메뉴 건너뛰기




Volumn 5, Issue 1, 2011, Pages 82-91

Fracture behavior of quenched poly(lactic acid)

Author keywords

Essential work of fracture (EWF); Mechanical properties; Physical aging; Poly(lactic acid) PLA

Indexed keywords


EID: 78650287441     PISSN: 1788618X     EISSN: None     Source Type: Journal    
DOI: 10.3144/expresspolymlett.2011.9     Document Type: Article
Times cited : (48)

References (42)
  • 1
    • 0033881609 scopus 로고    scopus 로고
    • Polymeric biomaterials
    • DOI: 10.1016/S1359-6454(99)00299-2
    • Griffith L. G.: Polymeric biomaterials. Acta Materialia, 48, 263-277 (2000). DOI: 10.1016/S1359-6454(99)00299-2
    • (2000) Acta Materialia , vol.48 , pp. 263-277
    • Griffith, L.G.1
  • 2
    • 53149134257 scopus 로고    scopus 로고
    • Processing technologies for poly(lactic acid)
    • DOI: 10.1016/j.progpolymsci.2008.05.004
    • Lim L-T., Auras R., Rubino M.: Processing technologies for poly(lactic acid). Progress in Polymer Science, 33, 820-852 (2008). DOI: 10.1016/j.progpolymsci.2008.05.004
    • (2008) Progress in Polymer Science , vol.33 , pp. 820-852
    • Lim, L.-T.1    Auras, R.2    Rubino, M.3
  • 3
    • 19944422474 scopus 로고    scopus 로고
    • Crystallinity and mechanical properties of optically pure polylactides and their blends
    • DOI: 10.1002/pen.20331
    • Sarasua J. R., Arraiza A. L., Balerdi P., Maiza I.: Crystallinity and mechanical properties of optically pure polylactides and their blends. Polymer Engineering and Science, 45, 745-753 (2005). DOI: 10.1002/pen.20331
    • (2005) Polymer Engineering and Science , vol.45 , pp. 745-753
    • Sarasua, J.R.1    Arraiza, A.L.2    Balerdi, P.3    Maiza, I.4
  • 4
    • 4744360239 scopus 로고    scopus 로고
    • An overview of polylactides as packaging materials
    • DOI: 10.1002/mabi.200400043
    • Auras R., Harte B., Selke S.: An overview of polylactides as packaging materials. Macromolecular Bioscience, 4, 835-864 (2004). DOI: 10.1002/mabi.200400043
    • (2004) Macromolecular Bioscience , vol.4 , pp. 835-864
    • Auras, R.1    Harte, B.2    Selke, S.3
  • 5
    • 0032186718 scopus 로고    scopus 로고
    • Crystallization behaviour of poly(L-lactide)
    • DOI: 10.1016/S0032-3861(97)10203-8
    • Miyata T., Masuko T.: Crystallization behaviour of poly(L-lactide). Polymer, 39, 5515-5521 (1998). DOI: 10.1016/S0032-3861(97)10203-8
    • (1998) Polymer , vol.39 , pp. 5515-5521
    • Miyata, T.1    Masuko, T.2
  • 6
    • 0029215899 scopus 로고
    • Physical aging of polymers
    • DOI: 10.1016/0079-6700(94)00001-I
    • Hutchinson J. M.: Physical aging of polymers. Progress in Polymer Science, 20, 703-760 (1995). DOI: 10.1016/0079-6700(94)00001-I
    • (1995) Progress in Polymer Science , vol.20 , pp. 703-760
    • Hutchinson, J.M.1
  • 7
    • 0017471117 scopus 로고
    • Physical aging in plastics and other glassy materials
    • DOI: 10.1002/pen.760170305
    • Strum L. C. E.: Physical aging in plastics and other glassy materials. Polymer Engineering and Science, 17, 165-173 (1977). DOI: 10.1002/pen.760170305
    • (1977) Polymer Engineering and Science , vol.17 , pp. 165-173
    • Strum, L.C.E.1
  • 8
    • 42649126355 scopus 로고    scopus 로고
    • Polylactide compositions. The influence of ageing on the structure, thermal and viscoelastic properties of PLA/calcium sulfate composites
    • DOI: 10.1016/j.polymdegradstab.2008.02.001
