Volumn 141, Issue 1, 2011, Pages 128-135

Rhodium supported on silica-stabilized alumina for catalytic decomposition of N2O

Author keywords

Al2O3; Decomposition; Nitrous oxide; Rhodium; SiO 2

Indexed keywords

AL2O3; CATALYTIC DECOMPOSITION; CATALYTIC PERFORMANCE; DECOMPOSITION PROCESS; NITROUS OXIDE; RHODIUM CATALYSTS; SIO 2; SUPPORTED ON SILICA; THERMALLY STABLE;

EID: 79651472467     PISSN: 1011372X     EISSN: 1572879X     Source Type: Journal    
DOI: 10.1007/s10562-010-0472-3     Document Type: Article
Times cited : (24)

References (25)
  • 7
    • 0020798130 scopus 로고
    • Influence of lanthanum oxide on the thermal stability of gamma alumina catalyst supports
    • DOI 10.1016/0166-9834(83)80009-8
    • H Schaper EBM Doesburg LL van Reijen 1983 Appl Catal 7 211 1:CAS:528:DyaL3sXlsVKrsrc%3D 10.1016/0166-9834(83)80009-8 (Pubitemid 14528637)
    • (1983) Applied catalysis , vol.7 , Issue.2 , pp. 211-220
    • Schaper, H.1    Doesburg, E.B.M.2    Van Reijen, L.L.3
  • 9
    • 0026205682 scopus 로고
    • Stabilization of alumina by addition of lanthanum
    • DOI 10.1016/S0166-9834(00)83128-0
    • B Beguin E Garbowski M Primet 1991 Appl Catal 75 119 1:CAS:528: DyaK3MXlsVemurc%3D 10.1016/S0166-9834(00)83128-0 (Pubitemid 21738009)
    • (1991) Applied catalysis , vol.75 , Issue.1 , pp. 119-132
    • Beguin Bernard1    Garbowski Edouard2    Primet Michel3
  • 11
    • 34547690958 scopus 로고    scopus 로고
    • An excellent support of Pd catalyst for methane combustion: Thermal-stable Si-doped alumina
    • DOI 10.1016/j.cattod.2007.06.011, PII S0920586107003549
    • X Wang Y Guo G Lu Y Hu L Jiang Y Guo Z Zhang 2007 Catal Today 126 369 1:CAS:528:DC%2BD2sXovFGgurg%3D 10.1016/j.cattod.2007.06.011 (Pubitemid 47212691)
    • (2007) Catalysis Today , vol.126 , Issue.SPEC. ISS. , pp. 369-374
    • Wang, X.1    Guo, Y.2    Lu, G.3    Hu, Y.4    Jiang, L.5    Guo, Y.6    Zhang, Z.7
  • 12
    • 0035478623 scopus 로고    scopus 로고
    • Maintenance of large surface area of alumina heated at elevated temperatures above 1300 C by preparing silica-containing pseudoboehmite aerogel
    • DOI 10.1016/S0022-3093(01)00817-1, PII S0022309301008171
    • T Horiuchi T Osaki T Sugiyama K Suzuki T Mori 2001 J Non-Cryst Solids 291 187 1:CAS:528:DC%2BD3MXntVCmtbs%3D 10.1016/S0022-3093(01)00817-1 (Pubitemid 32903761)
    • (2001) Journal of Non-Crystalline Solids , vol.291 , Issue.3 , pp. 187-198
    • Horiuchi, T.1    Osaki, T.2    Sugiyama, T.3    Suzuki, K.4    Mori, T.5
  • 13
    • 34249944823 scopus 로고    scopus 로고
    • Silica-doped alumina cryogels with high thermal stability
    • DOI 10.1016/j.jnoncrysol.2007.04.016, PII S0022309307004139
    • T Osaki K Nagashima K Watari K Tajiri 2007 J Non-Cryst Solids 353 2436 1:CAS:528:DC%2BD2sXmt1yksr0%3D 10.1016/j.jnoncrysol.2007.04.016 (Pubitemid 46879798)
    • (2007) Journal of Non-Crystalline Solids , vol.353 , Issue.24-25 , pp. 2436-2442
    • Osaki, T.1    Nagashima, K.2    Watari, K.3    Tajiri, K.4
  • 17
    • 0012918488 scopus 로고    scopus 로고
    • Thermal stabilization of catalyst supports and their application to high-temperature catalytic combustion
    • DOI 10.1016/0926-860X(95)00294-4
    • H Arai M Machida 1996 Appl Catal A 138 161 1:CAS:528:DyaK28XjtFSmur0%3D 10.1016/0926-860X(95)00294-4 (Pubitemid 126368955)
    • (1996) Applied Catalysis A: General , vol.138 , Issue.2 , pp. 161-176
    • Arai, H.1    Machida, M.2
  • 21
    • 0002340972 scopus 로고    scopus 로고
    • 1:CAS:528:DyaK1MXivF2ls7g%3D 10.1016/S0920-5861(99)00011-5
    • CP Hwang CT Yeh Q Zhu 1999 Catal Today 51 93 1:CAS:528:DyaK1MXivF2ls7g%3D 10.1016/S0920-5861(99)00011-5
    • (1999) Catal Today , vol.51 , pp. 93
    • Hwang, C.P.1    Yeh, C.T.2    Zhu, Q.3
  • 24
    • 0023981911 scopus 로고
    • 1:CAS:528:DyaL1cXhtlyms7Y%3D 10.1021/ja00215a010
    • P Basu D Panayotov JT Yates Jr 1988 J Am Chem Soc 110 2074 1:CAS:528:DyaL1cXhtlyms7Y%3D 10.1021/ja00215a010
    • (1988) J Am Chem Soc , vol.110 , pp. 2074
    • Basu, P.1    Panayotov, D.2    Yates, Jr.J.T.3
  • 25
    • 0342601368 scopus 로고    scopus 로고
    • 2O on metal oxide supports
    • DOI 10.1016/S0926-3373(96)00088-4, PII S0926337396000884
    • RS Drago K Jurczyk N Kob 1997 Appl Catal B 13 69 1:CAS:528: DyaK2sXlvFSgsb4%3D 10.1016/S0926-3373(96)00088-4 (Pubitemid 27451415)
    • (1997) Applied Catalysis B: Environmental , vol.13 , Issue.1 , pp. 69-79
    • Drago, R.S.1    Jurczyk, K.2    Kob, N.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.