1
-
-
77956496033
-
-
Patent EP 90 06-206
-
Fruchart D., Miraglia S., Mollard P., and Perrier de la Bâthie R., To Make Anisotropic Nd-Fe-B Powder using Waste Sintered Nd-Fe-B Magnets by Hydrogen Decrepitation, Desorption, and Subsequent Annealing Treatment, Patent EP 90 06-206, 1990.
-
(1990)
To Make Anisotropic Nd-Fe-B Powder Using Waste Sintered Nd-Fe-B Magnets by Hydrogen Decrepitation, Desorption, and Subsequent Annealing Treatment
-
-
Fruchart, D.1
-
2
-
-
0031131063
-
Hydrogen in hard magnetic materials
-
10.1016/S0925-8388(96)03063-0
-
D. Fruchart M. Bacmann P. De Rango O. Isnard S. Liesert S. Miraglia S. Obbade J.-L. Soubeyroux E. Tomey P. Wolfers 1997 Hydrogen in hard magnetic materials J. Alloys Compd. 253-254 1 121 10.1016/S0925-8388(96)03063-0
-
(1997)
J. Alloys Compd.
, vol.253-254
, Issue.1
, pp. 121
-
-
Fruchart, D.1
Bacmann, M.2
De Rango, P.3
Isnard, O.4
Liesert, S.5
Miraglia, S.6
Obbade, S.7
Soubeyroux, J.-L.8
Tomey, E.9
Wolfers, P.10
-
4
-
-
37349031473
-
Possible methods of recycling NdFeB-type sintered magnets using the HD/degassing process
-
DOI 10.1016/j.jallcom.2007.01.134, PII S0925838807003386
-
M. Zakotnik I.R. Harris A.J. Williams 2008 Possible methods of recycling NdFeB-type sintered magnets using the HD/degassing process J. Alloys Compd. 450 1-2 525 1:CAS:528:DC%2BD1cXltFGj 10.1016/j.jallcom.2007.01.134 (Pubitemid 350298816)
-
(2008)
Journal of Alloys and Compounds
, vol.450
, Issue.1-2
, pp. 525-531
-
-
Zakotnik, M.1
Harris, I.R.2
Williams, A.J.3
-
5
-
-
0024069845
-
14B (RE=Y, Nd, Ho, Tm)
-
1:CAS:528:DyaL1MXhslCmtw%3D%3D 10.1016/0022-5088(88)90176-2
-
14B (RE=Y, Nd, Ho, Tm) J. Less Common Met. 142 187 1:CAS:528:DyaL1MXhslCmtw%3D%3D 10.1016/0022-5088(88)90176-2
-
(1988)
J. Less Common Met.
, vol.142
, pp. 187
-
-
Pareti, L.1
Moze, O.2
Fruchart, D.3
L'Heritier, Ph.4
Yaouanc, A.5
-
6
-
-
33748291698
-
Improved magnetic properties and fracture strength of NdFeB by dehydrogenation
-
DOI 10.1016/j.jmmm.2006.02.240, PII S0304885306005865
-
M. Yan L.Q. Yu J.M. Wu X.G. Cui 2006 Improved magnetic properties and fracture strength of NdFeB by dehydrogenation J. Magn. Magn. Mater. 306 2 176 1:CAS:528:DC%2BD28Xpt1yhsLw%3D 10.1016/j.jmmm.2006.02.240 2006JMMM..306..176Y (Pubitemid 44331501)
-
(2006)
Journal of Magnetism and Magnetic Materials
, vol.306
, Issue.2
, pp. 176-180
-
-
Yan, M.1
Yu, L.Q.2
Wu, J.M.3
Cui, X.G.4
-
7
-
-
4444261173
-
Anisotropic and coercive Nd-Fe-B powder for bonded magnets
-
Sendai
-
Rivoirard S., Noudem J.G., De Rango P., Fruchart D., Liesert S., and Soubeyroux J.L., Anisotropic and coercive Nd-Fe-B powder for bonded magnets, [in] Proceedings of the 16th International Workshop on Rare-Earth Magnets and Their Applications, Sendai, 2000: 347.
