Volumn 29, Issue 8, 2010, Pages 984-990

Fracture behaviour of de-aged poly(lactic acid) assessed by essential work of fracture and J-Integral methods

Author keywords

Biodegradable polymer; De ageing; Essential work of fracture; J Integral; Material testing; PLA

Indexed keywords

DE-AGEING; ESSENTIAL WORK OF FRACTURE; J INTEGRAL; MATERIAL TESTING; PLA;

EID: 77957891571     PISSN: 01429418     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.polymertesting.2010.09.004     Document Type: Article
Times cited : (18)

References (23)
  • 1
    • 4744360239 scopus 로고    scopus 로고
    • An overview of polylactides as packaging materials
    • R. Auras, B. Harte, and S. Selke An overview of polylactides as packaging materials Macromol Biosci. 4 9 2004 5515
    • (2004) Macromol Biosci. , vol.4 , Issue.9 , pp. 5515
    • Auras, R.1    Harte, B.2    Selke, S.3
  • 2
    • 33746349311 scopus 로고    scopus 로고
    • Tensile fracture behavior of biodegradable polymer, poly(lactic acid)
    • K. Arakawa, T. Mada, D. S-Park, and M. Todo Tensile fracture behavior of biodegradable polymer, poly(lactic acid) Polym. Test. 25 2006 628
    • (2006) Polym. Test. , vol.25 , pp. 628
    • Arakawa, K.1    Mada, T.2    S-Park, D.3    Todo, M.4
  • 3
    • 78650075746 scopus 로고    scopus 로고
    • Effect of recycling and annealing on the mechanical and fracture properties of poly(lactic acid)
    • Doi:10.1007/s10924-010-0229-5
    • L. Nascimento, J. Gámez-Pérez, O.O. Santana, J.I. Velasco, M. Ll. Maspoch. Effect of recycling and annealing on the mechanical and fracture properties of poly(lactic acid). J Polym Environ. Doi:10.1007/s10924-010-0229-5
    • J Polym Environ.
    • Nascimento, L.1
  • 4
    • 35748946659 scopus 로고    scopus 로고
    • Roles of conformational and configurational defects on the physical aging of amorphous poly(lactic acid)
    • K. Aou, S.L. Hsu, L.W. Kleiner, and F.-W. Tang Roles of conformational and configurational defects on the physical aging of amorphous poly(lactic acid) J. Phys. Chem. B. 111 42 2007 12322
    • (2007) J. Phys. Chem. B. , vol.111 , Issue.42 , pp. 12322
    • Aou, K.1    Hsu, S.L.2    Kleiner, L.W.3    Tang, F.-W.4
  • 5
    • 0003459370 scopus 로고    scopus 로고
    • R.N. Haward, R.J. Young, second ed. Chapman & Hall
    • R.N. Haward, R.J. Young, The Physics of Glassy Polymers second ed. 1997 Chapman & Hall
    • (1997) The Physics of Glassy Polymers
  • 6
    • 33947572502 scopus 로고    scopus 로고
    • The effect of annealing on deformation and fracture behavior of injection molded PLA
    • J.K. Goto, S. Nakano, and T. Kuriyama The effect of annealing on deformation and fracture behavior of injection molded PLA Strength, Fracture and Complexity 4 2006 185
    • (2006) Strength, Fracture and Complexity , vol.4 , pp. 185
    • Goto, J.K.1    Nakano, S.2    Kuriyama, T.3
  • 7
    • 33749511246 scopus 로고    scopus 로고
    • Modified essential work of fracture model for polymer fracture
    • K. Duan, X. Hu, and G. Stachowiak Modified essential work of fracture model for polymer fracture Comp. Sci. Tech. 66 2006 3172
    • (2006) Comp. Sci. Tech. , vol.66 , pp. 3172
    • Duan, K.1    Hu, X.2    Stachowiak, G.3
  • 9
    • 0030230795 scopus 로고    scopus 로고
    • The essential fracture work concept for toughness measurement of ductile polymers
    • J. Wu, and Y.-W. Mai The essential fracture work concept for toughness measurement of ductile polymers Polym. Eng. Sci. 36 18 1996 2275