    • Pluta M., Murariu M., Alexandre M., Galeski A., Dubois P.: Polylactide compositions. The influence of ageing on the structure, thermal and viscoelastic properties of PLA/calcium sulfate composites. Polymer Degradation and Stability, 93, 925-931 (2008). DOI: 10.1016/j.polymdegradstab.2008.02.001
    • (2008) Polymer Degradation and Stability , vol.93 , pp. 925-931
    • Pluta, M.1    Murariu, M.2    Alexandre, M.3    Galeski, A.4    Dubois, P.5
  • 9
    • 42249085608 scopus 로고    scopus 로고
    • Thermal degradation and physical aging of poly(lactic acid) and its blends with starch
    • DOI: 10.1002/pen.21019
    • Acioli-Moura R., Sun X. S.: Thermal degradation and physical aging of poly(lactic acid) and its blends with starch. Polymer Engineering and Science, 48, 829-836 (2008). DOI: 10.1002/pen.21019
    • (2008) Polymer Engineering and Science , vol.48 , pp. 829-836
    • Acioli-Moura, R.1    Sun, X.S.2
  • 10
    • 35748946659 scopus 로고    scopus 로고
    • Roles of conformational and configurational defects on the physical aging of amorphous poly(lactic acid)
    • DOI: 10.1021/jp074509t
    • Aou K., Hsu S. L., Kleiner L. W., Tang F-W.: Roles of conformational and configurational defects on the physical aging of amorphous poly(lactic acid). Journal of Physical Chemistry B, 111, 12322-12327 (2007). DOI: 10.1021/jp074509t
    • (2007) Journal of Physical Chemistry B , vol.111 , pp. 12322-12327
    • Aou, K.1    Hsu, S.L.2    Kleiner, L.W.3    Tang, F.-W.4
  • 11
    • 38349122132 scopus 로고    scopus 로고
    • Enthalpy relaxation and embrittlement of poly(L-lactide) during physical aging
    • DOI: 10.1021/ma071737c
    • Pan P. J., Zhu B., Inoue Y.: Enthalpy relaxation and embrittlement of poly(L-lactide) during physical aging. Macromolecules, 40, 9664-9671 (2007). DOI: 10.1021/ma071737c
    • (2007) Macromolecules , vol.40 , pp. 9664-9671
    • Pan, P.J.1    Zhu, B.2    Inoue, Y.3
  • 12
    • 0031599028 scopus 로고    scopus 로고
    • Using the essential work of fracture method for studying physical aging in thin, ductile, polymeric films
    • DOI: 10.1002/pen.10179
    • Liu C-H., Nairn J. A.: Using the essential work of fracture method for studying physical aging in thin, ductile, polymeric films. Polymer Engineering and Science, 38, 186-193 (1998). DOI: 10.1002/pen.10179
    • (1998) Polymer Engineering and Science , vol.38 , pp. 186-193
    • Liu, C.-H.1    Nairn, J.A.2
  • 13
    • 0042882323 scopus 로고    scopus 로고
    • Plane stress fracture toughness of physically aged plasticized PETG as assessed by the essential work of fracture (EWF) method
    • DOI: 10.1016/S0032-3861(03)00590-1
    • Karger-Kocsis J., Bárány T., Moskala E. J.: Plane stress fracture toughness of physically aged plasticized PETG as assessed by the essential work of fracture (EWF) method. Polymer, 44, 5691-5699 (2003). DOI: 10.1016/S0032-3861(03)00590-1
    • (2003) Polymer , vol.44 , pp. 5691-5699
    • Karger-Kocsis, J.1    Bárány, T.2    Moskala, E.J.3
  • 14
    • 1842575872 scopus 로고    scopus 로고
    • Physical aging and time-temperature behavior concerning fracture performance of polycarbonate
    • DOI: 10.1016/j.tafmec.2003.11.008
    • Ho C. H., Vu-Khanh T.: Physical aging and time-temperature behavior concerning fracture performance of polycarbonate. Theoretical and Applied Fracture Mechanics, 41, 103-114 (2004). DOI: 10.1016/j.tafmec.2003.11.008
