메뉴 건너뛰기




Volumn 55, Issue 3, 2010, Pages 360-368

Molecular structure and fracture properties of ZrOX/Epoxysilane hybrid films

Author keywords

Adhesion; Fracture; FTIR; Hybrid materials; Thin film

Indexed keywords

3-GLYCIDOXYPROPYLTRIMETHOXYSILANE; AFM; COHESIVE FRACTURE; CRITICAL STRAIN ENERGY; FILM COMPOSITION; FILM STRUCTURE; FRACTURE PROPERTY; FRACTURE RESISTANCE; FRACTURE SURFACES; FTIR; HYBRID FILM; HYBRID SOL-GEL FILMS; MECHANICAL RELIABILITY; SILANE-CROSSLINKING; SUBSTRATE CHEMISTRY; SUBSTRATE COMPOSITION; XPS;

EID: 77956484500     PISSN: 09280707     EISSN: None     Source Type: Journal    
DOI: 10.1007/s10971-010-2262-1     Document Type: Article
Times cited : (34)

References (49)
  • 5
    • 37449008579 scopus 로고    scopus 로고
    • Fabrication and properties of an asymmetric waveguide containing nanoparticles
    • DOI 10.1007/s11664-007-0324-0
    • JL Zhang TF Kuech 2008 J Electron Mater 37 135 10.1007/s11664-007-0324-0 2008JEMat..37..135Z (Pubitemid 50000725)
    • (2008) Journal of Electronic Materials , vol.37 , Issue.2 , pp. 135-144
    • Zhang, J.L.1    Kuech, T.F.2
  • 9
    • 77956469599 scopus 로고    scopus 로고
    • US Pat. (2000) 6077885
    • US Pat. (2000) 6077885
  • 10
    • 77956482037 scopus 로고    scopus 로고
    • US Pat. (1998) 5 814 137
    • US Pat. (1998) 5 814 137
  • 11
    • 77956460805 scopus 로고    scopus 로고
    • US Pat. (1998) 5 849 110
    • US Pat. (1998) 5 849 110
  • 12
    • 77956473691 scopus 로고    scopus 로고
    • US Pat. (1999) 5 939 197
    • US Pat. (1999) 5 939 197
  • 13
    • 77956456871 scopus 로고    scopus 로고
    • US Pat. (1999) 5 958 578
    • US Pat. (1999) 5 958 578
  • 14
    • 77956480531 scopus 로고    scopus 로고
    • US Pat. (2000) 6 037 060
    • US Pat. (2000) 6 037 060
  • 17
    • 0035304601 scopus 로고    scopus 로고
    • Nanoscale mechanical degradation of titanium/PETI-5 adhesive interface due to thermal exposure
    • DOI 10.1023/A:1017524709046
    • J Holbery R Fisher 2001 J Mater Sci 36 1747 10.1023/A:1017524709046 (Pubitemid 32471613)
    • (2001) Journal of Materials Science , vol.36 , Issue.7 , pp. 1747-1753
    • Holbery, J.D.1    Fisher, R.M.2
  • 27
    • 34247582320 scopus 로고    scopus 로고
    • Anomalous debonding behavior of a polymer/inorganic interface
    • DOI 10.1016/j.actamat.2007.02.012, PII S1359645407001474
    • BM Sharratt LC Wang RH Dauskardt 2007 Acta Mater 55 3601 10.1016/j.actamat.2007.02.012 (Pubitemid 46670073)
    • (2007) Acta Materialia , vol.55 , Issue.10 , pp. 3601-3609
    • Sharratt, B.M.1    Wang, L.C.2    Dauskardt, R.H.3
  • 29
    • 0036470469 scopus 로고    scopus 로고
    • Moisture-assisted subcritical debonding of a polymer/metal interface
    • DOI 10.1063/1.1427139
    • SY Kook RH Dauskardt 2002 J Appl Phys 91 1293 10.1063/1.1427139 2002JAP....91.1293K (Pubitemid 34148792)
    • (2002) Journal of Applied Physics , vol.91 , Issue.3 , pp. 1293
    • Kook, S.-Y.1    Dauskardt, R.H.2
  • 30
    • 0036888549 scopus 로고    scopus 로고