    • (1996) Polym. Eng. Sci. , vol.36 , Issue.18 , pp. 2275
    • Wu, J.1    Mai, Y.-W.2
  • 11
    • 0000426729 scopus 로고    scopus 로고
    • Plane strain essential work of fracture in SENB geometry at low and high rates of PC/ABS blends
    • O.O. Santana, M. Ll Maspoch, and A.B. Martínez Plane strain essential work of fracture in SENB geometry at low and high rates of PC/ABS blends Polym. Bull. 39 4 1997 511
    • (1997) Polym. Bull. , vol.39 , Issue.4 , pp. 511
    • Santana, O.O.1    Ll Maspoch, M.2    Martínez, A.B.3
  • 12
    • 0037449646 scopus 로고    scopus 로고
    • The application of the essential work of fracture methodology to the plain strain fracture of ABS 3-point bend specimens
    • P. Luna, C. Bernal, A. Cisilino, P. Frontini, B. Coterell, and Y.-W. Mai The application of the essential work of fracture methodology to the plain strain fracture of ABS 3-point bend specimens Polymer 44 2003 1145
    • (2003) Polymer , vol.44 , pp. 1145
    • Luna, P.1    Bernal, C.2    Cisilino, A.3    Frontini, P.4    Coterell, B.5    Mai, Y.-W.6
  • 13
    • 78249236264 scopus 로고    scopus 로고
    • Natureworks® Natureworks LLC
    • Natureworks® PLA Polymer 2002D. Data Sheet Available form: 2005 Natureworks LLC http://www.natureworksllc.com [accesed 19.07.2010]
    • (2005) PLA Polymer 2002D. Data Sheet
  • 16
    • 38349122132 scopus 로고    scopus 로고
    • Entahlpy relaxation and embrittlement of Poly(L-lactide) during physical aging
    • P. Pan, B. Zhu, and Y. Inoue Entahlpy relaxation and embrittlement of Poly(L-lactide) during physical aging Macromolecules 40 2007 9664
    • (2007) Macromolecules , vol.40 , pp. 9664
    • Pan, P.1    Zhu, B.2    Inoue, Y.3
  • 17
    • 20444421237 scopus 로고    scopus 로고
    • The effect of crystallinity on the deformation mechanism and bulk mechanical properties of PLLA
    • A.C. Renouf-Glauser, J. Rose, D.F. Farrar, and R.E. Cameron The effect of crystallinity on the deformation mechanism and bulk mechanical properties of PLLA Biomaterials 26 2005 5771
    • (2005) Biomaterials , vol.26 , pp. 5771
    • Renouf-Glauser, A.C.1    Rose, J.2    Farrar, D.F.3    Cameron, R.E.4
  • 18
    • 78249245471 scopus 로고    scopus 로고
    • Brittle-ductile transition of quenched PLA
    • (in revision, July)
    • J. Gámez-Pérez, J. Velázquez, E. Franco-Urquiza, P. Pagés, F. Carrasco, O.O. Santana, M. Ll. Maspoch. Brittle-ductile transition of quenched PLA. Express Polymer Letters (in revision, July 2010)
    • (2010) Express Polymer Letters
    • Gámez-Pérez, J.1
  • 20
  • 21
    • 0024016036 scopus 로고
    • Slip-line field solutions for three-point notch-bend specimens
    • S.-X. Wu, B. Cotterell, and Y.-W. Mai Slip-line field solutions for three-point notch-bend specimens Int. J. Fract 37 1988 13
    • (1988) Int. J. Fract , vol.37 , pp. 13
    • Wu, S.-X.1    Cotterell, B.2    Mai, Y.-W.3
  • 22
    • 0025901409 scopus 로고
    • IC for Polymer Using the Single Specimen Method, in Elastic-Plastic Fracture Test Methods
    • American Society for Testing and Materials USA
    • IC for Polymer Using the Single Specimen Method, in Elastic-Plastic Fracture Test Methods ASTM STIP 114 The User's Experience vol. 2 1991 American Society for Testing and Materials USA pp: 320-339
    • (1991) The User's Experience , vol.2
    • Chung, W.N.1    Williams, J.G.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.