    • (2004) Theoretical and Applied Fracture Mechanics , vol.41 , pp. 103-114
    • Ho, C.H.1    Vu-Khanh, T.2
  • 15
    • 29144526727 scopus 로고    scopus 로고
    • In-plane and out-of-plane fracture toughness of physically aged polyesters as assessed by the essential work of fracture (EWF) method
    • DOI: 10.1007/s10704-005-3947-2
    • Bárány T., Ronkay F., Karger-Kocsis J., Czigány T.: In-plane and out-of-plane fracture toughness of physically aged polyesters as assessed by the essential work of fracture (EWF) method. International Journal of Fracture, 135, 251-265 (2005). DOI: 10.1007/s10704-005-3947-2
    • (2005) International Journal of Fracture , vol.135 , pp. 251-265
    • Bárány, T.1    Ronkay, F.2    Karger-Kocsis, J.3    Czigány, T.4
  • 16
    • 47249137162 scopus 로고    scopus 로고
    • Effect of thermal and hygrothermal aging on the plane stress fracture toughness of poly(ethylene terephthalate) sheets
    • DOI: 10.3144/expresspolymlett.2007.28
    • Bárány T., Földes E., Czigány T.: Effect of thermal and hygrothermal aging on the plane stress fracture toughness of poly(ethylene terephthalate) sheets. Express Polymer Letters, 1, 180-187 (2007). DOI: 10.3144/expresspolymlett.2007.28
    • (2007) Express Polymer Letters , vol.1 , pp. 180-187
    • Bárány, T.1    Földes, E.2    Czigány, T.3
  • 17
    • 84865187789 scopus 로고    scopus 로고
    • NatureWorks® PLA Polymer 2002D - Data Sheet
    • NatureWorks® PLA Polymer 2002D - Data Sheet (2005).
    • (2005)
  • 18
    • 84865166387 scopus 로고    scopus 로고
    • NatureWorks® PLA Polymer 4032D - Data Sheet
    • NatureWorks® PLA Polymer 4032D - Data Sheet (2006).
    • (2006)
  • 19
    • 35348962571 scopus 로고    scopus 로고
    • Effect of nucleation and plasticization on the crystallization of poly(lactic acid)
    • DOI: 10.1016/j.polymer.2007.09.020
    • Li H., Huneault M. A.: Effect of nucleation and plasticization on the crystallization of poly(lactic acid). Polymer, 48, 6855-6866 (2007). DOI: 10.1016/j.polymer.2007.09.020
    • (2007) Polymer , vol.48 , pp. 6855-6866
    • Li, H.1    Huneault, M.A.2
  • 20
    • 67249164465 scopus 로고    scopus 로고
    • Effect of plasticizer on the crystallization behavior of poly(lactic acid)
    • DOI: 10.1002/app.29955
    • Xiao H. W., Lu W., Yeh J-T.: Effect of plasticizer on the crystallization behavior of poly(lactic acid). Journal of Applied Polymer Science, 113, 112-121 (2009). DOI: 10.1002/app.29955
    • (2009) Journal of Applied Polymer Science , vol.113 , pp. 112-121
    • Xiao, H.W.1    Lu, W.2    Yeh, J.-T.3
  • 21
    • 73449084396 scopus 로고    scopus 로고
    • Processing of poly(lactic acid): Characterization of chemical structure, thermal stability and mechanical properties
    • DOI: 10.1016/j.polymdegradstab.2009.11.045
    • Carrasco F., Pagès P., Gámez-Pérez J., Santana O. O., Maspoch M. L.: Processing of poly(lactic acid): Characterization of chemical structure, thermal stability and mechanical properties. Polymer Degradation and Stability, 95, 116-125 (2010). DOI: 10.1016/j.polymdegradstab.2009.11.045
    • (2010) Polymer Degradation and Stability , vol.95 , pp. 116-125
    • Carrasco, F.1    Pagès, P.2    Gámez-Pérez, J.3    Santana, O.O.4    Maspoch, M.L.5
  • 22
    • 77957030526 scopus 로고    scopus 로고
    • Essential Work of Fracture
    • (eds.: Moore D. R., Williams J. G., Pavan A.), DOI: 10.1016/S1566-1369(01)80033-9
