Volumn 36, Issue 2, 2011, Pages 1828-1836

Investigation of MEA degradation in PEM fuel cell by on/off cyclic operation under different humid conditions

Author keywords

Durability; MEA degradation; On off cyclic operation; PEMFC; Relative humidity

Indexed keywords

CARBON CORROSION; CATHODE LAYERS; CELL VOLTAGES; CHARGE TRANSFER RESISTANCE; CYCLIC OPERATION; ELECTROCHEMICAL SURFACE AREA; HUMID CONDITIONS; MEA DEGRADATION; OHMIC RESISTANCE; PEM FUEL CELL; PEMFC; PLATINUM PARTICLES; POLYMER ELECTROLYTE; RELATIVE HUMIDITIES; RELATIVE HUMIDITY; TEM ANALYSIS; XRD;

EID: 79551488440     PISSN: 03603199     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ijhydene.2010.02.053     Document Type: Conference Paper
Times cited : (69)

References (18)
  • 2
    • 36549069667 scopus 로고    scopus 로고
    • Comparison between two PEM fuel cell durability tests performed at constant current and under solicitations linked to transport mission profile
    • B. Wahdame, D. Candusso, X. Franois, F. Harel, M.-C. Péra, and D. Hissel Comparison between two PEM fuel cell durability tests performed at constant current and under solicitations linked to transport mission profile Int J Hydrogen Energy 32 2007 4523 4536
    • (2007) Int J Hydrogen Energy , vol.32 , pp. 4523-4536
    • Wahdame, B.1    Candusso, D.2    Franois, X.3    Harel, F.4    Péra, M.-C.5    Hissel, D.6
  • 3
    • 39849106503 scopus 로고    scopus 로고
    • Performance and degradation of high temperature polymer electrolyte fuel cell catalysts
    • A.S. Aricó, A. Stassi, E. Modica, R. Ornelas, I. Gatto, and E. Passalacqua Performance and degradation of high temperature polymer electrolyte fuel cell catalysts J Power Source 178 2008 525 536
    • (2008) J Power Source , vol.178 , pp. 525-536
    • Aricó, A.S.1    Stassi, A.2    Modica, E.3    Ornelas, R.4    Gatto, I.5    Passalacqua, E.6
  • 4
    • 58649090445 scopus 로고    scopus 로고
    • Performance decay of proton-exchange membrane fuel cells under open circuit conditions induced by membrane decomposition
    • S. Sugawara, T. Maruyama, Y. Nagahara, S.S. Kocha, K. Shinohra, and K. Tsujita Performance decay of proton-exchange membrane fuel cells under open circuit conditions induced by membrane decomposition J Power Source 187 2008 324 331
    • (2008) J Power Source , vol.187 , pp. 324-331
    • Sugawara, S.1    Maruyama, T.2    Nagahara, Y.3    Kocha, S.S.4    Shinohra, K.5    Tsujita, K.6
  • 5
    • 41949108195 scopus 로고    scopus 로고
    • A review of the main parameters influencing long-term performance and durability of PEM fuel cells
    • W. Schmittinger, and A. Vahidi A review of the main parameters influencing long-term performance and durability of PEM fuel cells J Power Source 180 2008 1 14
    • (2008) J Power Source , vol.180 , pp. 1-14
    • Schmittinger, W.1    Vahidi, A.2
  • 6
    • 0021374947 scopus 로고
    • The influence of Pt-activation on the corrosion of carbon in gas diffusion electrodes - A DEMS study
    • J. Willsau, and J. Heitbaum The influence of Pt-activation on the corrosion of carbon in gas diffusion electrodes - a DEMS study J Electroanal Chem Interfacial Electrochem 161 1984 93 101
    • (1984) J Electroanal Chem Interfacial Electrochem , vol.161 , pp. 93-101
    • Willsau, J.1    Heitbaum, J.2
  • 8
    • 33745500659 scopus 로고    scopus 로고
    • Model of carbon corrosion in PEM fuel cells
