Volumn 13, Issue 11, 2010, Pages

Improved performance of all-solid-state lithium-ion batteries using nanosilicon active material with multiwalled-carbon-nanotubes as a conductive additive

Author keywords

[No Author keywords available]

Indexed keywords

ACETYLENE BLACK; ACTIVE MATERIAL; ALL-SOLID-STATE; ANODE MATERIAL; CONDUCTING ADDITIVES; CONDUCTIVE ADDITIVES; LI BATTERIES; LITHIUM-ION BATTERY; MULTI-WALLED; NANO-SILICON; REVERSIBLE CAPACITY; SI NANOPARTICLES; SILICON NANOPARTICLES; SOLID-STATE CONSTRUCTION; SPECIFIC CAPACITIES;

EID: 77956567145     PISSN: 10990062     EISSN: None     Source Type: Journal    
DOI: 10.1149/1.3479551     Document Type: Article
Times cited : (53)

References (32)
  • 4
    • 33644507105 scopus 로고    scopus 로고
    • Electrochemical behaviors of silicon based anode material
    • DOI 10.1016/j.jpowsour.2005.05.052, PII S0378775305007536, Selected Papers Presented at the 2004 Meeting of the International Battery Materials Association
    • M. Yoshio, S. Kugino, and N. Dimov, J. Power Sources JPSODZ 0378-7753, 153, 375 (2006). 10.1016/j.jpowsour.2005.05.052 (Pubitemid 43292482)
    • (2006) Journal of Power Sources , vol.153 , Issue.2 , pp. 375-379
    • Yoshio, M.1    Kugino, S.2    Dimov, N.3
  • 8
    • 33845622840 scopus 로고    scopus 로고
    • Nano- and bulk-silicon-based insertion anodes for lithium-ion secondary cells
    • DOI 10.1016/j.jpowsour.2006.09.084, PII S037877530602026X, Papers presented at the FUEL PROCESSING FOR HYDROGEN PRODUCTION SYMPOSIUM at the 230th American Chemical SocietyNational Meeting
    • U. Kasavajjula, C. Wang, and A. Appleby, J. Power Sources JPSODZ 0378-7753, 163, 1003 (2007). 10.1016/j.jpowsour.2006.09.084 (Pubitemid 44959613)
    • (2007) Journal of Power Sources , vol.163 , Issue.2 , pp. 1003-1039
    • Kasavajjula, U.1    Wang, C.2    Appleby, A.J.3
  • 12
    • 0142094732 scopus 로고    scopus 로고
    • ECCMF9 1388-2481,. 10.1016/j.elecom.2003.09.001
    • X. Wu, Z. Wang, L. Chen, and X. Huang, Electrochem. Commun. ECCMF9 1388-2481, 5, 935 (2003). 10.1016/j.elecom.2003.09.001
    • (2003) Electrochem. Commun. , vol.5 , pp. 935
    • Wu, X.1    Wang, Z.2    Chen, L.3    Huang, X.4
  • 16
    • 34447259040 scopus 로고    scopus 로고
    • 4 composites as anode materials for lithium ion batteries
    • DOI 10.1016/j.ssi.2007.05.011, PII S0167273807001774
    • X. Zhang, G. Pan, G. Li, J. Qu, and X. Gao, Solid State Ionics SSIOD3 0167-2738, 178, 1107 (2007). 10.1016/j.ssi.2007.05.011 (Pubitemid 47042230)
    • (2007) Solid State Ionics , vol.178 , Issue.15-18 , pp. 1107-1112
    • Zhang, X.N.1    Pan, G.L.2    Li, G.R.3    Qu, J.Q.4    Gao, X.P.5
  • 18
    • 34247247277 scopus 로고    scopus 로고
    • Preparation and characterization of silicon-based three-dimensional cellular anode for lithium ion battery
    • DOI 10.1016/j.elecom.2006.11.031, PII S1388248106005558
    • T. Jiang, S. Zhang, Z. Qiu, W. Zhu, and L. Chen, Electrochem. Commun. ECCMF9 1388-2481, 9, 930 (2007). 10.1016/j.elecom.2006.11.031 (Pubitemid 46617377)
    • (2007) Electrochemistry Communications , vol.9 , Issue.5 , pp. 930-934
    • Jiang, T.1    Zhang, S.2    Qiu, X.3    Zhu, W.4    Chen, L.5
  • 19
    • 65549123737 scopus 로고    scopus 로고
    • ELCAAV 0013-4686,. 10.1016/j.electacta.2009.03.055
    • X. Wang, Z. Wen, Y. Liu, and X. Wu, Electrochim. Acta ELCAAV 0013-4686, 54, 4662 (2009). 10.1016/j.electacta.2009.03.055
    • (2009) Electrochim. Acta , vol.54 , pp. 4662
    • Wang, X.1    Wen, Z.2    Liu, Y.3    Wu, X.4
  • 23
    • 48349107867 scopus 로고    scopus 로고
    • SSIOD3 0167-2738,. 10.1016/j.ssi.2008.01.095
    • P. Bruce, Solid State Ionics SSIOD3 0167-2738, 179, 752 (2008). 10.1016/j.ssi.2008.01.095
    • (2008) Solid State Ionics , vol.179 , pp. 752
    • Bruce, P.1
  • 24
    • 0037465265 scopus 로고    scopus 로고
    • ACMAFD 1359-6454,. 10.1016/S1359-6454(02)00514-1
    • P. Limthongkul, Y. Jang, N. Dudney, and Y. Chiang, Acta Mater. ACMAFD 1359-6454, 51, 1103 (2003). 10.1016/S1359-6454(02)00514-1
    • (2003) Acta Mater. , vol.51 , pp. 1103
    • Limthongkul, P.1    Jang, Y.2    Dudney, N.3    Chiang, Y.4
  • 25
    • 49749108228 scopus 로고    scopus 로고
    • JALCEU 0925-8388,. 10.1016/j.jallcom.2007.09.088
    • X. Yang, Z. Wen, L. Zhang, and M. You, J. Alloys Compd. JALCEU 0925-8388, 464, 265 (2008). 10.1016/j.jallcom.2007.09.088
    • (2008) J. Alloys Compd. , vol.464 , pp. 265
    • Yang, X.1    Wen, Z.2    Zhang, L.3    You, M.4
  • 26
  • 29
    • 0035871256 scopus 로고    scopus 로고
    • JAPIAU 0021-8979,. 10.1063/1.1356437
    • M. H. Yu, R. S. Ruoff, and M. J. Dyer, J. Appl. Phys. JAPIAU 0021-8979, 89, 4554 (2001). 10.1063/1.1356437
    • (2001) J. Appl. Phys. , vol.89 , pp. 4554
    • Yu, M.H.1    Ruoff, R.S.2    Dyer, M.J.3
  • 31
    • 33846996042 scopus 로고    scopus 로고
    • JESOAN 0013-4651,. 10.1149/1.2409862
    • J. Li and J. R. Dahn, J. Electrochem. Soc. JESOAN 0013-4651, 154, A156 (2007). 10.1149/1.2409862
    • (2007) J. Electrochem. Soc. , vol.154 , pp. 156
    • Li, J.1    Dahn, J.R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.