1
-
-
0036133483
-
Thermal cycling induced deformation and damage in carbon fiber reinforced copper composite
-
DOI 10.1016/S1359-6462(01)01217-9, PII S1359646201012179
-
MH Lin W Buchgraber G Korb PW Kao 2002 Thermal cycling induced deformation and damage in carbon fiber reinforces copper composite Scripta Mater. 46 169 173 1:CAS:528:DC%2BD3MXptlajsbg%3D 10.1016/S1359-6462(01)01217-9 (Pubitemid 33149494)
-
(2002)
Scripta Materialia
, vol.46
, Issue.2
, pp. 169-173
-
-
Lin, M.H.1
Buchgraber, W.2
Korb, G.3
Kao, P.W.4
-
2
-
-
0036802859
-
Friction and wear of copper-graphite composites made with Cu-coated and uncoated graphite powders
-
DOI 10.1016/S0043-1648(02)00038-8, PII S0043164802000388
-
SE Moustafa SA El-Badry AM Sanad B Kieback 2002 Friction and wear of copper-graphite composites made with Cu-coated and uncoated graphite powder Wear 253 699 710 1:CAS:528:DC%2BD38Xns1WrurY%3D 10.1016/S0043-1648(02)00038-8 (Pubitemid 35274044)
-
(2002)
Wear
, vol.253
, Issue.7-8
, pp. 699-710
-
-
Moustafa, S.F.1
El-Badry, S.A.2
Sanad, A.M.3
Kieback, B.4
-
3
-
-
0032155493
-
Effects of titanium impregnation on the thermal conductivity of carbon/copper composite materials
-
PII S0022311598004346
-
T Oku A Kurumada T Sogabe T Oku T Hiraoka K Kuroda 1998 Effects of titanium impregnation on the thermal conductivity of carbon/copper materials J. Nucl. Mater. 257 59 66 1:CAS:528:DyaK1cXmtl2ltLg%3D 10.1016/S0022-3115(98)00434- 6 (Pubitemid 128433673)
-
(1998)
Journal of Nuclear Materials
, vol.257
, Issue.1
, pp. 59-66
-
-
Oku, T.1
Kurumada, A.2
Sogabe, T.3
Oku, T.4
Hiraoka, T.5
Kuroda, K.6
-
4
-
-
0035384743
-
A novel electrical contact material with improved self-lubrification for railway current collectors
-
1:CAS:528:DC%2BD3MXkvF2ht74%3D 10.1016/S0043-1648(01)00700-1
-
DH He R Manory 2001 A novel electrical contact material with improved self-lubrification for railway current collectors Wear 249 626 636 1:CAS:528:DC%2BD3MXkvF2ht74%3D 10.1016/S0043-1648(01)00700-1
-
(2001)
Wear
, vol.249
, pp. 626-636
-
-
He, D.H.1
Manory, R.2
-
5
-
-
2142842403
-
-
P. Ramakrishnan (ed.) ASM International, India Chapter, Bombay
-
Feng, Y., Ying, M., Wang, C.: In: P. Ramakrishnan (ed.), Proceedings of Advances in composite materials. ASM International, India Chapter, Bombay, pp. 631-634 (1990)
-
(1990)
Proceedings of Advances in Composite Materials
, pp. 631-634
-
-
Feng, Y.1
Ying, M.2
Wang, C.3
-
6
-
-
0027060532
-
Tribological properties of metal matrix-graphite particle composites
-
PK Rohatgi S Ray Y Liu 1992 Tribological properties of metal matrix-graphite particle composites Int. Mater. Rev. 37 129 149 1:CAS:528:DyaK3sXhslent78%3D (Pubitemid 23567092)
-
(1992)
International Materials Reviews
, vol.37
, Issue.3
, pp. 129-149
-
-
Rohatgi, P.K.1
Ray, S.2
Liu, Y.3
-
7
-
-
0242440063
-
Viability study and mechanical characterisation of copper-graphite electrical contacts produced by adhesive joining
-
10.1016/S0924-0136(03)00476-X
-
JM Garcia-Marquez N Anton A Jimenez M Madrid MA Martinez JA Bas 2003 Viability study and mechanical characterisation of copper-graphite electrical contacts produced by adhesive joining J. Mater. Process. Technol. 143 144 290 293 10.1016/S0924-0136(03)00476-X
-
(2003)
