메뉴 건너뛰기




Volumn 31, Issue 3, 2011, Pages 361-368

Reactive infiltration processing (RIP) of ultra high temperature ceramics (UHTC) into porous C/C composite tubes

Author keywords

Ablation resistance; C C composites; Carbothermal reaction; Reactive infiltration processing; Sol gel; Vacuum infiltration; ZrB2

Indexed keywords

ABLATION RESISTANCE; C/C COMPOSITES; CARBOTHERMAL REACTION; REACTIVE INFILTRATION PROCESSING; VACUUM INFILTRATION; ZRB2;

EID: 78649475638     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jeurceramsoc.2010.10.013     Document Type: Article
Times cited : (110)

References (29)
  • 1
    • 14644400504 scopus 로고    scopus 로고
    • Aerothermodynamic study of UHTC-based thermal protection systems
    • Savino R. Aerothermodynamic study of UHTC-based thermal protection systems. Aerospace Science and Technology 2005, 9(2):151-160.
    • (2005) Aerospace Science and Technology , vol.9 , Issue.2 , pp. 151-160
    • Savino, R.1
  • 3
    • 38849190778 scopus 로고    scopus 로고
    • Research progress on thermal protection materials and structures of hypersonic vehicles
    • Yang Y., Yang J., Fang D. Research progress on thermal protection materials and structures of hypersonic vehicles. Applied Mathematics and Mechanics 2008, 29(1):51-60.
    • (2008) Applied Mathematics and Mechanics , vol.29 , Issue.1 , pp. 51-60
    • Yang, Y.1    Yang, J.2    Fang, D.3
  • 4
    • 4444246959 scopus 로고    scopus 로고
    • Thermophysical properties of carbon/carbon composites and physical mechanism of thermal expansion and thermal conductivity
    • Luo R.Y., Liu T., Li J.S., Zhang H.B., Chen Z.J., Tian G.L. Thermophysical properties of carbon/carbon composites and physical mechanism of thermal expansion and thermal conductivity. Carbon 2004, 42(14):2887-2895.
    • (2004) Carbon , vol.42 , Issue.14 , pp. 2887-2895
    • Luo, R.Y.1    Liu, T.2    Li, J.S.3    Zhang, H.B.4    Chen, Z.J.5    Tian, G.L.6
  • 5
    • 0029236041 scopus 로고
    • Oxidation and ablation of 3D carbon-carbon composite at up to 3000°C
    • Han J.C., He X.D., Du S.Y. Oxidation and ablation of 3D carbon-carbon composite at up to 3000°C. Carbon 1995, 33(4):473-478.
    • (1995) Carbon , vol.33 , Issue.4 , pp. 473-478
    • Han, J.C.1    He, X.D.2    Du, S.Y.3
  • 6
    • 0023209365 scopus 로고
    • The future of carbon-carbon composites
    • Fitzer E. The future of carbon-carbon composites. Carbon 1987, 25(2):163-190.
    • (1987) Carbon , vol.25 , Issue.2 , pp. 163-190
    • Fitzer, E.1
  • 7
    • 84985072251 scopus 로고
    • C/C composite materials for aircraft brakes
    • Awasthi E., Wood J.L. C/C composite materials for aircraft brakes. Advanced Ceramic Materials 1987, 3(5):449-451.
    • (1987) Advanced Ceramic Materials , vol.3 , Issue.5 , pp. 449-451
    • Awasthi, E.1    Wood, J.L.2
  • 8
    • 0141460534 scopus 로고    scopus 로고
    • Influence of fibre-matrix interface on the fracture behaviour of carbon-carbon composites
    • Blanco C., Casal E., Granda M., Menéndez R. Influence of fibre-matrix interface on the fracture behaviour of carbon-carbon composites. Journal of the European Ceramic Society 2003, 23(15):2857-2866.
    • (2003) Journal of the European Ceramic Society , vol.23 , Issue.15 , pp. 2857-2866
    • Blanco, C.1    Casal, E.2    Granda, M.3    Menéndez, R.4
  • 9
    • 0242335758 scopus 로고    scopus 로고
    • Studies on the mechanical and mechanical interfacial properties of carbon-carbon composites impregnated with an oxidation inhibitor
