1
-
-
77950370098
-
Correlations of electrochemical noise, acoustic emission and complementary monitoring techniques during intergranular stress-corrosion cracking of austenitic stainless steel
-
Kovač J., Alaux C., Marrow J., Govekar E., Legat A. Correlations of electrochemical noise, acoustic emission and complementary monitoring techniques during intergranular stress-corrosion cracking of austenitic stainless steel. Corros. Sci. 2010, 52:2015-2025.
-
(2010)
Corros. Sci.
, vol.52
, pp. 2015-2025
-
-
Kovač, J.1
Alaux, C.2
Marrow, J.3
Govekar, E.4
Legat, A.5
-
2
-
-
77952756741
-
Detection of corrosion on 304 stainless steel by acoustic emission measurement
-
Du G., Wang W.K., Song S.Z., Jin S.J. Detection of corrosion on 304 stainless steel by acoustic emission measurement. Anti-Corros. Methods Mater. 2010, 57:126-132.
-
(2010)
Anti-Corros. Methods Mater.
, vol.57
, pp. 126-132
-
-
Du, G.1
Wang, W.K.2
Song, S.Z.3
Jin, S.J.4
-
3
-
-
38749133788
-
Detection of stress corrosion cracking of high-strength steel used in prestressed concrete structures by acoustic emission technique
-
Ramadan S., Gaillet L., Tessier C., Idrissi H. Detection of stress corrosion cracking of high-strength steel used in prestressed concrete structures by acoustic emission technique. Appl. Surf. Sci. 2008, 254:2255-2261.
-
(2008)
Appl. Surf. Sci.
, vol.254
, pp. 2255-2261
-
-
Ramadan, S.1
Gaillet, L.2
Tessier, C.3
Idrissi, H.4
-
4
-
-
56649099033
-
AE response of type 304 stainless steel during stress corrosion crack propagation
-
Alvarez M.G., Lapitz P., Ruzzante J. AE response of type 304 stainless steel during stress corrosion crack propagation. Corros. Sci. 2008, 50:3382-3388.
-
(2008)
Corros. Sci.
, vol.50
, pp. 3382-3388
-
-
Alvarez, M.G.1
Lapitz, P.2
Ruzzante, J.3
-
5
-
-
33751516345
-
Evaluation of stress corrosion cracking phenomenon in an AISI type 316LN stainless steel using acoustic emission technique
-
Shaikh H., Amirthalingam R., Anita T., Sivaibharasi N., Jaykumar T., Manohar P., Khatak H.S. Evaluation of stress corrosion cracking phenomenon in an AISI type 316LN stainless steel using acoustic emission technique. Corros. Sci. 2007, 40:740-765.
-
(2007)
Corros. Sci.
, vol.40
, pp. 740-765
-
-
Shaikh, H.1
Amirthalingam, R.2
Anita, T.3
Sivaibharasi, N.4
Jaykumar, T.5
Manohar, P.6
Khatak, H.S.7
-
6
-
-
0024646644
-
Acoustic emission from intergranular subcritical crack growth
-
A
-
Jones R.H., Friesel M.A., Pathania R. Acoustic emission from intergranular subcritical crack growth. Metall. Trans. A 1989, 20A:637-648.
-
(1989)
Metall. Trans. A
, vol.20
, pp. 637-648
-
-
Jones, R.H.1
Friesel, M.A.2
Pathania, R.3
-
7
-
-
78149466623
-
Acoustic emission monitoring of slow strain rate tensile tests of 304L stainless steel in supercritical water environment
-
Máthis K., Prchal D., Novotný R., Hähner P. Acoustic emission monitoring of slow strain rate tensile tests of 304L stainless steel in supercritical water environment. Corros. Sci. 2011, 53:59-63.
-
(2011)
Corros. Sci.
, vol.53
, pp. 59-63
-
-
Máthis, K.1
Prchal, D.2
Novotný, R.3
Hähner, P.4
-
8
-
-
0027676224
-
The correlation of acoustic emission with rate of corrosion
-
Seal K.H.W., Lim K.B., Chew C.H., Teoh S.H. The correlation of acoustic emission with rate of corrosion. Corros. Sci. 1993, 34:1707-1713.
-
(1993)
Corros. Sci.