    • J.P. Meyers, and R.M. Darling Model of carbon corrosion in PEM fuel cells J Electrochem Soc 153 8 2006 A1432 A1442
    • (2006) J Electrochem Soc , vol.153 , Issue.8
    • Meyers, J.P.1    Darling, R.M.2
  • 9
    • 33748100890 scopus 로고    scopus 로고
    • PEM fuel cell cathode carbon corrosion due to the formation of air/fuel boundary at the anode
    • H. Tang, Z. Qi, M. Ramani, and J.F. Elter PEM fuel cell cathode carbon corrosion due to the formation of air/fuel boundary at the anode J Power Source 158 2006 1306 1312
    • (2006) J Power Source , vol.158 , pp. 1306-1312
    • Tang, H.1    Qi, Z.2    Ramani, M.3    Elter, J.F.4
  • 10
    • 0242509219 scopus 로고    scopus 로고
    • Kinetic model of platinum dissolution in PEMFCs
    • R.M. Darling, and J.P. Meyers Kinetic model of platinum dissolution in PEMFCs J Electrochem Soc 150 11 2003 A1523 A1527
    • (2003) J Electrochem Soc , vol.150 , Issue.11
    • Darling, R.M.1    Meyers, J.P.2
  • 11
    • 33748053026 scopus 로고    scopus 로고
    • Analytical TEM study of Pt particle deposition in the proton-exchange membrane of a membrane-electrode-assembly
    • T. Akita, A. Taniguchi, J. Maekawa, Z. Siroma, K. Tanaka, and M. Kohyama Analytical TEM study of Pt particle deposition in the proton-exchange membrane of a membrane-electrode-assembly J Power Source 159 2006 461 467
    • (2006) J Power Source , vol.159 , pp. 461-467
    • Akita, T.1    Taniguchi, A.2    Maekawa, J.3    Siroma, Z.4    Tanaka, K.5    Kohyama, M.6
  • 12
    • 33645451491 scopus 로고    scopus 로고
    • Platinum dissolution and deposition in the polymer electrolyte membrane of a PEM fuel cell as studied by potential cycling
    • K. Yasuda, A. Taniguchi, T. Akita, T. Ioroi, and Z. Siroma Platinum dissolution and deposition in the polymer electrolyte membrane of a PEM fuel cell as studied by potential cycling Phys Chem Chem Phys 8 2006 746 752
    • (2006) Phys Chem Chem Phys , vol.8 , pp. 746-752
    • Yasuda, K.1    Taniguchi, A.2    Akita, T.3    Ioroi, T.4    Siroma, Z.5
  • 16
    • 57949091575 scopus 로고    scopus 로고
    • A review of accelerated stress tests of MEA durability in PEM fuel cells
    • S. Zhang, X. Yuan, H. Wang, W. Mérida, H. Zhu, and J. Shen A review of accelerated stress tests of MEA durability in PEM fuel cells Int J Hydrogen Energy 34 2009 388 404
    • (2009) Int J Hydrogen Energy , vol.34 , pp. 388-404
    • Zhang, S.1    Yuan, X.2    Wang, H.3    Mérida, W.4    Zhu, H.5    Shen, J.6
  • 17
    • 0035799631 scopus 로고    scopus 로고
    • Electrochemical impedance study of PEM fuel cells. Experimental diagnostics and modeling of air cathodes
    • M. Ciureanu, and R. Roberge Electrochemical impedance study of PEM fuel cells. Experimental diagnostics and modeling of air cathodes J Phys Chem B 105 2001 3531 3539
    • (2001) J Phys Chem B , vol.105 , pp. 3531-3539
    • Ciureanu, M.1    Roberge, R.2
  • 18
    • 30344474640 scopus 로고    scopus 로고
    • Ex situ and in situ stability studies of PEMFC catalysts effect of carbon type and humidification on degradation of the carbon
    • D.A. Stevens, M.T. Hicks, G.M. Haugen, and J.R. Dhan Ex situ and in situ stability studies of PEMFC catalysts effect of carbon type and humidification on degradation of the carbon J Electrochem Soc 152 12 2005 A2309 A2315
    • (2005) J Electrochem Soc , vol.152 , Issue.12
    • Stevens, D.A.1    Hicks, M.T.2    Haugen, G.M.3    Dhan, J.R.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.