    • Park S.J., Seo M.K., Lee D.R. Studies on the mechanical and mechanical interfacial properties of carbon-carbon composites impregnated with an oxidation inhibitor. Carbon 2003, 41(15):2991-3002.
    • (2003) Carbon , vol.41 , Issue.15 , pp. 2991-3002
    • Park, S.J.1    Seo, M.K.2    Lee, D.R.3
  • 10
    • 0033676306 scopus 로고    scopus 로고
    • Effect of additives on mechanical properties of oxidation-resistant carbon/carbon composite fabricated by rapid CVD method
    • Luo R.Y., Yang Z., Li L.F. Effect of additives on mechanical properties of oxidation-resistant carbon/carbon composite fabricated by rapid CVD method. Carbon 2000, 38(15):2109-2115.
    • (2000) Carbon , vol.38 , Issue.15 , pp. 2109-2115
    • Luo, R.Y.1    Yang, Z.2    Li, L.F.3
  • 11
    • 0041578504 scopus 로고    scopus 로고
    • Improvement in properties and air oxidation resistance of carbon materials by boron oxide impregnation
    • Sogabe T., Okada O., Kuroda K., Inagaki M. Improvement in properties and air oxidation resistance of carbon materials by boron oxide impregnation. Carbon 1997, 35(1):67-72.
    • (1997) Carbon , vol.35 , Issue.1 , pp. 67-72
    • Sogabe, T.1    Okada, O.2    Kuroda, K.3    Inagaki, M.4
  • 12
    • 84963784490 scopus 로고
    • Thermogravimetric study of oxidation of ZrB2 in temperature range of 800°C to 1500°C
    • Tripp W.C., Graham H.C. Thermogravimetric study of oxidation of ZrB2 in temperature range of 800°C to 1500°C. Journal of the Electrochemical Society 1971, 118(7):1195.
    • (1971) Journal of the Electrochemical Society , vol.118 , Issue.7 , pp. 1195
    • Tripp, W.C.1    Graham, H.C.2
  • 13
    • 43349085320 scopus 로고    scopus 로고
    • Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites
    • Corral E.L., Loehman R.E. Ultra-high-temperature ceramic coatings for oxidation protection of carbon-carbon composites. Journal of the American Ceramic Society 2008, 91(5):1495-1502.
    • (2008) Journal of the American Ceramic Society , vol.91 , Issue.5 , pp. 1495-1502
    • Corral, E.L.1    Loehman, R.E.2
  • 14
    • 76049100313 scopus 로고    scopus 로고
    • UHTCs: ultra-high temperature ceramic materials for extreme environment applications
    • Wuchina E., Opila E., Fahrenholtz W.G., Talmy I.G. UHTCs: ultra-high temperature ceramic materials for extreme environment applications. Interface 2007, 16(4):30-36.
    • (2007) Interface , vol.16 , Issue.4 , pp. 30-36
    • Wuchina, E.1    Opila, E.2    Fahrenholtz, W.G.3    Talmy, I.G.4
  • 15
    • 0034772319 scopus 로고    scopus 로고
    • Zirconium diboride-based composites
    • PART
    • Monteverde F., Fabbriche D.D., Bellosi A. Zirconium diboride-based composites. Euro Ceramics 2002, Vii(Pt 1-3):961-964.
    • (2002) Euro Ceramics , vol.7 , Issue.1-3 , pp. 961-964
    • Monteverde, F.1    Fabbriche, D.D.2    Bellosi, A.3
  • 17
    • 42149116375 scopus 로고    scopus 로고
    • Processing and properties of ultra-high temperature ceramics for space applications
    • Monteverde F. Processing and properties of ultra-high temperature ceramics for space applications. Materials Science & Engineering. A. Structural Materials 2008, 485(1-2):415-421.
    • (2008) Materials Science & Engineering. A. Structural Materials , vol.485 , Issue.1-2 , pp. 415-421
    • Monteverde, F.1
  • 19
    • 0008595696 scopus 로고
    • High-temperature coatings on carbon fibers and carbon-carbon composites
    • William Andrew Inc., Norwich, J.D. Buckley, D.D. Edie (Eds.)
    • Sheehan J.E. High-temperature coatings on carbon fibers and carbon-carbon composites. Carbon-carbon materials and composites 1993, 223-266. William Andrew Inc., Norwich. J.D. Buckley, D.D. Edie (Eds.).