J. Mater. Process. Technol.
, vol.143
, Issue.144
, pp. 290-293
-
-
Garcia-Marquez, J.M.1
Anton, N.2
Jimenez, A.3
Madrid, M.4
Martinez, M.A.5
Bas, J.A.6
-
8
-
-
33750802493
-
A new processing technique for copper-graphite multifilamentary nanocomposite wire: Microstructures and electrical properties
-
DOI 10.1016/j.jmatprotec.2006.06.019, PII S0924013606006595
-
A Guillet E Yama Nzoma P Pareige 2007 A new processing technique for copper-graphite multifilamentary nanocomposite wire: microstructures and electrical properties J. Mater. Process. Technol. 182 50 57 1:CAS:528: DC%2BD28XhtF2ksr3P 10.1016/j.jmatprotec.2006.06.019 (Pubitemid 44711943)
-
(2007)
Journal of Materials Processing Technology
, vol.182
, Issue.1-3
, pp. 50-57
-
-
Guillet, A.1
Nzoma, E.Y.2
Pareige, P.3
-
10
-
-
0037413786
-
Wear performance of copper-graphite composite and a leaded copper alloy
-
M Kestursatya JK Kim PK Rohatgi 2001 Wear performance of copper-graphite composite and a leaded copper alloy Mater. Sci. Eng. A 399 150 158
-
(2001)
Mater. Sci. Eng. A
, vol.399
, pp. 150-158
-
-
Kestursatya, M.1
Kim, J.K.2
Rohatgi, P.K.3
-
11
-
-
0027007054
-
Friction and wear of aluminum-graphite composites: The smearing process of graphite during sliding
-
DOI 10.1016/0043-1648(92)90303-P
-
YB Liu SC Lim S Ray PK Rohatgi 1992 Friction and wear of aluminum-graphite composites: the smearing process of graphite during sliding Wear 159 201 205 1:CAS:528:DyaK3sXhvFKjsb4%3D 10.1016/0043-1648(92)90303-P (Pubitemid 23599837)
-
(1992)
Wear
, vol.159
, Issue.2
, pp. 201-205
-
-
Liu, Y.B.1
Lim, S.C.2
Ray, S.3
Rohatgi, P.K.4
-
12
-
-
0024751596
-
Dry sliding wear of sintered 6061 aluminium alloy. Graphite particle composites
-
DOI 10.1016/0301-679X(89)90147-3
-
AK Jaha SV Prasad GS Upadhyaya 1989 Dry sliding wear of sintered 6061 aluminum alloy graphite particle composites Tribol. Int. 22 321 327 10.1016/0301-679X(89)90147-3 (Pubitemid 20622980)
-
(1989)
Tribology International
, vol.22
, Issue.5
, pp. 321-327
-
-
Jha, A.K.1
Prasad, S.V.2
Upadhyaya, G.S.3
-
13
-
-
51249168555
-
Wear mechanisms in hybrid composites of graphite-20% SiC in 356 aluminum alloy (Al-7% Si-0.3% Mg)
-
1:CAS:528:DyaK2MXivV2is7c%3D 10.1007/BF02669796
-
W Ames AT Alpas 1995 Wear mechanisms in hybrid composites of graphite-20% SiC in 356 aluminum alloy (Al-7% Si-0.3% Mg) Metall. Mater. Trans. A 26A 85 98 1:CAS:528:DyaK2MXivV2is7c%3D 10.1007/BF02669796
-
(1995)
Metall. Mater. Trans. A
, vol.26
, pp. 85-98
-
-
Ames, W.1
Alpas, A.T.2
-
14
-
-
0035482143
-
The role of tribo-layers on the sliding wear behavior of graphitic aluminum matrix composites
-
PII S0043164801007967
-
AR Riahi AT Alpas 2001 The role of tribo-layers on the sliding wear behavior of graphite aluminum matrix composites Wear 251 1396 1407 10.1016/S0043-1648(01)00796-7 (Pubitemid 33071591)
