The interaction of Zr2Fe surface with O2 and H 2O at the temperature range 300-770 K

Author keywords

Degradation; Getter; Oxidation; Oxygen; Water vapor

Indexed keywords

ALLOY SURFACES; DEGRADATION AGENTS; HIGHER TEMPERATURES; HYDROXYL GROUPS; INITIAL STICKING COEFFICIENT; INWARD DIFFUSION; OPERATING TEMPERATURE; OXIDATION MECHANISMS; OXIDE LAYER; OXIDE THICKNESS; OXYGEN ATOM; OXYGEN DISSOLUTION; OXYGEN PRESSURE; PRESSURE DEPENDENT; TEMPERATURE RANGE; XPS;