    • (1993) Carbon-carbon materials and composites , pp. 223-266
    • Sheehan, J.E.1
  • 20
    • 0025839415 scopus 로고
    • ZrPt3 as a high-temperature, reflective, oxidation-resistant coating for carbon-carbon composites
    • Alvey M.D., George P.M. ZrPt3 as a high-temperature, reflective, oxidation-resistant coating for carbon-carbon composites. Carbon 1991, 29(415):523-530.
    • (1991) Carbon , vol.29 , Issue.415 , pp. 523-530
    • Alvey, M.D.1    George, P.M.2
  • 21
    • 33845279447 scopus 로고
    • Titanium, zirconium, and hafnium tetrahydroborates as "tailored" CVD precursors for metal diboride thin films
    • Jensen J.A., Gozum J.E., Pollina D.M., Girolami G.S. Titanium, zirconium, and hafnium tetrahydroborates as "tailored" CVD precursors for metal diboride thin films. Journal of the American Ceramic Society 1988, 110(5):1643-1644.
    • (1988) Journal of the American Ceramic Society , vol.110 , Issue.5 , pp. 1643-1644
    • Jensen, J.A.1    Gozum, J.E.2    Pollina, D.M.3    Girolami, G.S.4
  • 22
    • 33750251481 scopus 로고    scopus 로고
    • New route to synthesize ultra-fine zirconium diboride powders using inorganic-organic hybrid precursors
    • Yongjie Y., Zhengren H., Shaoming D., Dongliang J. New route to synthesize ultra-fine zirconium diboride powders using inorganic-organic hybrid precursors. Journal of the American Ceramic Society 2006, 89(11):3585-3588.
    • (2006) Journal of the American Ceramic Society , vol.89 , Issue.11 , pp. 3585-3588
    • Yongjie, Y.1    Zhengren, H.2    Shaoming, D.3    Dongliang, J.4
  • 23
    • 0023274584 scopus 로고
    • Oxidation behavior and protection of carbon-carbon composites
    • McKee D.W. Oxidation behavior and protection of carbon-carbon composites. Carbon 1987, 25(4):551-557.
    • (1987) Carbon , vol.25 , Issue.4 , pp. 551-557
    • McKee, D.W.1
  • 24
    • 13644259330 scopus 로고    scopus 로고
    • Silicon carbide coatings to protect carbon/carbon composites against oxidation
    • Fu Q.G., Li H.J., Shi X.H., Li K.Z., Sun G.D. Silicon carbide coatings to protect carbon/carbon composites against oxidation. Scripta Materialia 2005, 52(9):923-927.
    • (2005) Scripta Materialia , vol.52 , Issue.9 , pp. 923-927
    • Fu, Q.G.1    Li, H.J.2    Shi, X.H.3    Li, K.Z.4    Sun, G.D.5
  • 26
    • 0029229063 scopus 로고
    • Synthesis and characterization of boron-doped carbons
    • Cermignani W., Paulson T., Onneby C. Synthesis and characterization of boron-doped carbons. Carbon 1995, 33(4):367-374.
    • (1995) Carbon , vol.33 , Issue.4 , pp. 367-374
    • Cermignani, W.1    Paulson, T.2    Onneby, C.3
  • 27
    • 75749104062 scopus 로고    scopus 로고
    • Microstructural development of a Cf/ZrC composite manufactured by reactive melt infiltration
    • Zou L., Wali N., Yang J.-M., Bansal N.P. Microstructural development of a Cf/ZrC composite manufactured by reactive melt infiltration. Journal of the European Ceramic Society 2008, 30(6):1527-1535.
    • (2008) Journal of the European Ceramic Society , vol.30 , Issue.6 , pp. 1527-1535
    • Zou, L.1    Wali, N.2    Yang, J.-M.3    Bansal, N.P.4
  • 28
    • 0032099679 scopus 로고    scopus 로고
    • Evolution of in-situ refractories in the 20th century
    • Lee W.E., Moore R.E. Evolution of in-situ refractories in the 20th century. Journal of the American Ceramic Society 1998, 81(6):1385-1410.
    • (1998) Journal of the American Ceramic Society , vol.81 , Issue.6 , pp. 1385-1410
    • Lee, W.E.1    Moore, R.E.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.