    • The structural transformation and properties of spin-on poly(silsesquioxane) films by thermal curing
    • DOI 10.1016/S0022-3093(02)01373-X, PII S002230930201373X
    • WC Liu CC Yang WC Chen BT Dai MS Tsai 2002 J Non-Cryst Solids 311 233 10.1016/S0022-3093(02)01373-X 2002JNCS..311..233L (Pubitemid 35282376)
    • (2002) Journal of Non-Crystalline Solids , vol.311 , Issue.3 , pp. 233-240
    • Liu, W.-C.1    Yang, C.-C.2    Chen, W.-C.3    Dai, B.-T.4    Tsai, M.-S.5
  • 32
    • 33847314546 scopus 로고    scopus 로고
    • Inorganic-organic interpenetrating polymer networks involving polyhedral oligomeric silsesquioxane and poly(ethylene oxide)
    • DOI 10.1016/j.polymer.2007.01.007, PII S0032386107000420
    • JF Mu YH Liu SX Zheng 2007 Polymer 48 1176 10.1016/j.polymer.2007.01.007 (Pubitemid 46329033)
    • (2007) Polymer , vol.48 , Issue.5 , pp. 1176-1184
    • Mu, J.1    Liu, Y.2    Zheng, S.3
  • 35
    • 0035949920 scopus 로고    scopus 로고
    • Cyclization and self-organization in polymerization of trialkoxysilanes
    • DOI 10.1021/ma010136x
    • L Matejka O Dukh D Hlavata B Meissner J Brus 2001 Macromolecules 34 6904 10.1021/ma010136x 2001MaMol..34.6904M (Pubitemid 34217033)
    • (2001) Macromolecules , vol.34 , Issue.20 , pp. 6904-6914
    • Matejka, L.1    Dukh, O.2    Hlavata, D.3    Meissner, B.4    Brus, J.5
  • 39
    • 0033985443 scopus 로고    scopus 로고
    • Polymeric silsesquioxanes: Degree-of-intramolecular-condensation measured by mass spectrometry
    • DOI 10.1016/S0032-3861(99)00386-9, PII S0032386199003869
    • WE Wallace CM Guttman JM Antonucci 2000 Polymer 41 2219 10.1016/S0032-3861(99)00386-9 (Pubitemid 30025584)
    • (2000) Polymer , vol.41 , Issue.6 , pp. 2219-2226
    • Wallace, W.E.1    Guttman, C.M.2    Antonucci, J.M.3
  • 41
    • 28444439612 scopus 로고    scopus 로고
    • FTIR studies on selected mesoporous metallosilicate molecular sieves
    • DOI 10.1246/cl.2005.1290, CL-050835
    • M Selvaraj BH Kim TG Lee 2005 Chem Lett 34 1290 10.1246/cl.2005.1290 (Pubitemid 41737915)
    • (2005) Chemistry Letters , vol.34 , Issue.9 , pp. 1290-1291
    • Selvaraj, M.1    Byong, H.K.2    Tai, G.L.3
  • 48
    • 0022077979 scopus 로고
    • 10.1016/0022-3093(86)90107-9 1986JNCS.82.31P
    • G Philipp H Schmidt 1986 J Non-Cryst Solids 82 31 10.1016/0022-3093(86) 90107-9 1986JNCS...82...31P
    • (1986) J Non-Cryst Solids , vol.82 , pp. 31
    • Philipp, G.1    Schmidt, H.2
  • 49
    • 0035425895 scopus 로고    scopus 로고
    • On the influence of metal alkoxides on the epoxide ring-opening and condensation reactions of 3-glycidoxypropyltrimethoxysilane
    • DOI 10.1023/A:1011274301896
    • D Hoebbel M Nacken H Schmidt 2001 J Sol-Gel Sci Technol 21 177 10.1023/A:1011274301896 (Pubitemid 32690618)
    • (2001) Journal of Sol-Gel Science and Technology , vol.21 , Issue.3 , pp. 177-187
    • Hoebbel, D.1    Nacken, M.2    Schmidt, H.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.