    • Clutton E.: Essential work of fracture. in 'Fracture mechanics testing methods for polymers, adhesives and composites' (eds.: Moore D. R., Williams J. G., Pavan A.) Vol 28, 177-195 (2001). DOI: 10.1016/S1566-1369(01)80033-9
    • (2001) Fracture Mechanics Testing Methods For Polymers, Adhesives and Composite , vol.28 , pp. 177-195
    • Clutton, E.1
  • 23
    • 43649107926 scopus 로고    scopus 로고
    • Structural interpretations of deformation and fracture behavior of polypropylene/multi-walled carbon nanotube composites
    • DOI: 10.1016/j.actamat.2008.01.010
    • Ganß M., Satapathy B. K., Thunga M., Weidisch R., Pötschke P., Jehnichen D.: Structural interpretations of deformation and fracture behavior of polypropylene/multi-walled carbon nanotube composites. Acta Materialia, 56, 2247-2261 (2008). DOI: 10.1016/j.actamat.2008.01.010
    • (2008) Acta Materialia , vol.56 , pp. 2247-2261
    • Ganß, M.1    Satapathy, B.K.2    Thunga, M.3    Weidisch, R.4    Pötschke, P.5    Jehnichen, D.6
  • 24
    • 17444419326 scopus 로고    scopus 로고
    • Determination of essential work of fracture in EPBC sheets obtained by different transformation processes
    • DOI: 10.1007/s10853-005-1218-2
    • Gámez-Pérez J., Muñoz P., Velasco J. I., Martínez A. B., Maspoch M. L.: Determination of essential work of fracture in EPBC sheets obtained by different transformation processes. Journal of Material Science, 40, 1967-1974 (2005). DOI: 10.1007/s10853-005-1218-2
    • (2005) Journal of Material Science , vol.40 , pp. 1967-1974
    • Gámez-Pérez, J.1    Muñoz, P.2    Velasco, J.I.3    Martínez, A.B.4    Maspoch, M.L.5
  • 25
    • 0042009404 scopus 로고    scopus 로고
    • On tearing of ductile polymer films using the essential work of fracture (EWF) method
    • DOI: 10.1016/S1359-6454(03)00335-5
    • Wong J. S. S., Ferrer-Balas D., Li R. K. Y., Mai Y-W., Maspoch M. L., Sue H-J.: On tearing of ductile polymer films using the essential work of fracture (EWF) method. Acta Materialia, 51, 4929-4938 (2003). DOI: 10.1016/S1359-6454(03)00335-5
    • (2003) Acta Materialia , vol.51 , pp. 4929-4938
    • Wong, J.S.S.1    Ferrer-Balas, D.2    Li, R.K.Y.3    Mai, Y.-W.4    Maspoch, M.L.5    Sue, H.-J.6
  • 26
    • 69249240143 scopus 로고    scopus 로고
    • The essential work of fracture (EWF) method - Analyzing the post-yielding fracture mechanics of polymers
    • DOI: 10.1016/j.engfailanal.2009.04.027
    • Martínez A. B., Gámez-Pérez J., Sanchez-Soto M., Velasco J. I., Santana O. O., Maspoch M. L.: The essential work of fracture (EWF) method - Analyzing the post-yielding fracture mechanics of polymers. Engineering Failure Analysis, 16, 2604-2617 (2009). DOI: 10.1016/j.engfailanal.2009.04.027
    • (2009) Engineering Failure Analysis , vol.16 , pp. 2604-2617
    • Martínez, A.B.1    Gámez-Pérez, J.2    Sanchez-Soto, M.3    Velasco, J.I.4    Santana, O.O.5    Maspoch, M.L.6
  • 27
    • 77957578098 scopus 로고    scopus 로고
    • Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: A review
    • DOI: 10.1016/j.progpolymsci.2010.07.001
    • Bárány T., Czigány T., Karger-Kocsis J.: Application of the essential work of fracture (EWF) concept for polymers, related blends and composites: A review. Progress in Polymer Science, 35, 1257-1287 (2010). DOI: 10.1016/j.progpolymsci.2010.07.001
    • (2010) Progress in Polymer Science , vol.35 , pp. 1257-1287
