Volumn 509, Issue 2, 2011, Pages 486-489

An evaluation of Al2O3-ZrO2 composites produced by coprecipitation method

Author keywords

Alumina; Hardness; Mechanical properties; Sintering; Zirconia

Indexed keywords

ALUMINA-ZIRCONIA; ALUMINUM SULFATES; BRIDGING EFFECTS; CHEMICAL ROUTES; COARSE GRAINS; COPRECIPITATION METHOD; FINE EQUIAXED GRAINS; INDENTATION FRACTURE TOUGHNESS; NANO-SIZED POWDER; SEM; TRANSFORMATION TOUGHENING; UNI-AXIAL COMPRESSION; ZIRCONIA PARTICLES;

EID: 78149280370     PISSN: 09258388     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jallcom.2010.09.073     Document Type: Article
Times cited : (44)

References (17)
  • 3
  • 6
    • 43449111179 scopus 로고    scopus 로고
    • 2 composites by optimization of the processing parameters
    • 2 composites by optimization of the processing parameters Scripta Mater. 59 2008 155 158
    • (2008) Scripta Mater. , vol.59 , pp. 155-158
    • Sarraf, H.1    Herbig, R.2    Maryska, M.3
  • 8
    • 3242703878 scopus 로고    scopus 로고
    • Processing of alumina and zirconia nanopowders and compacts
    • Y. Wu, A. Bandyopadhyay, and S. Bose Processing of alumina and zirconia nanopowders and compacts Mater. Sci. Eng. A 380 2004 349 355
    • (2004) Mater. Sci. Eng. A , vol.380 , pp. 349-355
    • Wu, Y.1    Bandyopadhyay, A.2    Bose, S.3
  • 9
    • 84985095063 scopus 로고
    • Crack shape effects for indentation fracture toughness measurements
    • S.M. Smith, and O.R. Scattergood Crack shape effects for indentation fracture toughness measurements J. Am. Ceram. Soc. 75 1992 305 315
    • (1992) J. Am. Ceram. Soc. , vol.75 , pp. 305-315
    • Smith, S.M.1    Scattergood, O.R.2
  • 10
    • 33751229307 scopus 로고    scopus 로고
    • 2 nanocomposite. Part I. Powder synthesis and transformation behavior during fracture
    • 2 nanocomposite. Part I. Powder synthesis and transformation behavior during fracture Composites, Part A 38 2007 124 131
    • (2007) Composites, Part A , vol.38 , pp. 124-131
    • Sarkar, D.1    Adak, S.2    Mitra, N.K.3
  • 14
    • 0242440082 scopus 로고    scopus 로고
    • Fracture toughness of alumina and ZTA ceramics: Microstructural coarsening effects
    • D. Casellas, M.M. Nagl, L. Llanes, and M. Anglada Fracture toughness of alumina and ZTA ceramics: microstructural coarsening effects J. Mater. Process. Technol. 143-144 2003 148 152
    • (2003) J. Mater. Process. Technol. , vol.143-144 , pp. 148-152
    • Casellas, D.1    Nagl, M.M.2    Llanes, L.3    Anglada, M.4
  • 16
    • 0035399519 scopus 로고    scopus 로고
    • 3-TiC composites evaluated by direct indentation method
    • 3-TiC composites evaluated by direct indentation method J. Eur. Ceram. Soc. 21 2001 941 946
    • (2001) J. Eur. Ceram. Soc. , vol.21 , pp. 941-946
    • Gong, J.1    Zhao, Z.2    Guan, Z.3
  • 17
    • 0034030734 scopus 로고    scopus 로고
    • Toughness-curve behavior of alumina-SiC and ZTA-SiC composites
    • H. Toaszewski, M. Boniecki, and H. Weglarz Toughness-curve behavior of alumina-SiC and ZTA-SiC composites J. Eur. Ceram. Soc. 20 2000 1215 1224
    • (2000) J. Eur. Ceram. Soc. , vol.20 , pp. 1215-1224
    • Toaszewski, H.1    Boniecki, M.2    Weglarz, H.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.