-
(2000)
Proceedings of the 16th International Workshop on Rare-Earth Magnets and Their Applications
, pp. 347
-
-
Rivoirard, S.1
Noudem, J.G.2
De Rango, P.3
Fruchart, D.4
Liesert, S.5
Soubeyroux, J.L.6
-
8
-
-
0000162427
-
5-H system by strong magnetic fields
-
1:CAS:528:DyaL1MXhtVaks78%3D 10.1016/0375-9601(89)90695-6 1989PhLA.134.504Y
-
5-H system by strong magnetic fields Phys. Lett. A 134 8-9 504 1:CAS:528:DyaL1MXhtVaks78%3D 10.1016/0375-9601(89)90695-6 1989PhLA..134..504Y
-
(1989)
Phys. Lett. A
, vol.134
, Issue.89
, pp. 504
-
-
Yamaguchi, M.1
Yamamoto, I.2
Goto, T.3
Miura, S.4
-
9
-
-
0029752889
-
Magnetic field effects on the chemical equilibrium between metals and hydrogen
-
DOI 10.1016/0921-4526(95)00527-7
-
I. Yamamoto M. Yamaguchi M. Fujino F. Ishikawa T. Goto S. Miura 1996 Magnetic field effects on the chemical equilibrium between metals and hydrogen Phys. B 216 3-4 399 1:CAS:528:DyaK28XjtVCqsg%3D%3D 10.1016/0921-4526(95)00527-7 1996PhyB..216..399Y (Pubitemid 126366937)
-
(1996)
Physica B: Condensed Matter
, vol.216
, Issue.3-4
, pp. 399-402
-
-
Yamamoto, I.1
Yamaguchi, M.2
Fujino, M.3
Ishikawa, F.4
Goto, T.5
Miura, S.6
-
13
-
-
0028439485
-
Anisotropic hydrogen decrepitation and corrosion behaviour in NdFeB magnets
-
1:CAS:528:DyaK2cXlt1emtr0%3D 10.1016/0925-8388(94)90023-X
-
P.J. McGuiness L. Fitzpatrick V.A. Yartys I.R. Harris 1994 Anisotropic hydrogen decrepitation and corrosion behaviour in NdFeB magnets J. Alloys Compd. 206 2 L7 1:CAS:528:DyaK2cXlt1emtr0%3D 10.1016/0925-8388(94)90023-X
-
(1994)
J. Alloys Compd.
, vol.206
, Issue.2
, pp. 7
-
-
McGuiness, P.J.1
Fitzpatrick, L.2
Yartys, V.A.3
Harris, I.R.4
-
15
-
-
7544236275
-
Hydrogen location in hard magnet materials: Scheme, fundamental aspects, processes
-
1:CAS:528:DC%2BD2cXptFOrtrk%3D 10.1016/j.jallcom.2004.04.068
-
D. Fruchart S. Miraglia P. De Rango P. Wolfers 2004 Hydrogen location in hard magnet materials: scheme, fundamental aspects, processes J. Alloys Compd. 383 17 1:CAS:528:DC%2BD2cXptFOrtrk%3D 10.1016/j.jallcom.2004.04.068
-
(2004)
J. Alloys Compd.
, vol.383
, pp. 17
-
-
Fruchart, D.1
Miraglia, S.2
De Rango, P.3
Wolfers, P.4
-
17
-
-
20344371158
-
Preparation of NdFeB anisotropic alloys by ribbon crystallization under high magnetic field
-
Annecy
-
Rivoirard S., Givord D., Barthem V.M.T.S., Beaugnon E., and De miranda P.E.V., Preparation of NdFeB anisotropic alloys by ribbon crystallization under high magnetic field, [in] Proceeding of the 18th International Workshop on High Performance Magnets and their Applications (HPMA04), Annecy, 2004: 250.
-
(2004)
Proceeding of the 18th International Workshop on High Performance Magnets and Their Applications (HPMA04)
, pp. 250
-
-
Rivoirard, S.1
Givord, D.2
Barthem, V.M.T.S.3
Beaugnon, E.4
De Miranda, P.E.V.5
|