, vol.34
, pp. 1707-1713
-
-
Seal, K.H.W.1
Lim, K.B.2
Chew, C.H.3
Teoh, S.H.4
-
9
-
-
0018722865
-
Acoustic emission from corroding electrodes
-
Mansfeld F., Stocker P.J. Acoustic emission from corroding electrodes. Corrosion 1979, 35:541-543.
-
(1979)
Corrosion
, vol.35
, pp. 541-543
-
-
Mansfeld, F.1
Stocker, P.J.2
-
10
-
-
0023535081
-
Spectrum analysis of corrosion potential fluctuations for localized corrosion of type 304 stainless steel
-
Magaino S., Kawaguchi A., Hirata A., Osaka T. Spectrum analysis of corrosion potential fluctuations for localized corrosion of type 304 stainless steel. J. Electrochem. Soc. 1987, 134:2993-2996.
-
(1987)
J. Electrochem. Soc.
, vol.134
, pp. 2993-2996
-
-
Magaino, S.1
Kawaguchi, A.2
Hirata, A.3
Osaka, T.4
-
11
-
-
0000478673
-
Acoustic emission during pitting and transgranular crack initiation in type 304 stainless steel
-
Jones R.H., Friesel M.A. Acoustic emission during pitting and transgranular crack initiation in type 304 stainless steel. Corrosion 1992, 48:751-758.
-
(1992)
Corrosion
, vol.48
, pp. 751-758
-
-
Jones, R.H.1
Friesel, M.A.2
-
12
-
-
0029360971
-
An acoustic emission technique for monitoring pitting corrosion of austenitic stainless steels
-
Mazille H., Rothea R., Tronel C. An acoustic emission technique for monitoring pitting corrosion of austenitic stainless steels. Corros. Sci. 1995, 37:1365-1375.
-
(1995)
Corros. Sci.
, vol.37
, pp. 1365-1375
-
-
Mazille, H.1
Rothea, R.2
Tronel, C.3
-
13
-
-
0034831736
-
Monitoring pitting corrosion of AISI 316L austenitic stainless steel by acoustic emission technique: choice of representative acoustic parameters
-
Fregonese M., Idrissi H., Mazille H. Monitoring pitting corrosion of AISI 316L austenitic stainless steel by acoustic emission technique: choice of representative acoustic parameters. J. Mater. Sci. 2001, 36:557-563.
-
(2001)
J. Mater. Sci.
, vol.36
, pp. 557-563
-
-
Fregonese, M.1
Idrissi, H.2
Mazille, H.3
-
14
-
-
0035297662
-
Initiation and propagation steps in pitting corrosion of austenitic stainless steels: monitoring by acoustic emission
-
Fregonese M., Idrissi H., Mazille H., Renaud L., Cetre Y. Initiation and propagation steps in pitting corrosion of austenitic stainless steels: monitoring by acoustic emission. Corros. Sci. 2001, 43:627-641.
-
(2001)
Corros. Sci.
, vol.43
, pp. 627-641
-
-
Fregonese, M.1
Idrissi, H.2
Mazille, H.3
Renaud, L.4
Cetre, Y.5
-
15
-
-
0037411842
-
Investigation of pitting corrosion of stainless steel by means of acoustic emission and potentiodynamic methods
-
Darowicki K., Mirakowski A., Krakowiak S. Investigation of pitting corrosion of stainless steel by means of acoustic emission and potentiodynamic methods. Corros. Sci. 2003, 45:1747-1756.
-
(2003)
Corros. Sci.
, vol.45
, pp. 1747-1756
-
-
Darowicki, K.1
Mirakowski, A.2
Krakowiak, S.3
-
16
-
-
74449086906
-
Pitting and uniform corrosion source recognition using acoustic emission parameters
-
Jirarungsatian C., Prateepasen A. Pitting and uniform corrosion source recognition using acoustic emission parameters. Corros. Sci. 2010, 52:187-197.
-
(2010)
Corros. Sci.
, vol.52
, pp. 187-197
-
-
Jirarungsatian, C.1
Prateepasen, A.2
-
17
-
-
0141569674
-
Ability of acoustic emission technique for detection and monitoring of crevice corrosion on 304 austenitic stainless steel
-
Kim Y.P., Fregonese M., Mazille H., Feron D., Santarini G. Ability of acoustic emission technique for detection and monitoring of crevice corrosion on 304 austenitic stainless steel. NDT and E Int. 2003, 36:553-562.
