    • S.J. Xiao, G. Kenausi, and M. Textor Biochemical modification of titanium surfaces D.M. Brunette, P. Tengvall, M. Textor, P. Thomsen, Titanium in medicine 2001 Springer Berlin 417 455
    • (2001) Titanium in Medicine , pp. 417-455
    • Xiao, S.J.1    Kenausi, G.2    Textor, M.3
  • 8
    • 0242606916 scopus 로고    scopus 로고
    • Preparation of bioactive titanium metal via anodic oxidation treatment
    • DOI 10.1016/S0142-9612(03)00626-4
    • B. Yang, M. Uchida, H.M. Kim, X. Zhang, and T. Kokubo Preparation of bioactive titanium metal via anodic oxidation treatment Biomaterials 25 2004 1003 1010 (Pubitemid 37393291)
    • (2004) Biomaterials , vol.25 , Issue.6 , pp. 1003-1010
    • Yang, B.1    Uchida, M.2    Kim, H.-M.3    Zhang, X.4    Kokubo, T.5
  • 9
    • 0036131596 scopus 로고    scopus 로고
    • Characteristics of the surface oxides on turned and electrochemically oxidized pure titanium implants up to dielectric breakdown: The oxide thickness, micropore configurations, surface roughness, crystal structure and chemical composition
    • DOI 10.1016/S0142-9612(01)00131-4, PII S0142961201001314
    • Y.T. Sul, C.B. Johansson, S. Petronis, A. Krozer, Y. Jeong, and A. Wennerberg Characteristics of the surface oxides on turned and electrochemically oxidized pure titanium implants up to dielectric breakdown: The oxide thickness, micropore configuration, surface roughness, crystal structure and chemical composition Biomaterials 23 2002 491 501 (Pubitemid 33051037)
    • (2002) Biomaterials , vol.23 , Issue.2 , pp. 491-501
    • Sul, Y.-T.1    Johansson, C.B.2    Petronis, S.3    Krozer, A.4    Jeong, Y.5    Wennerberg, A.6    Albrektsson, T.7
  • 10
    • 1542298847 scopus 로고    scopus 로고
    • Biomimetic apatite coatings on micro-arc oxidized titania
    • DOI 10.1016/j.biomaterials.2003.09.103, PII S0142961203008974
    • W.H. Song, Y.K. Jun, Y. Han, and S.H. Hong Biomimetic apatite coatings on micro-acr oxidized titania Biomaterials 25 2004 3341 3349 (Pubitemid 38327025)
    • (2004) Biomaterials , vol.25 , Issue.17 , pp. 3341-3349
    • Song, W.-H.1    Jun, Y.-K.2    Han, Y.3    Hong, S.-H.4
  • 13
    • 14844339036 scopus 로고    scopus 로고
    • Growth of nano-scale hydroxyapatite using chemically treated titanium oxide nanotubes
    • DOI 10.1016/j.biomaterials.2005.01.048, PII S0142961205000840
    • S.-H. Oh, R.R. Finones, C. Daraio, L.-H. Chen, and S. Jin Growth of nano-scale hydroxyapatite using chemically treated titanium oxide nanotubes Biomaterials 26 2005 4938 4943 (Pubitemid 40354226)
    • (2005) Biomaterials , vol.26 , Issue.24 , pp. 4938-4943
    • Oh, S.-H.1    Finones, R.R.2    Daraio, C.3    Chen, L.-H.4    Jin, S.5
  • 15
    • 67349286533 scopus 로고    scopus 로고
    • Effect of nanostructured surfaces of light metals on hydroxyapatite coating
    • S. Ono, A. Kiyotake, and H. Asoh Effect of nanostructured surfaces of light metals on hydroxyapatite coating ECS Trans 11 15 2008 1 8
    • (2008) ECS Trans , vol.11 , Issue.15 , pp. 1-8
    • Ono, S.1    Kiyotake, A.2    Asoh, H.3
  • 16
    • 72949118679 scopus 로고    scopus 로고
    • Formation of a non-thickness-limited titanium dioxide mesosponge and its use in dye-sensitized solar cells
    • D. Kim, K. Lee, P. Roy, B.I. Birajdar, E. Spiecker, and P. Schmuki Formation of a non-thickness-limited titanium dioxide mesosponge and its use in dye-sensitized solar cells Angew Chem Int Ed 48 2009 9326 9329
    • (2009) Angew Chem Int Ed , vol.48 , pp. 9326-9329
    • Kim, D.1    Lee, K.2    Roy, P.3    Birajdar, B.I.4    Spiecker, E.5    Schmuki, P.6
  • 19
    • 77953305449 scopus 로고    scopus 로고
    • Size-selective separation of macromolecules by nanochannel titania membrane with self-leaning (declogging) ability
    • P. Roy, T. Dey, K. Lee, D. Kim, B. Fabry, and P. Schmuki Size-selective separation of macromolecules by nanochannel titania membrane with self-leaning (declogging) ability J Am Chem Soc 132 2010 7893 7895
    • (2010) J Am Chem Soc , vol.132 , pp. 7893-7895
    • Roy, P.1    Dey, T.2    Lee, K.3    Kim, D.4    Fabry, B.5    Schmuki, P.6
  • 21
    • 0023452883 scopus 로고
    • Fatigue and life-time of bioactive glass-ceramic A-W containing apatite and wollastonite
    • T. Kokubo, S. Ito, M. Shigematsu, S. Sakka, and T. Yamamuro Fatigue and life-time of bioactive glass-ceramic A-W containing apatite and wollastonite J Mater Sci 22 1987 4067 4070 (Pubitemid 18546263)
    • (1987) Journal of Materials Science , vol.22 , Issue.11 , pp. 4067-4070
    • Kokubo, T.1    Ito, S.2    Shigematsu, M.3    Sakka, S.4    Yamamuro, T.5
  • 22
    • 60549084488 scopus 로고    scopus 로고
    • Can bioactivity be tested in vitro with SBF solution?
    • M. Bohner, and J. Lemaitre Can bioactivity be tested in vitro with SBF solution? Biomaterials 30 2009 2175 2179
    • (2009) Biomaterials , vol.30 , pp. 2175-2179
    • Bohner, M.1    Lemaitre, J.2
  • 24
    • 0345688129 scopus 로고    scopus 로고
    • Biomimetic apatite formation on chemically treated titanium
    • DOI 10.1016/j.biomaterials.2003.08.009
    • L. Jonasova, F.A. Müller, A. Helebrant, J. Strnad, and P. Greil Biomimetic apatite formation on chemically treated titanium Biomaterials 25 2004 1187 1194 (Pubitemid 37476196)
    • (2004) Biomaterials , vol.25 , Issue.7-8 , pp. 1187-1194
    • Jonasova, L.1    Muller, F.A.2    Helebrant, A.3    Strnad, J.4    Greil, P.5
  • 25
    • 32644433065 scopus 로고    scopus 로고
    • - content and its influence on the composition of biomimetic apatites
    • DOI 10.1016/j.actbio.2005.11.001, PII S174270610500156X
    • 2 nanotubes Acta Biomater 2 2005 181 189 (Pubitemid 43239197)
    • (2006) Acta Biomaterialia , vol.2 , Issue.2 , pp. 181-189
    • Muller, L.1    Muller, F.A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.