-
(2001)
Wear
, vol.250-251
, Issue.PART 2
, pp. 1396-1407
-
-
Riahi, A.R.1
Alpas, A.T.2
-
15
-
-
0030268098
-
Effect of humidity on friction and wear of Al-Si eutectic alloy and Al-Si alloy-graphite composites
-
DOI 10.1016/0043-1648(96)06955-4
-
BK Yen T Ishihara 1996 Effect of humidity on friction and wear of Al-Si eutectic alloy and A1-Si alloy-graphite composites Wear 198 169 175 1:CAS:528:DyaK28XlsFans7w%3D 10.1016/0043-1648(96)06955-4 (Pubitemid 27072068)
-
(1996)
Wear
, vol.198
, Issue.1-2
, pp. 169-175
-
-
Yen, B.K.1
Ishihara, T.2
-
16
-
-
5544277047
-
(p) composites
-
DOI 10.1016/j.wear.2004.05.015, PII S004316480400122X
-
JB Yang CB Lin TC Wang HY Chu 2004 The tribological characteristics of A356.2Al alloy/Gr(p) composites Wear 257 941 952 1:CAS:528:DC%2BD2cXotlKgs7w%3D 10.1016/j.wear.2004.05.015 (Pubitemid 39366754)
-
(2004)
Wear
, vol.257
, Issue.9-10
, pp. 941-952
-
-
Yang, J.B.1
Lin, C.B.2
Wang, T.C.3
Chu, H.Y.4
-
18
-
-
0041600559
-
The mechanisms of wear of cast iron in dry sliding
-
10.1016/0043-1648(68)90558-9
-
E Takeuchi 1968 The mechanisms of wear of cast iron in dry sliding Wear 11 201 212 10.1016/0043-1648(68)90558-9
-
(1968)
Wear
, vol.11
, pp. 201-212
-
-
Takeuchi, E.1
-
19
-
-
0001331373
-
The influence of speed on metallic wear
-
1:CAS:528:DyaF3MXjslCisw%3D%3D 10.1098/rspa.1960.0220
-
W Hirst JK Lancaster 1960 The influence of speed on metallic wear Proc, R. Soc. Lond. Ser. A Math. Phys. Sci 259 1297 228 1:CAS:528:DyaF3MXjslCisw%3D%3D 10.1098/rspa.1960.0220
-
(1960)
Proc, R. Soc. Lond. Ser. A Math. Phys. Sci
, vol.259
, Issue.1297
, pp. 228
-
-
Hirst, W.1
Lancaster, J.K.2
-
20
-
-
0023012959
-
Wear characteristics of powder-extruded Al-Si alloys containing dispersed graphite particle
-
E Yuasa T Morooka F Hayama 1986 Wear characteristics of powder-extruded Al-Si alloys containing dispersed graphite particle J. Jpn inst. Met. 50 1032 1040 1:CAS:528:DyaL2sXntFGjtQ%3D%3D (Pubitemid 17557042)
-
(1986)
Nippon Kinzoku Gakkai-si
, vol.50
, Issue.12
, pp. 1032-1040
-
-
Yuasa Eiji1
Morooka Toshimasa2
Hayama Fusao3
-
21
-
-
0019560202
-
Dry wear of Al-graphite particle composites
-
DOI 10.1016/0043-1648(81)90181-2
-
SK Biswas BN Pramila Bai 1981 Dry wear of Al-graphite particle composites Wear 68 347 358 1:CAS:528:DyaL3MXlsFCqtLg%3D 10.1016/0043-1648(81)90181-2 (Pubitemid 12429822)
-
(1981)
Wear
, vol.68
, Issue.3
, pp. 347-358
-
-
Biswas, S.K.1
Bai B.N.Pramila2
-
22
-
-
58149086732
-
Surface modifications in tribological contacts
-
1:CAS:528:DC%2BD1MXhsVGitw%3D%3D 10.1016/j.wear.2008.04.035
-
S Jacobson S Hogmark 2009 Surface modifications in tribological contacts Wear 266 370 378 1:CAS:528:DC%2BD1MXhsVGitw%3D%3D 10.1016/j.wear.2008.04.035