-
(2003)
NDT and E Int.
, vol.36
, pp. 553-562
-
-
Kim, Y.P.1
Fregonese, M.2
Mazille, H.3
Feron, D.4
Santarini, G.5
-
19
-
-
84934953224
-
Environmental factors affecting the critical potential for pitting in 18-8 stainless steel
-
Leckie H.P., Uhlig H.H. Environmental factors affecting the critical potential for pitting in 18-8 stainless steel. J. Electrochem. Soc. 1966, 113:1262-1267.
-
(1966)
J. Electrochem. Soc.
, vol.113
, pp. 1262-1267
-
-
Leckie, H.P.1
Uhlig, H.H.2
-
20
-
-
0019579303
-
A point defet model for anodic passive films: II. Chemical breakdown and pit initiation
-
Lin L.F., Chao C.Y., Macdonald D.D. A point defet model for anodic passive films: II. Chemical breakdown and pit initiation. J. Electrochem. Soc. 1981, 128:1194-1198.
-
(1981)
J. Electrochem. Soc.
, vol.128
, pp. 1194-1198
-
-
Lin, L.F.1
Chao, C.Y.2
Macdonald, D.D.3
-
21
-
-
0001759975
-
A theory for breakdown of anodic oxide films on metals
-
Sato N. A theory for breakdown of anodic oxide films on metals. Electrochim. Acta 1971, 16.
-
(1971)
Electrochim. Acta
, vol.16
-
-
Sato, N.1
-
22
-
-
0025859693
-
Plate wave acoustic emission
-
Gorman M.R. Plate wave acoustic emission. J. Acoust. Soc. Am. 1991, 90:358-364.
-
(1991)
J. Acoust. Soc. Am.
, vol.90
, pp. 358-364
-
-
Gorman, M.R.1
-
23
-
-
0016941619
-
Acoustic emission method for monitoring corrosion reactions
-
Rettig T.W., Felsen M.J. Acoustic emission method for monitoring corrosion reactions. Corrosion 1976, 32:121-126.
-
(1976)
Corrosion
, vol.32
, pp. 121-126
-
-
Rettig, T.W.1
Felsen, M.J.2
-
24
-
-
25444486072
-
Analysis of modal acoustic emission signals of LY12CZ aluminum alloy at anodic and cathodic polarization
-
Chang H., Han E.H., Wang J.Q., Ke W. Analysis of modal acoustic emission signals of LY12CZ aluminum alloy at anodic and cathodic polarization. NDT and E Int. 2006, 39:8-12.
-
(2006)
NDT and E Int.
, vol.39
, pp. 8-12
-
-
Chang, H.1
Han, E.H.2
Wang, J.Q.3
Ke, W.4
-
25
-
-
55249127035
-
Modern concept of acoustic emission (AE) coupled with electrochemical measurements for monitoring the elastomer-coated carbon steel damage in phosphoric acid medium
-
Idrissi H., Ramadan S., Maghnouj J., Boulif R. Modern concept of acoustic emission (AE) coupled with electrochemical measurements for monitoring the elastomer-coated carbon steel damage in phosphoric acid medium. Prog. Org. Coat. 2008, 62:382-388.
-
(2008)
Prog. Org. Coat.
, vol.62
, pp. 382-388
-
-
Idrissi, H.1
Ramadan, S.2
Maghnouj, J.3
Boulif, R.4
-
26
-
-
67649770253
-
Correlation between corrosion rate and AE signal in an acidic environment for mild steel
-
Kasai N., Utatsu K., Park S., Kitsukawa S., Sekine K. Correlation between corrosion rate and AE signal in an acidic environment for mild steel. Corros. Sci. 2009, 51:1679-1684.
-
(2009)
Corros. Sci.
, vol.51
, pp. 1679-1684
-
-
Kasai, N.1
Utatsu, K.2
Park, S.3
Kitsukawa, S.4
Sekine, K.5
-
27
-
-
0036568097
-
Pit growth studies in stainless steel foils: I. Introduction and pit growth kinetics
-
Ernst P., Newman R.C. Pit growth studies in stainless steel foils: I. Introduction and pit growth kinetics. Corros. Sci. 2002, 44:927-941.
