Volumn 38, Issue 3, 2010, Pages 253-257

Wear mechanism for in situ tiC particle reinforced AZ91 magnesium matrix composites

Author keywords

Microstructure; Spray deposition; TiC AZ91 Mg composites; Wear mechanism

Indexed keywords

APPLIED LOADS; AZ91 MAGNESIUM; AZ91 MAGNESIUM ALLOYS; DRY SLIDING WEAR; HIGHER LOADS; IN-SITU; IN-SITU REACTIONS; MATRIX ALLOY; NORMAL LOADS; OXIDATIVE MECHANISM; PIN-ON-DISC MACHINE; SEM; SPRAY DEPOSITION; SPRAY-DEPOSITED; TIC PARTICLES; TIC/AZ91 MG COMPOSITES; WEAR BEHAVIORS; WEAR MECHANISMS; WEAR RATES;

EID: 77953684779     PISSN: 10238883     EISSN: None     Source Type: Journal    
DOI: 10.1007/s11249-010-9600-x     Document Type: Article
Times cited : (20)

References (15)
  • 1
    • 0031084106 scopus 로고    scopus 로고
    • Superplasticity of a AIN/Mg-5wt%Al alloy composite made by a vortex method
    • 10.1016/S1359-6462(96)00429-0 1:CAS:528:DyaK2sXhtlehtLo%3D
    • T Imai SW Lim D Jiang, et al. 1997 Superplasticity of a AIN/Mg-5wt%Al alloy composite made by a vortex method Scr. Mater. 36 611 616 10.1016/S1359-6462(96)00429-0 1:CAS:528:DyaK2sXhtlehtLo%3D.
    • (1997) Scr. Mater. , vol.36 , pp. 611-616
    • Imai, T.1    Lim, S.W.2    Jiang, D.3
  • 2
    • 34249294198 scopus 로고    scopus 로고
    • Chemistry Industry Press, Beijing, (in Chinese)
    • Chen, Z.H., Yan, H.G., Chen, J.H. et al.: Magnesium Alloys [M], p. 57. Chemistry Industry Press, Beijing (2004) (in Chinese)
    • (2004) Magnesium Alloys [M] , pp. 57
    • Chen, Z.H.1    Yan, H.G.2    Chen, J.H.3
  • 3
    • 0037350646 scopus 로고    scopus 로고
    • Fabrication of TiC particulate reinforced magnesium matrix composites
    • 10.1016/S1359-6462(02)00551-1 1:CAS:528:DC%2BD3sXmtVansg%3D%3D
    • QC Jiang XL Li HY Wang 2003 Fabrication of TiC particulate reinforced magnesium matrix composites Scr. Mater. 48 713 717 10.1016/S1359-6462(02)00551-1 1:CAS:528:DC%2BD3sXmtVansg%3D%3D.
    • (2003) Scr. Mater. , vol.48 , pp. 713-717
    • Jiang, Q.C.1    Li, X.L.2    Wang, H.Y.3
  • 4
    • 0029323614 scopus 로고
    • High strain rate superplasticity of TiC particulate reinforced magnesium alloy composite by vortex method
    • 10.1016/0956-716X(95)91591-C
    • SW Lim T Imai Y Nishida, et al. 1995 High strain rate superplasticity of TiC particulate reinforced magnesium alloy composite by vortex method Scr. Mater. 32 713 719 10.1016/0956-716X(95)91591-C.
    • (1995) Scr. Mater. , vol.32 , pp. 713-719
    • Lim, S.W.1    Imai, T.2    Nishida, Y.3
  • 6
    • 0037291550 scopus 로고    scopus 로고
    • The effect of a dilution agent on the dipping exothermic reaction process for fabricating a high-volume TiC-reinforced aluminum composite
    • 10.1016/S1359-6462(03)00014-9
    • IH Song DK Kim YD Hahn, et al. 2003 The effect of a dilution agent on the dipping exothermic reaction process for fabricating a high-volume TiC-reinforced aluminum composite Scr. Mater. 48 1349 1354 10.1016/S1359- 6462(03)00014-9
    • (2003) Scr. Mater. , vol.48 , pp. 1349-1354
    • Song, I.H.1    Kim, D.K.2    Hahn, Y.D.3
  • 7
    • 17044388249 scopus 로고    scopus 로고
    • Spray forming of AZ91 magnesium alloys with and without Si addition
    • Chen, C.Y., Tsao-Chi, Y.A.: Spray forming of AZ91 magnesium alloys with and without Si addition. J. Mater. Sci. 475/479, 2789-2794 (2005)
    • (2005) J. Mater. Sci. , vol.475-479 , pp. 2789-2794
    • Chen, C.Y.1    Tsao-Chi, Y.A.2
  • 8
    • 1942530627 scopus 로고    scopus 로고
    • Modeling of the solidification of gas-atomized alloy droplets during spray forming
