Volumn 86, Issue 7, 2010, Pages 726-741

The morphology and fracture properties of thermoplastic-toughened epoxy polymers

Author keywords

Epoxy; Fracture toughness; Morphology; Thermoplastic

Indexed keywords

0.2% PROOF STRESS; CONTINUOUS PHASE; END-GROUPS; EPOXY; EPOXY POLYMERS; FRACTURE PERFORMANCE; FRACTURE PROPERTY; LOW CONCENTRATIONS; PARTICULATE MORPHOLOGY; POLY(ETHER SULFONE); SPHERICAL PARTICLE; THERMOPLASTIC CONTENT; ULTIMATE TENSILE STRENGTH; WEIGHT PERCENTAGES; YOUNG'S MODULUS;