    • Bárány, T.1    Czigány, T.2    Karger-Kocsis, J.3
  • 28
    • 43049172138 scopus 로고    scopus 로고
    • Use of extensometers on essential work of fracture (EWF) tests
    • DOI: 10.1016/j.polymertesting.2008.02.002
    • Gámez-Pérez J., Santana O., Martinez A. B., Maspoch M. L.: Use of extensometers on essential work of fracture (EWF) tests. Polymer Testing, 27, 491-497 (2008). DOI: 10.1016/j.polymertesting.2008.02.002
    • (2008) Polymer Testing , vol.27 , pp. 491-497
    • Gámez-Pérez, J.1    Santana, O.2    Martinez, A.B.3    Maspoch, M.L.4
  • 29
    • 0742323430 scopus 로고    scopus 로고
    • Effects of storage time on properties of soybean protein-based plastics
    • DOI: 10.1023/A:1023831411521
    • Mo X. Q., Sun X. Z.: Effects of storage time on properties of soybean protein-based plastics. Journal of Polymers and the Environment, 11, 15-22 (2003). DOI: 10.1023/A:1023831411521
    • (2003) Journal of Polymers and The Environment , vol.11 , pp. 15-22
    • Mo, X.Q.1    Sun, X.Z.2
  • 30
    • 0020162443 scopus 로고
    • Physical ageing in glassy polymers. An i.r. spectroscopic investigation of poly (ethylene terephthalate)
    • DOI: 10.1016/0032-3861(82)90366-4
    • Aref-Azar A., Hay J. N.: Physical ageing in glassy polymers. An i.r. spectroscopic investigation of poly (ethylene terephthalate). Polymer, 23, 1129-1132 (1982). DOI: 10.1016/0032-3861(82)90366-4
    • (1982) Polymer , vol.23 , pp. 1129-1132
    • Aref-Azar, A.1    Hay, J.N.2
  • 31
    • 0032048910 scopus 로고    scopus 로고
    • Physical aging in poly(vinyl acetate). 2. Relative rates of volume and enthalpy relaxation
    • DOI: 10.1021/ma970287t
    • Cowie J. M. G., Harris S., McEwen I. J.: Physical aging in poly(vinyl acetate). 2. Relative rates of volume and enthalpy relaxation. Macromolecules, 31, 2611-2615 (1998). DOI: 10.1021/ma970287t
    • (1998) Macromolecules , vol.31 , pp. 2611-2615
    • Cowie, J.M.G.1    Harris, S.2    McEwen, I.J.3
  • 32
    • 0030282248 scopus 로고    scopus 로고
    • Crystallization kinetics of poly(L-lactide- co-meso-lactide)
    • DOI: 10.1002/(SICI)1097-4628(19961114)62:7<1079::AID-APP14>3.0.CO;2-1
    • Kolstad J. J.: Crystallization kinetics of poly(L-lactide- co-meso-lactide). Journal of Applied Polymer Science, 62, 1079-1091 (1996). DOI: 10.1002/(SICI)1097-4628(19961114)62:7<1079::AID-APP14>3.0.CO;2-1
    • (1996) Journal of Applied Polymer Science , vol.62 , pp. 1079-1091
    • Kolstad, J.J.1
  • 33
    • 28844477499 scopus 로고    scopus 로고
    • Influence of low-temperature nucleation on the crystallization process of poly(L-lactide)
    • DOI: 10.1021/bm050323t
    • Hernández Sánchez F., Molina Mateo J., Romero Colomer F. J., Salmerón Sánchez M., Gómez Ribelles J. L., Mano J. F.: Influence of low-temperature nucleation on the crystallization process of poly(L-lactide). Biomacromolecules, 6, 3283-3290 (2005). DOI: 10.1021/bm050323t
    • (2005) Biomacromolecules , vol.6 , pp. 3283-3290
    • Hernández, S.F.1    Molina, M.J.2    Romero, C.F.J.3    Salmerón, S.M.4    Gómez, R.J.L.5    Mano, J.F.6
  • 34
    • 17744400702 scopus 로고    scopus 로고
    • On the kinetics of melting and crystallization of poly(L-lactic acid) by TMDSC
    • DOI: 10.1016/j.tca.2005.01.066
    • Salmerón Sánchez M., Gómez Ribelles J. L., Hernández Sánchez F., Mano J. F.: On the kinetics of melting and crystallization of poly(L-lactic acid) by TMDSC. Thermochimica Acta, 430, 201-210 (2005). DOI: 10.1016/j.tca.2005.01.066