    • DOI 10.1016/j.msea.2003.12.041, PII S0921509304000292
    • DM Liu JZ Zhao HQ Ye 2004 Modeling of the solidification of gas-atomized alloy droplets during spray forming Mater. Sci. Eng. A 372 229 235 10.1016/j.msea.2003.12.041. (Pubitemid 38531669)
    • (2004) Materials Science and Engineering A , vol.372 , Issue.1-2 , pp. 229-234
    • Liu, D.1    Zhao, J.2    Ye, H.3
  • 10
    • 0035826964 scopus 로고    scopus 로고
    • 2-TiC composites with enhanced toughness
    • DOI 10.1016/S1359-6454(01)00034-9, PII S1359645401000349
    • 2-TiC composites with enhanced toughness Acta Mater. 49 1463 1468 10.1016/S1359-6454(01)00034-9 1:CAS:528:DC%2BD3MXisFChtb0%3D. (Pubitemid 32288022)
    • (2001) Acta Materialia , vol.49 , Issue.8 , pp. 1463-1470
    • Wen, G.1    Li, S.B.2    Zhang, B.S.3    Guo, Z.X.4
  • 11
    • 0031169471 scopus 로고    scopus 로고
    • Processing, microstructure and fracture behaviour of a spray atomized and deposited aluminium-silicon alloy
    • 10.1023/A:1018668332318 1:CAS:528:DyaK2sXktVKju7s%3D
    • S Anand TS Srivatsan Y Wu, et al. 1997 Processing, microstructure and fracture behaviour of a spray atomized and deposited aluminium-silicon alloy J. Mater. Sci. 32 2835 2839 10.1023/A:1018668332318 1:CAS:528:DyaK2sXktVKju7s%3D.
    • (1997) J. Mater. Sci. , vol.32 , pp. 2835-2839
    • Anand, S.1    Srivatsan, T.S.2    Wu, Y.3
  • 12
    • 0037413777 scopus 로고    scopus 로고
    • 2 composite by incorporation of carbon
    • DOI 10.1016/S0921-5093(02)00150-8, PII S0921509302001508
    • KL Tee L Lu MO Lai 2003 Improvement in mechanical properties of in-situ Al-TiB2 composite by incorporation of carbon Sci. Mater. Eng. A 339 227 232 10.1016/S0921-5093(02)00150-8. (Pubitemid 36178525)
    • (2003) Materials Science and Engineering A , vol.339 , Issue.1-2 , pp. 227-231
    • Tee, K.L.1    Lu, L.2    Lai, M.O.3
  • 13
    • 0035418565 scopus 로고    scopus 로고
    • Influence of Ti addition on wear properties of Al-Si eutectic alloys
    • DOI 10.1016/S0043-1648(01)00687-1
    • N Saheb T Laoui AR Daud, et al. 2001 Influence of Ti addition on wear properties of Al-Si eutectic alloys Wear 249 656 661 10.1016/S0043-1648(01) 00687-1 1:CAS:528:DC%2BD3MXlsFyqu7s%3D. (Pubitemid 32792222)
    • (2001) Wear , vol.249 , Issue.8 , pp. 656-662
    • Saheb, N.1    Laoui, T.2    Daud, A.R.3    Harun, M.4    Radiman, S.5    Yahaya, R.6
  • 14
    • 0033945333 scopus 로고    scopus 로고
    • Wear of spray deposited Al-6Cu-Mn alloy under dry sliding conditions
    • DOI 10.1016/S0043-1648(00)00354-9, PII S0043164800003549
    • MC Gui BK Suk LJ Moo 2000 Wear of spray deposited Al-6Cu-Mn alloy under dry sliding conditions Wear 240 186 191 10.1016/S0043-1648(00)00354-9 1:CAS:528:DC%2BD3cXjs1antbc%3D. (Pubitemid 30423343)
    • (2000) Wear , vol.240 , Issue.1-2 , pp. 186-198
    • Gui, M.1    Kang, S.B.2    Lee, J.M.3
  • 15
    • 0030081310 scopus 로고    scopus 로고
    • The sliding wear behaviour of Al-SiC particulate composites - II. The characterization of subsurface deformation and correlation with wear behaviour
    • DOI 10.1016/1359-6454(95)00218-9
    • B Venkataraman G Sundararajan 1996 The sliding wear behaviour of Al-SiC particulate composites-II. The characterization of subsurface deformation and correlation with wear behaviour Acta Mater. 44 461 469 10.1016/1359-6454(95) 00218-9 1:CAS:528:DyaK28Xls1Siuw%3D%3D.. (Pubitemid 126341870)
    • (1996) Acta Materialia , vol.44 , Issue.2 , pp. 461-473
    • Venkataraman, B.1    Sundararajan, G.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.