-
(2009)
Wear
, vol.266
, pp. 370-378
-
-
Jacobson, S.1
Hogmark, S.2
-
23
-
-
0021645427
-
The 3rd-body approach: A mechanical view of wear
-
M Godet 1984 The 3rd-body approach: a mechanical view of wear Wear 100 437 452 10.1016/0043-1648(84)90025-5 (Pubitemid 15488647)
-
(1984)
Wear
, vol.100
, Issue.1-3
, pp. 437-452
-
-
Godet Maurice1
-
24
-
-
33847143762
-
Influence of sliding speed on the dry sliding wear behaviour and the subsurface deformation on hybrid metal matrix composite
-
DOI 10.1016/j.wear.2006.10.016, PII S0043164806003644
-
S Basavarajappa G Chandramohan A Mahadevan M Thangavelu R Subramanian P Gopalakrishnan 2007 Influence of sliding speed on the dry sliding wear behaviour and the subsurface deformation on hybrid metal matrix composite Wear 262 7/8 1007 1012 1:CAS:528:DC%2BD2sXitFyktLY%3D 10.1016/j.wear.2006.10.016 (Pubitemid 46290573)
-
(2007)
Wear
, vol.262
, Issue.7-8
, pp. 1007-1012
-
-
Basavarajappa, S.1
Chandramohan, G.2
Mahadevan, A.3
Thangavelu, M.4
Subramanian, R.5
Gopalakrishnan, P.6
-
25
-
-
55249087627
-
Role of surface texture of harder surface on subsurface deformation
-
1:CAS:528:DC%2BD1cXhtlCrtb3K 10.1016/j.wear.2008.05.008
-
PL Menezes Kishore SV Kailas 2009 Role of surface texture of harder surface on subsurface deformation Wear 266 103 109 1:CAS:528:DC%2BD1cXhtlCrtb3K 10.1016/j.wear.2008.05.008
-
(2009)
Wear
, vol.266
, pp. 103-109
-
-
Menezes, P.L.1
Kishore2
Kailas, S.V.3
-
26
-
-
34748840930
-
The effect of sliding velocity on the tribological behavior of copper
-
DOI 10.1016/j.wear.2007.01.095, PII S0043164807004073
-
A Emgea S Karthikeyan HJ Kim DA Rigney 2007 The effect of sliding velocity on the tribological behavior of copper Wear 263 614 618 10.1016/j.wear.2007.01.095 (Pubitemid 47487410)
-
(2007)
Wear
, vol.263
, Issue.1-6 SPEC. ISS.
, pp. 614-618
-
-
Emge, A.1
Karthikeyan, S.2
Kim, H.J.3
Rigney, D.A.4
-
27
-
-
0023365789
-
Plastic flow process of surface layer in flow wear under boundary lubricated conditions
-
DOI 10.1016/0043-1648(87)90254-7
-
T Akagaki K Kato 1987 Plastic flow process of surface layer in flow wear under boundary lubricated conditions Wear 117 179 196 10.1016/0043-1648(87) 90254-7 (Pubitemid 17600972)
-
(1987)
Wear
, vol.117
, Issue.2
, pp. 179-196
-
-
Akagaki, T.1
Kato, K.2
-
28
-
-
84897371346
-
Plastic ratchetting as a mechanism of metallic wear
-
1:CAS:528:DyaK2cXlvVCqt7g%3D 10.1098/rspa.1994.0066
-
A Kapoor KL Johnson 1994 Plastic ratchetting as a mechanism of metallic wear Proc. R. Soc. London Ser.A 445 367 381 1:CAS:528:DyaK2cXlvVCqt7g%3D 10.1098/rspa.1994.0066
-
(1994)
Proc. R. Soc. London ser .A
, vol.445
, pp. 367-381
-
-
Kapoor, A.1
Johnson, K.L.2
|