-
(2002)
Corros. Sci.
, vol.44
, pp. 927-941
-
-
Ernst, P.1
Newman, R.C.2
-
28
-
-
0036568081
-
Pit growth studies in stainless steel foils: II. Effect of temperature, chloride concentration and sulphate addition
-
Ernst P., Newman R.C. Pit growth studies in stainless steel foils: II. Effect of temperature, chloride concentration and sulphate addition. Corros. Sci. 2002, 44:943-954.
-
(2002)
Corros. Sci.
, vol.44
, pp. 943-954
-
-
Ernst, P.1
Newman, R.C.2
-
29
-
-
34250229999
-
The detection of selective phase corrosion in cast nickel aluminium bronze by acoustic emission techniques
-
Culpan E.A., Foley A.G. The detection of selective phase corrosion in cast nickel aluminium bronze by acoustic emission techniques. J. Mater. Sci. 1982, 17:953-964.
-
(1982)
J. Mater. Sci.
, vol.17
, pp. 953-964
-
-
Culpan, E.A.1
Foley, A.G.2
-
30
-
-
11344283658
-
Hydrodynamic measurement of a single corrosion pit
-
Volkov A.O., Datta P.K., Burnell-Gray J.S., Couper R. Hydrodynamic measurement of a single corrosion pit. Corros. Sci. 2004, 46:7.
-
(2004)
Corros. Sci.
, vol.46
, pp. 7
-
-
Volkov, A.O.1
Datta, P.K.2
Burnell-Gray, J.S.3
Couper, R.4
-
31
-
-
0017717230
-
The effect of specimen position on the shape of corrosion pits in an austenitic stainless steel
-
Mankowski J., Szklarska-Smialowska Z. The effect of specimen position on the shape of corrosion pits in an austenitic stainless steel. Corros. Sci. 1977, 17.
-
(1977)
Corros. Sci.
, vol.17
-
-
Mankowski, J.1
Szklarska-Smialowska, Z.2
-
32
-
-
0016557181
-
Studies on accumulation of chloride ions in pits growing during anodic polarization
-
Mankowski J., Szklarska-Smialowska Z. Studies on accumulation of chloride ions in pits growing during anodic polarization. Corros. Sci. 1975, 15:493-501.
-
(1975)
Corros. Sci.
, vol.15
, pp. 493-501
-
-
Mankowski, J.1
Szklarska-Smialowska, Z.2
-
33
-
-
0002942886
-
Metastable pitting corrosion of stainless steel and the transition to stability
-
Pistorius P.C., Burstein G.T. Metastable pitting corrosion of stainless steel and the transition to stability. Philos. Trans. R. Soc. Lond. A 1992, 341:531-559.
-
(1992)
Philos. Trans. R. Soc. Lond. A
, vol.341
, pp. 531-559
-
-
Pistorius, P.C.1
Burstein, G.T.2
-
34
-
-
0031171653
-
The mechanism of lacy cover formation in pitting
-
Ernst P., Laycock N.J., Moayed M.H., Newman R.C. The mechanism of lacy cover formation in pitting. Corros. Sci. 1997, 39:1133-1136.
-
(1997)
Corros. Sci.
, vol.39
, pp. 1133-1136
-
-
Ernst, P.1
Laycock, N.J.2
Moayed, M.H.3
Newman, R.C.4
-
35
-
-
0023093392
-
Metastable pitting of stainless steel
-
Frankel G.S., Stockert L., Hunkeler F., Boehni H. Metastable pitting of stainless steel. Corrosion 1987, 43:429-436.
-
(1987)
Corrosion
, vol.43
, pp. 429-436
-
-
Frankel, G.S.1
Stockert, L.2
Hunkeler, F.3
Boehni, H.4
-
36
-
-
0019221108
-
Stress corrosion cracking of type 304 stainless steel at room temperature influence of chloride content and acidity
-
Torchio S. Stress corrosion cracking of type 304 stainless steel at room temperature influence of chloride content and acidity. Corros. Sci. 1980, 20:555-561.
-
(1980)
Corros. Sci.
, vol.20
, pp. 555-561
-
-
Torchio, S.1
|