메뉴 건너뛰기




Volumn 12, Issue 4, 2010, Pages 332-340

Effect of polyethylene terephthalate (PET) on the pyrolysis of brominated flame retardant-containing high-impact polystyrene (HIPS-Br)

Author keywords

Dioxins; e waste plastics; Flame retardant; HIPS Br; PET

Indexed keywords


EID: 78649701883     PISSN: 14384957     EISSN: 1436378X     Source Type: Journal    
DOI: 10.1007/s10163-010-0306-9     Document Type: Article
Times cited : (13)

References (12)
  • 1
    • 0034677043 scopus 로고    scopus 로고
    • New pathways in plastic recycling and current status of plastics recycling
    • Kaminsky W, Hartmann F (2000) New pathways in plastic recycling and current status of plastics recycling. Angew Chem Int Ed 39: 331-333.
    • (2000) Angew Chem Int Ed , vol.39 , pp. 331-333
    • Kaminsky, W.1    Hartmann, F.2
  • 2
    • 4043172950 scopus 로고    scopus 로고
    • Flame retardants: current trends in North America
    • Innes J, Innes A (2001) Flame retardants: current trends in North America. Plast Addit Comp 3(4): 22-26.
    • (2001) Plast Addit Comp , vol.3 , Issue.4 , pp. 22-26
    • Innes, J.1    Innes, A.2
  • 3
    • 0008946368 scopus 로고    scopus 로고
    • Mounting concern over brominated flame retardants
    • Kellyn SB (2001) Mounting concern over brominated flame retardants. Environ Sci Technol 35(13): 274A-275A.
    • (2001) Environ Sci Technol , vol.35 , Issue.13
    • Kellyn, S.B.1
  • 4
    • 0032182648 scopus 로고    scopus 로고
    • Mechanisms of thermal degradation of a polyester flame-retarded with antimony oxide/brominated polycarbonate studied by temperatureprogrammed analytical pyrolysis
    • Sato H, Kondo K, Tsuge S, Ohtani H, Sato N (1998) Mechanisms of thermal degradation of a polyester flame-retarded with antimony oxide/brominated polycarbonate studied by temperatureprogrammed analytical pyrolysis. Polym Degrad Stabil 62(1): 41.
    • (1998) Polym Degrad Stabil , vol.62 , Issue.1 , pp. 41
    • Sato, H.1    Kondo, K.2    Tsuge, S.3    Ohtani, H.4    Sato, N.5
  • 5
    • 0031069519 scopus 로고    scopus 로고
    • Recycling halogen-containing plastics
    • Kaufer H, von Quast O (1997) Recycling halogen-containing plastics. Kunststoffe 87(2): 190.
    • (1997) Kunststoffe , vol.87 , Issue.2 , pp. 190
    • Kaufer, H.1    von Quast, O.2
  • 6
    • 4043102629 scopus 로고    scopus 로고
    • Pyrolysis studies of PP/PE/PS/PVC/HIPS-Br plastics mixed with PET and dehalogenation (Br, Cl) of the liquid products
    • Bhaskar T, Kaneko J, Muto A, Sakata Y, Jakab E, Matsui T, Uddin MA (2004) Pyrolysis studies of PP/PE/PS/PVC/HIPS-Br plastics mixed with PET and dehalogenation (Br, Cl) of the liquid products. J Anal Appl Pyrolysis 72: 27-33.
    • (2004) J Anal Appl Pyrolysis , vol.72 , pp. 27-33
    • Bhaskar, T.1    Kaneko, J.2    Muto, A.3    Sakata, Y.4    Jakab, E.5    Matsui, T.6    Uddin, M.A.7
  • 7
    • 1842842247 scopus 로고    scopus 로고
    • Effect of poly(ethylene terephthalate) on the pyrolysis of brominated flame retardant containing high impact polystyrene and catalytic debromination of the liquid products
    • Bhaskar T, Kaneko J, Muto A, Sakata Y, Jakab E, Matsui T, Uddin MA (2004) Effect of poly(ethylene terephthalate) on the pyrolysis of brominated flame retardant containing high impact polystyrene and catalytic debromination of the liquid products. J Anal Appl Pyrolysis 71: 765-777.
    • (2004) J Anal Appl Pyrolysis , vol.71 , pp. 765-777
    • Bhaskar, T.1    Kaneko, J.2    Muto, A.3    Sakata, Y.4    Jakab, E.5    Matsui, T.6    Uddin, M.A.7
  • 9
    • 0030197040 scopus 로고    scopus 로고
    • Thermal degradation of polyethylene mixed with poly(vinyl chloride) and poly(ethyleneterephthalate)
    • Sakata Y, Uddin MA, Koizumi K, Murata K (1996) Thermal degradation of polyethylene mixed with poly(vinyl chloride) and poly(ethyleneterephthalate). Polym Degrad Stabil 53(1): 111-117.
    • (1996) Polym Degrad Stabil , vol.53 , Issue.1 , pp. 111-117
    • Sakata, Y.1    Uddin, M.A.2    Koizumi, K.3    Murata, K.4
  • 10
    • 0037810263 scopus 로고    scopus 로고
    • Thermal decomposition of flame-retarded high-impact polystyrene
    • Jakab E, Uddin MA, Bhaskar T, Sakata Y (2003) Thermal decomposition of flame-retarded high-impact polystyrene. J Anal Appl Pyrolysis 68-69: 83-99.
    • (2003) J Anal Appl Pyrolysis , vol.68-69 , pp. 83-99
    • Jakab, E.1    Uddin, M.A.2    Bhaskar, T.3    Sakata, Y.4
  • 11
    • 0037860957 scopus 로고    scopus 로고
    • 3 in brominated heating impact polystyrene (HIPSBr) on thermal degradation and debromination by iron oxide carbon composite catalyst (Fe-C)
    • 3 in brominated heating impact polystyrene (HIPSBr) on thermal degradation and debromination by iron oxide carbon composite catalyst (Fe-C). App Catal B Env 43: 229-241.
    • (2003) App Catal B Env , vol.43 , pp. 229-241
    • Bhaskar, T.1    Matsui, T.2    Uddin, M.A.3    Kaneko, J.4    Muto, A.5    Sakata, Y.6
  • 12
    • 0036784230 scopus 로고    scopus 로고
    • Basic study on a continuous flow reactor for thermal degradation of polymers
    • Murata K, Hirano Y, Sakata Y, Uddin MA (2002) Basic study on a continuous flow reactor for thermal degradation of polymers. J Anal Appl Pyrolysis 65: 71-90.
    • (2002) J Anal Appl Pyrolysis , vol.65 , pp. 71-90
    • Murata, K.1    Hirano, Y.2    Sakata, Y.3    Uddin, M.A.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.