    • (2005) Thermochimica Acta , vol.430 , pp. 201-210
    • Salmerón, S.M.1    Gómez, R.J.L.2    Hernández, S.F.3    Mano, J.F.4
  • 35
    • 0011786536 scopus 로고
    • Investigation of structure of solution grown crystals of lactide copolymers by means of chemical-reactions
    • DOI: 10.1007/BF01498927
    • Fischer E. W., Sterzel H. J., Wegner G.: Investigation of structure of solution grown crystals of lactide copolymers by means of chemical-reactions. Colloid and Polymer Science, 251, 980-990 (1973). DOI: 10.1007/BF01498927
    • (1973) Colloid and Polymer Science , vol.251 , pp. 980-990
    • Fischer, E.W.1    Sterzel, H.J.2    Wegner, G.3
  • 37
    • 0030567019 scopus 로고    scopus 로고
    • Effect of molecular weight and crystallinity on poly(lactic acid) mechanical properties
    • DOI: 10.1002/(SICI)1097-4628(19960103)59:1<37::AID-APP6>3.0.CO;2-N
    • Perego G., Cella G. D., Bastioli C.: Effect of molecular weight and crystallinity on poly(lactic acid) mechanical properties. Journal of Applied Polymer Science, 59, 37-43 (1996). DOI: 10.1002/(SICI)1097-4628(19960103)59:1<37::AID-APP6>3.0.CO;2-N
    • (1996) Journal of Applied Polymer Science , vol.59 , pp. 37-43
    • Perego, G.1    Cella, G.D.2    Bastioli, C.3
  • 38
    • 78650075746 scopus 로고    scopus 로고
    • Effect of the recycling and annealing on the mechanical and fracture properties of poly(lactic acid)
    • DOI: 10.1007/s10924-010-0229-5
    • Nascimento L., Gámez-Pérez J., Santana O. O., Velasco J. I., Maspoch M. L.: Effect of the recycling and annealing on the mechanical and fracture properties of poly(lactic acid). Journal of Polymers and the Environment, 18, 654-660 (2010). DOI: 10.1007/s10924-010-0229-5
    • (2010) Journal of Polymers and The Environment , vol.18 , pp. 654-660
    • Nascimento, L.1    Gámez-Pérez, J.2    Santana, O.O.3    Velasco, J.I.4    Maspoch, M.L.5
  • 39
    • 0442294242 scopus 로고    scopus 로고
    • Effect of annealing on the fracture toughness of poly(lactic acid)
    • DOI: 10.1023/B:JMSC.0000012957.02434.1e
    • Park S-D., Todo M., Arakawa K.: Effect of annealing on the fracture toughness of poly(lactic acid). Journal of Materials Science, 39, 1113-1116 (2004). DOI: 10.1023/B:JMSC.0000012957.02434.1e
    • (2004) Journal of Materials Science , vol.39 , pp. 1113-1116
    • Park, S.-D.1    Todo, M.2    Arakawa, K.3
  • 41
    • 0023366524 scopus 로고
    • The essential work of plane-stress ductile fracture of linear polyethylenes
    • DOI: 10.1002/pen.760271106
    • Mai Y-W., Cotterell B., Horlyck R., Vigna G.: The essential work of plane-stress ductile fracture of linear polyethylenes. Polymer Engineering and Science, 27, 804-809 (1987). DOI: 10.1002/pen.760271106
    • (1987) Polymer Engineering and Science , vol.27 , pp. 804-809
    • Mai, Y.-W.1    Cotterell, B.2    Horlyck, R.3    Vigna, G.4
  • 42
    • 1942523907 scopus 로고    scopus 로고
    • Fracture behaviour of polyethylene naphthalate (PEN)
    • DOI: 10.1016/S0032-3861(01)00623-1
    • Arkhireyeva A., Hashemi S.: Fracture behaviour of polyethylene naphthalate (PEN). Polymer, 43, 289-300 (2002). DOI: 10.1016/S0032-3861(01)00623-1
    • (2002) Polymer , vol.43 , pp. 289-300
    • Arkhireyeva, A.1    Hashemi, S.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.